CN105328977A - Halftone burning method - Google Patents

Halftone burning method Download PDF

Info

Publication number
CN105328977A
CN105328977A CN201510863802.XA CN201510863802A CN105328977A CN 105328977 A CN105328977 A CN 105328977A CN 201510863802 A CN201510863802 A CN 201510863802A CN 105328977 A CN105328977 A CN 105328977A
Authority
CN
China
Prior art keywords
half tone
exposure
halftone
described half
film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201510863802.XA
Other languages
Chinese (zh)
Other versions
CN105328977B (en
Inventor
崔朝阳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen Heyuda Technology Co ltd
Original Assignee
Shenzhen Heyuda Technology Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shenzhen Heyuda Technology Co ltd filed Critical Shenzhen Heyuda Technology Co ltd
Priority to CN201510863802.XA priority Critical patent/CN105328977B/en
Publication of CN105328977A publication Critical patent/CN105328977A/en
Application granted granted Critical
Publication of CN105328977B publication Critical patent/CN105328977B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a halftone burning method which comprises the following steps: (1) testing the exposure energy required by a halftone; (2) performing single exposure on the halftone; (3) performing double exposure on the halftone; and (4) performing P-face surprint exposure on the halftone. According to the halftone burning method, after a film is pasted on the halftone, single exposure is performed on the halftone, and then after the halftone is translated on a printer glass surface, double exposure is performed on the halftone; suppose a foreign matter is on the printer glass, the place blocked by the foreign matter during the single exposure is not photic, and after the halftone is translated, the place blocked by the foreign matter is moved away and photic, so that the phenomenon about halftone perforation caused by the foreign matter of the printer glass can be avoided. In addition, the P-face surprint exposure step performed on the halftone can strengthen the binding force of emulsion and grenadine can be strengthened in a non-printing area, so that the halftone is unlikely to perforate due to extrusion during the printing and using process, and the service life of the halftone can be greatly prolonged.

