CN104084451A - 机械零件塑性变形矫正的方法 - Google Patents

机械零件塑性变形矫正的方法 Download PDF

Info

Publication number
CN104084451A
CN104084451A CN201410303419.4A CN201410303419A CN104084451A CN 104084451 A CN104084451 A CN 104084451A CN 201410303419 A CN201410303419 A CN 201410303419A CN 104084451 A CN104084451 A CN 104084451A
Authority
CN
China
Prior art keywords
stress
plastic deformation
deformation
force
corrected
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410303419.4A
Other languages
English (en)
Other versions
CN104084451B (zh
Inventor
黄铁军
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhuhai long morning Technology Co., Ltd.
Original Assignee
WUXI WEIHAIDA MACHINERY MANUFACTURING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUXI WEIHAIDA MACHINERY MANUFACTURING Co Ltd filed Critical WUXI WEIHAIDA MACHINERY MANUFACTURING Co Ltd
Priority to CN201410303419.4A priority Critical patent/CN104084451B/zh
Publication of CN104084451A publication Critical patent/CN104084451A/zh
Application granted granted Critical
Publication of CN104084451B publication Critical patent/CN104084451B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种机械零件塑性变形矫正的方法,包括:首先检查零件塑性变形的方向,并检查塑性变形的大小;然后确定塑性变形的应力因素;然后对零件的变形部位进行局部高频加热,直至零件的局部产生晶相结构变化,然后对变形部位进行施加外部应力;所述外部应力根据根据应力因素进行确定。本发明所述的机械零件塑性变形矫正的方法,是针对零件的塑性变形进行设计,在实施的过程中,需要针对塑性变形的大小、变形的区域以及变形所致的应力因素进行修复,而在修复的过程中采用高频加热,对于变形部位来说,借助外力的作用可以逐步将变形部位恢复至原始形状。

Description

机械零件塑性变形矫正的方法
技术领域
本发明涉及一种机械零件塑性变形矫正的方法,属于是对机械零件产生的塑性变形进行矫正的方法。
背景技术
矿山机械配件在使用过程中的零件,变形是不可避免的,因此,在矿山机械大修时不能只检查配合面的磨损情况,对于相互位置精度也必须认真检查和修复。尤其对第一次大修矿山机械的变形情况要注意检查、修复,因为零件在内应力作用下的变形,通常在12—20个月内完成。
机械零件在长期使用条件下,会产生一定的塑性变形,这些塑性变形一般直接导致整个机械零件的报废,所以塑性变形对设备带来的损害非常大,而且也使整个机械设备的维修保养成本相当高。
经过统计和试验发现,有些塑性变形是可以通过人力进行复原的,这样就可以让机械零件重新投入使用,而这样复原的成本往往比购买一个新的零件的成本要低很多,特别是对一些大批量使用的零件,这些复原和矫正就显得非常有必要。
 
