CN104804579A - Interior wall paint for sleep improvement - Google Patents

Interior wall paint for sleep improvement Download PDF

Info

Publication number
CN104804579A
CN104804579A CN201410246236.3A CN201410246236A CN104804579A CN 104804579 A CN104804579 A CN 104804579A CN 201410246236 A CN201410246236 A CN 201410246236A CN 104804579 A CN104804579 A CN 104804579A
Authority
CN
China
Prior art keywords
essential oil
latex paint
low voc
wall latex
sleep
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410246236.3A
Other languages
Chinese (zh)
Inventor
陶伟钧
邢俊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Bauhinia Coating (shanghai) Co Ltd
Original Assignee
Bauhinia Coating (shanghai) Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Bauhinia Coating (shanghai) Co Ltd filed Critical Bauhinia Coating (shanghai) Co Ltd
Priority to CN201410246236.3A priority Critical patent/CN104804579A/en
Publication of CN104804579A publication Critical patent/CN104804579A/en
Pending legal-status Critical Current

Abstract

The invention relates to aqueous interior wall eco-friendly emulsion paint which has low volatile organic compound (VOC) content and a sleep improvement function. The aqueous interior wall eco-friendly emulsion paint comprises, by weight, 10-25% of rutile-type titanium dioxide, 20-35% of a filler, 10-30% of an acrylic polymer emulsion, 1-2% of a high-boiling point film forming auxiliary agent, 0.2-2% of a thickening agent, 0.5-2% of a dispersant, 0.2-0.6% of a wetting agent, 0.3-0.6% of an antifoaming agent, 0.1-0.3% of a high-boiling point pH conditioning agent, 0.2-0.5% of an antiseptic, 0.01-5% of an adsorbent, 0.01-2% of compound essential oil and the balance water. The aqueous interior wall eco-friendly emulsion paint has conventional performances of the interior wall emulsion paint, has the characteristics of low VOC content, safety, environmental friendliness and good fragrance, has functions of tranquilizing and allaying excitement and improving sleep, is prepared from common and easily available raw materials, can be prepared by simple and convenient processes, and is suitable for industrial production.

