CN105328977B - A kind of printing down method of halftone - Google Patents

A kind of printing down method of halftone Download PDF

Info

Publication number
CN105328977B
CN105328977B CN201510863802.XA CN201510863802A CN105328977B CN 105328977 B CN105328977 B CN 105328977B CN 201510863802 A CN201510863802 A CN 201510863802A CN 105328977 B CN105328977 B CN 105328977B
Authority
CN
China
Prior art keywords
halftone
exposure
carried out
film
surprint
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201510863802.XA
Other languages
Chinese (zh)
Other versions
CN105328977A (en
Inventor
崔朝阳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen Heyuda Technology Co ltd
Original Assignee
Shenzhen Heyuda Technology Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shenzhen Heyuda Technology Co ltd filed Critical Shenzhen Heyuda Technology Co ltd
Priority to CN201510863802.XA priority Critical patent/CN105328977B/en
Publication of CN105328977A publication Critical patent/CN105328977A/en
Application granted granted Critical
Publication of CN105328977B publication Critical patent/CN105328977B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A kind of printing down method of halftone, comprises the following steps:(1)Test the exposure energy that halftone needs;(2)First time step of exposure is carried out to halftone;(3)Second of step of exposure is carried out to halftone;(4)P surface covers are carried out to halftone and shine step of exposure.This method is carried out after the film is sticked on halftone after first time exposure, halftone is carried out second after the translation of printer glass planar to expose, assuming that there is foreign matter on printer glass, then when exposing first time, foreign matter gear residence can not have light, and former foreign matter gear residence can be removed light after halftone is translated, and avoid the halftone perforated phenomenon caused by printer glass foreign.Meanwhile P surface covers are carried out to halftone and shine step of exposure, the combination power of non-printed areas emulsion and grenadine can be strengthened, halftone is made to be not easy to perforate caused by extruding during use is printed, can significantly promote the service life of halftone.

