CN104017287A CN201310064920.5A CN201310064920A CN104017287A CN 104017287 A CN104017287 A CN 104017287A CN 201310064920 A CN201310064920 A CN 201310064920A CN 104017287 A CN104017287 A CN 104017287A
Authority
CN
China
Prior art keywords
resistant
aging
heat
elastomer material
pvc
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310064920.5A
Other languages
English (en)
Inventor
章磊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201310064920.5A priority Critical patent/CN104017287A/zh
Publication of CN104017287A publication Critical patent/CN104017287A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Compositions Of Macromolecular Compounds (AREA)
  • Injection Moulding Of Plastics Or The Like (AREA)

Abstract

本发明提供一种耐热耐磨抗老化PVC弹性体材料,通过添加CPVC树脂、铝酸酯偶联剂、亚磷酸酯、多元醇和氢氧化铝等成分,并限定各成分的含量,使添加的成分之间起到很好的协同作用,在保持了原有的二次注塑成型率高的基础上,其耐热性、耐磨性得到了显著增强,并且不容易老化,使用寿命长,其机械性能也得到了一定的加强。

Description

一种耐热耐磨抗老化PVC弹性体材料
技术领域
本发明涉及一种PVC弹性体材料,尤其是一种耐热耐磨抗老化PVC弹性体材料。
背景技术
现有技术中为解决PVC弹性体材料二次注塑成型效果不理想,注塑成品率低的问题,通过在PVC材料中添加氟醋、SBS、碳酸钙、硬脂酸等提高了二次注塑成型率,但是改进后的PVC材料耐热性、耐磨性均较差,并且容易老化,严重影响了PVC材料的使用。
发明内容
本发明提供一种耐热耐磨抗老化PVC弹性体材料,通过添加CPVC树脂、铝酸酯偶联剂、亚磷酸酯、多元醇和氢氧化铝等成分,并限定各成分的含量,使添加的成分之间起到很好的协同作用,在保持了原有的二次注塑成型率高的基础上,其耐热性、耐磨性得到了显著增强,并且不容易老化,使用寿命长,其机械性能也得到了一定的加强。
本发明提供一种耐热耐磨抗老化PVC弹性体材料,其组分及重量百分比为:
余量为CPVC树脂,并且纳米碳酸钙的粒子直径在30-50nm之间。
优选的方案为还包括低碱玻璃纤维,重量百分比为0.4-1.0,并且长度在0.8-2.5mm之间。
优选的方案为还包括马来酸酐,重量百分比为0.2-0.4。
本发明的与现有PVC材料相比,耐热性、耐磨性得到了显著增强,并且不容易老化,使用寿命长,其机械性能也得到了一定的加强,可以广泛应用到制鞋等二次注塑成型生产工艺中。
具体实施方式
下面对本发明作进一步详细的说明。
实施例1
一种耐热耐磨抗老化PVC弹性体材料,其组分及重量百分比为:
余量为CPVC树脂,并且纳米碳酸钙的粒子直径在30-50nm之间。
实施例2
对实施例1中的耐热耐磨抗老化PVC弹性体材料(记为样品1)和现有的PVC弹性体材料(记为样品2)进行耐热性和二次注塑成型率对比。
现有耐热耐磨PVC管材的按照下述重量配比准备原料:
PVC树脂50份,硬脂酸钙2.5份,硬脂酸锌1.5份,硬脂酸1.3份,氟醋12份,热塑性丁苯橡胶20份,碳酸钙80份。
经检测发现,样品1的Tg温度为116度,样品2的Tg温度88度;样品1的二次注塑成型率为99%,样品2的二次注塑成型率为97%。
由此可知,本发明的产品耐热性更好,二次注塑成型率基本保持不变。
实施例3
对样品1和样品2使用寿命进行实验检测:
样品1在平均温度为20度的室外环境中放置,发现330天后开始变为黄色;样品2在146天后即开始变为黄色。加入马来酸酐,样品1在同样的环境中385天后开始变为黄色。
说明本发明的产品不容易老化,使用寿命更长,通过实验发现,样品1相比样品2其耐磨性也得到了显著增强。
实施例4
对样品1和样品2进行机械性能检测:
发现样品1的弯曲强度为112MPa,压缩强度为83MPa,悬臂梁冲击强度为95.1J/m;样品2的弯曲强度为102MPa,压缩强度为76MPa,悬臂梁冲击强度为90.2J/m。加入重量百分比为0.4-1.0,并且长度在0.8-2.5mm之间的低碱玻璃纤维后,弯曲强度为135MPa,压缩强度为96MPa,悬臂梁冲击强度为110.2J/m。
由上述可知,本发明的机械性能得到了一定的加强。
以上内容是结合本发明的结构和工作过程对其所作的进一步详细说明,不能认定本发明的具体实施只局限于这些说明。对于本发明所属技术领域的普通技术人员来说,在不脱离本发明构思的前提下,还可以做出若干简单推演或替换,都应当视为属于本发明的保护范围。

Claims (3)

1.一种耐热耐磨抗老化PVC弹性体材料,其组分及重量百分比为:
余量为CPVC树脂,并且纳米碳酸钙的粒子直径在30-50nm之间。
2.根据权利要求1所述的耐热耐磨抗老化PVC弹性体材料,其特征在于:还包括低碱玻璃纤维,重量百分比为0.4-1.0,并且长度在0.8-2.5mm之间。
3.根据权利要求2所述的耐热耐磨抗老化PVC弹性体材料,其特征在于:还包括马来酸酐,重量百分比为0.2-0.4。
CN201310064920.5A 2013-02-28 2013-02-28 一种耐热耐磨抗老化pvc弹性体材料 Pending CN104017287A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201310064920.5A CN104017287A (zh) 2013-02-28 2013-02-28 一种耐热耐磨抗老化pvc弹性体材料

