CN105973471B - A kind of colour atla for automobile appearance repairing and preparation method thereof - Google Patents
A kind of colour atla for automobile appearance repairing and preparation method thereof Download PDFInfo
- Publication number
- CN105973471B CN105973471B CN201610321334.8A CN201610321334A CN105973471B CN 105973471 B CN105973471 B CN 105973471B CN 201610321334 A CN201610321334 A CN 201610321334A CN 105973471 B CN105973471 B CN 105973471B
- Authority
- CN
- China
- Prior art keywords
- colour atla
- ground
- mill base
- preparation
- group
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The invention discloses a kind of colour atla for automobile appearance repairing, including colour atla box and one group of colour atla volume, wherein colour atla box includes box body and lid, one group of dividing plate is provided with box body, the space size of one group of dividing plate composition is adapted with colour atla volume, and lid is L-shaped, and its one end is connected with box body side and can rotated around connecting line, the other end is provided with the first magnetic material, box body it is corresponding be provided with the second magnetic material;Colour atla volume includes one group of color effect colour atla, and ring buckle, and wherein color effect colour atla is provided with the bookbinding hole being adapted with ring buckle shape.Colour atla volume is easy to deposit, taken conveniently;Ring buckle can be opened to take out or add colour atla, adjust colour atla volume according to the actual requirements.
Description
Technical field
The present invention relates to the technical field of colour atla, more particularly to a kind of colour atla for automobile appearance repairing.
Background technology
Colour atla is color existing for nature in certain material(Such as:Paper, fabric, plastic cement etc.)On embodiment, for color
Selection, compare, link up, being that color realizes the instrument sought unity of standard within the specific limits, be the bridge between designer and product,
Use of the every profession and trade to colour atla at present is also more and more.Especially automobile maintenance industry, when grazing occurs in use for automobile, production
Raw cut is caused during cosmetic injury, it is necessary to repair again, can be with now with colour chart comparison color, reference formulation allotment paint
Play a part of quick paint, and color error can be substantially reduced.
At present, existing colour atla, which exists, uses and deposits the problem of inconvenient, bookbinding solidifies, and can not flexibly take, or root
According to being actually needed adjustment colour atla.
The content of the invention
The purpose of invention:The present invention discloses a kind of colour atla for automobile appearance repairing, is easy to take and deposits;User
Method is flexible, can adjust colour atla volume according to the actual requirements.
Technical scheme:In order to realize the above object the invention discloses a kind of colour atla for automobile appearance repairing, including
Colour atla box and one group of colour atla volume, wherein colour atla box include box body and lid, and one group of dividing plate is provided with box body, what one group of dividing plate formed
Space size is adapted with colour atla volume, and lid is L-shaped, and its one end is connected with box body side and can rotated around connecting line,
The other end is provided with the first magnetic material, box body it is corresponding be provided with the second magnetic material;Colour atla volume includes one group of color effect colour atla, with
And ring buckle, wherein color effect colour atla are provided with the bookbinding hole being adapted with ring buckle shape.This design colour atla volume is easy to
Deposit, take conveniently;Ring buckle can be opened to take out or add colour atla, adjust colour atla volume according to the actual requirements.
Further, a kind of above-mentioned colour atla for automobile appearance repairing, the colour atla volume also include one group of transparent effect
Colour atla.A variety of transparent effect colour atlas are added, can be covered on color effect colour atla, are combined into various different-effects, more shape
As, convenient various outward appearances and texture for embodying automobile.
Further, a kind of above-mentioned colour atla for automobile appearance repairing, the ring buckle include the first half-turn and second
Half-turn, wherein first half-turn one end is rotatablely connected with second half-turn one end, the first half-turn other end is provided with buckle, and the second half-turn is another
One end is provided with the neck being adapted with buckle shape.This design structure is simple, and ring buckle can be opened easily with engaging, and
Big opening can be unfolded into, is easy to loading and taking-up that colour atla is stacked.
Further, a kind of above-mentioned colour atla for automobile appearance repairing, the color effect colour atla include art paper, color
Pulp layer, back up layer.This design art paper density is high, and coating is thick, and indeformable after colour atla finished product stress, surface is smooth.
Further, it is above-mentioned it is a kind of for automobile appearance repairing colour atla, the transparent effect colour atla include PVC films and
Transparent color paste layer.This design PVC films transparency is high, the transparent color paste layer of sprayable different-effect, after colour atla finished product stress
Indeformable, surface is smooth.
