CN104043815A CN201410303524.8A CN201410303524A CN104043815A CN 104043815 A CN104043815 A CN 104043815A CN 201410303524 A CN201410303524 A CN 201410303524A CN 104043815 A CN104043815 A CN 104043815A
Authority
CN
China
Prior art keywords
working lining
ladle
maintaining
filled
boring
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410303524.8A
Other languages
English (en)
Inventor
李志强
李安刚
张成功
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Henan Bamboo Grove Nai Cai Co Ltd
Original Assignee
Henan Bamboo Grove Nai Cai Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Henan Bamboo Grove Nai Cai Co Ltd filed Critical Henan Bamboo Grove Nai Cai Co Ltd
Priority to CN201410303524.8A priority Critical patent/CN104043815A/zh
Publication of CN104043815A publication Critical patent/CN104043815A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Furnace Housings, Linings, Walls, And Ceilings (AREA)

Abstract

本发明公开了一种钢包工作衬的钻孔填充维修方法,将钢包冷却,内壁杂物清理干净,用圆柱形空心钻头将砖钻出,孔径30~80mm,钻孔深度5~10cm,内部清理干净,然后将相同直径大小、长度的圆柱形砖填充进去,填充至原工作面相平,周边缝隙用火泥填充,利用原工作衬余温或再次盛装钢水时的高温使火泥水分蒸发,使填充物与原工作衬结合。本发明维修方法方便实用,简单易行,成本低,适用于包壁或者渣线工作衬为镁碳砖或者铝镁碳砖的钢包的维修,也适用于铝碳化硅碳砖的铁包维修。

Description

一种钢包工作衬的钻孔填充维修方法
技术领域
本发明涉及一种钢包工作衬的钻孔填充维修方法,属于钢铁冶金钢包内衬的维修方法技术领域。
背景技术
钢包在使用中经常出现局部侵蚀严重或者熔洞,造成钢包寿命终止或者需要维修,目前,一般采用挖修或者从上部拆至出现问题部位,然后重新砌筑。但是,挖修容易出现补砖再次掉落,造成事故;如果拆修,需要从上部至问题部位拆成“V”字型,如果找不到砌筑平面需要继续往下部拆,如果熔洞面积很小,按此种修补方法导致投入成本增加。
发明内容
为克服上述问题,本发明的目的在于提供一种钢包工作衬钻孔填充的维修方法。
为实现上述目的,本发明采用如下技术方案:
一种钢包工作衬的钻孔填充维修方法,所述方法包括: 
将钢包冷却,内壁杂物清理干净,用圆柱形空心钻头将砖钻出,孔径30~80 mm,钻孔深度5~10 cm,内部清理干净,然后将相同直径大小、长度的圆柱形砖填充进去,填充至原工作面相平,周边缝隙用火泥填充,利用原工作衬余温或再次盛装钢水时的高温使火泥水分蒸发,使填充物与原工作衬结合。
根据上述的钢包工作衬的钻孔填充维修方法,所述的维修方法适用条件为:当钢包正常使用中,内壁有明显的凹陷,低于周边2~3 cm或者周边平滑,中间出现熔洞,对钢包进行维修。
根据上述的钢包工作衬的钻孔填充维修方法,所述的圆柱形砖材质与钢包工作衬材质相同。
根据上述的钢包工作衬的钻孔填充维修方法,所述的火泥的材质与钢包工作衬的材质相同。
本发明的积极有益效果
1、本发明钢包工作衬的钻孔填充维修方法方便实用,简单易行,成本低,适用于包壁或者渣线工作衬为镁碳砖或者铝镁碳砖的钢包的维修,也适用于铝碳化硅碳砖的铁包维修。
2、本发明钢包工作衬的钻孔填充维修方法维修周期短,钢包运转率高,降低维修工人劳动强度。
3、本发明通过钻孔填充修补,不破坏原有的烧结结构,对钢包的损伤程度降低到最低,大大提高安全性。
4、本发明填充所用圆柱形砖可提前生产,使用这种产品,可避免原有的因拆修造成的尺寸不固定,需要在砌筑现场不断切砖,不但造成材料浪费,而且容易因切砖不规范造成砌筑后有缝隙,出现漏钢、穿包现象。
具体实施方式
    下面结合一些具体实施例对本发明进一步说明。
实施例1
在广东韶关钢铁厂120吨钢的生产上试验成功,钢包包壁工作衬和包底工作衬为镁碳砖,理化指标:MgO≥67%,C≥8%,体积密度≥2.85g/cm3,常温耐压≥35Mpa,显气孔率≤8%;渣线工作衬为镁碳砖,理化指标:MgO≥72%,C≥13%,体积密度≥2.90g/cm3,常温耐压≥40 MPa,显气孔率≤4%;包壁工作衬厚度150~200 mm,渣线工作衬220~230 mm,包底工作衬230~250 mm。
上述钢包工作衬的钻孔填充维修方法为: 
当钢包正常使用中,发现内壁有明显的凹陷,低于周边2~3 cm或者周边很平滑,中间出现熔洞,熔洞较深,观察明显的时候,对钢包进行维修,首先将钢包冷却,内壁杂物清理干净,用直径50 mm空心钻头将出现熔洞部位的砖钻出,钻深8 cm,内部清理干净,然后将直径大小50 mm、长度8 cm的圆柱形镁碳砖填充进去,周边缝隙用镁碳火泥填充,使填充内壁与原来工作面相平,利用原工作衬余温或再次盛装钢水时的高温即可实现火泥水分的蒸发,火泥烧结后达到填充物与原工作衬的结合。使用本发明维修方法,广东韶关钢铁厂120吨钢包使用次数达到95次,工作衬使用周期为3~4天,每天冶炼20~30次,每次盛钢15~35 min。

