CN103996858B - 锂离子电池负极集流体材料及制备方法 - Google Patents
锂离子电池负极集流体材料及制备方法 Download PDFInfo
- Publication number
- CN103996858B CN103996858B CN201410235964.4A CN201410235964A CN103996858B CN 103996858 B CN103996858 B CN 103996858B CN 201410235964 A CN201410235964 A CN 201410235964A CN 103996858 B CN103996858 B CN 103996858B
- Authority
- CN
- China
- Prior art keywords
- lithium ion
- ion battery
- copper foil
- current collector
- base material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
Claims (4)