CN104208733A - Sustained-release chlorine dioxide powder applicable to purifying indoor air - Google Patents

Sustained-release chlorine dioxide powder applicable to purifying indoor air Download PDF

Info

Publication number
CN104208733A
CN104208733A CN201410434321.2A CN201410434321A CN104208733A CN 104208733 A CN104208733 A CN 104208733A CN 201410434321 A CN201410434321 A CN 201410434321A CN 104208733 A CN104208733 A CN 104208733A
Authority
CN
China
Prior art keywords
powder
chlorine dioxide
indoor air
applicable
slow
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410434321.2A
Other languages
Chinese (zh)
Inventor
梁宗贵
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chengdu Shunfa Disinfectant and Washing Technology Co Ltd
Original Assignee
Chengdu Shunfa Disinfectant and Washing Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chengdu Shunfa Disinfectant and Washing Technology Co Ltd filed Critical Chengdu Shunfa Disinfectant and Washing Technology Co Ltd
Priority to CN201410434321.2A priority Critical patent/CN104208733A/en
Publication of CN104208733A publication Critical patent/CN104208733A/en
Pending legal-status Critical Current

Abstract

The invention discloses sustained-release chlorine dioxide powder applicable to purifying indoor air. The formula of the sustained-release chlorine dioxide powder mainly comprises the following components in percentage by weight: 5-10 percent of a chlorine dioxide precursor, 12-20 percent of an activating agent, 5-10 percent of a sustained-releasing agent, 12-20 percent of gel, 43-47 percent of packing and 5-10 percent of activated carbon. The sustained-release chlorine dioxide powder can be used as air purifiers to remove formaldehyde, benzene series and the like in the air, and the chlorine dioxide released by the powder can be used for effectively oxidizing the formaldehyde in the indoor air, and no secondary pollutants generate in the oxidizing process, so that the sustained-release chlorine dioxide powder has an excellent application prospect in the fields of household environmental friendliness, healthy epidemic prevention and the like.

