CN104264508A - Method for producing transparent flax yarns - Google Patents

Method for producing transparent flax yarns Download PDF

Info

Publication number
CN104264508A
CN104264508A CN201410475505.3A CN201410475505A CN104264508A CN 104264508 A CN104264508 A CN 104264508A CN 201410475505 A CN201410475505 A CN 201410475505A CN 104264508 A CN104264508 A CN 104264508A
Authority
CN
China
Prior art keywords
yarn
yarns
minutes
dye
dye vat
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410475505.3A
Other languages
Chinese (zh)
Other versions
CN104264508B (en
Inventor
王雅琴
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU HUAXIN FLAX TEXTILE CO Ltd
Original Assignee
JIANGSU HUAXIN FLAX TEXTILE CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU HUAXIN FLAX TEXTILE CO Ltd filed Critical JIANGSU HUAXIN FLAX TEXTILE CO Ltd
Priority to CN201410475505.3A priority Critical patent/CN104264508B/en
Publication of CN104264508A publication Critical patent/CN104264508A/en
Application granted granted Critical
Publication of CN104264508B publication Critical patent/CN104264508B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention provides a method for producing transparent flax yarns. The method comprises the following steps: S1, pouring resultant yarns to be dyed into fixed-length hank yarns; S2, putting the hank yarns into a dye vat according to a predetermined standard; S3, performing chemical treatment on the hank yarns in the dye vat and lifting the hank yarns out of the dye vat after the treatment; S4, dyeing the hank yarns by use of a vat dye; S5, putting the dyed hank yarns into a spraying dye vat and performing natural oxidization, color development, washing and sizing; S6, performing spin-drying, beating, tightening, warping, denting, weaving, mending and coiling on the sized hank yarns to obtain the finished product, wherein the chemical treatment in the step S3 refers to adding of 1.5-2g/l of treating agent to react at 40-45 DEG C for 30-35 minutes. The method for producing the transparent flax yarns has the advantages that white spaces are formed on the surface of the yarns and are uneven in color and shade, and therefore, even but irregular stripe patterns different in shade are formed in the textile structure, and a vivid jump effect is produced.

