CN104816422A - 一种乳胶制品生产工艺 - Google Patents

一种乳胶制品生产工艺 Download PDF

Info

Publication number
CN104816422A
CN104816422A CN201510200407.3A CN201510200407A CN104816422A CN 104816422 A CN104816422 A CN 104816422A CN 201510200407 A CN201510200407 A CN 201510200407A CN 104816422 A CN104816422 A CN 104816422A
Authority
CN
China
Prior art keywords
powder
latex
weight ratio
ratio
latex product
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201510200407.3A
Other languages
English (en)
Other versions
CN104816422B (zh
Inventor
吴清照
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wenzhou super Thailand latex products Co., Ltd.
Original Assignee
吴清照
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 吴清照 filed Critical 吴清照
Priority to CN201510200407.3A priority Critical patent/CN104816422B/zh
Publication of CN104816422A publication Critical patent/CN104816422A/zh
Application granted granted Critical
Publication of CN104816422B publication Critical patent/CN104816422B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种乳胶制品生产工艺,其特征在于包括以下步骤:①将乳胶溶液、赭石粉和远红外陶瓷粉以一定重量比混合在一起;②将上述混合溶液和氧化锌、凝固剂加入到发泡设备,根据发泡密度需要加入适量空气,制成A料;③将乳胶溶液、磁石粉和负离子粉以一定重量比混合在一起;④将上述混合溶液和氧化锌、凝固剂以一定重量比加入到发泡设备,根据发泡密度需要加入适量空气,制成B料;⑤取合适A料、B料先后加入模具;⑥模具放到蒸箱内进行热蒸。采用上述生产工艺制得的乳胶制品,与纯天然乳胶制品无异,赭石粉、远红外陶瓷粉、磁石粉和负离子粉合理添加,具有平肝息风、远红外辐射、磁疗和负离子的保健作用,可广泛应用于枕头、床垫等床上用品。