Description

A kind of interior wall coating contributing to improving water flood
Technical field
The present invention relates to the wallcovering of indoor wall finishing, be specifically related to a kind of low VOC and help sleep interiro wall latex paint.
Background technology
Modern society's work rhythm is nervous, and the pressure of people is large, and a lot of people has suffered from the illness of insomnia.The normal spiritedness of insomniac is depressed, fatigue and weak, irritated, and dizzy, cardio palmus shape, badly influences the health of people, work and life.Annual March 21 is decided to be by UNESCO " international sleep day ", arouses the understanding of the whole people to sleep importance whereby.Therefore, how improving water flood quality is a problem highly furtherd investigate.At present, the method for improving water flood has a variety of, but great majority are calm class medicines, to human body toxic side effect, and champignon essence oil is as more novel mode, with its natural environmental-protective, smell is pure and fresh, easy to use, the advantages such as manufacture craft is simple, more and more receive publicity and accreditation.
Interiro wall latex paint is the common used material of Modern Family's finishing, VOC (volatile organic compounds) be wherein mainly contain harmful substances, can cause damage to HUMAN HEALTH when the VOC in room reaches finite concentration, national standard also has strict limitation requirement to the VOC content in interiro wall latex paint.
Along with the raising day by day of people's level of consumption, propose more functional requirements for interiro wall latex paint, client is also more and more higher for the requirement of environmental-protecting performance simultaneously.Therefore, how the functional of interiro wall latex paint and the feature of environmental protection to be organically combined, be the problem highly furtherd investigate.
Summary of the invention
A kind of low VOC is the object of the present invention is to provide to help sleep interiro wall latex paint, especially for the interiro wall latex paint being applied to bedroom finishing, on the basis keeping currently available products traditional performance, increase smell pure and fresh, the function of improving water flood, and VOC is lower, more environmental protection.
In the present invention's formula, what use is all not containing VOC or the very low starting material of VOC content, according to the detection method of present national standard " in GB 18582-2008 interior wall coating limits of harmful substances-compulsory standard ", VOC content not only substandard limitation 120g/L in the present invention's formula, more lower than the detection limit 2g/L of this detection method, can be assessed as " not detecting ", environmental-protecting performance is excellent.
In the present invention's formula, the compound essential oil of use is mixed by sandalwood essential oil, lavender essential oil, frankincense essential oil and sweet orange oil, wherein sandalwood essential oil has a kind of fragrant and sweet smell, and the calm speciality of tool, can pacify nervous and anxiety, people is loosened, helps to fall asleep; Lavender essential oil can tranquilizing and allaying excitement, pacifies palpitaition, improves headache, dizzy; Frankincense essential oil distributes warm pure wooden fragrance, appears again light fruital, can make us experiencing have no precedent loosen and releive, to spirit, frightened and anxious state of mind has sedation effect, can help in meditation; Sweet orange oil has dazzling warm sunlight speciality, gentle sweet perfume (or spice) breath, can expel intense strain and pressure, improve insomnia caused by anxiety.By these four kinds of essential oil mixing, compound essential oil sustained release dosage made by remix sorbent material, adds in interiro wall latex paint, after being painted on metope, slowly release the smell that essential oil is special, people can touch essential oil by inhaling the mode of hearing, thus reach effect of improving water flood.
The present invention designs a kind of low VOC and helps sleep interiro wall latex paint, it is characterized in that being made up of following constituent and weight percent:
Rutile type Titanium Dioxide (imperial boa titanium dioxide R-996) 10 ~ 25%,
Filler 20 ~ 35%,
Acrylate polymer emulsion 10 ~ 30%,
High boiling point film coalescence aid 1 ~ 2%,
Thickening material 0.2 ~ 2%,
Dispersion agent 0.5 ~ 2%,
Wetting agent 0.2 ~ 0.6%,
Defoamer (BASF FoamStar A10) 0.3 ~ 0.6%,
High boiling point pH adjusting agent 0.1 ~ 0.3%,
Sanitas (Bristol ACTICIDE MBS) 0.2 ~ 0.5%,
Sorbent material 0.01 ~ 5%,
Compound essential oil 0.01 ~ 2%,
Water surplus
Described acrylate polymer emulsion, be pure third, phenylpropyl alcohol or vinegar the third, preferred DOW Chemical DC-423V emulsion, this emulsion smell is low, and VOC content is very low, at below 500ppm.
Described filler is water-ground limestone, talcum powder, kaolin.
Described high boiling point film coalescence aid is Tri(propylene glycol)butyl ether,mixture of isomers, and this raw material boiling point is 274 DEG C, detects temperature 250 DEG C higher than coating VOC in national standard.
Described thickening material is Mierocrystalline cellulose or polyurethanes, the blue Natrosol 250HBR of preferred sub-bodyguard, or DOW Chemical ACRYSOL RM-8W.
Described dispersion agent is sodium polyacrylate salt, and preferably gloomy SUPERDES 680 likes in France.
Described wetting agent is phosphate ester surfactant, preferred Clariant Corporation Dispersogen LFA.
Described high boiling point pH adjusting agent is amine substance, preferred Taminco company VANTEX-T, and this raw material boiling point is 283 DEG C, detects temperature 250 DEG C higher than coating VOC in national standard.
Described sorbent material is one or more mixture of calcite, diatomite, precipitated silicate calcium, wilkinite, bamboo charcoal powder.
Described compound essential oil is the mixture of sandalwood essential oil, lavender essential oil, frankincense essential oil and sweet orange oil.
The invention provides the preparation method that described low VOC helps sleep interiro wall latex paint, comprise the following steps:
(1) sorbent material is mixed with compound essential oil, with the speed high speed dispersion of 1500 revs/min, obtain compound essential oil sustained release dosage.