Description

A kind ofly produce flax and to reveal the exact details the method for yarn
Technical field
The present invention relates to a kind of production method of spun articles, particularly a kind ofly produce flax and to reveal the exact details the method for yarn.
Background technology
Along with the raising of people's living standard and the quietly change of aesthetic standard.Pursuing textile product is natural, environment-friendly and green, novel top grade idea dressing, is the ideal of people.Also be a weaving people dream dreaming of, pursue diligently, and flax is one of the object that becomes people's favor that stands in the breach.What arise at the historic moment like this is exactly specific embodiment of the invention.
One flat dyadic is the consistent tradition of flax, and simultaneously due to its special fiber properties, the color and luster of dyeing is bright-coloured not, does not have lofty sense, and cloth cover is unromantic.
Summary of the invention
In order to solve above problem, the invention provides and a kind ofly realize flax and to reveal the exact details the production method of yarn.
Technical scheme of the present invention is achieved in that
The invention discloses and a kind ofly produce flax and to reveal the exact details the method for yarn, comprising:
S1. first resultant yarn to be contaminated is changed into the reeled yarn of fixed length;
S2. by the standard preset, described reeled yarn is loaded in dye vat;
S3. chemical treatment is carried out to the reeled yarn in described dye vat, after process, hang out dye vat;
S4. reducing dye is used to dye to described reeled yarn;
S5. the reeled yarn after described dyeing is positioned in spray-painting cylinder, autoxidation, color development, washing, starching;
S6. by the drying of the reeled yarn of described starching, yarning, tight cylinder, warping, denting, weave cotton cloth, mending, rolling, get product, wherein, the chemical treatment in described step S3, specifically comprises: use the finishing agent of 1.5 ~ 2g/l to be 40 ~ 45 DEG C of reactions 30 ~ 35 minutes in temperature.
Reveal the exact details in the method for yarn in production flax of the present invention, the reeled yarn weight of each fixed length in described step S1 is 195g ~ 205g.
Reveal the exact details in the method for yarn in production flax of the present invention, use reducing dye in described step S4 dyes to described reeled yarn, specifically comprise: first the caustic soda of 18 ~ 20g/l, the sodium hydrosulfite of 15 ~ 18g/l are made condiment, described condiment is added dye vat, adjust water level, after circulation, make basicity become 12g/l, sodium hydrosulfite becomes 10 ~ 12g/l, being hung in pot by reeled yarn makes yarn play reduction reaction again, circulating-heating to 60 DEG C, be incubated 30 minutes, add auxiliary agent more afterwards, circulate 10 minutes.
Reveal the exact details in the method for yarn in production flax of the present invention, in described step S5. the reeled yarn after described dyeing is positioned in spray-painting cylinder, autoxidation, color development, washing, starching, specifically comprising: autoxidation, after 2 ~ 3 hours, adds the soap powder of 5 ~ 5.5g/l, is color development 10 ~ 15 minutes in 95 ~ 98 DEG C in temperature, respectively after temperature is 80 DEG C, 70 DEG C, 55 DEG C washings, add 3g/l glacial acetic acid to neutralize, use slurry 2 ~ 3g/l, circulate and take the dish out of the pot after 10 minutes.
Reveal the exact details in the method for yarn in production flax of the present invention, described tight cylinder, specifically comprises: naturally got damp again 12 hours by dyed yarn after yarning, the tight cylinder of upper bobbin winder, and making can for normal yarn of weaving cotton cloth.
Implement of the present inventionly a kind ofly to produce flax and to reveal the exact details the method for yarn, there is following useful technique effect:
The present invention is different from prior art does not have chemical treatment step before dyeing, the different dyeing rates that the present invention utilizes each chemical constituent skewness between the distinctive chemical composition of linen fibre and cross section and produces, and the chemical treatment before upper (dye) look is carried out to fiber, on the surface of yarn formation stay white and color and luster and the depth uneven.Be embodied on fabric tissue, formed very evenly but irregular governed deep mixed barriness, produce lifelike great-jump-forward effect, finally define special cloth cover effect.
Detailed description of the invention
Embodiment one, a kind ofly produces flax and to reveal the exact details the method for yarn, comprising:
1, the preparation of yarn to be dyed.Flax yarn of revealing the exact details is resultant yarn dyeing product, first resultant yarn to be contaminated is changed into reeled yarn, requires each reeled yarn all fixed length, often twists weight at 195 grams;
2, fill cylinder, on request yarn is loaded in dye vat;
3, the pre-treatment before dyeing: will carry out chemical treatment to yarn before dyeing, strengthens uneven dyeing that this yarn itself occurs because structure is irregular (finishing agent 1.5g/l, 40 DEG C, 30 minutes), processes yarn afterwards and will hang out dye vat and treat subsequent processing;
4, according to the color of order, determine dyeing, use reducing dye to dye.First condiment is wanted: paying furnishing caustic soda 18g/l, sodium hydrosulfite 15g/l in cylinder before dyeing, adjust water level and squeeze into dye vat (dyestuff is 4%), basicity 12g/l, sodium hydrosulfite 10g/l is made after circulation, being hung in pot by creel makes yarn play reduction reaction again, circulating-heating to 60 DEG C insulation 30 minutes, add auxiliary agent mainly gelatine 10g/l afterwards again, circulate 10 minutes;
