Prior art keywords
parts
production method
plastic barrel
mixture
phenolic resin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510048909.9A
Other languages
English (en)
Inventor
杨斌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chongqing Canton Road Facilities Co Ltd
Original Assignee
Chongqing Canton Road Facilities Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chongqing Canton Road Facilities Co Ltd filed Critical Chongqing Canton Road Facilities Co Ltd
Priority to CN201510048909.9A priority Critical patent/CN105985607A/zh
Publication of CN105985607A publication Critical patent/CN105985607A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Ink Jet (AREA)

Abstract

本发明公开了一种塑料桶生产方法,其特征在于,包括如下步骤,1)按重量份数将酚醛树脂100‑120份,有机硅20‑25份,酚醛树脂150‑125份,增塑剂5‑10份、稳定剂0.5‑2份、润滑剂3‑5份混合;2)将上述混合物高温加热,使其融化,温度为 300℃ ‑330℃;3)将融化后的混合物,放入已做好的模具中,合模,注塑;4)经过冷却后打开模具取出制品,修去毛边即得成品;5)冷却,给制作好的塑料桶进行抛光;6)消毒;7)将消毒后的塑料桶进行激光印染。本发明提高了加工效率、成品率,降低生产成本,取得了本领域技术人员所预料不到的技术效果,并取得了比现有技术更好的加工效果。

Description

塑料桶生产方法
技术领域
本发明属于塑料领域,特别是涉及一种塑料桶生产方法。
背景技术
塑料制品和人们生活息息相关,其中塑料桶又是每家每户都必备的产品,消耗速度也比较快,目前塑料桶生产工艺成品率不高。
发明内容
有鉴于现有技术的上述缺陷,本发明所要解决的技术问题是提供一种塑料桶生产方法,该方法工艺简单,免去了很多重复性工序,提高了工作效率。
为实现上述目的,本发明提供了一种塑料桶生产方法,其特征在于,包括如下步骤,1)按重量份数将酚醛树脂100-120份,有机硅20-25份,酚醛树脂150-125份,增塑剂5-10份、稳定剂0.5-2份、润滑剂3-5份混合;2)将上述混合物高温加热,使其融化,温度为 300℃ -330℃ ;3)将融化后的混合物,放入已做好的模具中,合模,注塑 ;4)经过冷却后打开模具取出制品,修去毛边即得成品;5)冷却,给制作好的塑料桶进行抛光 ;6)消毒 ;7)将消毒后的塑料桶进行激光印染。
本发明的有益效果是:本发明提高了加工效率、成品率,降低生产成本,取得了本领域技术人员所预料不到的技术效果,并取得了比现有技术更好的加工效果。
具体实施方式
本发明的技术方案是一种塑料桶生产方法,包括如下步骤,1)按重量份数将酚醛树脂100-120份,有机硅20-25份,酚醛树脂150-125份,增塑剂5-10份、稳定剂0.5-2份、润滑剂3-5份混合。2)将上述混合物高温加热,使其融化,温度为 300℃ -330℃ ;3)将融化后的混合物,放入已做好的模具中,合模,注塑 ;4)经过冷却后打开模具取出制品,修去毛边即得成品;5)冷却,给制作好的塑料桶进行抛光 ;6)消毒 ;7)将消毒后的塑料桶进行激光印染。
本发明提高了加工效率、成品率,降低生产成本,取得了本领域技术人员所预料不到的技术效果,并取得了比现有技术更好的加工效果。
以上详细描述了本发明的较佳具体实施例。应当理解,本领域的普通技术人员无需创造性劳动就可以根据本发明的构思作出诸多修改和变化。因此,凡本技术领域中技术人员依本发明的构思在现有技术的基础上通过逻辑分析、推理或者有限的实验可以得到的技术方案,皆应在由权利要求书所确定的保护范围内。

Claims (1)