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201310064920.5A CN104017287A (zh) 2013-02-28 2013-02-28 一种耐热耐磨抗老化pvc弹性体材料

Publications (1)

Publication Number Publication Date
CN104017287A true CN104017287A (zh) 2014-09-03

Family

ID=51434304

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201310064920.5A Pending CN104017287A (zh) 2013-02-28 2013-02-28 一种耐热耐磨抗老化pvc弹性体材料

Country Status (1)

Country Link
CN (1) CN104017287A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108912545A (zh) * 2018-07-02 2018-11-30 芜湖航天特种电缆厂股份有限公司 抗老化电缆包装材料及其制备方法
CN109021437A (zh) * 2018-07-02 2018-12-18 芜湖航天特种电缆厂股份有限公司 抗紫外电缆包装材料及其制备方法

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101497727A (zh) * 2009-03-04 2009-08-05 南亚塑胶工业股份有限公司 一种pvc树脂组合物及其制品
CN102575070A (zh) * 2009-09-23 2012-07-11 巴斯夫欧洲公司 协同增效抗静电组合物
CN102850696A (zh) * 2012-09-20 2013-01-02 吴江市天源塑胶有限公司 一种高韧性聚氯乙烯管材
CN102863711A (zh) * 2011-07-06 2013-01-09 中国石油化工股份有限公司 一种耐热型pvc高抗冲管材及其制备方法
CN103102630A (zh) * 2011-11-14 2013-05-15 天津德昊超微新材料有限公司 一种氯化聚氯乙烯化工管件专用料

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101497727A (zh) * 2009-03-04 2009-08-05 南亚塑胶工业股份有限公司 一种pvc树脂组合物及其制品
CN102575070A (zh) * 2009-09-23 2012-07-11 巴斯夫欧洲公司 协同增效抗静电组合物
CN102863711A (zh) * 2011-07-06 2013-01-09 中国石油化工股份有限公司 一种耐热型pvc高抗冲管材及其制备方法
CN103102630A (zh) * 2011-11-14 2013-05-15 天津德昊超微新材料有限公司 一种氯化聚氯乙烯化工管件专用料
CN102850696A (zh) * 2012-09-20 2013-01-02 吴江市天源塑胶有限公司 一种高韧性聚氯乙烯管材

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
高俊刚,杨丽庭,李燕芳: "《改性聚氯乙烯新材料 第1版》", 31 October 2002, 化学工业出版社 *

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108912545A (zh) * 2018-07-02 2018-11-30 芜湖航天特种电缆厂股份有限公司 抗老化电缆包装材料及其制备方法
CN109021437A (zh) * 2018-07-02 2018-12-18 芜湖航天特种电缆厂股份有限公司 抗紫外电缆包装材料及其制备方法

Similar Documents

Publication Publication Date Title
BR112014018750A8 (pt) Polímero, processo e composição
BR112014010920A2 (pt) composição, e, método para preparar um (co)telômero
CN104292741A (zh) 一种abs复合材料及其制备方法
CN102367297A (zh) 一种高耐油氯丁胶弯管橡胶及其制备方法
CN104017288A (zh) 一种耐热耐磨抗老化pvc弹性体材料
CN104017287A (zh) 一种耐热耐磨抗老化pvc弹性体材料
CN103881181A (zh) 一种阻燃抗静电聚乙烯塑料及其制备方法
CN103289262B (zh) 一种耐热耐磨抗老化pvc弹性体材料
CN102719060A (zh) 一种高耐温高光泽pet/pbt复合材料及其制备方法
CN104448607A (zh) 一种高防火pvc-u管及其制备方法
CN105754259A (zh) 一种耐低温pvc管材及其制备方法
CN103289296A (zh) 高耐候性阻燃abs复合材料
CN103709631A (zh) 纳米复合材料增韧阻燃改性聚对苯二甲酸丁二醇酯
JP2014024995A (ja) タイヤ用ゴム組成物及びスタッドレスタイヤ
CN104017290A (zh) 一种新型耐热耐磨耐低温pvc管材
CN102070823B (zh) Aes树脂改性聚丙烯复合材料
CN107721284A (zh) 一种混凝土的配方
CN103289223B (zh) 一种耐热耐磨耐低温pvc管材
Liu et al. Research to performance of basalt fibre strengthen sbs modified asphalt mixture
CN104212119B (zh) 一种耐热水聚甲醛组合物及其制备方法
CN103724993B (zh) 一种快速吸水玻璃纤维增强尼龙6复合材料及其制备方法
BRPI0922894A8 (pt) Processo de preparo de um material polímero transparente, compreendendo nanopartículas minerais, tendo um fator de forma estritamente superior a 1,0
CN103937203A (zh) 一种汽车塑料件用聚氯乙烯改性聚苯醚材料
CN109401177B (zh) 一种耐高温耐磨苯乙烯弹性体
CN104341616A (zh) 一种阻燃耐老化橡胶电缆料及其制备方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
EXSB Decision made by sipo to initiate substantive examination
SE01 Entry into force of request for substantive examination
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20140903

WD01 Invention patent application deemed withdrawn after publication