5, spray-painting cylinder oxidation, color development, washing, starching: yarn is hung out, be placed in spray-painting cylinder, carry out autoxidation after 2 hours, add soap powder 5g/l, 95 DEG C, 10 minutes, after 80 DEG C, 70 DEG C, 55 DEG C washings, add about 3g/l glacial acetic acid to neutralize, use slurry 2g/l, circulate and take the dish out of the pot after 10 minutes;
6, the fiber after dyeing dries, yarning and shredding, oven dry (105 DEG C, 4 hours);
7, tight cylinder: after dry, dyed yarn gets damp again 12 hours naturally, the tight cylinder of upper bobbin winder, and making can for yarn normally of weaving cotton cloth;
8, warping, denting, weave cotton cloth, perching, mending, Final finishing, rolling packaging and warehousing;
Wherein, also to have in prior art and use cheese yarn dyeing, change autoxidation into hydrogen peroxide oxidation exactly with the above-mentioned difference that describes, add the hydrogen peroxide of 2g/l.But its shortcoming is abundant not as spray-painting of washing, to rear portion weave cotton cloth and Final finishing is made troubles.
Embodiment two, a kind ofly produces flax and to reveal the exact details the method for yarn, comprising:
1, the preparation of yarn to be dyed.Flax yarn of revealing the exact details is resultant yarn dyeing product, first resultant yarn to be contaminated is changed into reeled yarn, requires each reeled yarn all fixed length, often twists weight greatly about 200 grams;
2, fill cylinder, on request yarn is loaded in dye vat;
3, the pre-treatment before dyeing: will carry out chemical treatment to yarn before dyeing, strengthens uneven dyeing that this yarn itself occurs because structure is irregular (finishing agent 1.8g/l, 43 DEG C, 32 minutes), processes yarn afterwards and will hang out dye vat and treat subsequent processing;
4, according to the color of order, determine dyeing, use reducing dye to dye.First condiment is wanted before dyeing, paying furnishing caustic soda 19g/l, sodium hydrosulfite 17g/l in cylinder, adjust water level and squeeze into dye vat (dyestuff is 6%), basicity 12g/l, sodium hydrosulfite 11g/l is made after circulation, being hung in pot by creel makes yarn play reduction reaction again, circulating-heating to 60 DEG C insulation 30 minutes, adds auxiliary agent mainly gelatine 13g/l afterwards again, circulates 10 minutes;
5, spray-painting cylinder oxidation, color development, washing, starching: yarn is hung out, be placed in spray-painting cylinder, carry out autoxidation after 2.5 hours, add soap powder 5.2g/l, 96 DEG C, 12 minutes, after 80 DEG C, 70 DEG C, 55 DEG C washings, add about 3g/l glacial acetic acid to neutralize, use slurry 2.5g/l, circulate and take the dish out of the pot after 10 minutes;
6, the fiber after dyeing dries, yarning and shredding, oven dry (105 DEG C, 4 hours);
7, tight cylinder: after dry, dyed yarn gets damp again 12 hours naturally, the tight cylinder of upper bobbin winder, and making can for yarn normally of weaving cotton cloth;
8, warping, denting, weave cotton cloth, perching, mending, Final finishing, rolling packaging and warehousing;
Embodiment three, a kind ofly produces flax and to reveal the exact details the method for yarn, comprising:
1, the preparation of yarn to be dyed.Flax yarn of revealing the exact details is resultant yarn dyeing product, first resultant yarn to be contaminated is changed into reeled yarn, requires each reeled yarn all fixed length, often twists weight greatly about 205 grams;
2, fill cylinder, on request yarn is loaded in dye vat;
3, the pre-treatment before dyeing: will carry out chemical treatment to yarn before dyeing, strengthens uneven dyeing that this yarn itself occurs because structure is irregular (finishing agent 2g/l, 45 DEG C, 35 minutes), processes yarn afterwards and will hang out dye vat and treat subsequent processing;
4, according to the color of order, determine dyeing, use reducing dye to dye.First condiment is wanted before dyeing, paying furnishing caustic soda 20g/l, sodium hydrosulfite 18g/l in cylinder, adjust water level and squeeze into dye vat (dyestuff is 8%), basicity 12g/l, sodium hydrosulfite 12g/l is made after circulation, being hung in pot by creel makes yarn play reduction reaction again, circulating-heating to 60 DEG C insulation 30 minutes, adds auxiliary agent mainly gelatine 15g/l afterwards again, circulates 10 minutes;
5, spray-painting cylinder oxidation, color development, washing, starching: yarn is hung out, be placed in spray-painting cylinder, carry out autoxidation after 3 hours, add soap powder 5.5g/l, 98 DEG C, 15 minutes, after 80 DEG C, 70 DEG C, 55 DEG C washings, add about 3g/l glacial acetic acid to neutralize, use slurry 3g/l, circulate and take the dish out of the pot after 10 minutes;
6, the fiber after dyeing dries, yarning and shredding, oven dry (105 DEG C, 4 hours);
7, tight cylinder: after dry, dyed yarn gets damp again 12 hours naturally, the tight cylinder of upper bobbin winder, and making can for yarn normally of weaving cotton cloth;
8, warping, denting, weave cotton cloth, perching, mending, Final finishing, rolling packaging and warehousing;
Implement of the present inventionly a kind ofly to produce flax and to reveal the exact details the method for yarn, there is following useful technique effect:
The present invention is different from prior art does not have chemical treatment step before dyeing, the different dyeing rates that the present invention utilizes each chemical constituent skewness between the distinctive chemical composition of linen fibre and cross section and produces, and the chemical treatment before upper (dye) look is carried out to fiber, on the surface of yarn formation stay white and color and luster and the depth uneven.Be embodied on fabric tissue, formed very evenly but irregular governed deep mixed barriness, produce lifelike great-jump-forward effect, finally define special cloth cover effect.
The foregoing is only preferred embodiment of the present invention, not in order to limit the present invention, within the spirit and principles in the present invention all, any amendment done, equivalent replacement, improvement etc., all should be included within protection scope of the present invention.

