CN104608544A - Manufacturing method of cloth-cut picture product and cloth-cut picture product - Google Patents

Manufacturing method of cloth-cut picture product and cloth-cut picture product Download PDF

Info

Publication number
CN104608544A
CN104608544A CN201310579159.9A CN201310579159A CN104608544A CN 104608544 A CN104608544 A CN 104608544A CN 201310579159 A CN201310579159 A CN 201310579159A CN 104608544 A CN104608544 A CN 104608544A
Authority
CN
China
Prior art keywords
cloth
fabric
cutting
hot pressing
picture
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201310579159.9A
Other languages
Chinese (zh)
Other versions
CN104608544B (en
Inventor
肖丽荣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tianjin City Shear Bushaw Technology Co Ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201310579159.9A priority Critical patent/CN104608544B/en
Publication of CN104608544A publication Critical patent/CN104608544A/en
Application granted granted Critical
Publication of CN104608544B publication Critical patent/CN104608544B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

Embodiments in the invention disclose a manufacturing method of a cloth-cut picture product. The method comprises the following steps: employing a tightening agent for tightening original fabrics; hot-pressing an adhesive film to the back side of the fabrics after tightening treatment, cooling the fabrics after hot-pressing and pressing the fabrics flatly; and carving a pattern on the cooled fabrics by laser to obtain an exquisite cloth pattern like paper-cut. By using the embodiments in the invention, a cloth-cut picture with lines not liable to break, paper-cut effect, abundant details and fine and smooth lines is acquired, and a detail degree can reach 1mm. The cloth-cut picture is pressed on a cloth product made of fabrics such as cotton, chemical fiber, a knitting material and a tatting material, and a problem that the edge of the product bifurcates after washing does not exist.

Description

A kind of cloth of cutting is drawn the preparation method of product and cuts cloth picture product
Technical field
The present invention relates to the art work, artistic ornament and dress ornament garment technology field, particularly one is cut the making of cloth picture and compression method and is cut cloth and draws product.
Background technology
Paper-cut is loved by the people as a kind of folk art, but when paper-cut craft being applied on existing fabric or the fabric after prior art process, there is the problem that lines easily rupture, be difficult to depict on fabric there is paper-cut effect, detailed information is enriched, the cloth of cutting of lines exquisiteness is drawn, and therefore needs further development as the paper-cut of Traditional Folk Art.
In addition, existing cloth picture of cutting can be pressed together in the cloth products such as various dress ornament, bedding, Bu Bao, cloth shoes, but, existing cloth picture of cutting is pressed together in cloth products, after washing, easily occurs the problem of edge bifurcated.
Summary of the invention
The embodiment of the invention discloses a kind of cloth of cutting draw the preparation method of product and cut cloth picture product, with depict on fabric lines not easy fracture, the cloth of cutting with paper-cut effect draw, and the cloth of cutting preventing from being pressed together in cloth products is drawn occur edge bifurcation problem after washing.
For achieving the above object, the embodiment of the invention discloses a kind of preparation method of cutting cloth picture product, described method comprises:
With deflation agent, deflation process is carried out to original fabric;
By glued membrane hot pressing to the fabric back tightened after process, and cooling processing is carried out to the fabric after hot pressing;
Portray pattern with on the fabric of laser after cooling processing, obtain cutting cloth and draw.
Preferably, described deflation agent carries out deflation process to original fabric, comprising:
Heat water to 40-70 degree Celsius;
Add described deflation agent in water after the heating, obtain after mixing well tightening the agent aqueous solution;
Original fabric is soaked in 0.5-2 hour in the described deflation agent aqueous solution;
By soak after fabric draining and smooth oven dry, open-width.
Preferably, described original fabric is: silk-like fabric.
Preferably, the preparation method of cutting cloth picture product described in comprises further:
Described cloth picture of cutting is positioned on substrate fabric;
According to the temperature preset, pressure and time, described cloth picture of cutting is pressed together on substrate fabric.