Description

A kind of printing down method of half tone
Technical field
The present invention relates to screen printing technique field, particularly relate to a kind of printing down method of half tone.
Background technology
At present, silk-screen half tone all adopts exposure manufacture process, but, if there is foreign matter in printer glass in exposure manufacture process, because of foreign matter be in the light can cause half tone face by foreign matter gear residence cannot by photoactivate thus cause half tone face exist perforation phenomenon, simultaneously, for ensureing the precision of half tone pattern line, exposure energy can not be excessively strong, cross strong words and can cause lines distortion because of diffraction, but the exposure energy of suitable lines effectively can not ensure again the adhesion of emulsion and grenadine thus make easily to cause perforation because extrude in screen painting use procedure.
Summary of the invention
The object of the invention is to overcome above-mentioned the deficiencies in the prior art, a kind of printing down method with the half tone of re-expose step and P surface cover solarization step of exposure is provided.
The present invention is achieved in that a kind of printing down method of half tone, comprises the following steps:
(1) exposure energy that described half tone needs is tested
By the exposure energy A adopting exposure energy test pieces to test out described half tone needs;
(2) first time step of exposure is carried out to described half tone
After being sticked by the film on described half tone, first time exposure is carried out to described half tone, wherein, described half tone is carried out to the exposure energy B1=A*3/5 of first time exposure;
(3) carry out after second time step of exposure carries out first time step of exposure to described half tone in completing steps (2) to described half tone, by the translation on printer glass planar of described half tone, by described half tone on described printer glass planar after translation, second time step of exposure is carried out to described half tone, wherein, described half tone is carried out to the exposure energy B2=A*3/5 of second time exposure;
(4) P surface cover is carried out to described half tone and shine step of exposure
The both sides of the film printing zone of described half tone are extended out and forms surprint film region, after second time step of exposure being carried out to described half tone in completing steps (3), surprint film aligning is sticked on described surprint film region, the described surprint film blocks described film printing zone completely, and be put into and described printer carry out P surface cover and shine step of exposure, wherein, the exposure energy B3=2*A that P surface cover shines exposure is carried out to described half tone.
Preferably, in step (3), the scope of described half tone translation on printer glass planar is 1 ~ 5cm.
Preferably, in step (4), the scope that the both sides of the film printing zone of described half tone extend out is 1 ~ 3mm.
Beneficial effect of the present invention is: the printing down method of half tone provided by the invention, the film is sticked after on half tone and carries out first time exposure by the method, after first time has exposed, half tone is carried out after the translation of printer glass planar second time exposure, cause is in the translation on printer glass of the half tone under film state that is sticked, suppose that printer glass has foreign matter, then when first time exposure, foreign matter gear residence can not have light, and foreign matter gear residence former after half tone translation can be removed light, thus avoid the half tone perforated phenomenon that the foreign matter because of printer glass causes.Simultaneously, the film printing zone both sides of half tone are extended out, form surprint film region, after half tone double exposes, the surprint film is sticked on surprint film region, now, the surprint film blocks film printing zone completely, and is put into and printer carries out P surface cover and shine exposure, thus strengthens the adhesion of non-printed areas emulsion and grenadine, making half tone not easily cause perforation because extruding in printing use procedure, significantly can promote the service life of half tone.
Accompanying drawing explanation
In order to be illustrated more clearly in technical scheme of the present invention, be briefly described to the accompanying drawing used required in embodiment below, apparently, accompanying drawing in the following describes is only some embodiments of the present invention, for those of ordinary skill in the art, under the prerequisite not paying creative work, other accompanying drawing can also be obtained according to these accompanying drawings.
Fig. 1 is the schematic flow sheet of the printing down method of a kind of half tone that one embodiment of the invention provides.
Detailed description of the invention
In order to make technical problem solved by the invention, technical scheme and beneficial effect clearly understand, below in conjunction with drawings and Examples, the present invention is further elaborated.Should be appreciated that specific embodiment described herein only in order to explain the present invention, be not intended to limit the present invention.
As shown in Figure 1, the printing down method of a kind of half tone that the embodiment of the present invention provides, comprises the following steps:
S101, tests the exposure energy that described half tone needs
By the exposure energy A adopting exposure energy test pieces to test out described half tone needs;
S102, carries out first time step of exposure to described half tone
After being sticked by the film on described half tone, first time exposure is carried out to described half tone, wherein, described half tone is carried out to the exposure energy B1=A*3/5 of first time exposure;
S103, carries out second time step of exposure to described half tone
After completing in S102 first time step of exposure carried out to described half tone, by the translation on printer glass planar of described half tone, by described half tone on described printer glass planar after translation, second time step of exposure is carried out to described half tone, wherein, described half tone is carried out to the exposure energy B2=A*3/5 of second time exposure;
S104, carries out P surface cover to described half tone and shines step of exposure
The both sides of the film printing zone of described half tone are extended out and forms surprint film region, after completing in S103 second time step of exposure carried out to described half tone, surprint film aligning is sticked on described surprint film region, the described surprint film blocks described film printing zone completely, and be put into and described printer carry out P surface cover and shine step of exposure, wherein, the exposure energy B3=2*A that P surface cover shines exposure is carried out to described half tone.
In this example, the film is sticked after on half tone and carries out first time exposure, after first time has exposed, half tone is carried out after the translation of printer glass planar second time exposure, cause is in the half tone translation on printer glass (noticing that the relative half tone of the film just fixes and can not occur relative movement before first time exposure) under film state that is sticked, suppose that printer glass has foreign matter, then when first time exposure, foreign matter gear residence can not have light, and foreign matter gear residence former after half tone translation can be removed light, thus avoid the half tone perforated phenomenon that the foreign matter because of printer glass causes.
It should be noted that, in this example, half tone on printer glass after translation, on this half tone originally by the foreign matter gear residence above printer glass again by the concept that another one foreign matter blocks be distribute just very much in small probability event, completely negligible.
It should be noted that, in this example, draw through repeatedly contrast experiment, suppose that the emulsion of one piece of half tone is suitable for the words that light exposure energy is A, after the half tone of the film that is sticked is double exposed respectively, exposure energy B1 and B2 of double exposure is A*3/5, both can obtain the lines effect identical with once suitable exposure energy A
It should be noted that, in this example, in the suitable exposure energy developing process of normal half tone, this one deck emulsion in S face can not accept enough energy sensitizations because of the exposure energy A of suitable lines precision, cause not wash off when developing thus causing the adhesion of emulsion and grenadine to be deteriorated thus cause easily causing in printing process wearing, but, extended out by the both sides of the film printing zone of half tone and form surprint film region, after completing second time step of exposure carried out to half tone, surprint film aligning is sticked on surprint film region, the surprint film blocks film printing zone completely, and be put into and printer carry out P surface cover and shine exposure, the exposure energy B3=2*A that P surface cover shines exposure is carried out to half tone, like this, this one deck emulsion in S face is retained because P face adds heavy exposure, the film of surprint simultaneously covers film printing zone completely, therefore, P surface cover is shone can not affect lines precision, this layer, S face emulsion strengthens the adhesion with grenadine, make half tone in printing use procedure not easily because extruding causes perforation, significantly can promote the service life of half tone.
In this example, the film printing zone both sides of half tone are extended out, form surprint film region, after half tone double exposes, the surprint film is sticked on surprint film region, now, the surprint film blocks film printing zone completely, and is put into and printer carries out P surface cover and shine exposure, thus strengthens the adhesion of non-printed areas emulsion and grenadine, making half tone not easily cause perforation because extruding in printing use procedure, significantly can promote the service life of half tone.
Further, in S103, the scope of described half tone translation on printer glass planar is 1 ~ 5cm, is preferably 3cm.
Further, in S104, the scope that the both sides of the film printing zone of described half tone extend out is 1 ~ 3mm, is preferably 2cm.
Beneficial effect of the present invention is: the printing down method of half tone provided by the invention, the film is sticked after on half tone and carries out first time exposure by the method, after first time has exposed, half tone is carried out after the translation of printer glass planar second time exposure, cause is in the translation on printer glass of the half tone under film state that is sticked, suppose that printer glass has foreign matter, then when first time exposure, foreign matter gear residence can not have light, and foreign matter gear residence former after half tone translation can be removed light, thus avoid the half tone perforated phenomenon that the foreign matter because of printer glass causes.Simultaneously, the film printing zone both sides of half tone are extended out, form surprint film region, after half tone double exposes, the surprint film is sticked on surprint film region, now, the surprint film blocks film printing zone completely, and is put into and printer carries out P surface cover and shine exposure, thus strengthens the adhesion of non-printed areas emulsion and grenadine, making half tone not easily cause perforation because extruding in printing use procedure, significantly can promote the service life of half tone.
The foregoing is only preferred embodiment of the present invention, not in order to limit the present invention, all any amendments done within the spirit and principles in the present invention, equivalent replacement and improvement etc., all should be included within protection scope of the present invention.

