Prior art keywords
paint
parts
rosin
powder
phosphoric acid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410160215.XA
Other languages
Chinese (zh)
Inventor
高方周
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TONGREN GUANGCAI PAINT INDUSTRY Co Ltd
Original Assignee
TONGREN GUANGCAI PAINT INDUSTRY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TONGREN GUANGCAI PAINT INDUSTRY Co Ltd filed Critical TONGREN GUANGCAI PAINT INDUSTRY Co Ltd
Priority to CN201410160215.XA priority Critical patent/CN105176396A/en
Publication of CN105176396A publication Critical patent/CN105176396A/en
Pending legal-status Critical Current

Links

Abstract

The invention discloses a low-cost and environmental-protection paint including a paint powder, rosin, a mixture of rosin resin and linseed oil, a zeolite powder, phosphoric acid and a water solvent. The low-cost and environmental-protection paint has the beneficial effects: 1, the raw materials mainly are some common materials on markets and are easy to obtain, and the costs are not high; and 2, with addition of the phosphoric acid and rosin, the paint is quick to dry and good in viscosity, and does not fall off for a long time when an object is coated with the paint.

Description

A kind of low-cost environmental-protecting paint
Technical field
The present invention relates to a kind of low-cost environmental-protecting paint.
Background technology
The general composition of paint comprises: filmogen, pigment, solvent, auxiliary agent.Paint is that one firmly can cover body surface, plays protection, decoration, mark and the chemical mixture coating of other special purposes.More authoritative coating process one book of China's coating circle is definition like this: coating is a kind of material, and this material can be coated in article surface with different implementing process, forms adhere well, has some strength, continuous solid-state film.The film common name film of such formation, also known as paint film or coating.Belong to organic chemical industry's macromolecular material, the film formed belongs to macromolecular compound type.The classification of the Chemicals of passing through according to the modern times, coating belongs to fine chemical product.The whitewashing of modern paint not only can spread out of one taste be pungent, and can be not easy to do in the regular hour later, and very poor in viscosity, is easy to come off after exposing to wind and rain.
Summary of the invention
It is good that the technical problem to be solved in the present invention is to provide a kind of viscosity, fast drying and be applicable to using, at the paint of long-time difficult drop-off in any environment.
For achieving the above object, the invention provides following technical scheme:
A low-cost environmental-protecting paint, comprises paint powder, rosin, Gum Rosin and oleum lini mixture, zeolite powder, phosphoric acid and water solvent.
As preferred technical scheme, the content of described paint and each component is respectively:
Paint powder 20-30 part;
Rosin 5-8 part;
Gum Rosin and oleum lini mixture 10-18 part;
Zeolite powder 5-10 part;
Phosphatase 11-3 parts;
Water solvent 40-50 part.
As preferred technical scheme, the preparation process of described paint is as follows:
A) extract respectively by the deal of each content: paint 25 parts, powder, rosin 6 parts, Gum Rosin and 15 parts, oleum lini mixture, zeolite powder 7 parts, phosphoric acid 2 parts, water solvent 45 parts;
B) will paint 25 parts, powder, rosin 6 parts, zeolite powder 7 parts, water solvent 45 parts is put into processing units and is carried out, and temperature controls, at 45 DEG C-75 DEG C, then to carry out stirring 10-15 minute, makes it even, forms rarer paint;
C) then in the paint of dilution, add the Gum Rosin and 15 parts, oleum lini mixture with solidification, uniform stirring adds phosphoric acid 2 parts again after 15 minutes, is putting into equipment processed finished products paint;
D) finally paint by specific equipment be arranged on paint cylinder in.
The invention has the beneficial effects as follows:
1, raw material is mainly material common on some markets, easily obtains, and cost is not high;
2, of the present inventionly add phosphoric acid and rosin, make it paint fast drying, viscosity is good, brushes and can keep not coming off for a long time on object.
Embodiment
A low-cost environmental-protecting paint, comprises paint powder, rosin, Gum Rosin and oleum lini mixture, zeolite powder, phosphoric acid and water solvent.
Wherein, the content of described paint and each component is respectively:
Paint powder 20-30 part;
Rosin 5-8 part;
Gum Rosin and oleum lini mixture 10-18 part;
Zeolite powder 5-10 part;
Phosphatase 11-3 parts;
Water solvent 40-50 part.
The preparation process of described paint is as follows:
A) extract respectively by the deal of each content: paint 25 parts, powder, rosin 6 parts, Gum Rosin and 15 parts, oleum lini mixture, zeolite powder 7 parts, phosphoric acid 2 parts, water solvent 45 parts;