(2) water, dispersion agent, wetting agent, defoamer, Rutile type Titanium Dioxide, filler are mixed, within 1200 revs/min of high speed dispersion to particle diameter 50 microns, add acrylate polymer emulsion, high boiling point film coalescence aid, sanitas, add the said compound essential oil sustained release dosage of step (1) again, middling speed 700 revs/min dispersion ten minutes, adjust ph is to 8 ~ 9, regulate KU viscosity to 100 ± 2, filter and package.
Beneficial effect of the present invention is:
(1) low VOC of the present invention helps sleep interiro wall latex paint, compares now common on the market interiro wall latex paint, adds the function of improving water flood.And what the present invention adopted is plants essential oil that is nontoxic, safety and environmental protection, reaches slowly-releasing effect by adsorbent, extend the action time of essential oil.
(2) low VOC of the present invention helps sleep interiro wall latex paint, and VOC (volatile organic compounds) content is very low, more health environment-friendly.
(3) raw material of the present invention is common, is easy to buy, and technique is simple, convenient operation, is applicable to suitability for industrialized production.
Embodiment
Below in conjunction with specific embodiment, the invention will be further described.Should be understood that following examples only for illustration of the present invention but not for limiting scope of the present invention.The experimental technique of unreceipted actual conditions in the following example, usually conveniently condition, or the condition that manufacturer provides is carried out.
Embodiment 1
Get sorbent material diatomite 5kg, sandalwood essential oil 20kg, Herba Lysimachiae foenumgraeci quintessence oil 5kg, frankincense essential oil 10kg, sweet orange oil 8kg, with the speed high speed dispersion of 1500 revs/min, obtain compound essential oil sustained release dosage.
19 kg water are added successively in mixed cylinder, 0.5 kg.p.m. powder, 0.4 kilogram of wetting agent, 2 kilograms of high boiling point film coalescence aid, 0.3 kilogram of defoamer, 23 kilograms of Rutile type Titanium Dioxides, 8 kilograms of kaolin, 14 kilograms of water-ground limestones, after powder all adds, stir 5 minutes, add 0.5 kg of fibers element thickening material again, notice that Mierocrystalline cellulose interpolation speed can not be too fast in case cause powder to reunite, after Mierocrystalline cellulose all adds, rotating speed is adjusted to 1200 revs/min, high speed dispersion 30 minutes, detect fineness≤50um then to have disperseed, rotating speed is adjusted to 700 revs/min, add 30 kilograms of acrylate polymer emulsions successively, 0.5 kilogram of sanitas, 1 kilogram of compound essential oil sustained release dosage, in addition, available high boiling point pH adjusting agent, regulate the pH value that product is final, reach requirement with polyurethane thickener and water adjusting viscosity simultaneously, filter and package and can obtain low VOC of the present invention and help sleep interiro wall latex paint.The coating that the program makes, " GB/T 9756-2009 resin latex dope " premium grads index can be met, and meet " in GB 18582-2008 interior wall coating limits of harmful substances-compulsory standard " require and VOC detected result for " not detecting ".
Embodiment 2
Get sorbent material wilkinite 4kg, sandalwood essential oil 20kg, Herba Lysimachiae foenumgraeci quintessence oil 5kg, frankincense essential oil 10kg, sweet orange oil 8kg, with the speed high speed dispersion of 1500 revs/min, obtain compound essential oil sustained release dosage
33 kg water are added successively in mixed cylinder, 0.6 kg.p.m. powder, 0.2 kilogram of wetting agent, 1 kilogram of high boiling point film coalescence aid, 0.3 kilogram of defoamer, 10 kilograms of Rutile type Titanium Dioxides, 6 kilograms of kaolin, 4 kilograms of talcum powder, 25 kilograms of water-ground limestones, after powder all adds, stir 5 minutes, add 0.6 kg of fibers element thickening material again, notice that Mierocrystalline cellulose interpolation speed can not be too fast in case cause powder to reunite, after Mierocrystalline cellulose all adds, rotating speed is adjusted to 1200 revs/min, high speed dispersion 30 minutes, detect fineness≤50um then to have disperseed, rotating speed is adjusted to 700 revs/min, add 12 kg of polymer emulsions successively, 0.2 kilogram of sanitas, 1 kilogram of compound essential oil sustained release dosage, in addition, available high boiling point pH adjusting agent, regulate the pH value that product is final, reach requirement with polyurethane thickener and water adjusting viscosity simultaneously, filter and package and can obtain low VOC of the present invention and help sleep interiro wall latex paint.The coating that the program makes, " GB/T 9756-2009 resin latex dope " acceptable end product index can be met, and meet " in GB 18582-2008 interior wall coating limits of harmful substances-compulsory standard " require and VOC detected result for " not detecting ".
In above-described embodiment, Rutile type Titanium Dioxide is imperial boa titanium dioxide R-996.
Filler is water-ground limestone, talcum powder, kaolin.
Acrylate polymer emulsion, be pure third, phenylpropyl alcohol or vinegar Class C, preferred DOW Chemical DC-423V emulsion, this emulsion smell is low, and VOC content is very low, at below 500ppm.
High boiling point pH adjusting agent is amine substance, preferred Taminco company VANTEX-T, and this raw material boiling point is 283 DEG C, detects temperature 250 DEG C higher than coating VOC in national standard.
Thickening material is Mierocrystalline cellulose or polyurethanes, the blue Natrosol 250HBR of preferred sub-bodyguard, or DOW Chemical ACRYSOL RM-8W.
Dispersion agent is sodium polyacrylate salt, and preferably gloomy SUPERDES 680 likes in France.
Wetting agent is phosphate ester surfactant, preferred Clariant Corporation Dispersogen LFA.
Defoamer is BASF FoamStar A10.
High boiling point pH adjusting agent is amine substance, preferred Taminco company VANTEX-T, and this raw material boiling point is 283 DEG C, detects temperature 250 DEG C higher than coating VOC in national standard.
Sanitas is Bristol ACTICIDE MBS.
Sorbent material is one or more mixture of calcite, diatomite, precipitated silicate calcium, wilkinite, bamboo charcoal powder.
Compound essential oil is the mixture of sandalwood essential oil, lavender essential oil, frankincense essential oil and sweet orange oil.
Water is water purification.
Low VOC of the present invention helps sleep interiro wall latex paint using method identical with conventional interior wall coating, and by brushing, roller coat and this several frequently seen mode of spraying, construct on metope.

