CN105537000A - 一种重晶石抑制剂的制备方法 - Google Patents

一种重晶石抑制剂的制备方法 Download PDF

Info

Publication number
CN105537000A
CN105537000A CN201510967949.3A CN201510967949A CN105537000A CN 105537000 A CN105537000 A CN 105537000A CN 201510967949 A CN201510967949 A CN 201510967949A CN 105537000 A CN105537000 A CN 105537000A
Authority
CN
China
Prior art keywords
barite
inhibitor
preparation
minutes
present
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510967949.3A
Other languages
English (en)
Inventor
董宪久
戴晶平
许毓海
张笃
苏振华
刘兵
钟旭群
何晋勇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GUANGXI ZHONGJIN LINGNAN MINING Co Ltd
Original Assignee
GUANGXI ZHONGJIN LINGNAN MINING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GUANGXI ZHONGJIN LINGNAN MINING Co Ltd filed Critical GUANGXI ZHONGJIN LINGNAN MINING Co Ltd
Priority to CN201510967949.3A priority Critical patent/CN105537000A/zh
Publication of CN105537000A publication Critical patent/CN105537000A/zh
Pending legal-status Critical Current

Abstract

一种重晶石抑制剂的制备方法,包括如下步骤:在25-30℃下按重量比45:30:25加入硫酸铝、氯化铁、硫酸铁进行反应30分钟,然后加入30%的水玻璃进行反应10分钟,将反应产物进行浓缩和烘干,获得粉末状浅红色产品。该抑制剂能够在碱性介质中有效抑制重晶石,利于重晶石和脉石矿物的浮选分离。

Description

一种重晶石抑制剂的制备方法
一、技术领域
本发明涉及一种重晶石抑制剂的制备方法,适用于需要提高重晶石品位或者重晶石可浮性较差的矿石。
二、背景技术
盘龙铅锌矿是一种多金属矿石,在含有铅锌硫的基础上,还含有大量的重晶石,目前盘龙铅锌矿采用高碱流程来回收铅锌,由于矿浆碱度过高对于尾矿中的重晶石回收造成一定困难。铅锌高碱工艺中由于大量石灰的添加,造成尾矿碱度过高,重晶石表面被羟基和钙离子强烈抑制,需要加入大量硫酸来降低矿浆碱度和活化重晶石,对生产管路腐蚀严重,操作环境差。对于别钙离子强烈抑制的重晶石可以采用反浮选来进行选别,一方面可以在碱性矿浆中浮选,另一方面由于其它脉石矿物已经被钙离子活化,采用油酸类捕收剂容易实现脉石矿物的浮选,但该技术的关键在于对重晶石进行选择性抑制。目前国内外都是重晶石的浮选大部分都是关于捕收剂的研究,抑制剂报道比较少。
三、发明内容
本发明的目的在于提供一种重晶石抑制剂的制备方法,该抑制剂能够在碱性介质中有效抑制重晶石,利于重晶石和脉石矿物的浮选分离。
本发明的技术方案是:一种重晶石抑制剂的制备方法,包括如下步骤:在25-30℃下按重量比45:30:25加入硫酸铝、氯化铁、硫酸铁进行反应30分钟,然后加入30%的水玻璃进行反应10分钟,将反应产物进行浓缩和烘干,获得粉末状浅红色产品。
本发明的突出优点在于:
1、制备的抑制剂具有多种结构单元,产生协同抑制效应。抑制有效组分主要有羟基铁、羟基铝、羟基铁铝化合物、硫酸根和硅酸根等,其中羟基铁、羟基铝、羟基铁铝能够在对重晶石表面产生吸附,硫酸根能够和重晶石表面阳离子作用形成亲水膜,硅酸根离子能够在分散矿泥的情况下同时对重晶石产生抑制作用。
2、制备的抑制剂能够在石灰造成的碱性矿浆中使用,避免了硫酸对管路的腐蚀和环境污染,对碱度较高的硫化矿尾矿中回收重晶石提供了有利条件。
3、新药剂无毒无污染,是绿色环保产品。
四、具体实施方式
以下通过实施例对本发明的技术方案作进一步说明。
实施例1
本发明所述的重晶石抑制剂的制备方法,包括如下步骤:在25-30℃下按重量比45:30:25加入硫酸铝、氯化铁、硫酸铁进行反应30分钟,然后加入30%的水玻璃进行反应10分钟,将反应产物进行浓缩和烘干,获得粉末状浅红色产品。
实施例2
本实施例是本发明所述的重晶石抑制剂的制备方法制备得到的抑制剂在浮选铅锌矿尾矿中的应用实例。
1、矿物原料:广西某矿山铅锌矿尾矿,处理量每天300吨。尾矿含重晶石31%%,方解石40%,石英为26%,其它矿物3%。
2、药剂制度及操作条件:先将铅锌矿尾矿调浆5分钟,加入本发明所述的重晶石抑制剂800g/t,作用3分钟,再加入改性捕收剂331A800g/t,作用3分钟,经一粗三扫两精,获得重晶石品位为80%,回收浮选率85%的指标。
实施例3
本实施例是本发明所述的重晶石抑制剂的制备方法制备得到的抑制剂在浮选铅锌矿尾矿中的另一应用实例。
1、矿物原料:贵州某含重晶石铅锌矿尾矿,处理量每天200吨。尾矿含重晶石45%%,石英40%,赤铁矿10%,其它5%。
2、药剂制度及操作条件:首先将铅锌矿尾矿调浆5分钟,加入本发明所述的重晶石抑制剂1000g/t,作用3分钟,再加入改性捕收剂331A660g/t,作用3分钟,经一粗二扫一精,获得重晶石品位为85%,回收浮选率90%的指标。

Claims (2)

1.一种重晶石抑制剂的制备方法,其特征在于,包括如下步骤:在25-30℃下按重量比45:30:25加入硫酸铝、氯化铁、硫酸铁进行反应30分钟,然后加入30%的水玻璃进行反应10分钟,将反应产物进行浓缩和烘干,获得粉末状浅红色产品。
2.权利要求1所述的重晶石抑制剂的制备方法制备得到的抑制剂在浮选铅锌矿尾矿中的应用。
CN201510967949.3A 2015-12-22 2015-12-22 一种重晶石抑制剂的制备方法 Pending CN105537000A (zh)