CN104012458A - Method for preparing oxygen producer through byproduct large-particle sodium percarbonate - Google Patents

Method for preparing oxygen producer through byproduct large-particle sodium percarbonate Download PDF

Info

Publication number
CN104012458A
CN104012458A CN201410189663.2A CN201410189663A CN104012458A CN 104012458 A CN104012458 A CN 104012458A CN 201410189663 A CN201410189663 A CN 201410189663A CN 104012458 A CN104012458 A CN 104012458A
Authority
CN
China
Prior art keywords
sodium percarbonate
oxygen
byproduct
particle
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410189663.2A
Other languages
Chinese (zh)
Other versions
CN104012458B (en
Inventor
章小兵
章金龙
虞建立
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Jinke Daily Chemical New Materials Co ltd
Original Assignee
ZHEJIANG JINKE CHEMICALS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHEJIANG JINKE CHEMICALS CO Ltd filed Critical ZHEJIANG JINKE CHEMICALS CO Ltd
Priority to CN201410189663.2A priority Critical patent/CN104012458B/en
Publication of CN104012458A publication Critical patent/CN104012458A/en
Application granted granted Critical
Publication of CN104012458B publication Critical patent/CN104012458B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a method for preparing an oxygen producer through byproduct large-particle sodium percarbonate. The method is characterized by mainly comprising the following steps that (A) the byproduct large-particle sodium percarbonate and water are added to a mixer, the adding amount of the water is 1%-3% of the amount of the byproduct large-particle sodium percarbonate, the obtained mixture is stirred for 5 min to 10 min, and the mixture is pulverized by a pulverizer, wherein the byproduct large-particle sodium percarbonate particles are irregular particles, the mass percent of reactive oxygen of the byproduct large-particle sodium percarbonate is smaller than or equal to 10%, and the particle size of the byproduct large-particle sodium percarbonate is larger than or equal to 1.4 mm; (B) the pulverized materials enter a reactor, a hydrogen peroxide solution, a stabilizer and an adhesive are sprayed to the pulverized materials, granulation and drying are conducted, and the oxygen bearing sodium percarbonate of the oxygen producer is obtained; (C) the sodium percarbonate obtained in the step B and a release agent are evenly mixed according to the ratio of the sodium percarbonate to the release agent, i.e. 99.0-99.9 to 1-0.1, the materials are tabletted on a tabletting machine, and therefore the oxygen producer is prepared. Oxygen producing is conducted on aquatic water through the oxygen producer, manufacturing cost can be reduced, and pollution to the water and an environment by the oxygen producer is reduced.

