CN105398259A - 一种书法用毛笔及其制作方法 - Google Patents
一种书法用毛笔及其制作方法 Download PDFInfo
- Publication number
- CN105398259A CN105398259A CN201510795976.7A CN201510795976A CN105398259A CN 105398259 A CN105398259 A CN 105398259A CN 201510795976 A CN201510795976 A CN 201510795976A CN 105398259 A CN105398259 A CN 105398259A
- Authority
- CN
- China
- Prior art keywords
- writing brush
- minute
- rabbit hair
- stalk
- brush
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及毛笔技术领域,具体涉及一种书法用毛笔及其制作方法,包括笔杆和笔头,所述的笔头由狼毫、兔毛和改性秸秆构成,所述的狼毫重量百分比为30-40%,所述的兔毛重量百分比为20-40%,所述的改性秸秆重量百分比为30-40%,本发明具有弹性好、吸墨性强、软硬兼顾,能够适用多种书写变化要求。
Description
技术领域:
本发明涉及毛笔技术领域,具体涉及一种书法用毛笔及其制作方法。
背景技术:
毛笔是我国传统的书写工具,毛笔按照笔毛可以分为羊毫笔、狼毫笔、兔毛笔及兼毫笔等多种,狼毫笔是用黄鼠狼尾巴毛为原料制成的笔;羊毫笔是用山羊的毛为原料制成的笔;鼠须笔是用家鼠鬓须制成的笔;兼毫笔是用几种细毛混合在一起制成的毛笔,其刚柔适中。制作兼毫笔时,各种毛质的性能,特点的配比要适当,配制的比例、选材都有要合理,几种毛的长短、含量要计算准确才能达到如期的使用效果,因此兼毫的工艺高于其它笔的工艺,是要花费巨大的时间、人力、物力进行试验才能制成,现有的兼毫笔制作成本高昂、制作速度慢、制成之后需要进行防腐处理,而且长时间不使用后容易被腐蚀,另外,使用毛笔书写时常常需要通过调整手法、力度等以获得丰富的变化,而现有的兼毫笔很难达到这一要求。
发明内容:
本发明所要解决的技术问题在于克服现有的技术缺陷提供一种书法用毛笔及其制作方法。
本发明所要解决的技术问题采用以下的技术方案来实现:
一种书法用毛笔,包括笔杆和笔头,其特征在于:所述的笔头由狼毫、兔毛和改性秸秆构成,所述的狼毫重量百分比为30-40%,所述的兔毛重量百分比为20-40%,所述的改性秸秆重量百分比为30-40%。
一种书法用毛笔的制作方法,其特征在于包括下列步骤:
(1)改性秸秆处理方法:将秸秆平铺后,秸秆厚度为8-10厘米,然后在上面撒上一层石灰,石灰厚度为1-2厘米,最后洒水,至石灰半湿为准,保湿2-3天;将秸秆取出洗净,干燥后,放入密封酸化池中,往酸化池中均匀放入10%盐酸溶液,将酸化池的温度升高到130-140℃,压力升高到7-8MPa,20分钟后,再加入15%醋酸溶液,压力升高到10-11MPa,时间为30分钟,期间搅拌频率为50转/分钟;将秸秆取出用去离子水洗涤,再在30-40℃温度下进行干燥;将干燥后的秸秆分解,细度为35-80微米;
(2)狼毫处理方法:将狼毫根部朝上,锋豪朝下放置,然后使用70-80℃的纯碱溶液冲洗狼毫2-6分钟,再使用40-50℃的含有20%醋酸的乙醚溶液冲洗30-40分钟,最后使用去90-100℃离子水冲洗10-15分钟,然后进行20-30℃低温干燥;
(3)兔毛处理方法:将兔毛根部朝上,锋豪朝下放置,然后使用100-110℃的石灰水冲洗兔毛3-4分钟,再使用40-50℃的含有15%硫酸铵溶液冲洗10-15分钟,最后使用去80-90℃离子水冲洗10-15分钟,然后进行20-30℃低温干燥;
