CN104568584A - 城市污泥烧结页岩多孔砖抗压强度测试方法 - Google Patents

城市污泥烧结页岩多孔砖抗压强度测试方法 Download PDF

Info

Publication number
CN104568584A
CN104568584A CN201410763106.7A CN201410763106A CN104568584A CN 104568584 A CN104568584 A CN 104568584A CN 201410763106 A CN201410763106 A CN 201410763106A CN 104568584 A CN104568584 A CN 104568584A
Authority
CN
China
Prior art keywords
brick
cement paste
face
glass
municipal sludge
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410763106.7A
Other languages
English (en)
Inventor
黄榜彪
黎喜强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangxi University of Science and Technology
Original Assignee
Guangxi University of Science and Technology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangxi University of Science and Technology filed Critical Guangxi University of Science and Technology
Priority to CN201410763106.7A priority Critical patent/CN104568584A/zh
Publication of CN104568584A publication Critical patent/CN104568584A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种城市污泥烧结页岩多孔砖抗压强度测试方法,包括以下步骤:⑴、将多孔砖放在水中浸泡10~20分钟;取一平板玻璃水平放置,在玻璃上先铺上一层用水湿润过的纸张,在纸上涂上一层水泥净浆;⑵、将多孔砖放在净浆上;⑶、调整完后在砖表面上铺上一层5mm的水泥净浆,再将另一块多孔砖放在净浆上,错开放置;⑷、取另一玻璃板,铺上纸张和不得超过5mm厚的净浆,将步骤⑶凝固好的砖样翻转放置净浆上,养护3天;⑸、试件养护好后测量其受压面的长和宽,以4KN/s的速度垂直于受压面连续均匀平稳的加荷,直到试件破坏。本发明能准确获得城市污泥烧结页岩多孔砖的抗压强度。

Description

城市污泥烧结页岩多孔砖抗压强度测试方法
技术领域
本发明涉及建筑砖技术领域,尤其是一种城市污泥烧结页岩多孔砖抗压强度测试方法。
背景技术
随着我国城市的飞速发展,城市生活污水的排放量和污泥产量也逐年增加,而如何处理这些污水污泥已经成为城市发展中首要解决的问题。同时在全国“禁粘”以及大力发展新型墙体材料的大背景下,城市污泥烧结页岩砖的研究不仅符合国家政策要求,而且对我国城市化的发展起到促进作用。而对城市污泥烧结页岩砖砌体的基本力学性能——抗剪性能,应该进行研究分析,这样能为这种新型的墙体材料的推广提供坚实的基础和可靠保障。
发明内容
本发明针对现有技术的不足,提出一种城市污泥烧结页岩多孔砖抗压强度测试方法,操作简便,效果好。
为了实现上述发明目的,本发明提供以下技术方案:一种城市污泥烧结页岩多孔砖抗压强度测试方法,包括以下步骤:
⑴、将城市污泥烧结页岩多孔砖放在水中浸泡10~20分钟;取一平板玻璃水平放置,在玻璃上先铺上一层用水湿润过的纸张,在纸上涂上一层水泥净浆,且该净浆厚度不得超过5mm;
⑵、将浸泡好了的多孔砖放在净浆上,并在砖面上稍稍加压挤出气泡使砖面与净浆很好的粘贴在一起,并调整砖面水平度,使砖面与玻璃面保持平行;
⑶、调整完后在砖表面上铺上一层5mm的水泥净浆,然后再将另一块多孔砖放在净浆上,叠放时两块多孔砖应错开放置,轻轻加压另一块砖面,并调整砖面的水平度待其凝固;
⑷、取另一玻璃板,铺上纸张和不得超过5mm厚的净浆,将步骤⑶凝固好的砖样翻转放置净浆上,调整玻璃板使两块玻璃保持平行,将制作好的试件置于温度不低于10℃密闭的空间内养护3天;
⑸、试件养护好后测量其受压面的长和宽,受力面朝上,几何对中后,以4KN/s的速度垂直于受压面连续均匀平稳的加荷,直到试件破坏。
与现有技术相比,本发明具有以下优点:操作简便,测试方便,能准确获得城市污泥烧结页岩多孔砖的抗压强度,为这种新型的墙体材料的推广提供坚实的基础和可靠保障。
具体实施方式
下面结合实施例对本发明进行详细描述,本部分的描述仅是示范性和解释性,不应对本发明的保护范围有任何的限制作用。
一种城市污泥烧结页岩多孔砖抗压强度测试方法,包括以下步骤:
⑴、将城市污泥烧结页岩多孔砖放在水中浸泡10~20分钟;取一平板玻璃水平放置,在玻璃上先铺上一层用水湿润过的纸张,在纸上涂上一层水泥净浆,且该净浆厚度不得超过5mm;
⑵、将浸泡好了的多孔砖放在净浆上,并在砖面上稍稍加压挤出气泡使砖面与净浆很好的粘贴在一起,并调整砖面水平度,使砖面与玻璃面保持平行;
⑶、调整完后在砖表面上铺上一层5mm的水泥净浆,然后再将另一块多孔砖放在净浆上,叠放时两块多孔砖应错开放置,轻轻加压另一块砖面,并调整砖面的水平度待其凝固;
⑷、取另一玻璃板,铺上纸张和不得超过5mm厚的净浆,将步骤⑶凝固好的砖样翻转放置净浆上,调整玻璃板使两块玻璃保持平行,将制作好的试件置于温度不低于10℃密闭的空间内养护3天;
⑸、试件养护好后测量其受压面的长和宽,受力面朝上,几何对中后,以4KN/s的速度垂直于受压面连续均匀平稳的加荷,直到试件破坏。
以上所述仅是本发明的优选实施方式,应当指出,对于本技术领域的普通技术人员来说,在不脱离本发明原理的前提下,还可以做出若干改进和润饰,这些改进和润饰也应视为本发明的保护范围。

Claims (1)

1.一种城市污泥烧结页岩多孔砖抗压强度测试方法,包括以下步骤:
⑴、将城市污泥烧结页岩多孔砖放在水中浸泡10~20分钟;取一平板玻璃水平放置,在玻璃上先铺上一层用水湿润过的纸张,在纸上涂上一层水泥净浆,且该净浆厚度不得超过5mm;
⑵、将浸泡好了的多孔砖放在净浆上,并在砖面上稍稍加压挤出气泡使砖面与净浆很好的粘贴在一起,并调整砖面水平度,使砖面与玻璃面保持平行;
⑶、调整完后在砖表面上铺上一层5mm的水泥净浆,然后再将另一块多孔砖放在净浆上,叠放时两块多孔砖应错开放置,轻轻加压另一块砖面,并调整砖面的水平度待其凝固;
⑷、取另一玻璃板,铺上纸张和不得超过5mm厚的净浆,将步骤⑶凝固好的砖样翻转放置净浆上,调整玻璃板使两块玻璃保持平行,将制作好的试件置于温度不低于10℃密闭的空间内养护3天;
⑸、试件养护好后测量其受压面的长和宽,受力面朝上,几何对中后,以4KN/s的速度垂直于受压面连续均匀平稳的加荷,直到试件破坏。
CN201410763106.7A 2014-12-12 2014-12-12 城市污泥烧结页岩多孔砖抗压强度测试方法 Pending CN104568584A (zh)