CN104535385A - 城市污泥烧结页岩砖测试砌体 - Google Patents

城市污泥烧结页岩砖测试砌体 Download PDF

Info

Publication number
CN104535385A
CN104535385A CN201410763073.6A CN201410763073A CN104535385A CN 104535385 A CN104535385 A CN 104535385A CN 201410763073 A CN201410763073 A CN 201410763073A CN 104535385 A CN104535385 A CN 104535385A
Authority
CN
China
Prior art keywords
masonry
municipal sludge
shale brick
testing
sludge sintered
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410763073.6A
Other languages
English (en)
Inventor
黄榜彪
黎喜强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangxi University of Science and Technology
Original Assignee
Guangxi University of Science and Technology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangxi University of Science and Technology filed Critical Guangxi University of Science and Technology
Priority to CN201410763073.6A priority Critical patent/CN104535385A/zh
Publication of CN104535385A publication Critical patent/CN104535385A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种城市污泥烧结页岩砖砌体,包括九块页岩砖,均分为三层设置,中间层与上下两层固定连接。本发明结构简单,操作简便,测试方便,能准确获得城市污泥烧结页岩实心砖砌体的抗压强度,为这种新型的墙体材料的推广提供坚实的基础和可靠保障。

Description

城市污泥烧结页岩砖测试砌体
技术领域
本发明涉及建筑技术领域,尤其是一种城市污泥烧结页岩砖测试砌体。
背景技术
随着我国城市的飞速发展,城市生活污水的排放量和污泥产量也逐年增加,而如何处理这些污水污泥已经成为城市发展中首要解决的问题。同时在全国“禁粘”以及大力发展新型墙体材料的大背景下,城市污泥烧结页岩砖的研究不仅符合国家政策要求,而且对我国城市化的发展起到促进作用。而对城市污泥烧结页岩砖砌体的基本力学性能——抗剪性能,应该进行研究分析,这样能为这种新型的墙体材料的推广提供坚实的基础和可靠保障。
发明内容
本发明针对现有技术的不足,提出一种城市污泥烧结页岩砖测试砌体,结构巧妙,测试方便。
为了实现上述发明目的,本发明提供以下技术方案:一种城市污泥烧结页岩砖测试砌体,包括九块页岩砖,均分为三层设置,中间层与上下两层固定连接。
进一步地,每层为一横两竖排列,且相邻两层交叉设置。
进一步地,相邻页岩砖之间采用混合砂浆进行粘接。
与现有技术相比,本发明具有以下优点:操作简便,测试方便,能准确获得城市污泥烧结页岩实心砖砌体的抗压强度,为这种新型的墙体材料的推广提供坚实的基础和可靠保障。
附图说明
图1为本发明城市污泥烧结页岩砖测试砌体的结构示意图。
具体实施方式
下面结合附图对本发明进行详细描述,本部分的描述仅是示范性和解释性,不应对本发明的保护范围有任何的限制作用。
如图1所示的一种城市污泥烧结页岩砖测试砌体,将九块城市污泥烧结页岩砖1,分三层设置,每层为一横两竖排列,且相邻两层交叉设置,相邻实心砖用混合砂浆进行粘接,构成九砖砌体。
在测试时,将九砖砌体在室内自然条件下养护一个星期,当砂浆的强度上来以后,在砌体侧面靠边的两个受力面上抹上厚度1cm的水泥砂浆。
抹面完后,再养护三天同样在另一侧立面的中间受力砖面上抹砂浆,方法同前。抹面时不仅要保证砂浆表面平整,而且还要保证两个侧面的砂浆面要平行,同时要使受力面垂直于受剪面的灰缝,这样将应力集中和偏心的影响降到最低。抹好受力面后,在室内常温下养护,待砂浆达到其设计强度后即可进行抗剪试验。
通缝抗剪试验所采用的加载装置是屏显式电液伺服万能试验机,在开始试验时,先用吊锤找出试验机X、Y轴线所在位置用粉笔标出,然后将轴线所在位置引到试验机压板上 。标注好轴线后就可将画好中线的试件放置压板上,为了保证试件表面的平整度,可在压板表面铺一层薄薄的细砂,使试件的中线和试验机的轴线重合。为了使试验机顶板传来的荷载能够均匀的分布在试件的受力面,可在试件顶面中间砖的受力面先铺上层薄薄的细砂,然后再放一块2cm厚的钢板,钢板与试验机顶板相连直接承受试验机传来的荷载。
试验时先测量试件受剪面的截面尺寸,作好记录,然后将试件放置于试验机上,利用吊锤调整好试件的位置,保证试件的中线与试验机的轴线重合。打开电脑设置加荷速度匀速连续对试件加压,观察试件破坏形态,并尽量将试件控制在3分钟内破坏,记录试件破坏时所加荷载值。
以上所述仅是本发明的优选实施方式,应当指出,对于本技术领域的普通技术人员来说,在不脱离本发明原理的前提下,还可以做出若干改进和润饰,这些改进和润饰也应视为本发明的保护范围。

Claims (3)

1.一种城市污泥烧结页岩砖测试砌体,其特征在于:包括九块页岩砖,均分为三层设置,中间层与上下两层固定连接。
2.如权利要求1所述城市污泥烧结页岩砖测试砌体,其特征在于:每层为一横两竖排列,且相邻两层交叉设置。
3.如权利要求2所述城市污泥烧结页岩砖测试砌体,其特征在于:相邻页岩砖之间采用混合砂浆进行粘接。
CN201410763073.6A 2014-12-12 2014-12-12 城市污泥烧结页岩砖测试砌体 Pending CN104535385A (zh)