Preferably, described substrate fabric is the cloth cover of any one product following: dress ornament, bedding, the tablecloth, cloth shoes, Bu Bao, substrate cloth of mounting a picture.
Preferably, when described substrate fabric is any one cloth cover in dress ornament, bedding, the tablecloth, cloth shoes or cloth bag,
Described by the silk-like fabric back side after glued membrane hot pressing to deflation process, comprising:
Be that the glued membrane of 4-10 silk is with the fabric back after the temperature hot pressing of 80-100 degree Celsius to deflation process by PUR thickness.
Preferably, described cloth of cutting is drawn and is pressed together on substrate fabric by temperature, pressure and time that described basis is preset, comprising:
With the pressure of the temperature of 110-190 degree Celsius and 5-100 newton, within the time of 5-30 second, described cloth of cutting is drawn and is pressed together on substrate fabric.
Preferably, when described substrate fabric is when mounting a picture the cloth cover of substrate cloth,
Described by the fabric back after glued membrane hot pressing to deflation process, comprising:
Be that the glued membrane of 0.1-0.2 silk is with the fabric back after the temperature hot pressing of 50-80 degree Celsius to deflation process by glue thickness of mounting a picture.
Preferably, described cloth of cutting is drawn and is pressed together on substrate fabric by temperature, pressure and time that described basis is preset, comprising:
With the pressure of the temperature of 110-130 degree Celsius and 5-50 newton, within the time of 10-15 second, described cloth of cutting is drawn and is pressed together on substrate fabric.
For achieving the above object, the embodiment of the invention discloses a kind of cloth of cutting utilizing above-mentioned a kind of preparation method of cutting cloth picture product to make and drawing product.
From above technical scheme, the present invention program, by carrying out the mode tightening process and fabric back hot pressing glued membrane after treatment to original fabric, make this fabric can by laser incising draw lines not easy fracture, there is paper-cut effect, details is enriched, lines exquisiteness cut cloth draw, this is cut cloth picture to be pressed together on after on cloth products, there will not be edge bifurcation problem through washing.
Accompanying drawing explanation
In order to be illustrated more clearly in the embodiment of the present invention or technical scheme of the prior art, be briefly described to the accompanying drawing used required in embodiment or description of the prior art below, apparently, accompanying drawing in the following describes is only some embodiments of the present invention, for those of ordinary skill in the art, under the prerequisite not paying creative work, other accompanying drawing can also be obtained according to these accompanying drawings.
Fig. 1 a is that the edge diagram of product after washing drawn by existing cloth of cutting;
Fig. 1 b is that the edge diagram of product after washing drawn by the cloth of cutting that application the present invention program obtains;
A kind of schematic flow sheet cutting the preparation method of cloth picture product that Fig. 2 provides for the embodiment of the present invention;
Fig. 3 cuts the schematic flow sheet that the preparation method of product drawn by cloth for another kind that the embodiment of the present invention provides.
Detailed description of the invention
Below in conjunction with the accompanying drawing in the embodiment of the present invention, be clearly and completely described the technical scheme in the embodiment of the present invention, obviously, described embodiment is only the present invention's part embodiment, instead of whole embodiments.Based on the embodiment in the present invention, those of ordinary skill in the art, not making the every other embodiment obtained under creative work prerequisite, belong to the scope of protection of the invention.
In practical application, cutting cloth paintings is that ornament is widely used in cloth products, is making in the process of cutting cloth picture, when cut cloth draw lines exquisiteness time, easily there is the problem of wire fractures, therefore, common cloth of cutting draws general lines comparatively slightly, is difficult to the effect reaching paper-cut picture.Traditional cloth picture of cutting is pressed together in various cloth products, after washing, easily there is the problem of edge bifurcated, bifurcated as shown in fig. ia, if the lines cutting cloth picture are comparatively thick, the problem of edge bifurcated can be alleviated by the mode of lock seaming of embroidering, but when lines are thinner, then be difficult to be addressed this problem by lock seaming, and the method cost is high.