Description

A kind of slow released ClO 2 powder being applicable to indoor air purification
Technical field
The present invention is a kind of slow released ClO 2 powder being applicable to indoor air purification, is specifically related to the purified treatment of the harmful substances such as formaldehyde in indoor air, belongs to air purification field.
Background technology
Formaldehyde has another name called formaldehyde, it is a kind of colourless gas with penetrating odor, density is a little more than air, soluble in water, be a kind of organic compound of highly volatile, be mainly used in all kinds of ornament materials, such as wall covering fabric, subsides wall chemical fibre, carpet, foam plastics, paint and coating etc., therefore, be also one of the maximum indoor pollutant that is detrimental to health.In modern house environment, the concentration over-standard of formaldehyde can cause nausea, vomit, cough, uncomfortable in chest, the even symptom such as emphysema of panting, along with improving constantly of rapid development of economy and Living consumption, people are more and more higher to the comfort level of living environment, working environment, cosmetic requirements, meanwhile, the pollution problem of a series of improvement formaldehyde in indoor air is also brought.The method of existing improvement formaldehyde in indoor air mainly contains physical method, chemical method and biological method, and wherein, physical method adopts the physical measure such as ventilation, absorption, and can not produce secondary pollution, whole process is mild, consuming time longer; Chemical method then adopt can with the material of formaldehyde generation chemical reaction, produce the less novel substance of another kind of toxicity under certain condition with formaldehyde reaction or absorb formaldehyde, whole process is acutely, consuming time short, but can produce certain secondary thing pollutant; The formaldehyde pollution that biological method mainly uses plant to come in clean room's environment, by photosynthesis and the adsorption of plant, decompose formaldehyde a small amount of in air, whole process can not produce secondary pollution, but because plant is Passive intake formaldehyde, therefore, less to the effect controlling concentration of formaldehyde.
In recent years, constantly burning hot along with indoor decoration, eliminate the formaldehyde that upholstery material comes out, become people's question of common concern, and chlorine dioxide is as a kind of new and effective disinfection sanitizer, not only eliminate in the report of pollutants in air formaldehyde at many sections and carried out record, at patent documentation CN1887356 (a kind of slow released ClO 2 air disinfectant, 2007.01.03), CN2841013 (the air disinfection and refreshing box of slowly-releasing chlorine dioxide gas, 2006.11.29) in also have disclosure, mainly utilize the oxidisability of chlorine dioxide, by oxidation of formaldehyde formic acid until carbon dioxide and being removed, when using in reality, boiling point due to chlorine dioxide is only 11 DEG C, boiling point is lower, when producing, the chlorine dioxide of gaseous state exists again vivaciously and the characteristics such as instability, often need to carry out extemporaneous preparation, cause concentration wayward, therefore, result of use is unsatisfactory, if use the silica gel product that patent documentation CN1887356 discloses, then there is the defects such as complex manufacturing process, the present invention arises at the historic moment for this reason.
Summary of the invention
The object of the present invention is to provide a kind of slow released ClO 2 powder being applicable to indoor air purification, a kind of powder product of powder form is mainly provided, in actual use, its chlorine dioxide discharged can not only effectively be oxidized the formaldehyde in room air, the generation of oxidizing process non-secondary pollution thing, also has the advantages such as easy preservation, long shelf-life.
The present invention is achieved through the following technical solutions: a kind of slow released ClO 2 powder being applicable to indoor air purification, overcome in prior art and adopt silica gel to make slow released ClO 2 air disinfectant and the numerous and diverse defect of the manufacturing process that exists as colloidal powder, provide a kind of product form of powdery, the formula of described slow released ClO 2 powder is primarily of chlorine dioxide precursor, activator, slow releasing agent, gel, filler and active carbon composition, preparation process of the present invention is very simple, for subsequent use after carrying out separately drying by the component in formula, and then proportioning to carry out hybrid reaction on request, be specially adapted to industrialized large-scale production, cost of manufacture is cheap.
Further, by weight, the chlorine dioxide precursor of described composition slow released ClO 2 powder is 5 ~ 10%, activator is 12 ~ 20%, slow releasing agent is 5 ~ 10%, gel is 12 ~ 20%, filler is 43 ~ 47%, active carbon is 5 ~ 10%.
Optimize, by weight, the chlorine dioxide precursor of described composition slow released ClO 2 powder is 8%, activator is 16%, slow releasing agent is 8%, gel is 16%, filler is 45%, active carbon is 7%.
In the present invention, described chlorine dioxide precursor comprises the mixture of one or more compositions in sodium chlorite, potassium chlorite, barium chlorite, magnesium chlorite.
To better implement the present invention, described activator comprises the mixture of one or more compositions in sodium bisulfate, sodium sulfate, potassium acid sulfate, potassium sulfate, Magnesium hydrogen sulfate.
Described slow releasing agent comprises the mixture of one or more compositions in macrogol, polyvinyl alcohol, polyacrylamide, crosslinked polyethylene, this reagent is by delaying the absorption rate of moisture, reach the object of delayed response speed, thus further improve the stability of each component in formula of the present invention, avoid the generation of oneself's reaction.