(4)将处理过的改性秸秆、兔毛和狼毫按百分比均匀混合后,结扎成笔头;
(5)将结扎好的笔头装入已绞孔好的笔杆中即可。
本发明使用改性秸秆、兔毛和狼毫相结合的技术,脱脂更加彻底,而且不伤锋豪,不添加任何防腐剂,保存时间长,采用秸秆也可以降低成本,本发明具有弹性好、吸墨性强、软硬兼顾,能够适用多种书写变化要求。
具体实施方式:
为了使本发明实现的技术手段、创作特征、达成目的与功效易于明白了解,下面进一步阐述本发明。
实施例中:一种书法用毛笔,包括笔杆和笔头,其特征在于:所述的笔头由狼毫、兔毛和改性秸秆构成,所述的狼毫重量百分比为35%,所述的兔毛重量百分比为30%,所述的改性秸秆重量百分比为35%。
一种书法用毛笔的制作方法,其特征在于包括下列步骤:
(1)改性秸秆处理方法:将秸秆平铺后,秸秆厚度为9厘米,然后在上面撒上一层石灰,石灰厚度为1厘米,最后洒水,至石灰半湿为准,保湿2.5天;将秸秆取出洗净,干燥后,放入密封酸化池中,往酸化池中均匀放入10%盐酸溶液,将酸化池的温度升高到135℃,压力升高到7.5MPa,20分钟后,再加入15%醋酸溶液,压力升高到10.5MPa,时间为30分钟,期间搅拌频率为50转/分钟;将秸秆取出用去离子水洗涤,再在35℃温度下进行干燥;将干燥后的秸秆分解,细度为70微米;
(2)狼毫处理方法:将狼毫根部朝上,锋豪朝下放置,然后使用75℃的纯碱溶液冲洗狼毫4分钟,再使用45℃的含有20%醋酸的乙醚溶液冲洗35分钟,最后使用去95℃离子水冲洗12分钟,然后进行25℃低温干燥;
(3)兔毛处理方法:将兔毛根部朝上,锋豪朝下放置,然后使用105℃的石灰水冲洗兔毛3.5分钟,再使用45℃的含有15%硫酸铵溶液冲洗12分钟,最后使用去85℃离子水冲洗13分钟,然后进行25℃低温干燥;
(4)将处理过的改性秸秆、兔毛和狼毫按百分比均匀混合后,结扎成笔头;
(5)将结扎好的笔头装入已绞孔好的笔杆中即可。
以上显示和描述了本发明的基本原理和主要特征和本发明的优点。本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下,本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内。本发明要求保护范围由所附的权利要求书及其等效物界定。
Claims (2)
1.一种书法用毛笔,包括笔杆和笔头,其特征在于:所述的笔头由狼毫、兔毛和改性秸秆构成,所述的狼毫重量百分比为30-40%,所述的兔毛重量百分比为20-40%,所述的改性秸秆重量百分比为30-40%。
2.一种书法用毛笔的制作方法,其特征在于包括下列步骤:
(1)改性秸秆处理方法:将秸秆平铺后,秸秆厚度为8-10厘米,然后在上面撒上一层石灰,石灰厚度为1-2厘米,最后洒水,至石灰半湿为准,保湿2-3天;将秸秆取出洗净,干燥后,放入密封酸化池中,往酸化池中均匀放入10%盐酸溶液,将酸化池的温度升高到130-140℃,压力升高到7-8MPa,20分钟后,再加入15%醋酸溶液,压力升高到10-11MPa,时间为30分钟,期间搅拌频率为50转/分钟;将秸秆取出用去离子水洗涤,再在30-40℃温度下进行干燥;将干燥后的秸秆分解,细度为35-80微米;
(2)狼毫处理方法:将狼毫根部朝上,锋豪朝下放置,然后使用70-80℃的纯碱溶液冲洗狼毫2-6分钟,再使用40-50℃的含有20%醋酸的乙醚溶液冲洗30-40分钟,最后使用去90-100℃离子水冲洗10-15分钟,然后进行20-30℃低温干燥;
(3)兔毛处理方法:将兔毛根部朝上,锋豪朝下放置,然后使用100-110℃的石灰水冲洗兔毛3-4分钟,再使用40-50℃的含有15%硫酸铵溶液冲洗10-15分钟,最后使用去80-90℃离子水冲洗10-15分钟,然后进行20-30℃低温干燥;
(4)将处理过的改性秸秆、兔毛和狼毫按百分比均匀混合后,结扎成笔头;
(5)将结扎好的笔头装入已绞孔好的笔杆中即可。