Embodiments provide a kind of cloth of cutting draw the preparation method of product and cut cloth picture product, in this programme, deflation process is carried out to original fabric, and fabric back hot pressing glued membrane after treatment, portray pattern finally by laser fabric after treatment, obtain cutting cloth and draw.Application the present invention program, can also cut cloth and draw and be pressed together on substrate fabric, obtains other and cuts cloth and draw product, these cut in cloth picture product to cut cloth picture case beautiful, wash rear smooth, do not shrink.
Cloth of cutting in the embodiment of the present invention is drawn product and can be drawn for cutting cloth, also can have the cloth products of cutting cloth and drawing for pressing, and such as, pressing has cuts dress ornament, the pressing that cloth draws and have sheet, the sportswear of cutting cloth picture, etc.
What application the present invention program obtained cuts cloth picture product, is pressed together in various cloth products, after washing, there will not be the problem of edge bifurcated, as shown in Figure 1 b.
In addition, what application the present invention program obtained cuts cloth picture product, detect through authoritative department, fiber content, content of formaldehyde, pH value, the color fastness of resistance to dry friction, color fastness to water, colour fastness to perspiration, peculiar smell, decomposable asymmetric choice net aromatic amine dyestuff all meet state specified standards parameter request, especially decomposable asymmetric choice net aromatic amine dyestuff wherein belongs to prohibitive dye in textile industry, and draws in product do not detect this dyestuff at the cloth of cutting that application the present invention program obtains.
Below by specific embodiment, the present invention is described in detail.
A kind of schematic flow sheet cutting the preparation method of cloth picture product that Fig. 2 provides for the embodiment of the present invention, the method comprises the following steps:
Step 101: deflation process is carried out to original fabric with deflation agent.
Wherein, original fabric refers to undressed fabric.In embodiments of the present invention, original fabric can select silk-like fabric.Silk is the zephyr of the plain weave obtained through special process and special finishing with polyster fibre long filament, and it has the outward appearance of similar real silk, gloss, soft feature.
Preferably, original fabric can select organizine to be: 3303 points of special row superfine denier polyester back twistings 2400 twists/m, tram is: 33.3 points of special row superfine denier polyester forwards twist the silk-like fabric of 3600 twists/m, find that this silk-like fabric is applied in the present invention can obtain preferably effect through many experiments.
Certainly, the application is just described for above-mentioned, and in practical application, original fabric is not limited in silk-like fabric, selects the silk-like fabric being also not limited only to during silk-like fabric select to meet above-mentioned organizine, tram parameter.
In practical application, tightening agent is a kind of milky thick liquid, and ph value is 7-7.5.
In this deflation agent preparation process, the mass percent of various raw material is as follows:
Acrylonitrile, mass percent is 1.8-17%; Leveler 102, mass percent is 2%; NMA, mass percent is 3-6%; Lauryl sodium sulfate, mass percent is 2%; Butyl acrylate, mass percent is 70-80%; Ammonium persulfate, mass percent is 0.2-0.5%; Resin of thickening and protecting glue, mass percent is 5-20%.
