CN105648455A - Novel high-performance boiler cleaning agent and preparation method thereof - Google Patents
Novel high-performance boiler cleaning agent and preparation method thereof Download PDFInfo
- Publication number
- CN105648455A CN105648455A CN201610042723.7A CN201610042723A CN105648455A CN 105648455 A CN105648455 A CN 105648455A CN 201610042723 A CN201610042723 A CN 201610042723A CN 105648455 A CN105648455 A CN 105648455A
- Authority
- CN
- China
- Prior art keywords
- parts
- water
- novel high
- boilercompound
- cleaning agent
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a novel high-performance boiler cleaning agent and a preparation method thereof. The novel high-performance boiler cleaning agent comprises the following raw materials in parts by weight: 4-8 parts of nonyl phenol polyoxyethylene ether, 3-5 parts of polyethylene glycol, 5-10 parts of sodium oxalate, 4-7 parts of sodium carbonate, 1-3 parts of mandarin oil, 2-5 parts of sodium lignin sulfonate, 0.5-2 parts of 4A zeolite and 150-200 parts of water. The boiler cleaning agent disclosed by the invention can be used for dissolving water scale components such as calcium carbonate, magnesium calcium sulfate, carbonate, calcium silicate, iron oxide and the like, is non-corrosive to metals, is non-toxic, is odorless, can be used for quickly and completing removing water scales attached to the inner wall of the boiler; and meanwhile, the boiler cleaning agent further has the advantages of low cost, less dose, a simple preparation process, safe and convenient use, and the like, and has good economical, social and ecological benefits.
Description
Technical field
The invention belongs to article of everyday use technical field, specifically a kind of novel high-performance boilercompound and preparation method thereof.
Background technology
Cleaning boiler is also referred to as clean the boiler, refer to a kind of chemical agent that can remove boiler internal incrustation scale, it is widely used in electric boiler scale removal, oil burning boiler scale removal, gas fired-boiler scale removal, coal-fired boiler descaling, boiler scale removal, hot-water boiler scale removal, heating boiler scale removal, bath boiler scale removal, steam boiler scale removal and plate type heat exchanger scale removal etc. Boiler operatiopn a period of time Hou Shui side can have substantial amounts of calcium carbonate and magnesium carbonate dirt and corrosion product etc., these dirts are firmly attached to boiler inner surface, cause that heat transfer deterioration, fire coal increase, affect the operational efficiency of boiler, cause bigger economic loss, bring serious harm to the safe operation of boiler. Boiler must carry out regular cleaning and descaling, finally makes boiler inner wall water side cleaning clean, improves coal-fired utilization rate, save a large amount of coal simultaneously, reduce environmental pollution, prolonged boiler service life.
Presently commercially available boilercompound kind is a lot, and conventional has mordant and alkali cleaning agent two kinds. Existing boilercompound comparison of ingredients is single, is only mordant or alkali cleaning agent, first carries out alkali cleaning pickling again, complex operation in cleaning process, and labour force is big, uses strong acid or highly basic as abluent main component, and corrosivity is strong, it is easy to infringement boiler. Existing boilercompound there is problems: the problems such as scale removal DeGrain, relatively costly, reagent dosage big, scavenging period length.
Summary of the invention
Present invention aims to boilercompound Problems existing, it is provided that a kind of non-corrosiveness, features high scale-removing effect, cheap novel high-performance boilercompound.
In order to realize object above, the technical solution used in the present invention is as follows:
A kind of novel high-performance boilercompound, is made up of the raw material of following weight portion:
Polyoxyethylene nonyl phenyl vinyl Ether 4-8 part
Polyethylene Glycol 3-5 part
Disodium oxalate. 5-10 part
Sodium carbonate 4-7 part
Citrus seed oil 1-3 part
Sodium lignin sulfonate 2-5 part
4A zeolite 0.5-2 part
Water 150-200 part.
As preferred embodiments of the present invention, above-described a kind of novel high-performance boilercompound, it is made up of the raw material of following weight portion:
Polyoxyethylene nonyl phenyl vinyl Ether 7 parts
Polyethylene Glycol 4.5 parts
Disodium oxalate. 7 parts
Sodium carbonate 5 parts
Citrus seed oil 2.5 parts
Sodium lignin sulfonate 4 parts
1 part of 4A zeolite
170 parts of water.