Further, above-mentioned a kind of colour atla for automobile appearance repairing, the colour atla volume are additionally provided with front cover, back cover, divided
One group of see-through card not being covered on front cover and back cover.See-through card plays a part of protecting colour atla volume.
Further, above-mentioned a kind of colour atla for automobile appearance repairing, on color paste layer and the back up layer respectively
Covered with transparent protective film.This design can protect color paste layer and back up layer, prevent abrasion and color oxidation, wear,
Cause color error and influence to contrast, and there is preferable waterproof action, service life can be improved.
A kind of preparation method of colour atla for automobile appearance repairing provided by the invention, its step include:1)Modulate color
Slurry, by organic or inorganic pigment, dimethylbenzene, butyl acetate, softening agent, levelling agent mixed, allocated;2)Draw a design test, use
The mill base modulated carries out sample making and test, until sample passes;3)Mill base is diluted, it is dilute to mill base progress to add diluent
Release;4)Spraying, the mill base after dilution is added in spray equipment, ground is sprayed;5)Baking, the ground that spraying is finished
Toasted 1 hour under conditions of 70 DEG C;6)Dry, 25 DEG C of constant temperature and humidities of ground that baking finishes are dried 8 hours;7)Cutting,
Ground is cut into sizeable square with hand papercutter;8)Cross cutting, guillotine, the sanction of guillotine are put into by the ground cut
Cut the appearance profile that mould cuts out colour atla on ground.This preparation method simplifies step, disposable spray finishing in place, disposably
Baking in place, is then disposably dried, and improves production efficiency, reduces production cost, while can ensure product quality, and colour atla is put down
It is whole, substantially without warpage, temperature stability is good with humidity stability, and the ability of resistant to bending stresses is strong, also can under rugged environment
Ensure its smooth, few warpage, ensure reliable and available in structure.
Further, a kind of preparation method of above-mentioned colour atla for automobile appearance repairing, the proportioning of the mill base are:Two
Toluene accounts for the 20% of mill base gross weight, and butyl acetate accounts for the 25% of mill base gross weight, and organic or inorganic pigment accounts for mill base gross weight
50%, softening agent accounts for the 3% of mill base gross weight, and levelling agent accounts for the 2% of mill base gross weight.The mill base painting effect of formula modulation is good,
Color is accurate, small with the aberration of standard jig contrast, is easy to spray, stability is good;The coating of finished product is smooth, uniform, coating table
Face without chrysanthemum skin, grow dim, no pinprick.
Further, a kind of preparation method of above-mentioned colour atla for automobile appearance repairing, the spraying process include:a)
One group of steel plate is fixed in circular loop suspended chain;b)Install the ground of respective numbers respectively on one group of steel plate;c)Start
Automatic spray apparatus;d)Circular loop suspended chain starts to rotate, and first ground is moved into spraying area;e)Automatic spraying dress
Put and first ground is sprayed;f)Circular loop suspended chain starts to rotate, and second ground is moved into spraying area, together
When first ground be moved to drying area;g)Automatic spray apparatus sprays to second ground, while constant temperature and humidity
Blowing device carries out skin drying to first ground;h)By that analogy, and continual cycle operation, when ground passes through second
After secondary spraying and skin drying, remove and replace with new ground.This design improves production efficiency, can be achieved continual
Spray coating operations;Its spraying effect is good, can improve product quality, and the coating of finished product is smooth, uniform, coating surface without chrysanthemum skin, grow dim,
Without pinprick.
Above-mentioned technical proposal can be seen that the present invention and have the advantages that:One kind of the present invention is used for automobile
The colour atla of outward appearance repairing, colour atla volume are easy to deposit, taken conveniently;Ring buckle can be opened to take out or add colour atla, according to reality
Demand adjusts colour atla volume;A variety of transparent effect colour atlas are added, can be covered on color effect colour atla, are combined into various differences
Effect, vivider, the convenient various outward appearances and texture for embodying automobile;A kind of automobile appearance that is used for provided by the invention is repaired
Colour atla preparation method, step simplifies, improves production efficiency, reduce production cost, while can ensure product quality;Finished product
Coating uniform, surface is smooth, and the smooth no warpage of colour atla, indeformable after stress;Stability is good, service life length.
