CN105436291A - Production and inspection process of reinforced panel - Google Patents
Production and inspection process of reinforced panel Download PDFInfo
- Publication number
- CN105436291A CN105436291A CN201510918528.1A CN201510918528A CN105436291A CN 105436291 A CN105436291 A CN 105436291A CN 201510918528 A CN201510918528 A CN 201510918528A CN 105436291 A CN105436291 A CN 105436291A
- Authority
- CN
- China
- Prior art keywords
- production
- reinforced panel
- inspection process
- steel band
- film perforation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a production and inspection process of a reinforced panel, and relates to the technical field of processing of flexible printed circuit boards. The production and inspection process comprises the following steps: positioning holes 5 and reinforced panel holes 7 are punched in a steel strip by a punching knife; and the steel strip is transmitted to a punching platform through a carrying roller 1. According to the production and inspection process, whether the formed size of the reinforced panel is qualified or not can be recognized through a fool-proofing pin, and when accumulated errors of one end are too large, marks are generated around the reinforced panel holes, so that the reorganization of defective products is facilitated.
Description
Technical field
The present invention relates to flexible PCB processing technique field, particularly a kind of production of reinforcing chip and checkout procedure.
Background technology
When current reinforcing chip with holes makes, if hole is to the hypotelorism on limit, when external form and hole punching press simultaneously, easily cause hole to limit flange, the qualities such as distortion are bad.Therefore hole and external form mostly are punching press respectively, bad to reduce quality.But punching press has the accumulation apart from error respectively, causes the reinforcement film perforation cut out bad to the relative size on limit, and because trickleer, naked eyes None-identified, quality omits increased risk.
Summary of the invention
The technical problem to be solved in the present invention is: when existing reinforcing chip with holes occurs that size is bad, is difficult to the problem of screening.
For solving the problems of the technologies described above, the invention provides a kind of production and checkout procedure of reinforcing chip, comprising the following steps: that step one, steel band punch out locating hole 5 and reinforcement film perforation 7 by punching cutter;
Step 2, steel band step one obtained transfer to die-cut platform by transfer roller 1;
The die-cut steel band 6 of step 3, die-cut platform, lead 2 inserts in locating hole 5 and carries out correcting, and punching cutter 3 punches out reinforcing chip profile, and fool proof pin 4 inserts reinforcement film perforation 7;
With or without the marking around step 4, inspection reinforcement film perforation 7.
By fool proof pin, this reinforcing chip production testing process can identify that whether reinforcing chip compact dimensions is qualified, one end accumulation of error is excessive, will produce the marking, and be convenient to identify defective products around reinforcement film perforation.
Accompanying drawing explanation
Fig. 1 is the schematic diagram of the fool proof decompressor of reinforcing chip of the present invention.
Detailed description of the invention
Below in conjunction with drawings and Examples, the specific embodiment of the present invention is described in further detail.Following examples for illustration of the present invention, but are not used for limiting the scope of the invention.
The fool proof decompressor of reinforcing chip as shown in Figure 1, comprising: transfer roller 1, lead 2, punching cutter 3 and fool proof pin 4.Transfer roller 1, for the steel band 6 of conveyer belt locating hole 5, steel band 6 is also provided with reinforcement film perforation 7.Lead 2 mates with locating hole 5, and lead 2 inserts in locating hole 5 and carries out correcting.Lead 2, punching cutter 3, fool proof pin 4 are positioned in identical platform and move simultaneously, and punching cutter 3 is for punching products profile, and fool proof pin 4 and reinforcement film perforation 7 match.
Place to prevent steel band 6 and put upside down, locating hole 5 has two rows, and wherein the diameter of a row is greater than another row, and when placing wrong, steel band cannot punching press.
The production of above-mentioned reinforcing chip and checkout procedure are:
Step one, steel band punch out locating hole 5 and reinforcement film perforation 7 by punching cutter;
Step 2, steel band step one obtained transfer to die-cut platform by transfer roller 1;
The die-cut steel band 6 of step 3, die-cut platform, lead 2 inserts in locating hole 5 and carries out correcting, and punching cutter 3 punches out reinforcing chip profile, and fool proof pin 4 inserts reinforcement film perforation 7;
With or without the marking around step 4, inspection reinforcement film perforation 7.
By fool proof pin, this reinforcing chip production testing process can identify that whether reinforcing chip compact dimensions is qualified, one end accumulation of error is excessive, will produce the marking, and be convenient to identify defective products around reinforcement film perforation.
Above embodiment is only for illustration of the present invention; and be not limitation of the present invention; the those of ordinary skill of relevant technical field; without departing from the spirit and scope of the present invention; can also make a variety of changes and modification; therefore all equivalent technical schemes also belong to category of the present invention, and scope of patent protection of the present invention should be defined by the claims.
Claims (1)
1. the production of reinforcing chip and a checkout procedure, is characterized in that, comprise the following steps:
Step one, steel band punch out locating hole (5) and reinforcement film perforation (7) by punching cutter;
Step 2, steel band step one obtained transfer to die-cut platform by transfer roller (1);
Step 3, the die-cut steel band of die-cut platform (6), lead (2) inserts in locating hole (5) and carries out correcting, and punching cutter (3) punches out reinforcing chip profile, and fool proof pin (4) inserts reinforcement film perforation (7);
Step 4, inspection reinforcement film perforation (7) are around with or without the marking.