Description

A kind of method of utilizing by-product bulky grain SODIUM PERCARBONATE to prepare oxygenation agent
Technical field
The invention belongs to chemical field, be specifically related to a kind of preparation method of oxygenation agent, particularly utilize by-product bulky grain SODIUM PERCARBONATE to prepare oxygenation agent method.
Background technology
Preparation SODIUM PERCARBONATE preparation technology is divided into wet method and dry method substantially both at home and abroad at present.The most important effect of SODIUM PERCARBONATE is as washing assisant, and in order to guarantee effective compatibility of itself and other cleaning ingredients, the particle diameter that is exactly generally product to one of quality requirement of SODIUM PERCARBONATE product is controlled need be between 0.3-1.4mm.And in the production process of percarbonic acid acid sodium, dry, packing technology etc. all can occur that fluidized-bed layer lumps and produces oarse-grained by product, by product accounts for the 5-30% left and right of output.In by product particulate material, soda ash content is higher simultaneously, causes the active oxygen of product on the low side, cannot normally use.For this underproof by-product bulky grain SODIUM PERCARBONATE, generally can only carry out relevant treatment using it as waste product landfill or as salkali waste, make manufacturing cost significantly increase on the one hand, cause on the other hand the wasting of resources, be also unfavorable for environmental protection.
While, along with cultural technique, aquaculture cost improves constantly, is to pursue high yield, and the fishes and shrimps stocking rate of unit water surface area is also more and more higher.But highdensity cultivation easily causes cultivation pool oxygen content on the low side, particularly fishes and shrimps more concentrated region oxygen content in bottom, pool is lower, can cause fishes and shrimps death by suffocation, particularly in weather sultry period.Therefore cultivation can be carried out oxygenation to pool per family over a period to come.
Existing oxygenation agent, oxygenation agent as difunctional in hydrogen peroxide phosphoamide and carbonic acid amide high oxygen-enriching agent, in these oxygenation agents, all contain the harmful substances such as organic matter and heavy metal ion, and with certain penetrating odor, in aquaculture, oxygen inhalation health, can produce certain harm to human body, be unfavorable for people's health; Oxygenation agent stability is bad simultaneously, and when temperature is higher or period of storage is longer, oxygenation agent easily decomposes, and active oxygen amount decline in use, effect reduce.
Summary of the invention
For overcoming above-mentioned defect of the prior art, the invention provides a kind of method of utilizing by-product bulky grain SODIUM PERCARBONATE to prepare oxygenation agent.The oxygenation agent that employing is prepared by the method carries out oxygenation to breeding water body can reduce manufacturing cost, and reduces the pollution of existing oxygenation agent to water body, environment.
Utilize by-product bulky grain SODIUM PERCARBONATE to prepare a method for oxygenation agent, it is characterized in that, mainly comprise the following steps:
(A) in blender, add by-product bulky grain SODIUM PERCARBONATE and water, the addition of water is the 1%-3% of by-product bulky grain percarbonic acid mass percent, stirs 5-10 minute, with cracker, pulverizes; Described by-product bulky grain SODIUM PERCARBONATE is the irregular particle of active oxygen≤10%, particle size >=1.4mm;
(B) material after pulverizing enters spray hydrogen peroxide solution and stabilizing agent and adhesive in reactor, carries out granulation, dries, obtain oxygenation agent containing oxygen raw material SODIUM PERCARBONATE;
(C) ratio that is 99.0~99.9 ︰s 1~0.1 with releasing agent according to mass percent by step B gained SODIUM PERCARBONATE mixes, and on tablet press machine, compressing tablet makes oxygenation agent product.
Further, in steps A, blender is bipyramid or single cone ribbon mixer.
In step B, reactor is bipyramid ribbon mixer.The principle of bipyramid ribbon mixer is exactly to carry out granulation by means of the physical force of chemical reaction and bipyramid ribbon itself.Bipyramid ribbon mixer on the one hand can be even by mixing of materials well, and the product that its ribbon can react hydrogen peroxide with comminuting matter simultaneously wraps up effectively, prepares densification, uniform particle.
In step B, the mass concentration of hydrogen peroxide is 27.5%-70%.Hydrogen peroxide concentration also can regulate according to the active oxygen of product.
Stabilizing agent described in step B is one or more in HEDP, triethanolamine, magnesium sulfate, EDTA-2Na or ATMP, and the consumption of stabilizing agent is the 0.1%-2% of hydrogen peroxide mass fraction.
Adhesive described in step B is flower bulb alkali, the 0.1-1% that its consumption is comminuting matter.
The particle diameter of SODIUM PERCARBONATE described in step B is 0.3-1.4mm, and active oxygen is 12.0%-14.0%.
Releasing agent described in step C is dolomol, odium stearate or both mixtures.
The present invention utilizes by-product bulky grain SODIUM PERCARBONATE to prepare the method for oxygenation agent, by the substandard product in SODIUM PERCARBONATE production process (by-product bulky grain SODIUM PERCARBONATE) twice laid, oxygenation agent for the preparation of aquaculture, environmentally friendly, equipment investment is little, technique is simple, can prepare high-quality oxygenation agent product, Product Activity oxygen is high, heat endurance and wet good stability.
The present invention also provides the oxygenation agent being prepared from by said method.
The oxygenation agent of being prepared by SODIUM PERCARBONATE belongs to solid oxygen, and it is new and effective oxygenation agent, adopts special cylindrical particle design, can directly sink to pond bottom, after reacting with water, produce a large amount of oxygen, the water body dissolved oxygen that increases sharply, and can maintain for a long time the high dissolved oxygen in water; In producing the process of a large amount of small oxygen bubbles risings at the bottom of pond, can effectively be dissolved in water body, pond bottom He Zhong lower floor water body is carried out to oxygenation, reach the effect of " three-dimensional oxygenation ", really efficiently solve the problem of bottom anoxic.
Adopt this oxygenation agent to carry out oxygenation to breeding water body and can reduce manufacturing cost, and reduce the pollution of existing oxygenation agent to water body, environment.
Embodiment
embodiment 1
Get 500kg active oxygen and be 8%, the by-product bulky grain SODIUM PERCARBONATE of particle size >=1.4mm, add the 1000L(mono-) in bipyramid ribbon mixer, open after stirring and slowly add 10kg running water, stir discharging after 5 minutes, material carries out the pulverizing of skin cylinder.Material after pulverizing is transferred in another one bipyramid ribbon mixer, spray 50% hydrogen peroxide 145kg, 2.9kg HEDP and 2.5kg flower bulb alkali and carry out granulation, granulation discharging after 10 minutes, dries, detection of active oxygen is 12.8%, and particle diameter is between 500-800mm.After getting SODIUM PERCARBONATE 500kg that granulation is good and mixing with 1kg dolomol, add compressing tablet in tablet press machine to make sheet oxygenation agent.
embodiment 2
Get 500kg active oxygen and be 10%, the by-product bulky grain SODIUM PERCARBONATE of particle size >=1.4mm, add the 1000L(mono-) in bipyramid ribbon mixer, open after stirring and slowly add 5kg running water, stir discharging after 5 minutes, material carries out the pulverizing of skin cylinder.Material after pulverizing is transferred in another one bipyramid ribbon mixer, and spray 30% hydrogen peroxide 105kg, 5.25kgEDTA-2Na and 1kg flower bulb alkali carry out granulation, and granulation discharging after 5 minutes is dried, and detection of active oxygen is 13.4%, and particle diameter is between 700-900mm.After getting SODIUM PERCARBONATE 500kg that granulation is good and mixing with 0.5kg odium stearate, add compressing tablet in tablet press machine to make sheet oxygenation agent.
embodiment 3:
Get 500kg active oxygen and be 7%, the by-product bulky grain SODIUM PERCARBONATE of particle size >=1.4mm, add the 1000L(mono-) in bipyramid ribbon mixer, open after stirring and slowly add 12kg running water, stir discharging after 10 minutes, material carries out the pulverizing of skin cylinder.Material after pulverizing is transferred in another one bipyramid ribbon mixer, and spray 60% hydrogen peroxide 105kg, 5.25kgEDTA-2Na and 1kg flower bulb alkali carry out granulation, and granulation discharging after 5 minutes is dried, and detection of active oxygen is 13.8%, and particle diameter is between 700-900mm.After getting SODIUM PERCARBONATE 500kg that granulation is good and mixing with 0.5kg odium stearate, add compressing tablet in tablet press machine to make sheet oxygenation agent.
embodiment 4:
While adopting SODIUM PERCARBONATE oxygenation agent of the present invention to carry out oxygenation to breeding water body:
Dry to spill pre-oxygen deficit proof consumption be 100 grams/acre, suitably increases consumption (every mu is calculated by 1 meter of depth of water) during severe depletion of oxygen:
When 1, fish, shrimp, the general anoxic of crab are raised the nose above water to breathe, every mu of water surface is shed 150 grams/acre.
When 2, fish, shrimp, crab severe depletion of oxygen are raised the nose above water to breathe, every mu is used 200 grams/acre, and emphasis is shed to fish, shrimp, crab close quarters.
3,, in the time of to water quality improvement and use medicine therapy, every mu of water surface is used this product 100-200 gram/acre, contributes to water body improvement and builds good environment effect.
4,, during live transport, this product 20-30 gram for water per ton, supplemented once about every 2-3 hour.

