CN104692609A - 适用真空脱水的土水混合物配药方法 - Google Patents
适用真空脱水的土水混合物配药方法 Download PDFInfo
- Publication number
- CN104692609A CN104692609A CN201310683888.9A CN201310683888A CN104692609A CN 104692609 A CN104692609 A CN 104692609A CN 201310683888 A CN201310683888 A CN 201310683888A CN 104692609 A CN104692609 A CN 104692609A
- Authority
- CN
- China
- Prior art keywords
- water mixture
- soil
- extraction
- vacuum hydro
- dispensing method
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
土水混合物因其含水率高,给土水混合物的储存、运输及土的再利用带来诸多不便。为解决土水混合物难以脱水的问题,本发明提供一种适用真空脱水的土水混合物配药方法。在土水混合物内加入土水混合物重量0.05%-0.8%的碳化钙,碳化钙与土水混合物中的水产生化学反应,生成氢氧化钙和乙炔。经机械均匀搅拌,使乙炔溶于土水混合物产生气隙,使土水混合物能适用于真空脱水。
Description
技术领域
本发明涉及一种土水混合物真空脱水的配药方法,更具体说涉及含水量在30%-80%之间的污泥、淤泥、泥浆的真空脱水前需进行预先调理的配药方法。
技术背景
土水混合物因其含水率高,给土水混合物的储存、运输及土的再利用带来诸多不便。
目前,土水混合物脱水的外加剂分为两类,一类是无机絮凝剂,另一类是有机高分子絮凝剂。这两类均存在成本高、不适用于真空脱水处理的缺点。因此,急需开发低成本并适用于真空脱水的外加剂。
发明内容
本发明目的在于提供一种适用真空脱水的土水混合物配药方法。
本发明的设计原理是在土水混合物内加入土水混合物重量0.05%-0.8%的碳化钙(CaC),碳化钙与土水混合物中的水产生化学反应,生成氢氧化钙(Ca(OH)2)和乙炔(C2H2)。经机械均匀搅拌,使乙炔溶于土水混合物产生气隙,使土水混合物能适用于真空脱水。
本发明适用真空脱水的土水混合物配药方法的使用方法如下:将碳化钙粉粹成直径5mm左右的颗粒状,土水混合物在机械搅拌机内搅拌,边搅拌边加碳化钙,搅拌3分钟即可制成适用于真空脱水的土水混合物,经真空脱水机脱水后使土水分离。
具体实施方法
实施例1
取气密性较好的污水处理厂剩余污泥,含水量60%,真空脱水后得到泥饼厚度3mm,含水35%。
实施例2
取气密性较好的污水处理厂剩余污泥,含水量60%,加入污泥重量0.1%的碳化钙,搅拌均匀,真空脱水后得到泥饼厚度5mm,含水20%,比原污泥真空脱水后得到泥饼厚度增加2mm,含水率降低15%。
实施例3
取气密性较好的污水处理厂剩余污泥,含水量60%,加入污泥重量0.2%的碳化钙,搅拌均匀,真空脱水后得到泥饼厚度6mm,含水20%,比原污泥真空脱水后得到泥饼厚度增加3mm,含水率降低15%。
实施例4
取气密性较好的污水处理厂剩余污泥,含水量60%,加入污泥重量0.3%的碳化钙,搅拌均匀,真空脱水后得到泥饼厚度7mm,含水20%,比原污泥真空脱水后得到泥饼厚度增加4mm,含水率降低15%。
实施例5
取气密性较好的污水处理厂剩余污泥,含水量60%,加入污泥重量0.4%的碳化钙,搅拌均匀,真空脱水后得到泥饼厚度8mm,含水19%,比原污泥真空脱水后得到泥饼厚度增加5mm,含水率降低16%。
实施例6
取气密性较好的污水处理厂剩余污泥,含水量60%,加入污泥重量0.5%的碳化钙,搅拌均匀,真空脱水后得到泥饼厚度9mm,含水19%,比原污泥真空脱水后得到泥饼厚度增加6mm,含水率降低16%。
实施例7
取气密性较好的污水处理厂剩余污泥,含水量60%,加入污泥重量0.6%的碳化钙,搅拌均匀,真空脱水后得到泥饼厚度10mm,含水18%,比原污泥真空脱水后得到泥饼厚度增加7mm,含水率降低17%。
Claims (1)
1.一种适用真空脱水的土水混合物配药方法,其特征是:土水混合物内均匀加入土水混合物重量0.05%-0.8%的碳化钙。