The preparation process of this deflation agent comprises the following steps:
According to above-mentioned raw materials proportioning, add water, leveler 102 and lauryl sodium sulfate successively in a kettle., stir 0.5 hour, material in polymeric kettle is fully dissolved, wherein water is 1.5 times of all raw material total amounts in pulp furnish, in practical application, can according to circumstances material in rapid stirring polymeric kettle, fully dissolve to make material in polymeric kettle; In polymeric kettle, add butyl acrylate, acrylonitrile, NMA successively, every quality is 25% of every mass ratio in above-mentioned raw materials proportioning, and stirs; Add the initiator ammonium persulfate aqueous solution, its quality is 10% of mass ratio in above-mentioned raw materials proportioning; Heated polymerizable still to 80 degree Celsius; In polymeric kettle, add remaining butyl acrylate, acrylonitrile, NMA and ammonium sulfate successively, in practical application, above-mentioned raw materials can be added according to the change of temperature and the extent of reaction at 0.5-1.5 hour; With the heating temperatures polymeric kettle 1-1.5 hour of 82-85 degree Celsius; Cooling polymeric kettle to 70 degree Celsius; In polymeric kettle, add protecting glue polyvinyl alcohol water solution and thickener ammonium acrylate according to pulp furnish, wherein the ratio of protecting glue and thickener is 1:1, can suitably adjust this ratio in practical application according to actual conditions; Material 0.5-1 hour in polymeric kettle is distilled under the pressure of 48kpa; Cooling polymeric kettle and interior material thereof are to room temperature; By ammoniacal liquor adjustment ph value to 7-7.5, obtain deflation agent.
The deflation agent obtained according to above-mentioned steps need reach: solid content (quality) percentage is 30-50%, and pH value is the quality index of 7-7.5.
When deflation process being carried out to original fabric with this deflation agent, first, heat water to 40-70 degree Celsius; Add this deflation agent in water after the heating again, obtain tightening the agent aqueous solution after mixing well, wherein, the ratio tightening agent and water can be 1:50-1:10, wherein, learns that this ratio is that 1:20 effect is better through many experiments; Original fabric is soaked in and tightens 0.5-2 hour in the agent aqueous solution, repeatedly stir evenly and original fabric is soaked in the deflation agent aqueous solution completely, wherein, learn that immersion 1 hour effect is better through many experiments; Finally by soak after fabric draining and smooth oven dry, open-width.It should be noted that, when adding deflation agent in water after the heating, can slowly add, soluble in water preferably to ensure tightening agent.
After above-mentioned deflation process, the organizine of fabric and tram are all reinforced and more crypto set, thus not easy fracture, such as, but fabric has contracting width to a certain degree, the fabric width of original fabric is 1.5 meters, by the oven dry of this fabric, open-width to 1.3 meter after tightening process, also, this fabric fabric width after tightening process is 1.3 meters.Meanwhile, the shade fabric after this deflation agent process is bright-coloured, soft, and wear resistance is high, and color fastness is high.
Step 102: by glued membrane hot pressing to the fabric back tightened after process, and cooling processing is carried out to the fabric after hot pressing.
In practical application, glued membrane comprises hot melt adhesive film, glued membrane etc. type of mounting a picture, and according to the preferred embodiment of the present invention, for dissimilar glued membrane, its corresponding glue can select different thickness to reach optimum efficiency in actual applications respectively.Such as: in hot melt adhesive film, the thickness of PUR can be 6-8 silk, the thickness drawing in glued membrane glue of mounting a picture can be 0.1-0.2 silk etc.
When hot pressing glued membrane, different hot pressing temperatures can be selected according to the different-thickness of glue in glued membrane, such as: when PUR thickness is 6-8 silk, the hot pressing temperature of 80-100 degree Celsius can be selected; When glue thickness of mounting a picture is 0.1-0.2 silk, hot pressing temperature of 50-80 degree Celsius etc. can be selected.
Certainly, the application is just described for above-mentioned, and the hot pressing temperature in practical application in glued membrane, glued membrane when the thickness of glue and hot pressing glued membrane is all not limited only to the situation of foregoing description.
In this step, fabric back refers in the two sides of fabric, and non-producer specifies the one side will presenting to user.Such as, in the two sides of some fabric, it is smooth that one side has fabric, and brightly painted feature, then producer can specify and user is presented in this face, then another side is the back side of fabric.
Step 103: portray pattern with on the fabric of laser after cooling processing, obtains cutting cloth and draws.
Enrich because traditional paper-cut picture has detailed information, the feature of lines exquisiteness, therefore, according to when pattern portrayed by the fabric of paper-cut craft after cooling processing in practical application, thinner laser need be selected to portray, such as, the laser incising picture case that line thickness can be made to reach 1 millimeter is selected.