Description

一种乳胶制品生产工艺
【技术领域】
本发明涉及一种乳胶制品生产工艺。
【背景技术】
随着人们生活水平的提高,纯天然乳胶制成的枕头、床垫作为一种高档床上用品,已经越来越多的进入普通百姓人家,天然乳胶具有防螨防菌、良好透气性和吸湿性,其独特的柔软触觉和乳胶高弹性能够顺应人体头部及身体轮廓,不仅更符合了长久的睡眠习惯,更让天然乳胶制品带给使用者健康舒适的睡眠。另外,市场上其它的各种非乳胶保健枕头、保健床垫也不断涌现,它们为提高睡眠质量、人体保健确实也起到一定的作用,其中含有赭石的床垫,它是依靠在床垫表面铺设赭石片来实现的,赭石具有平肝息风的保健作用,但是如果把赭石片直接应用到乳胶枕头或床垫上,显然就会破坏乳胶独特的柔软触觉,因此需要将赭石片磨成粉末添加到乳胶中。但是,赭石粉与乳胶完全混合,不仅需要大量的赭石粉,而赭石粉只是与人体靠近的部位才能体现其真正的平肝息风的保健作用,这样就造成赭石浪费,更为重要的是,乳胶枕头、床垫中往往会添加磁石粉,磁石粉具有磁疗的保健作用,如果磁石粉与赭石粉混合,它们会磁性相吸并结块,不能与乳胶充分混合,不仅影响乳胶制品质量,同时起不到应有的保健作用;另外,为增加保健功能,有些乳胶枕头、床垫中往往还会添加负离子粉,负离子粉在乳胶中的分布密度小,起不到应有的保健作用,而如果分布密度大,整个乳胶枕头、床垫中需要加入大量的负离子粉,根本没有必要,也会造成浪费。同样,远红外陶瓷粉在常温区具有红外线辐射、促进和改善人体血液循环的保健作用,但如何在乳胶中合理进行添加也是目前存在的问题。
【发明内容】
为解决背景技术存在的不足,本发明是采取如下技术方案来实现的:
一种乳胶制品生产工艺,其特征在于包括以下步骤:①将60%固态含量的乳胶溶液、赭石粉和远红外陶瓷粉以重量比100∶1.5∶1.5的比例混合在一起高速搅拌,搅拌速度300转/分钟,时间25分钟;②将上述制得的混合溶液和氧化锌、凝固剂以重量比100∶2.5∶1.5的比例一起加入到发泡设备进行发泡,根据发泡密度需要加入适量空气,制成A料;③将60%固态含量的乳胶溶液、磁石粉和负离子粉以重量比100∶1.5∶2.0的比例混合在一起高速搅拌,搅拌速度300转/分钟,时间25分钟;④将上述制得的混合溶液和氧化锌、凝固剂以重量比100∶2.5∶1.5的比例一起加入到发泡设备进行发泡,根据发泡密度需要加入适量空气,制成B料;⑤取合适B料加入模具,再取合适A料覆盖在B料上面,A料重量不超过总重量的二分之一;⑥模具放到蒸箱内进行热蒸,A料、B料蒸熟后开模取出乳胶制品的成品。
采用上述技术方案后,首先制作A料、B料作为备用,A料中富含赭石粉和远红外陶瓷粉,B料中富含磁石粉和负离子粉,赭石粉、远红外陶瓷粉、磁石粉和负离子粉合理添加,不会造成浪费,利于环保,同时赭石粉和磁石粉互不影响,负离子粉具有高分布密度,除赭石粉、远红外陶瓷粉、磁石粉和负离子粉不同外,A料、B料中的其它组份相同,然后将A料、B料按先后顺序加入到模具中随模具一起热蒸,蒸熟后A料、B料的乳胶部分已完全合为一体,于是制成的乳胶制品与普通纯天然乳胶无异,但赭石粉存在于乳胶表面,与人体靠近起到良好的平肝息风的保健作用,负离子粉存在于乳胶底部,由于具有高分布密度,所以能够起到理想的负离子的保健作用,而远红外陶瓷粉在乳胶中起到促进和改善人体血液循环的保健作用,磁石粉起到磁疗保健作用。在上述的乳胶制品的生产过程中,氧化锌起到乳胶硫化的作用,凝固剂起到乳胶凝固的作用。
【具体实施方式】
本发明的乳胶制品生产工艺,包括以下步骤:①将60%固态含量的乳胶溶液赭石粉和远红外陶瓷粉以重量比100∶1.5∶1.5的比例混合在一起放到搅拌机内高速搅拌,搅拌速度300转/分钟,时间25分钟;②将上述制得的混合溶液和氧化锌、凝固剂(选用氟硅酸钠)以重量比100∶2.5∶1.5的比例一起加入到发泡设备进行发泡,根据发泡密度需要加入适量空气,搅拌10秒时间,温度控制在32℃,制成A料;③将60%固态含量的乳胶溶液、磁石粉和负离子粉以重量比100∶1.5∶2.0的比例混合在一起放到搅拌机内高速搅拌,搅拌速度300转/分钟,时间25分钟;④将上述制得的混合溶液和氧化锌、凝固剂(选用氟硅酸钠)以重量比100∶2.5∶1.5的比例一起加入到发泡设备进行发泡,根据发泡密度需要加入适量空气,搅拌10秒时间,温度控制在32℃,制成B料;⑤取合适B料加入模具,再取合适A料覆盖在B料上面,A料重量不超过总重量的二分之一;⑥模具放到蒸箱内进行热蒸,A料、B料蒸熟后开模取出乳胶制品的成品。

Claims (1)

1.一种乳胶制品生产工艺,其特征在于包括以下步骤:①将60%固态含量的乳胶溶液、赭石粉和远红外陶瓷粉以重量比100∶1.5∶1.5的比例混合在一起高速搅拌,搅拌速度300转/分钟,时间25分钟;②将上述制得的混合溶液和氧化锌、凝固剂以重量比100∶2.5∶1.5的比例一起加入到发泡设备进行发泡,根据发泡密度需要加入适量空气,制成A料;③将60%固态含量的乳胶溶液、磁石粉和负离子粉以重量比100∶1.5∶2.0的比例混合在一起高速搅拌,搅拌速度300转/分钟,时间25分钟;④将上述制得的混合溶液和氧化锌、凝固剂以重量比100∶2.5∶1.5的比例一起加入到发泡设备进行发泡,根据发泡密度需要加入适量空气,制成B料;⑤取合适B料加入模具,再取合适A料覆盖在B料上面,A料重量不超过总重量的二分之一;⑥模具放到蒸箱内进行热蒸,A料、B料蒸熟后开模取出乳胶制品的成品。
CN201510200407.3A 2015-04-21 2015-04-21 一种乳胶制品生产工艺 Active CN104816422B (zh)