CN104029551A - 钢琴外壳涂层树脂色浆手工绘画生产工艺 - Google Patents
钢琴外壳涂层树脂色浆手工绘画生产工艺 Download PDFInfo
- Publication number
- CN104029551A CN104029551A CN201410268187.3A CN201410268187A CN104029551A CN 104029551 A CN104029551 A CN 104029551A CN 201410268187 A CN201410268187 A CN 201410268187A CN 104029551 A CN104029551 A CN 104029551A
- Authority
- CN
- China
- Prior art keywords
- mill base
- piano
- color
- unsaturated polyester
- color paste
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明提供一种钢琴外壳涂层树脂色浆手工绘画生产工艺,采用以下步骤:挑选用料;外壳木质表面处理;不饱和聚酯树脂漆涂底漆;干燥;研磨;手工绘画:用色浆颜料把预备好的景物、名画手工绘制在外壳涂层漆面上,所述色浆颜料为采用画面所需的树脂色浆与不饱和聚酯树脂、促进剂、固化剂、苯乙烯进行调制,达到一种色浆能遮盖住另一种颜色,而且在手工绘画过程中,需要控制两种颜色之间的间隔;干燥;不饱和聚酯树脂油漆在画好的画面上涂面漆;干燥;研磨;抛光。本发明用树脂色浆作颜料,并与不饱和聚酯树脂、促进剂、固化剂、苯乙烯进行调制后,通过手工绘画艺术把各种景物名画绘制钢琴外壳涂层内,所画的景物清晰透明,极大地提高了钢琴外观之美。
Description
技术领域
本发明涉及—种钢琴外壳涂层树脂色浆手工绘画生产工艺,属于绘画工艺技术领域。
背景技术
随着人们物质文化生活水平的提高,钢琴单纯声音好的内在美已不能满足人们的需求,而即具有内在美,同时又具有欣赏收藏价值的外观美的艺术钢琴,才是当今社会对钢琴的完美追求,使钢琴在具有演奏价值的同时也具有欣赏收藏价值。
发明内容
针对以上不足,本发明提供一种钢琴外壳涂层树脂色浆手工绘画生产工艺,用树脂色浆把人们最喜爱的景物名画手工绘画到钢琴外壳油漆涂层内,经干燥研磨抛光后,达到外壳画面景物清晰透明,光亮如镜。
本发明的目的是通过下述技术方案实现的,钢琴外壳涂层树脂色浆手工绘画生产工艺,采用以下步骤:
(1)挑选用料:选取无腐蚀、暇庇木质板材作为外壳,干燥后备用;
(2)外壳木质表面处理:达到光、平;
(3)涂底漆:涂刷不饱和聚酯树脂漆2至3遍;
(4)干燥:在温度24-30℃、空气湿度20-40%的室内干燥24-36小时;
(5)研磨:用260-300目砂纸轻砂;
(6)手工绘画:用色浆颜料把预备好的景物、名画手工绘制在外壳底涂漆面上;
(7)干燥:在温度24-30℃、空气湿度30-60%的室内干燥24-36小时;
(8)涂面漆:用不饱和聚酯树脂油漆在画好的景物画面上刷涂3-5遍;
(9)干燥:在温度24-30℃、空气湿度30-40%的室内干燥72小时以上;
(10)研磨:依次用280、400、600、800、1000目砂纸研磨;
(11)抛光:用专用抛光机抛光达到光、平、亮。
所述步骤(6)采用的色浆颜料,其调制方法为:将画面所需的树脂色浆与不饱和聚酯树脂、促进剂、固化剂、苯乙烯进行调制,达到一种色浆能遮盖住另一种颜色。
所述步骤(6)在手工绘画过程中,需要控制两种颜色之间的间隔,即画一种颜色时,在该颜色干了之后才能绘制下一个颜色。
本发明的优点:本发明通过把树脂色浆与不饱和聚酯树脂、促进剂、固化剂、苯乙烯有机调和,形成绘画色浆颜料,利用绘画大师的手工绘画到钢琴外壳油漆涂层内,通过研磨抛光后,涂层画面景物犹如镜中观画,水中望月。钢琴外观配上雕刻镶嵌描金,全琴浑然一体,相得益彰,让人们在聆听优美音乐之余,欣赏艺术之美,品味艺术享受。
具体实施方式
钢琴外壳涂层树脂色浆手工绘画生产工艺,采用以下步骤:
(1)挑选用料:选取无腐蚀、暇庇木质板材作为外壳,干燥后备用;
(2)外壳木质表面处理:达到光、平;
(3)涂底漆:涂刷不饱和聚酯树脂漆2至3遍;
(4)干燥:在温度24-30℃、空气湿度20-40%的室内干燥24-36小时;
(5)研磨:用80-120目砂纸轻砂;
(6)手工绘画:用色浆颜料把预备好的景物、名画手工绘制在外壳底涂漆面上,所述色浆颜料为采用画面所需的树脂色浆与不饱和聚酯树脂、促进剂、固化剂、苯乙烯进行调制,达到一种色浆能遮盖住另一种颜色,而且在手工绘画过程中,需要控制两种颜色之间的间隔,即画一种颜色时,在该颜色干透之后才能绘制下一个颜色;
(7)干燥:在温度24-30℃、空气湿度30-60%的室内干燥24-36小时;
(8)涂面漆:用不饱和聚酯树脂油漆在画好的画面上刷涂3-5遍;
(9)干燥:在温度24-30℃、空气湿度30-40%的室内干燥72小时以上;
(10)研磨:依次用280、400、600、800、1000目砂纸研磨;
(11)抛光:用专用抛光机抛光达到光、平、亮。
本发明用树脂色浆作颜料,并与不饱和聚酯树脂、促进剂、固化剂、苯乙烯进行调制后,通过手工绘画艺术把各种景物名画绘制钢琴外壳涂层内,所画的景物清晰透明,极大地提高了钢琴外观之美。
Claims (3)
1.钢琴外壳涂层树脂色浆手工绘画生产工艺,其特征在于采用以下步骤:
(1)挑选用料:选取无腐蚀、暇庇木质板材作为外壳,干燥后备用;
(2)外壳木质表面处理:达到光、平;
(3)涂底漆:涂刷不饱和聚酯树脂漆2至3遍;
(4)干燥:在温度24-30℃、空气湿度20-40%的室内干燥24-36小时;
(5)研磨:用260-300目砂纸轻砂;
(6)手工绘画:用色浆颜料把预备好的景物、名画手工绘制在外壳底涂漆面上;
(7)干燥:在温度24-30℃、空气湿度30-60%的室内干燥24-36小时;
(8)涂面漆:用不饱和聚酯树脂油漆在画好的景物画面上刷涂3-5遍;
(9)干燥:在温度24-30℃、空气湿度30-40%的室内干燥72小时以上;
(10)研磨:依次用280、400、600、800、1000目砂纸研磨;
(11)抛光:用专用抛光机抛光达到光、平、亮。
2.如权利要求1所述的钢琴外壳涂层树脂色浆手工绘画生产工艺,其特征在于所述步骤(6)采用的色浆颜料,其调制方法为:将画面所需的树脂色浆与不饱和聚酯树脂、促进剂、固化剂、苯乙烯进行调制,达到一种色浆能遮盖住另一种颜色。
3.如权利要求1所述的钢琴外壳涂层树脂色浆手工绘画生产工艺,其特征在于所述步骤(6)在手工绘画过程中,需要控制两种颜色之间的间隔,即画一种颜色时,在该颜色干透之后才能绘制下一个颜色。