B) will paint 25 parts, powder, rosin 6 parts, zeolite powder 7 parts, water solvent 45 parts is put into processing units and is carried out, and temperature controls, at 45 DEG C-75 DEG C, then to carry out stirring 10-15 minute, makes it even, forms rarer paint;
C) then in the paint of dilution, add the Gum Rosin and 15 parts, oleum lini mixture with solidification, uniform stirring adds phosphoric acid 2 parts again after 15 minutes, is putting into equipment processed finished products paint;
D) finally paint by specific equipment be arranged on paint cylinder in.
The invention has the beneficial effects as follows: 1, raw material is mainly material common on some markets, easily obtains, and cost is not high;
2, of the present inventionly add phosphoric acid and rosin, make it paint fast drying, viscosity is good, brushes and can keep not coming off for a long time on object.
Concrete enforcement 1
A low-cost environmental-protecting paint, comprises paint powder, rosin, Gum Rosin and oleum lini mixture, zeolite powder, phosphoric acid and water solvent.
Paint powder 20-30 part; Polyvinyl alcohol contracting fourth 5-8 part; Gum Rosin and oleum lini mixture 10-18 part; Zeolite powder 5-10 part; Phosphatase 11-3 parts; Water solvent 40-50 part.
The preparation process of described paint is as follows:
A) extract respectively by the deal of each content: paint 25 parts, powder, rosin 6 parts, Gum Rosin and 15 parts, oleum lini mixture, zeolite powder 7 parts, phosphoric acid 2 parts, water solvent 45 parts;
B) will paint 25 parts, powder, rosin 6 parts, zeolite powder 7 parts, water solvent 45 parts is put into processing units and is carried out, and temperature controls, at 45 DEG C-75 DEG C, then to carry out stirring 10-15 minute, makes it even, forms rarer paint;
C) then in the paint of dilution, add the Gum Rosin and 15 parts, oleum lini mixture with solidification, uniform stirring adds phosphoric acid 2 parts again after 15 minutes, is putting into equipment processed finished products paint;
D) finally paint by specific equipment be arranged on paint cylinder in.
When through test, whitewashing through 2 months expose to wind and rain and be exposed to the sun under burning sun, is still completely set on metope on exterior wall, and therefore this formula paint is adapted at the severe environment such as countryside and uses.
Concrete enforcement 2
A low-cost environmental-protecting paint, comprises paint powder, rosin, Gum Rosin and oleum lini mixture, zeolite powder, phosphoric acid and water solvent.
Paint powder 20-30 part; Polyvinyl alcohol contracting fourth 5-8 part; Gum Rosin and oleum lini mixture 10-18 part; Zeolite powder 5-10 part; Phosphatase 11-3 parts; Water solvent 40-50 part.
The preparation process of described paint is as follows:
A) extract respectively by the deal of each content: paint 20 parts, powder, rosin 8 parts, Gum Rosin and 18 parts, oleum lini mixture, zeolite powder 7 parts, phosphoric acid 2 parts, water solvent 45 parts;
B) will paint 20 parts, powder, rosin 8 parts, zeolite powder 7 parts, water solvent 45 parts is put into processing units and is carried out, and temperature controls, at 45 DEG C-75 DEG C, then to carry out stirring 10-15 minute, makes it even, forms rarer paint;
C) then in the paint of dilution, add the Gum Rosin and 18 parts, oleum lini mixture with solidification, uniform stirring adds phosphoric acid 2 parts again after 15 minutes, is putting into equipment processed finished products paint;
D) finally paint by specific equipment be arranged on paint cylinder in.
When through test, whitewashing at home on interior wall through the time of 2 months, not through wind and hyperthermia drying, whitewash on the complete wall cohered of paint on the wall, it takes also difficult drop-off with instrument.
To those skilled in the art, obviously the invention is not restricted to the details of above-mentioned one exemplary embodiment, and when not deviating from spirit of the present invention or essential characteristic, the present invention can be realized in other specific forms.Therefore, no matter from which point, all should embodiment be regarded as exemplary, and be nonrestrictive, scope of the present invention is limited by claims instead of above-mentioned explanation, and all changes be therefore intended in the implication of the equivalency by dropping on claim and scope are included in the present invention.
In addition, be to be understood that, although this specification sheets is described according to embodiment, but not each embodiment only comprises an independently technical scheme, this narrating mode of specification sheets is only for clarity sake, those skilled in the art should by specification sheets integrally, and the technical scheme in each embodiment also through appropriately combined, can form other embodiments that it will be appreciated by those skilled in the art that.