1.一种塑料桶生产方法,其特征在于,包括如下步骤,1)按重量份数将酚醛树脂100-120份,有机硅20-25份,酚醛树脂150-125份,增塑剂5-10份、稳定剂0.5-2份、润滑剂3-5份混合;2)将上述混合物高温加热,使其融化,温度为 300℃ -330℃ ;3)将融化后的混合物,放入已做好的模具中,合模,注塑 ;4)经过冷却后打开模具取出制品,修去毛边即得成品;5)冷却,给制作好的塑料桶进行抛光 ;6)消毒 ;7)将消毒后的塑料桶进行激光印染。
CN201510048909.9A 2015-01-30 2015-01-30 塑料桶生产方法 Pending CN105985607A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201510048909.9A CN105985607A (zh) 2015-01-30 2015-01-30 塑料桶生产方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201510048909.9A CN105985607A (zh) 2015-01-30 2015-01-30 塑料桶生产方法

Publications (1)

Publication Number Publication Date
CN105985607A true CN105985607A (zh) 2016-10-05

Family

ID=57035922

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201510048909.9A Pending CN105985607A (zh) 2015-01-30 2015-01-30 塑料桶生产方法

Country Status (1)

Country Link
CN (1) CN105985607A (zh)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109968631A (zh) * 2019-04-19 2019-07-05 江苏惠源新材料股份有限公司 高硬质尿素桶的生产方法
CN112980132A (zh) * 2021-03-04 2021-06-18 湖北隆泰达塑业有限公司 一种高耐候建筑工程用塑料桶及生产工艺
CN115042357A (zh) * 2022-06-28 2022-09-13 罗小如 一种双色大口缸的制作方法

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109968631A (zh) * 2019-04-19 2019-07-05 江苏惠源新材料股份有限公司 高硬质尿素桶的生产方法
CN112980132A (zh) * 2021-03-04 2021-06-18 湖北隆泰达塑业有限公司 一种高耐候建筑工程用塑料桶及生产工艺
CN115042357A (zh) * 2022-06-28 2022-09-13 罗小如 一种双色大口缸的制作方法

Similar Documents

Publication Publication Date Title
PH12018000089A1 (en) Method of manufacturing a thermoset polymer utility vault lid
CN105985607A (zh) 塑料桶生产方法
CN106435123B (zh) 一种快速压力淬火热处理工装
WO2019104320A8 (en) Tool assembly for manufacturing parts and a method of producing a tooling assembly
CN104960135A (zh) 一种pp塑料注塑工艺
CN102700070B (zh) 一种减少变形均匀冷却细长把手注塑模具及生产工艺
CN110293648B (zh) 谐波减速器用刚轮的制备方法以及谐波减速器
CN206328431U (zh) 一种快速压力淬火热处理工装
CN105478733A (zh) 一种铸件浇冒口的切割方法
CN204263463U (zh) 具有散热针的汽车前门用注塑模具
CN204149390U (zh) 一种自动热切边机
BR112015007043A2 (pt) processo para a produção de núcleos salinos para a produção de peças de trabalho por técnica de fundição
CN106182586A (zh) 全自动镶嵌注塑系统
CN204194471U (zh) 高耐磨性内壁加工装置
CN204222109U (zh) 高成形质量的注塑模具
CN102173028A (zh) 医疗实验室生物细胞筛的制作方法
CN204209909U (zh) 一种注塑模具模内装配的模具结构
CN204566550U (zh) 一种带有内牙零件的热流道模具
CN202540677U (zh) 一种高光注塑设备
CN102107488A (zh) 两次注塑成型生产牙刷刷柄的方法
CN209736557U (zh) 一种合金热电偶专用射蜡机
CN207273776U (zh) 一种注塑模具顶出板调整机构
CN203854147U (zh) 一种注塑剪裁一体机
CN204109257U (zh) 一种模具
CN111055521A (zh) 一种塑料瓶的生产工艺

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20161005

WD01 Invention patent application deemed withdrawn after publication