Brief description of the drawings
Fig. 1 is a kind of overall structure figure of colour atla for automobile appearance repairing of the present invention;
Fig. 2 is a kind of structure chart of the colour atla volume of colour atla for automobile appearance repairing of the present invention;
Fig. 3 is a kind of side structure of the color effect colour atla of colour atla for automobile appearance repairing of the present invention
Figure;
Fig. 4 is a kind of side structure of the transparent effect colour atla of colour atla for automobile appearance repairing of the present invention
Figure;
In figure:1- colour atla boxes, 2- colour atla volumes, 21- front covers, 22- back covers, 23- see-through cards, 3- box bodys, 31- dividing plates, 32-
Two magnetic materials, 33- labels, 4- lids, 41- the first magnetic materials, 5- color effect colour atlas, 51- art papers, 52- color paste layers, 53-
Back up layer, 54- transparent protective films, 6- ring buckles, the half-turns of 61- first, the half-turns of 62- second, 7- transparent effect colour atlas, 71-
PVC films, the transparent color paste layers of 72-.
Embodiment
Below in conjunction with the accompanying drawings, the specific embodiment of the invention is described in detail.
Embodiment
A kind of colour atla for automobile appearance repairing of the present invention, as shown in Figures 1 to 4, including:Colour atla box 1 and one group
Colour atla volume 2, wherein colour atla box 1 include box body 3 and lid 4, dividing plate 31 are provided with box body 3, dividing plate 31, which includes one, to be had necessarily
The vertical clapboard of width and evenly spaced two horizontal baffles, space size and the colour atla volume 2 of composition are adapted, vertical clapboard
Label 33 is provided with, for the information for the colour atla volume 2 for indicating and indicating to deposit in each space, lid 4 is L-shaped, its one end and box
The side of body 3 is connected and can rotated around connecting line, and the other end is provided with the first magnetic material 41, box body 3 it is corresponding be provided with the
Two magnetic materials 32;Colour atla volume 2 includes one group of color effect colour atla 5 and one group of transparent effect colour atla 7, and ring buckle 6, and it is prized
Color effect colour atla 5 and transparent effect colour atla 7 are equipped with the bookbinding hole being adapted with the shape of ring buckle 6.The ring buckle 6 includes
First half-turn 61 and the second half-turn 62, wherein the one end of the first half-turn 61 is rotatablely connected with the one end of the second half-turn 62, the first half-turn 61
The other end is provided with buckle, and the other end of the second half-turn 62 is provided with the neck being adapted with buckle shape, the first half-turn 61 and the second half
Circle 62 can be unfolded into a larger angle.The color effect colour atla 5 includes art paper 51, color paste layer 52, back side print
Brush layer 53;The back up floor 53 of color effect colour atla 5 is printed on vehicle, color number, Aksu color number, color designation, base coat
Color masterbatch and weight table, the color masterbatch of water paint and weight table, the detailed information for showing each color, are easy to the allotment of user;
Transparent protective film 54 has been covered each by color paste layer 52 and back up layer 53.The transparent effect colour atla 7 includes PVC films 71
With transparent color paste layer 72, wherein transparent color paste layer 72 can also set special-effect, such as pearl effect or flash effect.It is described
Colour atla volume 2 is additionally provided with front cover 21, back cover 22, one group of see-through card 23 being respectively overlay on front cover and back cover.
