CN104891783A - 一种玻璃电熔窑用的熔化玻璃的电极水套 - Google Patents
一种玻璃电熔窑用的熔化玻璃的电极水套 Download PDFInfo
- Publication number
- CN104891783A CN104891783A CN201510254853.2A CN201510254853A CN104891783A CN 104891783 A CN104891783 A CN 104891783A CN 201510254853 A CN201510254853 A CN 201510254853A CN 104891783 A CN104891783 A CN 104891783A
- Authority
- CN
- China
- Prior art keywords
- millimeters
- electrode
- water jacket
- pipe
- glass
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种玻璃电熔窑用的熔化玻璃的电极水套,由钢板环、钢管、进水管和出水管组成,在电极外面为钢管,钢管两端用环形钢板封闭,从封闭钢管一端的钢板环穿入两钢管,一钢管为进水管,侧壁打排眼,冷却水直接喷淋到电极,另一钢管为出水管,该电极水套克服了间接冷却电极水套冷却效果不好,易损坏电极的缺点。本发明具有结构简单,安全可靠且保护性能好等特点。
Description
技术领域
本发明涉及一种玻璃电熔窑熔化玻璃的电极水套,具体涉及一种直接冷却电极的水套。
背景技术
电极是电熔窑的关键设备,电极水套对电极保护的好坏,直接决定电容窑的寿命。目前的电极和电极水套是分开的两个独立体,水套包在电极外面,和电极之间有一间隙,故冷却效果不佳,经常出现电极由于保护不好而被氧化的事故。
发明内容
本发明的目的在于针对现有技术中的不足,提供一种结构简单,安装方便,安全可靠的直接冷却电极水套。
为解决上述技术问题,本发明的技术方案为:
一种玻璃电熔窑用的熔化玻璃的电极水套,它包括钢板环、钢管、进水管和出水管,所述钢管设置在电极外围,钢管两端用钢板环封闭,所述进水管和出水管从钢管一端的钢板环穿入,所述进水管侧壁设置若干个孔。
所述电极水套的直径在50毫米到250毫米之间。
所述钢管的直径在50毫米到250毫米之间,长度在80毫米到200毫米之间,壁厚在2毫米到20毫米之间。
所述钢板环的内径比要保护的电极的直径大1毫米到5毫米,外径在50毫米到250毫米之间。
所述钢板环的厚度在2毫米到40毫米之间。
所述进水管的直径在6毫米到50毫米之间,壁厚在1.5毫米到5毫米之间,长度在300毫米到2300毫米之间。
所述进水管沿电极一侧的母线上开有多个孔,孔径在1毫米到5毫米之间,孔与孔的间距在3毫米到20毫米之间
所述出水管的直径在6毫米到50毫米之间,壁厚在1.5毫米到5毫米之间,长度在300毫米到2300毫米之间。
所述进水管一端到钢板环内壁的距离在50毫米到100毫米之间。
所述出水管深入到钢板环内5毫米到30毫米之间。
本发明对电极直接冷却,具有如下优点:
(1)水套直接焊在电极末端,结构简单;
(2)冷却水通过进水管上设置的若干孔眼直接喷淋到所保护的电极上,冷却效果好,安全可靠。
附图说明
下面结合附图和具体实施例对本发明的内容作详细说明。
图1为本发明主视示意图。
图2为本发明俯视示意图。
具体实施方式
如附图1、2所示,电极水套由钢板环1、钢管2、进水管3、另一钢板环4和出水管5组成,钢管2的一端焊接钢板环1,另一端焊接另一钢板环4,从另一钢板环4处穿进进水管3和出水管5,钢板环1和另一钢板环4的内径比要保护的电极的直径大1毫米到5毫米,外径在50毫米到250毫米之间,厚度在2毫米到40毫米之间;钢管2的直径在50毫米到250毫米之间,长度在80毫米到200毫米之间,壁厚在2毫米到20毫米之间;进水管3和出水管5的直径在6毫米到50毫米之间,壁厚在1.5毫米到5毫米之间,长度在300毫米到2300毫米之间;进水管3一端到钢板环1的距离在50毫米到100毫米之间,钢管2内的进水管3沿电极一侧的母线上开有多个孔7,孔径在1毫米到5毫米之间,孔与孔的间距在3毫米到20毫米之间,出水管5深入到钢管2内5毫米到30毫米之间。
冷却水从进水管3进去,直接喷到电极上,对其进行充分的冷却,然后从出水管5排出。
以上显示和描述了本发明的基本原理和主要特征和本发明的优点。本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下,本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内。本发明要求保护范围由所附的权利要求书及其等效物界定。
Claims (10)
1.一种玻璃电熔窑用的熔化玻璃的电极水套,其特征在于:它包括钢板环、钢管、进水管和出水管,所述钢管设置在电极外围,钢管两端用钢板环封闭,所述进水管和出水管从钢管一端的钢板环穿入,所述进水管侧壁设置若干个孔。
2.根据权利要求1所述的一种玻璃电熔窑用的熔化玻璃的电极水套,其特征在于:所述电极水套的直径在在50毫米到250毫米之间。
3.根据权利要求1所述的一种玻璃电熔窑用的熔化玻璃的电极水套,其特征在于:所述钢管的直径在50毫米到250毫米之间,长度在80毫米到200毫米之间,壁厚在2毫米到20毫米之间。
4.根据权利要求1所述的一种玻璃电熔窑用的熔化玻璃的电极水套,其特征在于:所述钢板环的内径比要保护的电极的直径大1毫米到5毫米,外径在50毫米到250毫米之间。
5.根据权利要求1所述的一种玻璃电熔窑用的熔化玻璃的电极水套,其特征在于:所述钢板环的厚度在2毫米到40毫米之间。
6.根据权利要求1所述的一种玻璃电熔窑用的熔化玻璃的电极水套,其特征在于:所述进水管的直径在6毫米到50毫米之间,壁厚在1.5毫米到5毫米之间,长度在300毫米到2300毫米之间。
7.根据权利要求1所述的一种玻璃电熔窑用的熔化玻璃的电极水套,其特征在于:所述进水管沿电极一侧的母线上开有多个孔,孔径在1毫米到5毫米之间,孔与孔的间距在3毫米到20毫米之间。
8.根据权利要求1所述的一种玻璃电熔窑用的熔化玻璃的电极水套,其特征在于:所述出水管的直径在6毫米到50毫米之间,壁厚在1.5毫米到5毫米之间,长度在300毫米到2300毫米之间。
9.根据权利要求1所述的一种玻璃电熔窑用的熔化玻璃的电极水套,其特征在于:所述进水管一端到钢板环内壁的距离在50毫米到100毫米之间。
10.根据权利要求1所述的一种玻璃电熔窑用的熔化玻璃的电极水套,其特征在于:所述出水管深入到钢板环内5毫米到30毫米之间。