CN105274862A - 一种改善tpu复合织物表面外观的方法 - Google Patents
一种改善tpu复合织物表面外观的方法 Download PDFInfo
- Publication number
- CN105274862A CN105274862A CN201510579551.2A CN201510579551A CN105274862A CN 105274862 A CN105274862 A CN 105274862A CN 201510579551 A CN201510579551 A CN 201510579551A CN 105274862 A CN105274862 A CN 105274862A
- Authority
- CN
- China
- Prior art keywords
- tpu
- composite fabric
- fabric
- bottoming
- tpu composite
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明为解决需要经常更换层压辊以满足客户对于TPU复合织物不同外观要求的技术问题而提供一种改善TPU复合织物表面外观的方法。本发明所采取的技术方案是:一种改善TPU复合织物表面外观的方法,核心技术为:打底处理后的织物在挤出流延TPU薄膜时,将一道离型纸贴合在TPU膜的另一侧;复合后再将离型纸与TPU复合织物分离并分别收卷。采取三明治似的复合方法,比如打底处理织物+TPU薄膜+离型纸。所述的离型纸表面经过有机硅处理,与TPU膜不粘,复合完成后可以直接与TPU织物剥离,其表面效果根据客户需求可以是亚光的,也可以是镜面的,亦或是带纹路的,等等。
Description
技术领域
本发明属于纺织涂层面料生产技术领域,特别是涉及一种改善TPU复合织物表面外观的方法。
背景技术
TPU(Thermoplasticpolyurethanes)名称为热塑性聚氨酯弹性体,具有其他材料无法比拟的强度高、韧性好、耐磨、耐寒、耐老化、耐气候等特性,同是还具有高防水性透湿性、防风、防寒、抗菌、防霉、保暖、抗紫外线以及能量释放等许多优异的功能,在日用品、体育用品、玩具、装饰材料等领域得到广泛应用。TPU复合织物就是用TPU薄膜复合在各种织物上形成一种复合材料,结合两者的特性得到一种新型面料。
在常规的TPU复合织物的生产方法中,织物经过打底处理后直接挤出流延TPU膜,这样生产出来的TPU复合织物的表面外观基本取决于层压辊的表面,亚光辊生产出来的产品便是亚光效果,镜面辊生产出来的产品便是镜面效果,纹路辊生产出来的产品便是纹路效果,等等。不同客户需要的TPU复合织物表面外观是不同的,因此经常需要更换层压辊;这不仅浪费时间浪费人力,增加劳动强度,而且会增加层压辊及其连接结构的磨损,降低层压辊使用寿命,增加生产成本。
发明内容
本发明为解决需要经常更换层压辊以满足客户对于TPU复合织物不同外观要求的技术问题而提供一种改善TPU复合织物表面外观的方法,在不更换层压辊的前提下改变TPU复合织物的表面外观效果,同时不影响复合织物的其他性能指标。
本发明所采取的技术方案是:一种改善TPU复合织物表面外观的方法,核心技术为:打底处理后的织物在挤出流延TPU薄膜时,将一道离型纸贴合在TPU膜的另一侧;复合后再将离型纸与TPU复合织物分离并分别收卷。采取三明治似的复合方法,比如打底处理织物+TPU薄膜+离型纸。所述的离型纸表面经过有机硅处理,与TPU膜不粘,复合完成后可以直接与TPU织物剥离,其表面效果根据客户需求可以是亚光的,也可以是镜面的,亦或是带纹路的,等等。
上述改善TPU复合织物表面外观的方法,主要包括以下步骤:
(1)打底:通过刮刀刮涂的方式对织物进行涂胶打底并烘燥,根据剥离牢度要求,可以涂一道或者两道;
(2)TPU挤出流延复合:TPU挤出流延,离型纸和打底处理后的织物同时放卷,同时贴合TPU薄膜,进行复合;
(3)冷却定型:复合完成后经过冷却定型辊进行冷却定型;
(4)收卷:冷却定型后将离型纸直接与TPU复合织物剥离,分别卷取,离型纸可以重复利用。
作为优选,所述打底温度为150-190℃。
作为优选,所述打底烘燥时间为1-2min。
本发明具有的优点和积极效果是:由于本发明采用如上技术方案,在不更换层压辊的前提下,实现不同外观效果的切换,如亚光效果、镜面效果、纹路效果;TPU复合织物表面外观有了很大的改变,满足了不同客户的需求,节约人力和时间,也节约了成本。本发明主要用于对TPU复合织物表面外观有特殊要求的产品,比如服装面料,箱包等。外观更加精美,深受客户喜爱。
具体实施方式
实施例1
一种改善TPU复合织物表面外观的方法,主要包括以下步骤:
(1)打底:通过刮刀刮涂的方式对织物进行涂胶打底并烘燥,刮涂一道,打底温度为150℃,烘燥时间为2min;
(2)TPU挤出流延复合:TPU挤出流延,离型纸和打底处理后的织物同时放卷,同时贴合TPU薄膜,进行复合;
(3)冷却定型:复合完成后经过冷却定型辊进行冷却定型;
(4)收卷:冷却定型后将离型纸直接与TPU复合织物剥离,分别卷取,离型纸可以重复利用。
离型纸表面经过有机硅处理,与TPU膜不粘,复合完成后可以直接与TPU织物剥离,其表面效果根据客户需求可以是亚光的,也可以是镜面的,亦或是带纹路的,等等。
实施例2
一种改善TPU复合织物表面外观的方法,主要包括以下步骤:
(1)打底:通过刮刀刮涂的方式对织物进行涂胶打底并烘燥,刮涂两道,打底温度为190℃,烘燥时间为1min;
(2)TPU挤出流延复合:TPU挤出流延,离型纸和打底处理后的织物同时放卷,同时贴合TPU薄膜,进行复合;
(3)冷却定型:复合完成后经过冷却定型辊进行冷却定型;
(4)收卷:冷却定型后将离型纸直接与TPU复合织物剥离,分别卷取,离型纸可以重复利用。
离型纸表面经过有机硅处理,与TPU膜不粘,复合完成后可以直接与TPU织物剥离,其表面效果根据客户需求可以是亚光的,也可以是镜面的,亦或是带纹路的,等等。
以上对本发明的2个实施例进行了详细说明,但所述内容仅为本发明的较佳实施例,不能被认为用于限定本发明的实施范围。凡依本发明申请范围所作的均等变化与改进等,均应仍归属于本发明的专利涵盖范围之内。
Claims (4)
1.一种改善TPU复合织物表面外观的方法,其特征在于,打底处理后的织物在挤出流延TPU薄膜时,将一道离型纸贴合在TPU膜的另一侧;复合后再将离型纸与TPU复合织物分离并分别收卷。
2.根据权利要求1所述的一种改善TPU复合织物表面外观的方法,其特征在于,主要包括以下步骤:
(1)打底:通过刮刀刮涂的方式对织物进行涂胶打底并烘燥;
(2)TPU挤出流延复合:TPU挤出流延,离型纸和打底处理后的织物同时放卷,同时贴合TPU薄膜,进行复合;
(3)冷却定型:复合完成后经过冷却定型辊进行冷却定型;
(4)收卷:冷却定型后将离型纸直接与TPU复合织物剥离,分别卷取,离型纸可以重复利用。
3.根据权利要求2所述的一种改善TPU复合织物表面外观的方法,其特征在于,所述打底温度为150-190℃。
4.根据权利要求2所述的一种改善TPU复合织物表面外观的方法,其特征在于,所述打底烘燥时间为1-2min。