A kind of preparation method of colour atla for automobile appearance repairing of the present invention, its step include:
1)Modulate the mill base modulator approach of mill base, wherein color effect colour atla 5:By organic or inorganic pigment, dimethylbenzene, second
Acid butyl ester, softening agent, levelling agent are mixed, allocated, and the proportioning of the mill base is:Dimethylbenzene accounts for the 20% of mill base gross weight, second
Acid butyl ester accounts for the 25% of mill base gross weight, and organic or inorganic pigment accounts for the 50% of mill base gross weight, and softening agent accounts for mill base gross weight
3%, levelling agent accounts for the 2% of mill base gross weight;The mill base modulator approach of transparent effect colour atla 7:By transparent mill base or with special effect
The mill base of fruit is added in PVC dedicated transparent varnish, is stirred 5 minutes, then vibrate 5 minutes;
2)Draw a design test, sample making and test are carried out with the mill base modulated, until sample passes;
3)Mill base is diluted, diluent is added and mill base is diluted, the proportioning of mill base and diluent is:Mill base accounts for gross weight
70%, diluent accounts for the 30% of gross weight, and wherein diluent components are with proportioning:N-butyl acetate accounts for diluent gross weight
30%, dimethylbenzene accounts for the 30% of diluent gross weight, and 2-Butoxyethyl acetate accounts for the 40% of diluent gross weight;
4)Spraying, the mill base after dilution is added in spray equipment, ground sprayed, the spraying process includes:
a)One group of steel plate, b are fixed in circular loop suspended chain)Install the ground of respective numbers, c respectively on one group of steel plate)Open
Dynamic automatic spray apparatus, d)Circular loop suspended chain starts to rotate, and first ground is moved into spraying area, e)Automatic spraying
Device sprays to first ground, f)Circular loop suspended chain starts to rotate, and second ground is moved into spraying area,
First ground is moved to drying area, g simultaneously)Automatic spray apparatus sprays to second ground, while constant temperature is permanent
Wet blowing device carries out skin drying, h to first ground)By that analogy, and continual cycle operation, when ground is by the
After secondary spraying and skin drying, remove and replace with new ground;
5)Baking, the ground that spraying finishes is toasted 1 hour under conditions of 70 DEG C;
6)Dry, 25 DEG C of constant temperature and humidities of ground that baking finishes are dried 8 hours;
7)Cutting, sizeable square is cut into hand papercutter by ground;
8)Cross cutting, the ground cut is put into guillotine, the cutting mould of guillotine cuts out the outer of colour atla on ground
Shape profile, guillotine are provided with heater, and it is connected with cutting mould, cut quality to improve, colour atla edge impulse- free robustness is not
Together;
9)Punching, is organized into one group by the colour atla for cutting appearance profile, processes bookbinding hole, complete the system of individual colour atla
Make;
10)Bookbinding, is bound into book form colour atla with ring buckle 6;
11)Colour atla box 1 is made, and colour atla volume 2 is neatly loaded into colour atla box 1, product is completed.
Further, for the making of color effect colour atla 5, need to carry out the printing of back up layer 53 before spraying,
During the spraying of front, back up layer 53 is protected using pallet, and with U.S. line paper all round closure, prevents from being contaminated;After drying also
Pad pasting need to be carried out, transparent protective film 54 is covered each by positive color paste layer 52 and back up layer 53, carries out again afterwards
Cutting.
Below by way of realize data further illustrate beneficial effects of the present invention.
According to GB/T 14916-2006《Identification card physical characteristic》In the 8.5th article of " card size under the conditions of epidemic disaster
The regulation and method of testing of stability and warpage ", carry out following test:
(1)The warpage of colour atla under the conditions of hot and humid
Colour atla is exposed 1 hour, 0.5 day, 1 day, 3 days respectively in following temperature and relative humidity:Temperature 50 C, relatively
Humidity 95%;Then the full card warpage of test target.
(2)The warpage of colour atla under the conditions of low temperature and low humidity
Colour atla is exposed 1 hour, 0.5 day, 1 day, 3 days respectively in following temperature and relative humidity:- 35 DEG C of temperature, phase
To humidity 5%;Then the full card warpage of test target.
(3)The warpage of colour atla under the conditions of ambient temperature and moisture
Colour atla is exposed 1 hour, 0.5 day, 1 day, 3 days respectively in following temperature and relative humidity:20 DEG C of temperature, relatively
Humidity 60%;Then the full card warpage of test target.
The method of the full card warpage of test target, according to GB/T 14916-2006《Identification card physical characteristic》In
The regulation of 8.11, colour atla is placed on horizontal stiffness platform, measured any from horizontal stiffness platform to colour atla convex surfaces
Partial ultimate range.
Full card warpage test data is as follows:
Including thickness (0.76 ± 0.08) mm of colour atla itself.
According to GB/T 14916-2006《Identification card physical characteristic》In the 8.11st article of regulation, from horizontal stiffness platform
1.5mm should be not more than to any portion of ultimate range of colour atla convex surfaces, the present invention not only meets this standard, better than this mark
It is accurate.
Described above is only the preferred embodiment of the present invention, it should be noted that for those skilled in the art
For, under the premise without departing from the principles of the invention, some improvement can also be made, these improvement also should be regarded as the guarantor of the present invention
Protect scope.