Claims (9)

1. utilize by-product bulky grain SODIUM PERCARBONATE to prepare a method for oxygenation agent, it is characterized in that, mainly comprise the following steps:
(A) in blender, add by-product bulky grain SODIUM PERCARBONATE and water, the addition of water is the 1%-3% of by-product bulky grain percarbonic acid mass percent, stirs 5-10 minute, with cracker, pulverizes; Described by-product bulky grain SODIUM PERCARBONATE is the irregular particle of active oxygen≤10%, particle size >=1.4mm;
(B) material after pulverizing enters spray hydrogen peroxide solution and stabilizing agent and adhesive in reactor, carries out granulation, dries, obtain oxygenation agent containing oxygen raw material SODIUM PERCARBONATE;
(C) ratio that is 99.0~99.9 ︰s 1~0.1 with releasing agent according to mass percent by step B gained SODIUM PERCARBONATE mixes, and on tablet press machine, compressing tablet makes oxygenation agent product.
2. method according to claim 1, is characterized in that, in steps A, blender is bipyramid or single cone ribbon mixer.
3. method according to claim 1, is characterized in that, in step B, reactor is bipyramid ribbon mixer.
4. method according to claim 1, is characterized in that, in step B, the mass concentration of hydrogen peroxide is 27.5%-70%.
5. method according to claim 1, it is characterized in that, stabilizing agent described in step B is one or more in HEDP, triethanolamine, magnesium sulfate, EDTA-2Na or ATMP, and the consumption of stabilizing agent is the 0.1%-2% of hydrogen peroxide mass fraction.
6. method according to claim 1, is characterized in that, adhesive described in step B is flower bulb alkali, the 0.1-1% that its consumption is comminuting matter.
7. method according to claim 1, is characterized in that, the particle diameter of SODIUM PERCARBONATE described in step B is 0.3-1.4mm, and active oxygen is 12.0%-14.0%.
8. method according to claim 1, is characterized in that, releasing agent described in step C is dolomol, odium stearate or both mixtures.
9. the oxygenation agent being prepared from according to the described method of one of claim 1-8.
CN201410189663.2A 2014-05-07 2014-05-07 A kind of method utilizing by-product bulky grain SODIUM PERCARBONATE to prepare oxygenation agent Active CN104012458B (en)