For better controlling the volatility of chlorine dioxide, described gel is AQUAGEL PLUS gel.
Component of the present invention has the effect of removing the harmful substances such as formaldehyde after reaction, in real reaction process, then need moisture just can react, therefore, the present invention adds active carbon in its formula, it can active absorption moisture, delay the response speed of recipe ingredient, suitable long-time preservation, in the case, reasonable arrangement activator, slow releasing agent, gel, filler and chlorine dioxide precursor proportional amount, after mixing with moisture, the colloid containing chlorine dioxide can be obtained, simultaneously, effectively the volatility of the effective ingredient (chlorine dioxide) in powder is controlled, to meet PARA FORMALDEHYDE PRILLS(91,95) purification in room air, in the present invention, described filler is anhydrous sodium sulfate, anhydrous slufuric acid barium, anhydrous potassium sulfate, the mixture of one or more compositions in anhydrous magnesium sulfate.
The present invention compared with prior art, has the following advantages and beneficial effect:
(1) the present invention is powder product, can directly be positioned in indoor environment, the chlorine dioxide physical ability of its release is oxidized for the formaldehyde in room air, can by oxidation of formaldehyde formic acid until carbon dioxide and being removed, the generation of oxidizing process non-secondary pollution thing, practical effect is good.
(2) production method of the present invention is simple, is particularly useful for industrialized large-scale production, has the advantages such as operating process is simple, cost of manufacture is cheap.
(3) rationally, the composition of gel, slow releasing agent and filler, improves the stability in packing of product storage process all effectively, avoids reacting between each component, and reach the object extending shelf life of products, practicality is extremely strong in recipe ingredient preparation of the present invention.
(4) after the present invention uses, owing to being added with gel, therefore, after reacting with moisture in air, colloid form can be changed into by powder forms, because gel selects AQUAGEL PLUS gel, effectively can also control the rate of release of chlorine dioxide in colloid form, there is the advantages such as easy preservation, long shelf-life.
Detailed description of the invention
Below in conjunction with embodiment, the present invention is described in further detail, but embodiments of the present invention are not limited thereto.
Embodiment 1:
The present invention relates to a kind of slow released ClO 2 powder being applicable to indoor air purification, overcome in prior art and adopt silica gel to make slow released ClO 2 air disinfectant and the numerous and diverse defect of the manufacturing process that exists as colloidal powder, provide a kind of product form of powdery, this powder product is adsorbable and the harmful substances such as formaldehyde are removed in reaction, have and purify air, kill antibacterial in air, remove the effects such as air abnormal flavour, be mainly used as air disinfection and purification agent and use.
In the present embodiment, this slow released ClO 2 sterilizing and purifying wp formula is primarily of the chlorine dioxide precursor of 10%, activator, the slow releasing agent of 5%, gel, the filler of 47%, the active carbon composition of 10% of 12% of 20%.
Make as follows:
A: get the raw materials ready, prepares chlorine dioxide precursor, activator, slow releasing agent, gel, filler and active carbon respectively:
The sodium chlorite of chlorine dioxide precursor choice of powder shape and potassium chlorite, by weight, sodium chlorite: the proportioning of potassium chlorite is 2:1; The sodium bisulfate of activator choice of powder shape and sodium sulfate, by weight, the proportioning of sodium bisulfate and sodium sulfate is 2:1; The object of slow releasing agent is then the speed controlling moisture absorption, has the effect slowly absorbing moisture, in actual process for preparation, can select powdery polyethylene glycol and polyvinyl alcohol, by weight, and macrogol: the proportioning of polyvinyl alcohol is 1:1; The AQUAGEL PLUS gel of gel choice of powder shape; The anhydrous sodium sulfate of filler choice of powder shape and anhydrous slufuric acid barium, by weight, anhydrous sodium sulfate: the proportioning of anhydrous slufuric acid barium is 1:1.
B: dry: chlorine dioxide precursor, activator, filler and active carbon being put into respectively thermostatic drying chamber, to carry out drying for subsequent use afterwards, wherein,
Chlorine dioxide precursor: the baking temperature in thermostatic drying chamber is set as 60 degrees Celsius, drying time is 8 hours;
Activator: the baking temperature in thermostatic drying chamber is set as 50 degrees Celsius, drying time is 10 hours, and stirs once every 20 minutes;
Filler: the baking temperature in thermostatic drying chamber is set as 60 degrees Celsius, drying time is 4 hours;
Active carbon: the baking temperature in thermostatic drying chamber is set as 80 degrees Celsius, drying time is 4 hours;
C: mixing, measure according to formula proportion, after chlorine dioxide precursor for subsequent use and filler mix homogeneously, add slow releasing agent, gel, active carbon, activator again, and mix homogeneously, load container namely to have prepared, under normal circumstances, the powder humidity applicable industry dehumidifier be mixed into controls moisture content below 40%.
The air purification effect of the slow released ClO 2 sterilizing and purifying powder that the present embodiment prepares is detected, result shows, chlorine dioxide has good deodorizing effect to room air, be 95% to the deodorization rate of ammonia, be 90% to the deodorization rate of benzene, be 99% to the deodorization rate of acetic acid, be 100% to the deodorization rate of hydrogen sulfide, the elimination factor of PARA FORMALDEHYDE PRILLS(91,95) is 50%, meanwhile, also having good bactericidal effect, is 100% to sterilizing rate colibacillary in air, use rear air purification effect good, and meet national standard.