Description

A kind of printing down method of halftone
Technical field
The present invention relates to screen printing technique field more particularly to a kind of printing down methods of halftone.
Background technology
At present, silk-screen halftone is using exposure manufacture process, still, if there are foreign matter on printer glass in exposure manufacture process, Because being in the light for foreign matter can cause halftone face that can not be had perforation by photosensitizer so as to cause halftone face by foreign matter gear residence Phenomenon, meanwhile, to ensure the precision of halftone pattern line, exposure energy cannot be too strong, can be because diffraction causes line if too strong Distortion, but the combination power of emulsion and grenadine cannot be effectively ensured again so that in screen painting suitable for the exposure energy of lines It easily causes to perforate because squeezing during use.
The content of the invention
It is an object of the invention to overcome above-mentioned the deficiencies in the prior art, provide a kind of with re-expose step and P faces The printing down method of the halftone of surprint step of exposure.
The present invention is achieved in that a kind of printing down method of halftone, comprises the following steps:
(1)Test the exposure energy that the halftone needs
The exposure energy A of the halftone needs is tested out by using exposure energy testing piece;
(2)First time step of exposure is carried out to the halftone
After the film is sticked on the halftone, first time exposure is carried out to the halftone, wherein, to the halftone Carry out exposure energy B1=A*3/5 of first time exposure;
(3)Second of step of exposure is carried out to the halftone and completes step(2)In to the halftone carry out first time exposure After light step, the halftone is translated on printer glass planar, by the halftone in the printer glass planar After upper translation, second of step of exposure is carried out to the halftone, wherein, second of exposure energy exposed is carried out to the halftone Measure B2=A*3/5;
(4)P surface covers are carried out to the halftone and shine step of exposure
The both sides of the film printing zone of the halftone are extended out to form surprint film region, complete step(3)In it is right After the halftone carries out second of step of exposure, surprint film aligning is sticked on the surprint film region, the set It shines the film and blocks the film printing zone completely, and be put on the printer and carry out P surface covers solarization step of exposure, wherein, it is right The halftone carries out exposure energy B3=2*A that P surface covers shine exposure.
Preferably, step(3)In, the scope that the halftone translates on printer glass planar is 1 ~ 5cm.
Preferably, step(4)In, the scope that the both sides of the film printing zone of the halftone extend out is 1 ~ 3mm.
Beneficial effects of the present invention are:The film is sticked in halftone by the printing down method of halftone provided by the invention, this method It carries out first time exposure afterwards above, after the completion of exposing for the first time, halftone is carried out second after the translation of printer glass planar Exposure, because the halftone under the film state that is sticked translates on printer glass, it is assumed that have foreign matter on printer glass, then exist Foreign matter gear residence can not have a light when exposing for the first time, and after halftone is translated former foreign matter gear residence can be removed by Light, so as to avoid the halftone perforated phenomenon caused by the foreign matter of printer glass.Meanwhile by the film printing zone two of halftone While extending out, surprint film region is formed, after halftone is double exposed, the surprint film is sticked in surprint film region On, at this point, the surprint film blocks film printing zone completely, and is put on printer and carries out the solarization exposure of P surface covers, it is non-so as to strengthen The combination power of printing zone emulsion and grenadine makes halftone be not easy to perforate caused by extruding during use is printed, can be significantly Promote the service life of halftone.
Description of the drawings
In order to illustrate more clearly of technical scheme, letter will be made to attached drawing needed in the embodiment below Singly introduce, it should be apparent that, the accompanying drawings in the following description is only some embodiments of the present invention, for the common skill in this field For art personnel, without creative efforts, other attached drawings are can also be obtained according to these attached drawings.
Fig. 1 is a kind of flow diagram of the printing down method for halftone that one embodiment of the invention provides.
Specific embodiment
In order to which technical problem solved by the invention, technical solution and advantageous effect is more clearly understood, below in conjunction with Accompanying drawings and embodiments, the present invention will be described in further detail.It should be appreciated that specific embodiment described herein is only used To explain the present invention, it is not intended to limit the present invention.
As shown in Figure 1, a kind of printing down method of halftone provided in an embodiment of the present invention, comprises the following steps:
S101 tests the exposure energy that the halftone needs
The exposure energy A of the halftone needs is tested out by using exposure energy testing piece;
S102 carries out first time step of exposure to the halftone
After the film is sticked on the halftone, first time exposure is carried out to the halftone, wherein, to the halftone Carry out exposure energy B1=A*3/5 of first time exposure;
S103 carries out second of step of exposure to the halftone
After carrying out first time step of exposure to the halftone in S102 is completed, the halftone is put down in printer glass It is translated on face, after the halftone is translated on the printer glass planar, second is carried out to the halftone and is exposed Step, wherein, second of exposure energy B2=A*3/5 exposed is carried out to the halftone;
S104 carries out P surface covers to the halftone and shines step of exposure
The both sides of the film printing zone of the halftone are extended out to form surprint film region, to described in S103 is completed After halftone carries out second of step of exposure, surprint film aligning is sticked on the surprint film region, the surprint is luxuriant and rich with fragrance Woods blocks the film printing zone completely, and is put on the printer and carries out P surface covers solarization step of exposure, wherein, to described Halftone carries out exposure energy B3=2*A that P surface covers shine exposure.
In this example, first time exposure is carried out after the film is sticked on halftone, after the completion of exposing for the first time, halftone is existed Second is carried out after the translation of printer glass planar to expose, because being sticked under film state(Pay attention to the film with respect to halftone first Just being fixed before secondary exposure cannot relatively move)Halftone translated on printer glass, it is assumed that on printer glass There is foreign matter, then foreign matter gear residence can not have light when exposing first time, and former foreign matter keeps off residence after halftone is translated Light can be removed, so as to avoid the halftone perforated phenomenon caused by the foreign matter of printer glass.
It should be noted that in this example, halftone is after translation above printer glass, originally by printer on the halftone The concept that foreign matter gear residence above glass is blocked again by another foreign matter is the small probability event in being just distributed very much, It is completely negligible.
It it should be noted that in this example, is drawn by multiple contrast experiment, it is assumed that the emulsion of one piece of halftone exposes suitable for light If light energy is A, after the halftone for the film that is sticked is double exposed respectively, the exposure energy B1 and B2 of double exposure Be A*3/5, both can obtain with once suitable for the identical lines effects of exposure energy A,
It should be noted that in this example, in the suitable exposure energy developing process of normal halftone, this layer of emulsion in S faces Because enough energy sensitizations cannot be received suitable for the exposure energy A of lines precision, cause not wash off in development so as to cause The combination power of emulsion and grenadine is deteriorated to easily cause in printing process to wear, and still, passes through the film printing zone of halftone Both sides extend out to form surprint film region, complete to halftone carry out second of step of exposure after, by surprint film aligning It is sticked on surprint film region, the surprint film blocks film printing zone completely, and is put on printer and carries out the solarization exposure of P surface covers Light carries out halftone exposure energy B3=2*A that P surface covers shine exposure, in this way, this layer of emulsion in S faces is strengthened exposing because of P faces To reservation, while the surprint film covers film printing zone completely, and therefore, the solarization of P surface covers does not interfere with lines precision, this layer of S faces Emulsion strengthens and the combination power of grenadine, and halftone is made to be not easy to perforate caused by extruding during use is printed, can significantly be carried Rise the service life of halftone.
In this example, the film printing zone both sides of halftone are extended out, surprint film region is formed, is exposed twice in halftone After light, the surprint film is sticked on surprint film region, at this point, the surprint film blocks film printing zone completely, and is put P surface covers are carried out on to printer and shine exposure, so as to strengthen the combination power of non-printed areas emulsion and grenadine, halftone are made to make in printing With being not easy to perforate caused by extruding in the process, the service life of halftone can be significantly promoted.
Further, in S103, the scope that the halftone translates on printer glass planar is 1 ~ 5cm, is preferably 3 cm。
Further, in S104, the scope that the both sides of the film printing zone of the halftone extend out is 1 ~ 3mm, preferably For 2 cm.
Beneficial effects of the present invention are:The film is sticked in halftone by the printing down method of halftone provided by the invention, this method It carries out first time exposure afterwards above, after the completion of exposing for the first time, halftone is carried out second after the translation of printer glass planar Exposure, because the halftone under the film state that is sticked translates on printer glass, it is assumed that have foreign matter on printer glass, then exist Foreign matter gear residence can not have a light when exposing for the first time, and after halftone is translated former foreign matter gear residence can be removed by Light, so as to avoid the halftone perforated phenomenon caused by the foreign matter of printer glass.Meanwhile by the film printing zone two of halftone While extending out, surprint film region is formed, after halftone is double exposed, the surprint film is sticked in surprint film region On, at this point, the surprint film blocks film printing zone completely, and is put on printer and carries out the solarization exposure of P surface covers, it is non-so as to strengthen The combination power of printing zone emulsion and grenadine makes halftone be not easy to perforate caused by extruding during use is printed, can be significantly Promote the service life of halftone.
The foregoing is merely illustrative of the preferred embodiments of the present invention, is not intended to limit the invention, all essences in the present invention All any modification, equivalent and improvement made within refreshing and principle etc., should all be included in the protection scope of the present invention.