Claims (4)

1.一种钢包工作衬的钻孔填充维修方法,其特征在于,所述方法为:将钢包冷却,内壁杂物清理干净,用圆柱形空心钻头将砖钻出,孔径30~80 mm,钻孔深度5~10 cm,内部清理干净,然后将相同直径大小、长度的圆柱形砖填充进去,填充至原工作面相平,周边缝隙用火泥填充,利用原工作衬余温或再次盛装钢水时的高温使火泥水分蒸发,使填充物与原工作衬结合。
2.根据权利要求1所述的钢包工作衬的钻孔填充维修方法,其特征在于,所述的维修方法适用条件为:当钢包正常使用中,内壁有明显的凹陷,低于周边2~3 cm或者周边平滑,中间出现熔洞,对钢包进行维修。
3.根据权利要求1所述的钢包工作衬的钻孔填充维修方法,其特征在于,所述的圆柱形砖材质与钢包工作衬材质相同。
4.根据权利要求1所述的钢包工作衬的钻孔填充维修方法,其特征在于,所述火泥的材质与钢包工作衬材质相同。
CN201410303524.8A 2014-06-30 2014-06-30 一种钢包工作衬的钻孔填充维修方法 Pending CN104043815A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410303524.8A CN104043815A (zh) 2014-06-30 2014-06-30 一种钢包工作衬的钻孔填充维修方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410303524.8A CN104043815A (zh) 2014-06-30 2014-06-30 一种钢包工作衬的钻孔填充维修方法

Publications (1)

Publication Number Publication Date
CN104043815A true CN104043815A (zh) 2014-09-17

Family

ID=51497481

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410303524.8A Pending CN104043815A (zh) 2014-06-30 2014-06-30 一种钢包工作衬的钻孔填充维修方法

Country Status (1)

Country Link
CN (1) CN104043815A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106424692A (zh) * 2016-10-26 2017-02-22 舞阳钢铁有限责任公司 一种电炉用钢包小修或挖修的砌筑修补方法
CN111438350A (zh) * 2020-05-21 2020-07-24 北京联合荣大工程材料股份有限公司 一种钢包工作衬砖的修补方法

