CN104845426A - Novel fireproof coating - Google Patents

Novel fireproof coating Download PDF

Info

Publication number
CN104845426A
CN104845426A CN201510197863.7A CN201510197863A CN104845426A CN 104845426 A CN104845426 A CN 104845426A CN 201510197863 A CN201510197863 A CN 201510197863A CN 104845426 A CN104845426 A CN 104845426A
Authority
CN
China
Prior art keywords
fire retardant
fireproof coating
novel
novel fireproof
diatomite
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510197863.7A
Other languages
Chinese (zh)
Inventor
何益庆
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tongling Xiangyun Fire Fighting Technology Co Ltd
Original Assignee
Tongling Xiangyun Fire Fighting Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tongling Xiangyun Fire Fighting Technology Co Ltd filed Critical Tongling Xiangyun Fire Fighting Technology Co Ltd
Priority to CN201510197863.7A priority Critical patent/CN104845426A/en
Publication of CN104845426A publication Critical patent/CN104845426A/en
Pending legal-status Critical Current

Abstract

The invention discloses a novel fireproof coating. The novel fireproof coating comprises 40-50% of an inorganic filler, 20-30% of an adhesive, 20-30% of an additive, 10-20% of a solvent and 10-20% of a fire retardant. The fire retardant comprises 13-14% of antimony dioxide, 0.2-0.3% of ammonium sulfate, 10-20% of magnesium hydroxide, 10-20% of citric acid, and the balance of diatomite. The novel fireproof coating appropriately integrating various fireproof components can continuously perform fireproofing and protection effects, increases the flame retardation effect of a coat layer and prolongs the effective fireproof time of the coat layer; and the fire retardant has the advantages of reasonable formula, low cost and good flame retardation effect.

Description

A kind of Novel fire retardant coating
Technical field
The present invention relates to fire-proof product field, specifically a kind of Novel fire retardant coating.
Background technology
Expanding fire-proof paint is the frie retardant coating kind be most widely used at present, after expanding fire-proof paint film forming, common paint film at normal temperatures, under flame or high temperature action, coating expands charing, form the original thickness of ratio large tens times even the cell foams shape carbonaceous layer do not fired of hundred times, fire retardant module can cut off the heating of extraneous burning things which may cause a fire disaster to base material, thus plays fire retardation.
At present, known a lot of articles for daily use comprise furniture, floor, wallpaper etc., and it, while bringing practicality, attractive in appearance, fashion for life, also also exists a lot of hidden danger; Produce a large amount of obnoxious flavoures during burning, it is unfavorable not only to bring the healthy safety of people, also destroys the ecotope of periphery simultaneously.Although fire retardant is widely used in all respects of life, when fire-retardant finish is carried out to article, still there is new technical problem.
Summary of the invention
A kind of Novel fire retardant coating, it consists of: mineral filler 40% ~ 50%, tackiness agent 20% ~ 30%, additive 20% ~ 30%, solvent 10% ~ 20%, fire retardant 10% ~ 20%.Consisting of of described fire retardant: tellurium dioxide 13% ~ 14%, amine sulfate 0.2% ~ 0.3%, magnesium hydroxide 10% ~ 20%, citric acid 10% ~ 20%, all the other are diatomite.
As further scheme, described fire retardant is mixed by the composition of following volume ratio and forms, and tellurium dioxide 13.5%, amine sulfate 0.25%, magnesium hydroxide 15%, citric acid 15%, all the other are diatomite.
Compared with prior art, the invention has the beneficial effects as follows: the appropriate cooperation of the multiple fire-resistant composition of Novel fire retardant coating collection provided by the invention, the effect of sustainable performance flameproof protection, increase the flame retardant effect of coating and extend effective fire prevention time of coating; The formula of fire retardant is reasonable, with low cost, good flame retardation effect.
Embodiment
Below in conjunction with the embodiment of the present invention, be clearly and completely described the technical scheme in the embodiment of the present invention, obviously, described embodiment is only the present invention's part embodiment, instead of whole embodiments.Based on the embodiment in the present invention, those of ordinary skill in the art, not making the every other embodiment obtained under creative work prerequisite, belong to the scope of protection of the invention.
A kind of Novel fire retardant coating, it consists of: mineral filler 40% ~ 50%, tackiness agent 20% ~ 30%, additive 20% ~ 30%, solvent 10% ~ 20%, fire retardant 10% ~ 20%.Consisting of of described fire retardant: tellurium dioxide 13% ~ 14%, amine sulfate 0.2% ~ 0.3%, magnesium hydroxide 10% ~ 20%, citric acid 10% ~ 20%, all the other are diatomite.The appropriate cooperation of the multiple fire-resistant composition of Novel fire retardant coating collection provided by the invention, the effect of sustainable performance flameproof protection, increases the flame retardant effect of coating and extends effective fire prevention time of coating; The formula of fire retardant is reasonable, with low cost, good flame retardation effect.
As further scheme, described fire retardant is mixed by the composition of following volume ratio and forms, and tellurium dioxide 13.5%, amine sulfate 0.25%, magnesium hydroxide 15%, citric acid 15%, all the other are diatomite.
To those skilled in the art, obviously the invention is not restricted to the details of above-mentioned one exemplary embodiment, and when not deviating from spirit of the present invention or essential characteristic, the present invention can be realized in other specific forms.Therefore, no matter from which point, all should embodiment be regarded as exemplary, and be nonrestrictive, scope of the present invention is limited by claims instead of above-mentioned explanation, and all changes be therefore intended in the implication of the equivalency by dropping on claim and scope are included in the present invention.
In addition, be to be understood that, although this specification sheets is described according to embodiment, but not each embodiment only comprises an independently technical scheme, this narrating mode of specification sheets is only for clarity sake, those skilled in the art should by specification sheets integrally, and the technical scheme in each embodiment also through appropriately combined, can form other embodiments that it will be appreciated by those skilled in the art that.

Claims (2)

1. a Novel fire retardant coating, is characterized in that, it consists of: mineral filler 40% ~ 50%, tackiness agent 20% ~ 30%, additive 20% ~ 30%, solvent 10% ~ 20%, fire retardant 10% ~ 20%.Consisting of of described fire retardant: tellurium dioxide 13% ~ 14%, amine sulfate 0.2% ~ 0.3%, magnesium hydroxide 10% ~ 20%, citric acid 10% ~ 20%, all the other are diatomite.
2. a kind of Novel fire retardant coating according to claim 1, is characterized in that, described fire retardant is mixed by the composition of following volume ratio and forms, and tellurium dioxide 13.5%, amine sulfate 0.25%, magnesium hydroxide 15%, citric acid 15%, all the other are diatomite.
CN201510197863.7A 2015-04-23 2015-04-23 Novel fireproof coating Pending CN104845426A (en)