CN105196722A - Method for improving adhesion between paper and printing ink - Google Patents
Method for improving adhesion between paper and printing ink Download PDFInfo
- Publication number
- CN105196722A CN105196722A CN201510634829.1A CN201510634829A CN105196722A CN 105196722 A CN105196722 A CN 105196722A CN 201510634829 A CN201510634829 A CN 201510634829A CN 105196722 A CN105196722 A CN 105196722A
- Authority
- CN
- China
- Prior art keywords
- paper
- ink
- printing ink
- dry
- adhesion
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a method for improving the adhesion between paper and printing ink. The method comprises the steps of adding a defined amount of photosensitizer to the printing ink in the first place, wherein the mass of the photosensitizer accounts for 3-8% that of the printing ink, then applying the printing ink to the surface of the paper through a printing process, finally, placing the paper which is coated with the printing ink as conducted in the previous step under ultraviolet lamplight, and conducting drying and formation. The method for improving the adhesion between the paper and the printing ink has the advantages that the photosensitizer is added to the printing ink, so that when the printing ink is dried, the drying rate is high, and the adhesion between the paper and the printing ink is accelerated.
Description
Technical field
The invention belongs to paper printing field, be specifically related to a kind of method improving paper and ink adhesion.
Background technology
In present typography, paper and ink directly print, and usually can the adhesive force of ink be followed bad due to paper surface and easily come off after causing ink setting or burst, bring press quality problem.Especially aluminium plating transfer paper and aluminizer extrusion coating paper, surface is that paper and aluminium film bond, and then prints on aluminium film, and the adhesive force of itself and ink is poorer.Be more prone to occur after ink setting, outburst comes off or the problem such as explosion.
Summary of the invention
In order to solve the problem, the invention provides a kind of method improving paper and ink adhesion, concrete technical scheme is as follows:
Improve a method for paper and ink adhesion, comprise the following steps:
Steps A: add appropriate sensitising agent in ink, sensitising agent quality is 3 ~ 8% of ink quality;
Step B: by typography, is coated in paper surface by ink;
Step C: under the paper having scribbled ink in step B is placed on ultraviolet light is dry, shaping.
In the method, first ink is transformed into light curable type ink, directly come dry by ultraviolet light, more more convenient than heating, drying, printing time shortens, and, just obtain the compact siro spinning technology that dry products can realize ink and paper surface at short notice, improve the adhesive force between paper and ink, the problem that there will not be ink to come off or burst.
Further improvement is: the sensitising agent kind added in described steps A is two kinds.
Add two kinds of sensitising agents, owing to responding to different wavelength, cooperatively interact, mutually inspire, the drying of ink can be accelerated.
Further improvement is: before carrying out typography, paper surface is coated with last layer acrylic emulsion, dries.
Because paper surface can exist rough situation, impact is had on printing, be therefore coated with last layer acrylic emulsion at paper surface, the flatness of paper surface can be strengthened.
Further improvement is: after the acrylic emulsion of paper surface is dry, then coat ionic cellulose cellulose solution, dry.
Just there is cellulosic component on plain paper surface, cellulose is the polymer with very polyhydric long-chain ring type structure, containing hydroxyl on its each chain link, hydroxyl is polar group, therefore the surface of paper is polar surfaces, containing polar molecule in main component in ink, when the polar molecule of paper, ink is close to each other, two like magnetic poles repel each other between intrinsic polarity, there is a natural attraction between the sexes, molecule is orientated by the state that heteropole is adjacent in space, intermolecular secondary adhesion makes ink be attached on paper, can strengthen the adhesive force that it is mutual.But in order to overcome the concavo-convex of paper surface, after coating acrylic emulsion, coating cellulose solution again, above-mentioned effect can be reached.
Especially for those plated surface aluminium papers, itself is in order to beautiful, surperficial smoother, in order to ink and its adhesive force in printing, also can be coated with last layer cellulose solution.
Beneficial effect of the present invention: a kind of method improving paper and ink adhesion provided by the invention, by adding sensitising agent in ink, during ink setting, rate of drying is very fast, accelerates the attachment between paper and ink.
Detailed description of the invention
In order to deepen understanding of the present invention, be described in further detail the present invention below in conjunction with embodiment, this embodiment, only for explaining the present invention, not forming protection domain and limiting.
Improve a method for paper and ink adhesion, comprise the following steps:
Steps A: add sensitising agent ethyl mercaptan and silver iodide in ink, both quality are respectively 5% and 3% of ink quality; Photosensitive wavelength range due to ethyl mercaptan is 280 ~ 400nm, and the wavelength photoreceptor of silver iodide is 420 ~ 700nm, and wave-length coverage photosensitive is between the two relatively wider, can mutually cause, and increases the effect of subsequent optical solidification.
Step B: be coated with last layer acrylic emulsion at paper surface, dries, and then coats cellulosic silver ammino solution, again dry; By coating acrylic emulsion, after drying, form rete, surface is relatively uniform, then after coating cellulose solution, after to be dried, cellulose is evenly distributed on paper surface, makes the polar functional group on its side chain and the polar substances in ink form intermolecular power, strengthens adhesion effect.
Step C: by typography, is coated in paper surface by ink;
Step D: under the paper having scribbled ink in step C is placed on ultraviolet light is dry, shaping; Dry by uviol lamp, can not only rate of drying be accelerated, and moment dry rapidly, the adhesive force between ink and paper is very large.The drying of tradition heat cure, not only speed is slow, and printed liquid is also easily affected.
Claims (4)
1. improve a method for paper and ink adhesion, it is characterized in that: comprise the following steps:
Steps A: add appropriate sensitising agent in ink, sensitising agent quality is 3 ~ 8% of ink quality;
Step B: by typography, is coated in paper surface by ink;
Step C: under the paper having scribbled ink in step B is placed on ultraviolet light is dry, shaping.
2. a kind of method improving paper and ink adhesion according to claim 1, is characterized in that: the sensitising agent kind added in described steps A is two kinds.
3. a kind of method improving paper and ink adhesion according to claim 1, is characterized in that: before carrying out typography, paper surface is coated with last layer acrylic emulsion, dries.
4. a kind of method improving paper and ink adhesion according to claim 3, is characterized in that: after the acrylic emulsion of paper surface is dry, then coat ionic cellulose cellulose solution, dry.