The preparation method of above-described a kind of novel high-performance boilercompound, comprises the steps: to weigh each raw material according to following raw material: polyoxyethylene nonyl phenyl vinyl Ether 4-8 part, Polyethylene Glycol 3-5 part, Disodium oxalate. 5-10 part, sodium carbonate 4-7 part, citrus seed oil 1-3 part, sodium lignin sulfonate 2-5 part, 4A zeolite 0.5-2 part and water 150-200 part; Suitable quantity of water is added in reactor, add polyoxyethylene nonyl phenyl vinyl Ether, Polyethylene Glycol, Disodium oxalate., sodium carbonate, sodium lignin sulfonate, be stirring 20-30min under 300-500r/min at rotating speed, add 4A zeolite, citrus seed oil and remaining water, stir, obtain boilercompound.
Compared with prior art, the invention have the benefit that
1, the boilercompound of the present invention can dissolve the incrustation scale compositions such as calcium carbonate, magnesium carbonate, calcium sulfate, calcium silicates and ferrum oxide, and metal is corrosion-free, nontoxic, tasteless, quick, thorough removing is attached to the incrustation scale of boiler inner wall.
2, the abluent stable in properties of the present invention, in use occurs without lamination, improves clean effect.
3, abluent cost of the present invention is low, have that consumption is few, preparation technology simple, use the advantage such as safely and conveniently, it is easy to realize industrialized production.
Detailed description of the invention
Below in conjunction with specific embodiment mode, the present invention is further described, but is not limited to protection scope of the present invention.
Embodiment 1
A kind of novel high-performance boilercompound, is made up of the raw material of following weight portion:
Polyoxyethylene nonyl phenyl vinyl Ether 4 parts
Polyethylene Glycol 4 parts
Disodium oxalate. 6 parts
Sodium carbonate 4 parts
Citrus seed oil 1 part
Sodium lignin sulfonate 3 parts
0.5 part of 4A zeolite
150 parts of water.
The preparation method of the abluent of the present embodiment is: comprise the steps: to weigh each raw material according to above raw material; The water of 80 parts are added in reactor, add polyoxyethylene nonyl phenyl vinyl Ether, Polyethylene Glycol, Disodium oxalate., sodium carbonate, sodium lignin sulfonate, be stirring 30min under 300r/min at rotating speed, add 4A zeolite, citrus seed oil and remaining water, stir, obtain boilercompound.
Embodiment 2
A kind of novel high-performance boilercompound, is made up of the raw material of following weight portion:
Polyoxyethylene nonyl phenyl vinyl Ether 5 parts
Polyethylene Glycol 3 parts
Disodium oxalate. 5 parts
Sodium carbonate 6 parts
Citrus seed oil 1.5 parts
Sodium lignin sulfonate 2 parts
1 part of 4A zeolite
150 parts of water.
The preparation method of the abluent of the present embodiment is: comprise the steps: to weigh each raw material according to above raw material; The water of 80 parts are added in reactor, add polyoxyethylene nonyl phenyl vinyl Ether, Polyethylene Glycol, Disodium oxalate., sodium carbonate, sodium lignin sulfonate, be stirring 25min under 350r/min at rotating speed, add 4A zeolite, citrus seed oil and remaining water, stir, obtain boilercompound.
Embodiment 3
A kind of novel high-performance boilercompound, is made up of the raw material of following weight portion:
Polyoxyethylene nonyl phenyl vinyl Ether 6 parts
Polyethylene Glycol 5 parts
Disodium oxalate. 8 parts
Sodium carbonate 7 parts
Citrus seed oil 2 parts
Sodium lignin sulfonate 3 parts
2 parts of 4A zeolite
180 parts of water.
The preparation method of the abluent of the present embodiment is: comprise the steps: to weigh each raw material according to above raw material; The water of 100 parts are added in reactor, add polyoxyethylene nonyl phenyl vinyl Ether, Polyethylene Glycol, Disodium oxalate., sodium carbonate, sodium lignin sulfonate, be stirring 20min under 500r/min at rotating speed, add 4A zeolite, citrus seed oil and remaining water, stir, obtain boilercompound.
