CN104147746A - 一种飞灰固化处理方法 - Google Patents

一种飞灰固化处理方法 Download PDF

Info

Publication number
CN104147746A
CN104147746A CN201410343468.0A CN201410343468A CN104147746A CN 104147746 A CN104147746 A CN 104147746A CN 201410343468 A CN201410343468 A CN 201410343468A CN 104147746 A CN104147746 A CN 104147746A
Authority
CN
China
Prior art keywords
cement
metering device
fly ash
conveying
flying dust
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410343468.0A
Other languages
English (en)
Inventor
陈庆林
胡达科
金豪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GUANGDONG HESTIA ENERGY SAVING & ENVIRONMENT PROTECTION Co Ltd
Original Assignee
GUANGDONG HESTIA ENERGY SAVING & ENVIRONMENT PROTECTION Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GUANGDONG HESTIA ENERGY SAVING & ENVIRONMENT PROTECTION Co Ltd filed Critical GUANGDONG HESTIA ENERGY SAVING & ENVIRONMENT PROTECTION Co Ltd
Priority to CN201410343468.0A priority Critical patent/CN104147746A/zh
Publication of CN104147746A publication Critical patent/CN104147746A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种飞灰固化处理方法,主要用于垃圾焚烧后产生的飞灰处理,该方法是这样实现的:飞灰从飞灰储罐送出到计量装置进行计量输送,水泥从水泥储罐送出到计量装置进行计量输送,螯合剂进行计量输送,然后,从计量装置输送出来的飞灰、水泥和上螯合剂均输送进混炼机里进行混合搅拌,搅拌后出来的成品在养护后送填埋场作填埋处理;本发明旨在提供一种处理过程简单、设备投资少、水泥用量少且稳定的飞灰固化处理方法。

Description

一种飞灰固化处理方法
技术领域
本发明涉及固废处理技术领域,具体地说,尤其涉及一种飞灰固化处理方法,主要用于垃圾焚烧后产生的飞灰处理。
背景技术
近几年来,随着我国经济建设和城市建设的高速发展,城市框架越来越大,人口不断增加,生活垃圾量也日益俱增,许多城市未对垃圾分类分倒,垃圾成份复杂,水分高,热值不稳定,使垃圾处理较为困难,垃圾三化处理已成为我国各级政府面临的重要问题。因此越来越多的城市已建或在建设生活垃圾焚烧厂,全国每年产生大量的焚烧飞灰,它不仅富集Pb、Cd、Hg等低沸点重金属,而且也是致癌祸首,在世界范围内被公认为是一种危害性较大的废弃物,而目前处理这些飞灰的方法主要有水泥固化、熔融固化和化学药剂稳定三种方法,水泥固化技术在经济性和可操作方面具有明显的优势,但水泥的用量高,导致固化体增容率高,随着时间推移,固化体部分有毒物质可能会逐渐溶出,对环境存在长期的、潜在的威胁;熔融固化技术对残渣的减容率高,固化效果好,但缺点是部分有毒物质会挥发出来,必须采取尾气处理措施,所以其系统较复杂,运行成本高;化学药剂稳定技术具有处理过程简单,设备投资少等优点,但会产生高浓度无机盐废水,需要进一步处理。
发明内容
本发明的目的是克服现有技术中的不足之处,提供一种处理过程简单、设备投资少、水泥用量少且稳定的飞灰固化处理方法。
本发明的技术方案是这样实现的:一种飞灰固化处理方法,包括:首先飞灰从飞灰储罐送出到计量装置进行计量输送,水泥从水泥储罐送出到计量装置进行计量输送,有机物从有机物储罐送出到计量装置进行计量输送到液体混合机,同时水也从水储罐输送到液体混合机里,有机物和水混合成的混合物被送到计量装置里进行计量输送,然后,从计量装置输送出来的飞灰、水泥和上述的混合物均输送进混炼机里进行混合搅拌,搅拌后出来的成品送去作填埋处理。
上述的一种飞灰固化处理方法中,所述的有机物为一种螯合高分子物,该螯合高分子物与水混合后即得螯合剂,该螯合剂中的水比例为16%~23%,螯合高分子物比例为1%~2%。
上述的一种飞灰固化处理方法中,所述的水泥比例为17%~20%,所述的飞灰比例为59%~62%。
本发明的有益效果是:本发明通过螯合剂与飞灰中的易溶性金属反应形成稳定的络合物,进而固定在飞灰和水泥中,从而降低飞灰中有害成分的析出,使填埋处理更安全,而且该方法过程简单,用的水泥和螯合剂比例少即可处理大量的飞灰,降低成本。
附图说明
图1是本发明的飞灰处理的流程图。
具体实施方式
下面结合实施例和附图对本发明进一步详细的描述,但本发明创造的实施方式不限于此。
如图1所示的一种飞灰固化处理方法,首先飞灰从飞灰储罐送出到计量装置进行计量输送,水泥从水泥储罐送出到计量装置进行计量输送,有机物从有机物储罐送出到计量装置进行计量输送到液体混合机,同时水也从水储罐输送到液体混合机里,有机物和水混合成的混合物被送到计量装置里进行计量输送,所述的有机物为一种螯合高分子物,该螯合高分子物与水混合后即得出螯合剂,然后,从计量装置输送出来的飞灰、水泥和上述的混合物均输送进混炼机里进行混合搅拌,在计量过程中,其最佳比例分别是:水泥比例为17%~20%,飞灰比例为59%~62%,水比例为16%~23%,螯合高分子物比例为1%~2%;在混炼机混合搅拌过程中,螯合剂与飞灰中的易溶性金属发生反应,其中飞灰中的易溶性金属包括有Pb、Cd等,这些易溶性金属与螯合剂发生反应产生稳定性络合物,进而固定在飞灰与水泥的混合物里,从而降低飞灰中有害成分的析出,从混炼机混合处理后的成品送去作填埋处理。
使用本发明的方法后作填埋处理更安全,而且该方法过程简单,用的水泥和螯合剂比例少即可处理大量的飞灰,降低成本。

Claims (3)

1.一种飞灰固化处理方法,其特征在于,该飞灰固化处理方法包括:首先飞灰从飞灰储罐送出到计量装置进行计量输送,水泥从水泥储罐送出到计量装置进行计量输送,有机物从有机物储罐送出到计量装置进行计量输送到液体混合机,同时水也从水储罐输送到液体混合机里,有机物和水混合成的混合物被送到计量装置里进行计量输送,然后,从计量装置输送出来的飞灰、水泥和上述的混合物均输送进混炼机里进行混合搅拌,搅拌后出来的成品送去作填埋处理。
2.根据权利要求1所述的一种飞灰固化处理方法,其特征在于,所述的有机物为一种螯合高分子物,该螯合高分子物与水混合后即得螯合剂,该螯合剂中的水比例为16%~23%,螯合高分子物比例为1%~2%。
3.根据权利要求1所述的一种飞灰固化处理方法,其特征在于,所述的水泥比例为17%~20%,所述的飞灰比例为59%~62%。
CN201410343468.0A 2014-07-18 2014-07-18 一种飞灰固化处理方法 Pending CN104147746A (zh)