发明内容
为了解决机械零件塑性变形进行矫正和复原的问题,本发明提供一种机械零件塑性变形矫正的方法。
本发明的目的通过以下技术方案来具体实现:
机械零件塑性变形矫正的方法,包括:
首先检查零件塑性变形的方向,并检查塑性变形的大小;
然后确定塑性变形的应力因素;
然后对零件的变形部位进行局部高频加热,直至零件的局部产生晶相结构变化,然后对变形部位进行施加外部应力;
所述外部应力根据根据应力因素进行确定;
所述外形应力采用曲面结构并且采用多点施力复原,针对变形位置最大的部位,施加的外部应力也最大,然后根据变形的大小逐步缩小应力,当外部变形不太明显时,只围绕变形部位的中心对变形部位的一半施加外部应力,然后在外部应力的作用下,会有部分变形复原至初始状态,此时要逐步缩小外部应力的施加面积;
然后逐渐减少高频加热的温度,一般采用阶梯式降温,直至降温至室温为止;
对于零件复原后仍有残缺或磨损的部位,采用局部舒缓的方式进行找平;
然后再对找平的部位进行高频加热,然后重复阶梯式降温至室温;
最后再次检测零件是否有应力残余,如果有应力残余则再做一次应力消除。
对零件的磨损部位进行修补;
修补后的零件如果有新的应力产生,重新将零件置于高温条件下直至应力消除。
所述变形应力采用多点施加,并且每个应力点均采用曲面结构。
所述应力因素包括是单次应力、持续应力还是多次应力重复,或者是多次大小不同的应力,并且还包括是应力形成过程中是尖端施力、曲面施力、平面施力还是不规则表面施力。
本发明所述的机械零件塑性变形矫正的方法,是针对零件的塑性变形进行设计,在实施的过程中,需要针对塑性变形的大小、变形的区域以及变形所致的应力因素进行修复,而在修复的过程中采用高频加热,对于变形部位来说,借助外力的作用可以逐步将变形部位恢复至原始形状。
具体实施方式
本发明实施例所述的机械零件塑性变形矫正的方法,包括:
首先检查零件塑性变形的方向,并检查塑性变形的大小;
然后确定塑性变形的应力因素;
然后对零件的变形部位进行局部高频加热,直至零件的局部产生晶相结构变化,然后对变形部位进行施加外部应力;
所述外部应力根据根据应力因素进行确定;
所述外形应力采用曲面结构并且采用多点施力复原,针对变形位置最大的部位,施加的外部应力也最大,然后根据变形的大小逐步缩小应力,当外部变形不太明显时,只围绕变形部位的中心对变形部位的一半施加外部应力,然后在外部应力的作用下,会有部分变形复原至初始状态,此时要逐步缩小外部应力的施加面积;
然后逐渐减少高频加热的温度,一般采用阶梯式降温,直至降温至室温为止;
对于零件复原后仍有残缺或磨损的部位,采用局部舒缓的方式进行找平;
然后再对找平的部位进行高频加热,然后重复阶梯式降温至室温;
最后再次检测零件是否有应力残余,如果有应力残余则再做一次应力消除。
对零件的磨损部位进行修补;
修补后的零件如果有新的应力产生,重新将零件置于高温条件下直至应力消除。
所述变形应力采用多点施加,并且每个应力点均采用曲面结构。
所述应力因素包括是单次应力、持续应力还是多次应力重复,或者是多次大小不同的应力,并且还包括是应力形成过程中是尖端施力、曲面施力、平面施力还是不规则表面施力。
本发明所述的机械零件塑性变形矫正的方法,是针对零件的塑性变形进行设计,在实施的过程中,需要针对塑性变形的大小、变形的区域以及变形所致的应力因素进行修复,而在修复的过程中采用高频加热,对于变形部位来说,借助外力的作用可以逐步将变形部位恢复至原始形状。

Claims (4)

1.机械零件塑性变形矫正的方法,包括:
首先检查零件塑性变形的方向,并检查塑性变形的大小;
然后确定塑性变形的应力因素;
然后对零件的变形部位进行局部高频加热,直至零件的局部产生晶相结构变化,然后对变形部位进行施加外部应力;
所述外部应力根据根据应力因素进行确定;
所述外形应力采用曲面结构并且采用多点施力复原,针对变形位置最大的部位,施加的外部应力也最大,然后根据变形的大小逐步缩小应力,当外部变形不太明显时,只围绕变形部位的中心对变形部位的一半施加外部应力,然后在外部应力的作用下,会有部分变形复原至初始状态,此时要逐步缩小外部应力的施加面积;
然后逐渐减少高频加热的温度,一般采用阶梯式降温,直至降温至室温为止;
对于零件复原后仍有残缺或磨损的部位,采用局部舒缓的方式进行找平;
然后再对找平的部位进行高频加热,然后重复阶梯式降温至室温;
最后再次检测零件是否有应力残余,如果有应力残余则再做一次应力消除。
2.如权利要求1所述的机械零件塑性变形矫正的方法,其特征在于,对零件的磨损部位进行修补;
修补后的零件如果有新的应力产生,重新将零件置于高温条件下直至应力消除。
3.如权利要求1所述的机械零件塑性变形矫正的方法,其特征在于,所述变形应力采用多点施加,并且每个应力点均采用曲面结构。
4.如权利要求1所述的机械零件塑性变形矫正的方法,其特征在于,所述应力因素包括是单次应力、持续应力还是多次应力重复,或者是多次大小不同的应力,并且还包括是应力形成过程中是尖端施力、曲面施力、平面施力还是不规则表面施力。
CN201410303419.4A 2014-06-30 2014-06-30 机械零件塑性变形矫正的方法 Expired - Fee Related CN104084451B (zh)