Embodiment 2:
In the present embodiment, this slow released ClO 2 sterilizing and purifying wp formula is primarily of the chlorine dioxide precursor of 5%, activator, the slow releasing agent of 10%, gel, the filler of 43%, the active carbon composition of 10% of 20% of 12%.
Make as follows:
A: get the raw materials ready, prepares chlorine dioxide precursor, activator, slow releasing agent, gel, filler and active carbon respectively:
The sodium chlorite of chlorine dioxide precursor choice of powder shape, by weight; The sodium bisulfate of activator choice of powder shape; The object of slow releasing agent is then the speed controlling moisture absorption, has the effect slowly absorbing moisture, in actual process for preparation, can select powdery polyethylene glycol; The AQUAGEL PLUS gel of gel choice of powder shape; The anhydrous sodium sulfate of filler choice of powder shape.
B: dry: chlorine dioxide precursor, activator, filler and active carbon being put into respectively thermostatic drying chamber, to carry out drying for subsequent use afterwards, wherein,
Chlorine dioxide precursor: the baking temperature in thermostatic drying chamber is set as 70 degrees Celsius, drying time is 10 hours;
Activator: the baking temperature in thermostatic drying chamber is set as 60 degrees Celsius, drying time is 15 hours, and stirs once every 30 minutes;
Filler: the baking temperature in thermostatic drying chamber is set as 80 degrees Celsius, drying time is 7 hours;
Active carbon: the baking temperature in thermostatic drying chamber is set as 90 degrees Celsius, drying time is 6 hours;
C: mixing, measure according to formula proportion, after chlorine dioxide precursor for subsequent use and filler mix homogeneously, add active carbon, slow releasing agent, gel, activator again, and mix homogeneously, load container namely to have prepared, under normal circumstances, the powder humidity applicable industry dehumidifier be mixed into controls moisture content below 40%.
The air purification effect of the slow released ClO 2 sterilizing and purifying powder that the present embodiment prepares is detected, result shows, chlorine dioxide has good deodorizing effect to room air, be 98% to the deodorization rate of ammonia, be 92% to the deodorization rate of benzene, be 99% to the deodorization rate of acetic acid, be 100% to the deodorization rate of hydrogen sulfide, the elimination factor of PARA FORMALDEHYDE PRILLS(91,95) is 51%, meanwhile, also having good bactericidal effect, is 100% to sterilizing rate colibacillary in air, use rear air purification effect good, and meet national standard.
Embodiment 3:
In the present embodiment, this slow released ClO 2 sterilizing and purifying wp formula is primarily of the chlorine dioxide precursor of 8%, activator, the slow releasing agent of 8%, gel, the filler of 45%, the active carbon composition of 7% of 16% of 16%.
Make as follows:
A: get the raw materials ready, prepares chlorine dioxide precursor, activator, slow releasing agent, gel, filler and active carbon respectively:
The sodium chlorite of chlorine dioxide precursor choice of powder shape, potassium chlorite and barium chlorite, by weight, sodium chlorite: potassium chlorite: the proportioning of barium chlorite is 1:1:1; The sodium bisulfate of activator choice of powder shape, sodium sulfate and Magnesium hydrogen sulfate, by weight, the proportioning of sodium bisulfate, sodium sulfate and Magnesium hydrogen sulfate is 1:1:1; The object of slow releasing agent is then the speed controlling moisture absorption, there is the effect slowly absorbing moisture, in actual process for preparation, powdery polyethylene glycol, polyvinyl alcohol and polyacrylamide can be selected, by weight, macrogol: polyvinyl alcohol: the proportioning of polyacrylamide is 1:1:1; The AQUAGEL PLUS gel of gel choice of powder shape; The anhydrous sodium sulfate of filler choice of powder shape, anhydrous slufuric acid barium and anhydrous potassium sulfate, by weight, anhydrous sodium sulfate: anhydrous slufuric acid barium: the proportioning of anhydrous potassium sulfate is 1:1:1.
B: dry: chlorine dioxide precursor, activator, filler and active carbon being put into respectively thermostatic drying chamber, to carry out drying for subsequent use afterwards, wherein,
Chlorine dioxide precursor: the baking temperature in thermostatic drying chamber is set as 65 degrees Celsius, drying time is 9 hours;
Activator: the baking temperature in thermostatic drying chamber is set as 70 degrees Celsius, drying time is 12.5 hours, and stirs once every 25 minutes;
Filler: the baking temperature in thermostatic drying chamber is set as 70 degrees Celsius, drying time is 5.5 hours;
Active carbon: the baking temperature in thermostatic drying chamber is set as 85 degrees Celsius, drying time is 5 hours;
C: mixing, measure according to formula proportion, after chlorine dioxide precursor for subsequent use and filler mix homogeneously, add gel, slow releasing agent, active carbon, activator again, and mix homogeneously, load container namely to have prepared, under normal circumstances, the powder humidity applicable industry dehumidifier be mixed into controls moisture content below 40%.
The air purification effect of the slow released ClO 2 sterilizing and purifying powder that the present embodiment prepares is detected, result shows, chlorine dioxide has good deodorizing effect to room air, be 97% to the deodorization rate of ammonia, be 92% to the deodorization rate of benzene, be 99% to the deodorization rate of acetic acid, be 100% to the deodorization rate of hydrogen sulfide, the elimination factor of PARA FORMALDEHYDE PRILLS(91,95) is 55%, meanwhile, also having good bactericidal effect, is 100% to sterilizing rate colibacillary in air, use rear air purification effect good, and meet national standard.
The above is only preferred embodiment of the present invention, and not do any pro forma restriction to the present invention, every any simple modification, equivalent variations done above embodiment according to technical spirit of the present invention, all falls within protection scope of the present invention.