Claims (1)

1. a kind of printing down method of halftone, which is characterized in that comprise the following steps:
(1) exposure energy that the halftone needs is tested
The exposure energy A of the halftone needs is tested out by using exposure energy testing piece;
(2) first time step of exposure is carried out to the halftone
After the film is sticked on the halftone, first time exposure is carried out to the halftone, wherein, the halftone is carried out The exposure energy B1=A*3/5 of exposure for the first time;
(3) second of step of exposure is carried out to the halftone
After carrying out first time step of exposure to the halftone in step (2) is completed, the halftone is put down in printer glass It is translated on face, after the halftone is translated on the printer glass planar, second is carried out to the halftone and is exposed Step, wherein, second of exposure energy B2=A*3/5 exposed is carried out to the halftone;
(4) P surface covers are carried out to the halftone and shines step of exposure
The both sides of the film printing zone of the halftone are extended out to form surprint film region, to described in step (3) is completed After halftone carries out second of step of exposure, surprint film aligning is sticked on the surprint film region, the surprint is luxuriant and rich with fragrance Woods can block the film printing zone completely, and be put on the printer and carry out P surface covers solarization step of exposure, wherein, it is right The halftone carries out the exposure energy B3=2*A that P surface covers shine exposure;The scope that the halftone translates on printer glass planar For 1~5cm;The scope that the both sides of the film printing zone of the halftone extend out is 1~3mm.
CN201510863802.XA 2015-12-01 2015-12-01 A kind of printing down method of halftone Expired - Fee Related CN105328977B (en)