Embodiment 4
A kind of novel high-performance boilercompound, is made up of the raw material of following weight portion:
Polyoxyethylene nonyl phenyl vinyl Ether 7 parts
Polyethylene Glycol 4.5 parts
Disodium oxalate. 7 parts
Sodium carbonate 5 parts
Citrus seed oil 2.5 parts
Sodium lignin sulfonate 4 parts
1 part of 4A zeolite
170 parts of water.
The preparation method of the abluent of the present embodiment is: comprise the steps: to weigh each raw material according to above raw material; The water of 90 parts are added in reactor, add polyoxyethylene nonyl phenyl vinyl Ether, Polyethylene Glycol, Disodium oxalate., sodium carbonate, sodium lignin sulfonate, be stirring 25min under 500r/min at rotating speed, add 4A zeolite, citrus seed oil and remaining water, stir, obtain boilercompound.
Embodiment 5
A kind of novel high-performance boilercompound, is made up of the raw material of following weight portion:
Polyoxyethylene nonyl phenyl vinyl Ether 8 parts
Polyethylene Glycol 4 parts
Disodium oxalate. 10 parts
Sodium carbonate 5 parts
Citrus seed oil 3 parts
Sodium lignin sulfonate 5 parts
1.5 parts of 4A zeolite
200 parts of water.
The preparation method of the abluent of the present embodiment is: comprise the steps: to weigh each raw material according to above raw material; The water of 90 parts are added in reactor, add polyoxyethylene nonyl phenyl vinyl Ether, Polyethylene Glycol, Disodium oxalate., sodium carbonate, sodium lignin sulfonate, be stirring 20min under 500r/min at rotating speed, add 4A zeolite, citrus seed oil and remaining water, stir, obtain boilercompound.
Being added in boiler by the abluent of the present invention, adding with abluent weight ratio is the water of 20:1, soaks 24 hours, emptying sewage, can complete the cleaning of boiler. This abluent can dissolve the incrustation scale compositions such as calcium carbonate, magnesium carbonate, calcium sulfate, calcium silicates and ferrum oxide, metal is corrosion-free, nontoxic, tasteless, quick, thorough can remove the incrustation scale being attached to boiler inner wall.
Claims (3)
1. a novel high-performance boilercompound, it is characterised in that: it is made up of the raw material of following weight portion:
Polyoxyethylene nonyl phenyl vinyl Ether 4-8 part
Polyethylene Glycol 3-5 part
Disodium oxalate. 5-10 part
Sodium carbonate 4-7 part
Citrus seed oil 1-3 part
Sodium lignin sulfonate 2-5 part
4A zeolite 0.5-2 part
Water 150-200 part.
2. a kind of novel high-performance boilercompound according to claim 1, it is characterised in that: it is made up of the raw material of following weight portion:
Polyoxyethylene nonyl phenyl vinyl Ether 7 parts
Polyethylene Glycol 4.5 parts
Disodium oxalate. 7 parts
Sodium carbonate 5 parts
Citrus seed oil 2.5 parts
Sodium lignin sulfonate 4 parts
1 part of 4A zeolite
170 parts of water.
3. the preparation method of a kind of novel high-performance boilercompound as claimed in claim 1, it is characterised in that: comprise the steps: to weigh each raw material according to following raw material: polyoxyethylene nonyl phenyl vinyl Ether 4-8 part, Polyethylene Glycol 3-5 part, Disodium oxalate. 5-10 part, sodium carbonate 4-7 part, citrus seed oil 1-3 part, sodium lignin sulfonate 2-5 part, 4A zeolite 0.5-2 part and water 150-200 part; Suitable quantity of water is added in reactor, add polyoxyethylene nonyl phenyl vinyl Ether, Polyethylene Glycol, Disodium oxalate., sodium carbonate, sodium lignin sulfonate, be stirring 20-30min under 300-500r/min at rotating speed, add 4A zeolite, citrus seed oil and remaining water, stir, obtain boilercompound.