Claims (8)

1. be applicable to a slow released ClO 2 powder for indoor air purification, it is characterized in that: the formula of described slow released ClO 2 powder forms primarily of chlorine dioxide precursor, activator, slow releasing agent, gel, filler and active carbon.
2. a kind of slow released ClO 2 powder being applicable to indoor air purification according to claim 1, it is characterized in that: by weight, the chlorine dioxide precursor of described composition slow released ClO 2 powder is 5 ~ 10%, activator is 12 ~ 20%, slow releasing agent is 5 ~ 10%, gel is 12 ~ 20%, filler is 43 ~ 47%, active carbon is 5 ~ 10%.
3. a kind of slow released ClO 2 powder being applicable to indoor air purification according to claim 2, it is characterized in that: by weight, the chlorine dioxide precursor of described composition slow released ClO 2 powder is 8%, activator is 16%, slow releasing agent is 8%, gel is 16%, filler is 45%, active carbon is 7%.
4. a kind of slow released ClO 2 powder being applicable to indoor air purification according to any one of claim 1 ~ 3, is characterized in that: described chlorine dioxide precursor comprises the mixture of one or more compositions in sodium chlorite, potassium chlorite, barium chlorite, magnesium chlorite.
5. a kind of slow released ClO 2 powder being applicable to indoor air purification according to any one of claim 1 ~ 3, is characterized in that: described activator comprises the mixture of one or more compositions in sodium bisulfate, sodium sulfate, potassium acid sulfate, potassium sulfate, Magnesium hydrogen sulfate.
6. a kind of slow released ClO 2 powder being applicable to indoor air purification according to any one of claim 1 ~ 3, is characterized in that: described slow releasing agent comprises the mixture of one or more compositions in macrogol, polyvinyl alcohol, polyacrylamide, crosslinked polyethylene.
7. a kind of slow released ClO 2 powder being applicable to indoor air purification according to any one of claim 1 ~ 3, is characterized in that: described gel is AQUAGEL PLUS gel.
8. a kind of slow released ClO 2 powder being applicable to indoor air purification according to any one of claim 1 ~ 3, is characterized in that: described filler is the mixture of one or more compositions in anhydrous sodium sulfate, anhydrous slufuric acid barium, anhydrous potassium sulfate, anhydrous magnesium sulfate.
CN201410434321.2A 2014-08-29 2014-08-29 Sustained-release chlorine dioxide powder applicable to purifying indoor air Pending CN104208733A (en)