Claims (5)

1. produce flax to reveal the exact details the method for yarn, it is characterized in that, comprising:
S1. first resultant yarn to be contaminated is changed into the reeled yarn of fixed length;
S2. by the standard preset, described reeled yarn is loaded in dye vat;
S3. chemical treatment is carried out to the reeled yarn in described dye vat, after process, hang out dye vat;
S4. reducing dye is used to dye to described reeled yarn;
S5. the reeled yarn after described dyeing is positioned in spray-painting cylinder, autoxidation, color development, washing, starching;
S6. by the drying of the reeled yarn of described starching, yarning, tight cylinder, warping, denting, weave cotton cloth, mending, rolling, get product, wherein, the chemical treatment in described step S3, specifically comprises: use the finishing agent of 1.5 ~ 2g/l to be 40 ~ 45 DEG C of reactions 30 ~ 35 minutes in temperature.
2. production flax according to claim 1 is revealed the exact details the method for yarn, and it is characterized in that, the reeled yarn weight of each fixed length in described step S1 is 195g ~ 205g.
3. production flax according to claim 1 is revealed the exact details the method for yarn, it is characterized in that, use reducing dye in described step S4 dyes to described reeled yarn, specifically comprise: first the caustic soda of 18 ~ 20g/l, the sodium hydrosulfite of 15 ~ 18g/l are made condiment, described condiment is added dye vat, adjust water level, after circulation, make basicity become 12g/l, sodium hydrosulfite becomes 10 ~ 12g/l, being hung in pot by reeled yarn makes yarn play reduction reaction again, circulating-heating to 60 DEG C, is incubated 30 minutes, add auxiliary agent more afterwards, circulate 10 minutes.
4. production flax according to claim 1 is revealed the exact details the method for yarn, it is characterized in that, in described step S5. the reeled yarn after described dyeing is positioned in spray-painting cylinder, autoxidation, color development, washing, starching, specifically comprise: autoxidation is after 2 ~ 3 hours, add the soap powder of 5 ~ 5.5g/l, be color development 10 ~ 15 minutes in 95 ~ 98 DEG C in temperature, respectively after temperature is 80 DEG C, 70 DEG C, 55 DEG C washings, add 3g/l glacial acetic acid to neutralize, use slurry 2 ~ 3g/l, circulate and take the dish out of the pot after 10 minutes.
5. production flax according to claim 1 is revealed the exact details the method for yarn, and it is characterized in that, described tight cylinder, specifically comprises: naturally got damp again 12 hours by dyed yarn after yarning, the tight cylinder of upper bobbin winder, and making can for yarn normally of weaving cotton cloth.
CN201410475505.3A 2014-09-16 2014-09-16 A kind of produce Caulis et Folium Lini and reveal the exact details the method for yarn Active CN104264508B (en)