As seen from the above, in the present invention program, original fabric is after tightening process, the organizine of fabric and tram become more crypto set and not easily rupture, again after the process of hot pressing glued membrane, this fabric can be drawn by laser incising there is paper-cut effect, details is enriched, the cloth of cutting of lines exquisiteness draws, and this is cut cloth and draw and be pressed together in cloth products, after washing, this is cut cloth and draws the problem that there will not be edge bifurcated.
Fig. 3 cuts the schematic flow sheet that the preparation method of product drawn by cloth for another kind that the embodiment of the present invention provides, and the method comprises the following steps.
Step 201: deflation process is carried out to original fabric with deflation agent.
Step 202: by glued membrane hot pressing to the fabric back tightened after process, and cooling processing is carried out to the fabric after hot pressing.
Step 203: portray pattern with on the fabric of laser after cooling processing, obtains cutting cloth and draws.
It should be noted that, step 201 ~ step 203 in the embodiment of the present invention, can be identical with middle step 101 ~ step 103 embodiment illustrated in fig. 2 respectively, no longer repeat here.
Step 204: described cloth picture of cutting is positioned on substrate fabric.
In this step, substrate fabric can be any one in cloth products, such as, and any one cloth cover etc. in dress ornament, bedding, the tablecloth, cloth shoes, Bu Bao or substrate cloth of mounting a picture.Wherein, the fabric of cloth products can be knitting class fabric, tatting class fabric, chemical fibre class fabric or cotton class fabric etc., and certainly, the application is just described for above-mentioned, and in practical application, the fabric kind of cloth products is not limited thereto.
Traditional calligraphy and painting mostly is paper drawing, and after paper drawing suspension time length, both sides easily bending, out-of-flatness, and the easy moisture absorption of paper drawing, Keep away from sun.But cloth is drawn then different, cloth is drawn long-term suspension and be there will not be that both sides are bending, irregular problem, and is not afraid of tide also not Keep away from sun.Therefore, this can be cut cloth picture and be applied in the technology of mounting a picture, using the cloth cover of substrate cloth of mounting a picture as substrate fabric, be made into mounting cloth and draw.Wherein, the cloth cover of substrate cloth of mounting a picture can be substrate damask fabric, but is not limited in this.
Step 205: described cloth picture of cutting is pressed together on substrate fabric according to the temperature preset, pressure and time.
Because substrate fabric material is different, not identical with the time by cutting the temperature, the pressing pressure that need when cloth is drawn and is pressed together on substrate fabric yet.
In a kind of detailed description of the invention of the present invention, when described substrate fabric is the cloth cover of any one in dress ornament, bedding, the tablecloth, cloth shoes or cloth bag, can be that the glued membrane of 4-10 silk is with the fabric back after the temperature hot pressing of 80-100 degree Celsius to deflation process by PUR thickness.Find through multiple comparison test in practical application, PUR thickness is that after the glued membrane hot pressing of 6-8 silk, effect is better.
Obtaining cutting after cloth draws, will cut cloth and draw when being pressed together on substrate fabric, with the pressure of the temperature of 110-190 degree Celsius and 5-100 newton, can will cut cloth picture and be pressed together on substrate fabric in the time of 5-30 second.
It should be noted that, pressing-in temp, pressing time and pressing pressure can according to substrate fabric, cut the cloth thickness etc. that draws lines and suitably adjust.