Claims (11)

1. low VOC helps a sleep interiro wall latex paint, it is characterized in that being made up of following constituent and weight percent:
Rutile type Titanium Dioxide 10 ~ 25%,
Filler 20 ~ 35%,
Acrylate polymer emulsion 10 ~ 30%,
High boiling point film coalescence aid 1 ~ 2%,
Thickening material 0.2 ~ 2%,
Dispersion agent 0.5 ~ 2%,
Wetting agent 0.2 ~ 0.6%,
Defoamer 0.3 ~ 0.6%,
High boiling point pH adjusting agent 0.1 ~ 0.3%,
Sanitas 0.2 ~ 0.5%,
Sorbent material 0.01 ~ 5%,
Compound essential oil 0.01 ~ 2%,
Water surplus.
2. helping sleep interiro wall latex paint by the low VOC of one according to claim 1, it is characterized in that described acrylate polymer emulsion, is pure third, phenylpropyl alcohol or vinegar the third, preferred DOW Chemical DC-423V emulsion.
3. help sleep interiro wall latex paint by the low VOC of one according to claim 1, it is characterized in that described filler is water-ground limestone, talcum powder, kaolin.
4. help sleep interiro wall latex paint by the low VOC of one according to claim 1, it is characterized in that described high boiling point film coalescence aid is Tri(propylene glycol)butyl ether,mixture of isomers.
5. help sleep interiro wall latex paint by the low VOC of one according to claim 1, it is characterized in that described thickening material is Mierocrystalline cellulose or polyurethanes, the blue Natrosol 250HBR of preferred sub-bodyguard, or DOW Chemical ACRYSOL RM-8W.
6. help sleep interiro wall latex paint by the low VOC of one according to claim 1, it is characterized in that described dispersion agent is sodium polyacrylate salt, preferably gloomy SUPERDES 680 likes in France.
7. help sleep interiro wall latex paint by the low VOC of one according to claim 1, it is characterized in that described wetting agent is phosphate ester surfactant, preferred Clariant Corporation Dispersogen LFA.
8. help sleep interiro wall latex paint by the low VOC of one according to claim 1, it is characterized in that described high boiling point pH adjusting agent is amine substance, preferred Taminco company VANTEX-T.
9. help sleep interiro wall latex paint by the low VOC of one according to claim 1, it is characterized in that described sorbent material is one or more mixture of calcite, diatomite, precipitated silicate calcium, wilkinite, bamboo charcoal powder.
10. help sleep interiro wall latex paint by the low VOC of one according to claim 1, it is characterized in that described compound essential oil is the mixture of sandalwood essential oil, lavender essential oil, frankincense essential oil and sweet orange oil.
11. help the preparation method of sleep interiro wall latex paint by low VOC a kind of described in claim 1, it is characterized in that comprising the following steps:
(1) sorbent material is mixed with compound essential oil, with the speed high speed dispersion of 1500 revs/min, obtain compound essential oil sustained release dosage.
(2) water, dispersion agent, wetting agent, defoamer, Rutile type Titanium Dioxide, filler are mixed, within 1200 revs/min of high speed dispersion to particle diameter 50 microns, add acrylate polymer emulsion, high boiling point film coalescence aid, sanitas, add the said compound essential oil sustained release dosage of step (1) again, middling speed 700 revs/min dispersion ten minutes, adjust ph is to 8 ~ 9, regulate KU viscosity to 100 ± 2, filter and package.
CN201410246236.3A 2014-06-05 2014-06-05 Interior wall paint for sleep improvement Pending CN104804579A (en)