Claims (3)

1. a low-cost environmental-protecting paint, is characterized in that: comprise paint powder, rosin, Gum Rosin and oleum lini mixture, zeolite powder, phosphoric acid and water solvent.
2. paint according to claim 1, is characterized in that: the content of described paint and each component is respectively:
Paint powder 20-30 part;
Rosin 5-8 part;
Gum Rosin and oleum lini mixture 10-18 part;
Zeolite powder 5-10 part;
Phosphatase 11-3 parts;
Water solvent 40-50 part.
3. paint according to claim 1 and 2 and preparation method thereof, is characterized in that: the preparation process of described paint is as follows:
A) extract respectively by the deal of each content: paint 25 parts, powder, rosin 6 parts, Gum Rosin and 15 parts, oleum lini mixture, zeolite powder 7 parts, phosphoric acid 2 parts, water solvent 45 parts;
B) will paint 25 parts, powder, rosin 6 parts, zeolite powder 7 parts, water solvent 45 parts is put into processing units and is carried out, and temperature controls, at 45 DEG C-75 DEG C, then to carry out stirring 10-15 minute, makes it even, forms rarer paint;
C) then in the paint of dilution, add the Gum Rosin and 15 parts, oleum lini mixture with solidification, uniform stirring adds phosphoric acid 2 parts again after 15 minutes, is putting into equipment processed finished products paint;
D) finally paint by specific equipment be arranged on paint cylinder in.
CN201410160215.XA 2014-04-22 2014-04-22 Low-cost and environmental-protection paint Pending CN105176396A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410160215.XA CN105176396A (en) 2014-04-22 2014-04-22 Low-cost and environmental-protection paint

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410160215.XA CN105176396A (en) 2014-04-22 2014-04-22 Low-cost and environmental-protection paint

Publications (1)

Publication Number Publication Date
CN105176396A true CN105176396A (en) 2015-12-23

Family

ID=54898854

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410160215.XA Pending CN105176396A (en) 2014-04-22 2014-04-22 Low-cost and environmental-protection paint

Country Status (1)

Country Link
CN (1) CN105176396A (en)

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106084939A (en) * 2016-07-12 2016-11-09 天长市银狐漆业有限公司 A kind of preparation technology of seagoing vessel red lead anti-corrosive paint
CN106883761A (en) * 2017-03-23 2017-06-23 柳州弘天科技有限公司 A kind of resistance to scraped finish paint
CN106905755A (en) * 2017-03-23 2017-06-30 柳州弘天科技有限公司 One kind paint
CN106905740A (en) * 2017-03-23 2017-06-30 柳州弘天科技有限公司 A kind of loss of weight paint
CN106916533A (en) * 2017-03-23 2017-07-04 柳州弘天科技有限公司 A kind of paint of long service life
CN106916532A (en) * 2017-03-23 2017-07-04 柳州弘天科技有限公司 A kind of quick drying paint

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106084939A (en) * 2016-07-12 2016-11-09 天长市银狐漆业有限公司 A kind of preparation technology of seagoing vessel red lead anti-corrosive paint
CN106883761A (en) * 2017-03-23 2017-06-23 柳州弘天科技有限公司 A kind of resistance to scraped finish paint
CN106905755A (en) * 2017-03-23 2017-06-30 柳州弘天科技有限公司 One kind paint
CN106905740A (en) * 2017-03-23 2017-06-30 柳州弘天科技有限公司 A kind of loss of weight paint
CN106916533A (en) * 2017-03-23 2017-07-04 柳州弘天科技有限公司 A kind of paint of long service life
CN106916532A (en) * 2017-03-23 2017-07-04 柳州弘天科技有限公司 A kind of quick drying paint

Similar Documents

Publication Publication Date Title
CN103173126A (en) Paint
CN105176396A (en) Low-cost and environmental-protection paint
CN104327559A (en) Paint coating
WO2011101364A3 (en) Composition of pigments soluble in water and/or in organic solvents
CN104694008A (en) Oil paint
CN103173121A (en) Quick drying paint and preparation method thereof
CN106543805B (en) High-solid content polyvinyl chloride film gravure white ink and preparation method thereof
CN104530788A (en) Paint
CN106590201A (en) Special-effect formaldehyde and smell removal wall finish and preparation method thereof
CN103131229B (en) Sealant used for aqueous acrylic acid ester emulsion coating and application method
CN106280663B (en) Anti-yellowing plasticizer for hot-melt marking paint and preparation method thereof
CN107868526A (en) A kind of formula of moisture-resisting lacquer
CN101875796B (en) Paint remover formula
KR101558842B1 (en) Natural paint composition
CN104151955A (en) Machine packaging coating and preparation method thereof
CN106752497A (en) A kind of indoor decorative paint
CN103725175B (en) A kind of thick-film modified alkyd paint and preparation method thereof
CN107365526A (en) One kind paint and its processing method
CN105086567B (en) One kind paints special radioresistance solvent and preparation method thereof
CN105255280A (en) Single-component acrylics waterproof coating capable of being rapidly dried on wet base layer
CN106147553A (en) A kind of environmental protection clean taste transparent priming
CN104369490B (en) The preparation method of colorful flexible brick
CN104059439A (en) Antimicrobial anticorrosive latex paint
CN107629695A (en) A kind of anti-dropout paint and its processing method
CN108373612A (en) A kind of coating and its manufacture craft

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
WD01 Invention patent application deemed withdrawn after publication
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20151223