CN104592910A - Chloroprene rubber adhesive - Google Patents
Chloroprene rubber adhesive Download PDFInfo
- Publication number
- CN104592910A CN104592910A CN201310525574.6A CN201310525574A CN104592910A CN 104592910 A CN104592910 A CN 104592910A CN 201310525574 A CN201310525574 A CN 201310525574A CN 104592910 A CN104592910 A CN 104592910A
- Authority
- CN
- China
- Prior art keywords
- chloroprene rubber
- rubber adhesive
- portions
- resin
- adhesive
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a chloroprene rubber adhesive, which includes the following raw materials by weight: 100 portions of chloroprene rubber, 30 portions of terpene resin and 90 portions of 2402 resin. The chloroprene rubber adhesive provided by the invention employs a mixed tackifier with high softening point to modify chloroprene rubber, so as to greatly improve the bonding strength of the chloroprene rubber adhesive and thermal resistance of coating, and enhance the applicability.
Description
Technical field
The present invention relates to a kind of tackiness agent, be specifically related to a kind of neoprene adhesive.
Background technology
At present, in shoemaking adhesive technology, mostly neoprene adhesive is used.The method of conventional neoprene adhesive modification be with esters monomer to chloroprene rubber graft copolymerization, carry out chemical modification.
Summary of the invention
The object of the invention is to, a kind of neoprene adhesive is provided, adopt the mixing tackifier of high softening-point to carry out modification to chloroprene rubber, substantially increase the bonding strength of neoprene adhesive and the thermotolerance of glued membrane, improve applicability.
Described neoprene adhesive, comprises the raw material of following weight part:
Chloroprene rubber 100 parts, terpine resin 30 parts, 2402 resin 90 parts.
Neoprene adhesive provided by the invention, its beneficial effect is, adopts the mixing tackifier of high softening-point to carry out modification to chloroprene rubber, substantially increases the bonding strength of neoprene adhesive and the thermotolerance of glued membrane, improve applicability.
Embodiment
Below in conjunction with an embodiment, neoprene adhesive provided by the invention is described in detail.
Embodiment
Described neoprene adhesive, comprises the raw material of following weight part:
Chloroprene rubber 100 g, terpine resin 30 g, 2402 resin 90 g.
Claims (1)
1. a neoprene adhesive, is characterized in that: it comprises the raw material of following weight part:
Chloroprene rubber 100 parts, terpine resin 30 parts, 2402 resin 90 parts.