Such as, when various substrates fabric, hot pressing temperature, hot pressing time and hot pressing pressure are respectively:
When substrate fabric is cotton, hot pressing temperature is 150-190 degree Celsius, and hot pressing time is 15-25 second, and hot pressing pressure is 20-100 newton, and wherein, hot pressing temperature is 160-180 degree Celsius, and hot pressing time is 20 seconds, and hot pressing pressure is 30-60 Newtonian time best results;
When substrate fabric is chemical fiber plus material, hot pressing temperature is, 130-150 degree Celsius, and hot pressing time is 10-20 second, and hot pressing pressure is 5-50 newton, and wherein, hot pressing temperature is 140-150 degree Celsius, and hot pressing time is 15 seconds, and hot pressing pressure is 5-30 Newtonian time best results;
When substrate fabric is quick-drying shell fabric, hot pressing temperature is 110-150 degree Celsius, and hot pressing time is 5-15 second, and hot pressing pressure is 5-50 newton, and wherein, hot pressing temperature is 120-140 degree Celsius, and hot pressing time is 10 seconds, and hot pressing pressure is 5-30 Newtonian time best results.
When substrate fabric is identical, according to cut cloth draw line weight, pressing time is suitably adjusted, when cut cloth draw lines thinner time, reduce hot pressing time, otherwise, cut cloth draw lines thicker time, increase hot pressing time.
Such as, substrate fabric for cotton, cut cloth be depicted as meticulous lines cut cloth draw time, hot pressing temperature is 150-190 degree Celsius, hot pressing time is 5-20 second, hot pressing pressure is 20-100 newton, and wherein, hot pressing temperature is 160-180 degree Celsius, hot pressing time is 10-15 second, and hot pressing pressure is 30-60 Newtonian time best results.
In another kind of detailed description of the invention of the present invention, when substrate fabric is when mounting a picture the cloth cover of substrate cloth, can be by glue thickness of mounting a picture the glued membrane of 0.1-0.2 silk with the temperature hot pressing of 50-80 degree Celsius to the fabric back tightened after process.
Obtaining cutting after cloth draws, will cut cloth and draw when being pressed together on substrate fabric, with the pressure of the temperature of 110-130 degree Celsius and 5-50 newton, within the time of 10-15 second, described cloth picture of cutting can be pressed together on substrate fabric.
Those skilled in the art are understandable that, when cutting cloth picture and be pressed together on substrate fabric, cut whether cloth picture location for paste has projection, whether whether having obviously infiltration light sensation and firm sense to judge, cutting cloth picture is firmly pasted onto on fabric by observing.
As seen from the above, the present invention program, by carrying out the mode tightening process and fabric back hot pressing glued membrane after treatment to original fabric, make this fabric can by laser incising draw lines not easy fracture, there is paper-cut effect, details is enriched, lines exquisiteness cut cloth draw, this is cut cloth picture to be pressed together on after on cloth products, there will not be edge bifurcation problem through washing.
In one embodiment of the present of invention, can obtain one according to the method provided embodiment illustrated in fig. 2 and cut cloth picture product, this is cut cloth picture product and can be pressed together in various cloth products, plays good decoration function.When this product detailed information is abundant, lines are fine and smooth, not easily there is the situation of wire fractures, the effect of paper-cut picture can be reached, and after washing, there will not be edge bifurcation problem.
In an alternative embodiment of the invention, one can be obtained according to the method provided embodiment illustrated in fig. 3 and cut cloth picture product, this product is that pressing has the cloth products of cutting cloth and drawing on cloth cover, and such as, pressing has the various dress ornaments, bedding, tablecloth, Bu Bao, cloth shoes etc. cutting cloth and draw.This is cut the cloth of cutting that cloth draws in product and draws and can reach that detailed information is enriched, the paper-cut picture effect of lines exquisiteness, and there will not be the problem of edge bifurcated after washing.In addition, according to the different fabrics of cloth products, the technological parameters such as the pressing time in adjustable process of producing product, pressing-in temp, pressing pressure, film thickness, therefore this is cut cloth picture product and can produce many derived products, is applied to the every aspect of life.This cut cloth draw product with the product quality of asepsis environment-protecting for theory, have essential distinction with the chemical printing technology product such as screen printing, offset printing.And compared with chemical Printing, it is more bright-coloured beautiful that this cuts cloth picture product pattern color, and surface is more smooth agile.