Claims (10)
- A kind of 1. preparation method of colour atla for automobile appearance repairing, it is characterised in that:Its step includes:1)Mill base is modulated, organic or inorganic pigment, dimethylbenzene, butyl acetate, softening agent and levelling agent are mixed and allocated;2)Draw a design test, sample making and test are carried out with the mill base modulated, until sample passes;3)Mill base is diluted, diluent is added and mill base is diluted;4)Spraying, the mill base after dilution is added in spray equipment, ground is sprayed;5)Baking, the ground that spraying finishes is toasted 1 hour under conditions of 70 DEG C;6)Dry, 25 DEG C of constant temperature and humidities of ground that baking finishes are dried 8 hours;7)Cutting, sizeable square is cut into hand papercutter by ground;8)Cross cutting, is put into guillotine, the cutting mould of guillotine cuts out the profile wheel of colour atla on ground by the ground cut It is wide.
- A kind of 2. preparation method of colour atla for automobile appearance repairing according to claim 1, it is characterised in that:It is described The proportioning of mill base is:Dimethylbenzene accounts for the 20% of mill base gross weight, and butyl acetate accounts for the 25% of mill base gross weight, organic or inorganic pigment The 50% of mill base gross weight is accounted for, softening agent accounts for the 3% of mill base gross weight, and levelling agent accounts for the 2% of mill base gross weight.
- A kind of 3. preparation method of colour atla for automobile appearance repairing according to claim 1, it is characterised in that:It is described Spraying process includes:a)One group of steel plate is fixed in circular loop suspended chain;b)Install the ground of respective numbers respectively on one group of steel plate;c)Start automatic spray apparatus;d)Circular loop suspended chain starts to rotate, and first ground is moved into spraying area;e)Automatic spray apparatus sprays to first ground;f)Circular loop suspended chain starts to rotate, and second ground is moved into spraying area, while first ground is moved To drying area;g)Automatic spray apparatus sprays to second ground, while constant temperature and humidity blowing device carries out table to first ground Dry in face;h)By that analogy, and continual cycle operation, when ground is after second of spraying and skin drying, removes and change Upper new ground.
- A kind of 4. preparation method of colour atla for automobile appearance repairing according to claim 1, it is characterised in that:Including Colour atla box(1)With one group of colour atla volume(2), wherein colour atla box(1)Including box body(3)And lid(4), box body(3)Inside it is provided with one group Dividing plate(31), one group of dividing plate(31)The space size of composition and colour atla volume(2)It is adapted, lid(4)It is L-shaped, its one end and box Body(3)Side is connected and can rotated around connecting line, and the other end is provided with the first magnetic material(41), box body(3)Corresponding Provided with the second magnetic material(32);Colour atla volume(2)Including one group of color effect colour atla(5), and ring buckle(6), wherein colored effect Fruit colour atla(5)It is provided with and ring buckle(6)The adaptable bookbinding hole of shape.
- A kind of 5. preparation method of colour atla for automobile appearance repairing according to claim 4, it is characterised in that:It is described Colour atla volume(2)Also include one group of transparent effect colour atla(7).
- A kind of 6. preparation method of colour atla for automobile appearance repairing according to claim 4, it is characterised in that:It is described Ring buckle(6)Including the first half-turn(61)With the second half-turn(62), wherein the first half-turn(61)One end and the second half-turn(62)One End rotation connection, the first half-turn(61)The other end is provided with buckle, the second half-turn(62)The other end is provided with and is adapted with buckle shape Neck.
- A kind of 7. preparation method of colour atla for automobile appearance repairing according to claim 4, it is characterised in that:It is described Color effect colour atla(5)Including art paper(51), color paste layer(52)With back up layer(53).
- A kind of 8. preparation method of colour atla for automobile appearance repairing according to claim 5, it is characterised in that:It is described Transparent effect colour atla(7)Including PVC films(71)With transparent color paste layer(72).
- A kind of 9. preparation method of colour atla for automobile appearance repairing according to claim 4, it is characterised in that:It is described Colour atla volume(2)It is additionally provided with front cover(21), back cover(22)And it is respectively overlay in one group of see-through card on front cover and back cover(23).
- A kind of 10. preparation method of colour atla for automobile appearance repairing according to claim 7, it is characterised in that:Institute State color paste layer(52)With back up layer(53)On be covered each by transparent protective film(54).