Claims (3)

1. a printing down method for half tone, is characterized in that, comprise the following steps:
(1) exposure energy that described half tone needs is tested
By the exposure energy A adopting exposure energy test pieces to test out described half tone needs;
(2) first time step of exposure is carried out to described half tone
After being sticked by the film on described half tone, first time exposure is carried out to described half tone, wherein, described half tone is carried out to the exposure energy B1=A*3/5 of first time exposure;
(3) second time step of exposure is carried out to described half tone
After first time step of exposure being carried out to described half tone in completing steps (2), by the translation on printer glass planar of described half tone, by described half tone on described printer glass planar after translation, second time step of exposure is carried out to described half tone, wherein, described half tone is carried out to the exposure energy B2=A*3/5 of second time exposure;
(4) P surface cover is carried out to described half tone and shine step of exposure
The both sides of the film printing zone of described half tone are extended out and forms surprint film region, after second time step of exposure being carried out to described half tone in completing steps (3), surprint film aligning is sticked on described surprint film region, described film printing zone can block by the described surprint film completely, and be put into and described printer carry out P surface cover and shine step of exposure, wherein, the exposure energy B3=2*A that P surface cover shines exposure is carried out to described half tone.
2. the printing down method of a kind of half tone according to claim 1, is characterized in that, in step (3), the scope of described half tone translation on printer glass planar is 1 ~ 5cm.
3. the printing down method of a kind of half tone according to claim 1, is characterized in that, in step (4), the scope that the both sides of the film printing zone of described half tone extend out is 1 ~ 3mm.
CN201510863802.XA 2015-12-01 2015-12-01 A kind of printing down method of halftone Expired - Fee Related CN105328977B (en)