It should be noted that, in this article, the such as relational terms of first and second grades and so on is only used for an entity or operation to separate with another entity or operating space, and not necessarily requires or imply the relation that there is any this reality between these entities or operation or sequentially.And, term " comprises ", " comprising " or its any other variant are intended to contain comprising of nonexcludability, thus make to comprise the process of a series of key element, method, article or equipment and not only comprise those key elements, but also comprise other key elements clearly do not listed, or also comprise by the intrinsic key element of this process, method, article or equipment.When not more restrictions, the key element limited by statement " comprising ... ", and be not precluded within process, method, article or the equipment comprising described key element and also there is other identical element.
The foregoing is only preferred embodiment of the present invention, be not intended to limit protection scope of the present invention.All any amendments done within the spirit and principles in the present invention, equivalent replacement, improvement etc., be all included in protection scope of the present invention.

Claims (10)

1. cut the preparation method that product drawn by cloth, it is characterized in that, described method comprises:
With deflation agent, deflation process is carried out to original fabric;
By glued membrane hot pressing to the fabric back tightened after process, and cooling processing is carried out to the fabric after hot pressing;
Portray pattern with on the fabric of laser after cooling processing, obtain cutting cloth and draw.
2. method according to claim 1, is characterized in that, described deflation agent carries out deflation process to original fabric, comprising:
Heat water to 40-70 degree Celsius;
Add described deflation agent in water after the heating, obtain after mixing well tightening the agent aqueous solution;
Original fabric is soaked in 0.5-2 hour in the described deflation agent aqueous solution;
By soak after fabric draining and smooth oven dry, open-width.
3. method according to claim 1, is characterized in that, described original fabric is: silk-like fabric.
4. the method according to any one of claims 1 to 3, is characterized in that, described method comprises further:
Described cloth picture of cutting is positioned on substrate fabric;
According to the temperature preset, pressure and time, described cloth picture of cutting is pressed together on substrate fabric.
5. method according to claim 4, is characterized in that, described substrate fabric is the cloth cover of any one product following: dress ornament, bedding, the tablecloth, cloth shoes, Bu Bao, substrate cloth of mounting a picture.
6. method according to claim 5, is characterized in that, when described substrate fabric is any one cloth cover in dress ornament, bedding, the tablecloth, cloth shoes or cloth bag,
Described by the silk-like fabric back side after glued membrane hot pressing to deflation process, comprising:
Be that the glued membrane of 4-10 silk is with the fabric back after the temperature hot pressing of 80-100 degree Celsius to deflation process by PUR thickness.
7. method according to claim 6, is characterized in that, described cloth of cutting is drawn and is pressed together on substrate fabric by temperature, pressure and time that described basis is preset, comprising:
With the pressure of the temperature of 110-190 degree Celsius and 5-100 newton, within the time of 5-30 second, described cloth of cutting is drawn and is pressed together on substrate fabric.
8. method according to claim 5, is characterized in that, when described substrate fabric is when mounting a picture the cloth cover of substrate cloth,
Described by the fabric back after glued membrane hot pressing to deflation process, comprising:
Be that the glued membrane of 0.1-0.2 silk is with the fabric back after the temperature hot pressing of 50-80 degree Celsius to deflation process by glue thickness of mounting a picture.
9. method according to claim 8, is characterized in that, described cloth of cutting is drawn and is pressed together on substrate fabric by temperature, pressure and time that described basis is preset, comprising:
With the pressure of the temperature of 110-130 degree Celsius and 5-50 newton, within the time of 10-15 second, described cloth of cutting is drawn and is pressed together on substrate fabric.
10. product drawn by the cloth of cutting utilizing the method as described in any one of claim 1 to 9 to make.
CN201310579159.9A 2013-11-18 2013-11-18 A kind of cloth of cutting draws the preparation method of product and cuts cloth picture product Active CN104608544B (en)