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH11267820A (ja) * 1998-03-24 1999-10-05 Kurosaki Refract Co Ltd 溶鋼通過孔の内面の補修材とその補修材を使用する溶鋼通過孔の内面の補修方法
CN101844224A (zh) * 2009-03-23 2010-09-29 鞍钢股份有限公司 一种钢包透气砖热修补方法
CN203401074U (zh) * 2013-08-28 2014-01-22 武汉钢铁集团精鼎工业炉有限责任公司 一种钢包透气座砖热态修补装置
CN103736985A (zh) * 2014-01-11 2014-04-23 莱芜钢铁集团有限公司 一种钢包工作衬及其渣线部位的修砌方法

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH11267820A (ja) * 1998-03-24 1999-10-05 Kurosaki Refract Co Ltd 溶鋼通過孔の内面の補修材とその補修材を使用する溶鋼通過孔の内面の補修方法
CN101844224A (zh) * 2009-03-23 2010-09-29 鞍钢股份有限公司 一种钢包透气砖热修补方法
CN203401074U (zh) * 2013-08-28 2014-01-22 武汉钢铁集团精鼎工业炉有限责任公司 一种钢包透气座砖热态修补装置
CN103736985A (zh) * 2014-01-11 2014-04-23 莱芜钢铁集团有限公司 一种钢包工作衬及其渣线部位的修砌方法

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106424692A (zh) * 2016-10-26 2017-02-22 舞阳钢铁有限责任公司 一种电炉用钢包小修或挖修的砌筑修补方法
CN111438350A (zh) * 2020-05-21 2020-07-24 北京联合荣大工程材料股份有限公司 一种钢包工作衬砖的修补方法
CN111438350B (zh) * 2020-05-21 2021-09-10 北京联合荣大工程材料股份有限公司 一种钢包工作衬砖的修补方法

Similar Documents

Publication Publication Date Title
CN108690893A (zh) 高炉铁口流铁孔道的修复方法
CN104043815A (zh) 一种钢包工作衬的钻孔填充维修方法
CN104141021A (zh) 一种高炉开铁口的方法及高炉开铁口设备系统
CN101892337B (zh) 一种高炉铁口的维护方法
CN204939506U (zh) 一种阻止高炉炉缸底部温度升高的装置
AU2014363701B2 (en) Tap-hole refurbishing
CN103011858B (zh) 高炉出铁口用炮泥
CN106702073A (zh) 一种转炉底吹元件热更换方法
CN204017916U (zh) 一种锤式破碎机筛板结构
CN202157079U (zh) 用于放堵残铁的铁沟残铁孔
CN201746559U (zh) 一种快速处理铁口泥套的工具
CN201778038U (zh) 高炉铁口灌浆压头
CN207308957U (zh) 改进的连铸中间包
JP5920026B2 (ja) 転炉底吹き羽口の熱間設置方法
EP1233077B1 (en) Apparatus for repairing blast furnace taphole facings
CN101748224B (zh) 高炉解剖时分区冷却高炉的方法
CN206636223U (zh) 一种模板拉杆的处理结构
CN105041197A (zh) 一种在基岩破碎带中的大直径竖井孔内反循环成孔施工方法
CN103900429B (zh) 一种混凝土空心立柱的爆破方法
CN208532838U (zh) 一种高炉、初炼炉堵铁口耐火钻杆及堵铁口装置
CN113213961B (zh) 一种陶瓷内衬复合钢管孔加工工艺
CN207648814U (zh) 一种工业危险废物出渣机的链排回程滑道
CN103757166A (zh) 一种高炉铁口孔道压浆方法
CN202532888U (zh) 一种出钢口砖
CN203764968U (zh) 一种用于精炼钢包渣线的预制件

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
AD01 Patent right deemed abandoned

Effective date of abandoning: 20161019

C20 Patent right or utility model deemed to be abandoned or is abandoned