CN104084111A - 一种借助于稀土元素改性的氨气体吸附剂 - Google Patents

一种借助于稀土元素改性的氨气体吸附剂 Download PDF

Info

Publication number
CN104084111A
CN104084111A CN201410358637.8A CN201410358637A CN104084111A CN 104084111 A CN104084111 A CN 104084111A CN 201410358637 A CN201410358637 A CN 201410358637A CN 104084111 A CN104084111 A CN 104084111A
Authority
CN
China
Prior art keywords
earth element
rare earth
ammonia gas
gas adsorbent
slag
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410358637.8A
Other languages
English (en)
Inventor
不公告发明人
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Qingdao Bo Ruilin New Material Co Ltd
Original Assignee
Qingdao Bo Ruilin New Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Qingdao Bo Ruilin New Material Co Ltd filed Critical Qingdao Bo Ruilin New Material Co Ltd
Priority to CN201410358637.8A priority Critical patent/CN104084111A/zh
Publication of CN104084111A publication Critical patent/CN104084111A/zh
Pending legal-status Critical Current

Abstract

本发明的目的是提供一种借助于稀土元素改性的氨气体吸附剂,为实现上述目的,本发明采用的技术方案如下:将燃煤炉渣粉碎,取一定量炉渣粉,放入质量分数为5%的盐酸溶液中,慢速搅拌以去除表面有机物及其它杂质,待1-5h后过滤取出,用去离子水反复冲洗几次,再投入到2-6%的稀土元素氯化物氯化镧溶液中,在室温20℃下浸渍,待6-12h后取出于600℃焙烧1-5h,装瓶备用,即得该氨气吸附剂。

Description

一种借助于稀土元素改性的氨气体吸附剂
技术领域
本发明涉及氨气吸附领域,具体涉及一种借助于稀土元素改性的氨气体吸附剂。
背景技术
氨气,无机化合物,常温下为气体,无色有刺激性恶臭的气体,易溶于水,氨溶于水时,氨分子跟水分子通过氢键结合成一水合氨,一水合氨能小部分电离成氨离子和氢氧根离子,故氨水显弱碱性,能灼伤皮肤、眼睛、呼吸器官的粘膜,人吸入过多,能引起肺肿胀,以致死亡。
由于城市污水及工业废水的大量产生,以及尾气排放,造成环境越来越恶化。情况的日益严重,致使治理工作势在必行。
吸附法是处理废水和废气中有害和难降解污染物的一种重要的物化方法, 活性炭是最常用的吸附材料, 但由于原料缺乏、成本较高、再生困难等原因使其应用受到限制。以工业和农业废弃物为原料,制备和开发廉价、高效吸附材料取代活性炭是吸附材料研究的重要方向。
发明内容
本发明的目的是提供一种借助于稀土元素改性的氨气体吸附剂,以克服现有技术存在的原料缺乏,成本高的缺点。为实现上述目的,本发明采用的技术方案如下:
将燃煤炉渣粉碎,取一定量炉渣粉, 放入质量分数为5%的盐酸溶液中,慢速搅拌以去除表面有机物及其它杂质,待1-5h后过滤取出,用去离子水反复冲洗几次,再投入到2-6%的稀土元素氯化物氯化镧溶液中,在室温20℃下浸渍,待6-12h后取出于600℃焙烧1-5h,装瓶备用,即得该氨气吸附剂。
在本发明具有以下显著特点:
(1) 发明所述氨气吸附剂,原料来源广泛,价格低廉; 
(2) 发明所述氨气吸附剂制备方法简单,吸附率高;
(3) 发明所述氨气吸附剂性能稳定,寿命长,可以长期保存使用。
具体实施方式:
实施例1:
将燃煤炉渣粉碎,称取100 g 粉煤灰,放入质量分数为5%的盐酸溶液中,慢速搅拌以去除表面有机物及其它杂质,待1h后过滤取出,用去离子水反复冲洗3次,再投入到2%的稀土元素氯化物氯化镧溶液中,在室温20℃下浸渍,待6h后取出于600℃焙烧1h,装瓶备用,即得该氨气吸附剂。
实施例2:
将燃煤炉渣粉碎,称取100 g 粉煤灰,放入质量分数为5%的盐酸溶液中,慢速搅拌以去除表面有机物及其它杂质,待3h后过滤取出,用去离子水反复冲洗3次,再投入到3%的稀土元素氯化物氯化镧溶液中,在室温20℃下浸渍,待8h后取出于600℃焙烧3h,装瓶备用,即得该氨气吸附剂。
实施例3:
将燃煤炉渣粉碎,称取100 g 粉煤灰,放入质量分数为5%的盐酸溶液中,慢速搅拌以去除表面有机物及其它杂质,待5h后过滤取出,用去离子水反复冲洗3次,再投入到6%的稀土元素氯化物氯化镧溶液中,在室温20℃下浸渍,待12h后取出于600℃焙烧5h,装瓶备用,即得该氨气吸附剂。

Claims (1)

1.本发明公开了一种借助于稀土元素改性的氨气体吸附剂,为实现上述目的,本发明采用的技术方案如下:
将燃煤炉渣粉碎,取一定量炉渣粉, 放入质量分数为5%的盐酸溶液中,慢速搅拌以去除表面有机物及其它杂质,待1-5h后过滤取出,用去离子水反复冲洗几次,再投入到2-6%的稀土元素氯化物氯化镧溶液中,在室温20℃下浸渍,待6-12h后取出于600℃焙烧1-5h,装瓶备用,即得该氨气吸附剂。
CN201410358637.8A 2014-07-26 2014-07-26 一种借助于稀土元素改性的氨气体吸附剂 Pending CN104084111A (zh)