Summary of the invention
Goal of the invention: for the problem of prior art, first object of the present invention there is provided a kind of preparation method of children special-purpose bicycle riding apparel.Second object of the present invention there is provided a kind of children special-purpose bicycle riding apparel.
Technical scheme: in order to solve the problems of the technologies described above, the invention provides a kind of preparation method of children special-purpose bicycle riding apparel, concrete steps are as follows:
A) cutting: 20 ~ 40 degree celsius temperature and 40 ~ 50% humidity under cotton cloth carried out cutting respectively according to the requirement of the height of children, body weight, style obtain garment piece;
B) make: various types of garment pieces step a) obtained are made respectively and obtained clothes just finished product, and described method of sewing comprises one or more in overseam, flat-seam class, eyelet class and chain seam class; Wide three lines of the tape edge obtained after making are 0.35cm, and four lines are 0.5cm, and five lines are 0.7cm;
C) wholely to scald: riding apparel just finished product whole boiling hot time, strictly will control the temperature of flatiron, the weight that the temperature of flatiron is good should be determined according to the formation of grey cloth kind and fibrous raw material, control temperature, pressure, time and quantity of steam well;
D) arrangement, inspection, packaging get product.
Wherein, the whole boiling hot concrete steps of described step c) are as follows: by the spot of the first finished product PUT pneumatic spraying decontamination rifle alignment surface of the clothes made, spray distance is 40 ~ 80 mm, nozzle bore is 0.6 ~ 0.8mm, rated pressure is 0.4 ~ 0.6 Mpa, emitted dose is 80 ~ 110ml/min, mist amplitude is Φ 10 ~ Φ 40 mm, adhesive tape is adopted the end of a thread on surface and dust to be sticked out, then whole scalding is started, the pressure of flatiron is 30 ~ 50Mpa, time is 1 ~ 5h, quantity of steam is 5kw/h, whole boiling hot be all-cotton fabric then temperature at 185 ~ 195 DEG C, whole boiling hot be dacron then temperature between 150 ~ 165 DEG C, if be the comprehensive of all-cotton fabric and dacron, then temperature is at 170 ~ 180 DEG C, after riding apparel plates.
Wherein, the age of the children of step a) is 5 ~ 10 years old, height comprises 80 ~ 90cm, 90 ~ 100cm, 100 ~ 110cm, 110 ~ 120cm, 120 ~ 130cm, 130cm ~ 140cm, and different weight comprises 15 ~ 20kg, 20 ~ 25kg, 25 ~ 30kg, 30 ~ 35kg, 35 ~ 40kg, 40 ~ 45kg, 45 ~ 50kg, 50 ~ 55kg.
The size of children special-purpose riding apparel that wherein prepared by said method has XXXS, XXS, XS, S, M, L 6 kinds of models.
Wherein, the material behavior that the knee portions of leg regions of described riding apparel adopts is: Unit Weight is 1 00g/m
2, thickness is 0.8mm, and heat insulation temperature is 0.7Clo, and rigidity is within 3, and elastic modelling quantity forward is through being 0.7, and elastic modelling quantity returns through being 0.7, and elastic modelling quantity forward latitude is 0.7, and elastic modelling quantity returns latitude latitude 0.6, retardation through being 0.2, retardation latitude latitude 0.2.
Beneficial effect: the present invention is relative to prior art, have the following advantages: preparation method's simple possible of the present invention, by collecting relevant parameter and the feature of 5 ~ 10 years old children, prepare the special riding apparel for children, and knee position is provided with the material of property, make this partial elastic aspect be more suitable for the principle of children's ergonomics, add the comfort level that children ride, the problem preventing from children from overexerting causing knee injury can be played.
Detailed description of the invention
Below in conjunction with specific embodiment, the present invention is further described.
Embodiment 1:
A preparation method for children special-purpose bicycle riding apparel, concrete steps are as follows:
A) cutting: 20 degree celsius temperature and 40% humidity under cotton cloth carried out cutting respectively according to the requirement of the height of children, body weight, style obtain garment piece;
B) make: various types of garment pieces step a) obtained are made respectively and obtained clothes just finished product, and described method of sewing comprises one or more in overseam, flat-seam class, eyelet class and chain seam class; Wide three lines of the tape edge obtained after making are 0.35cm, and four lines are 0.5cm, and five lines are 0.7cm;
C) wholely to scald: riding apparel just finished product whole boiling hot time, strictly will control the temperature of flatiron, the weight that the temperature of flatiron is good should be determined according to the formation of grey cloth kind and fibrous raw material, control temperature, pressure, time and quantity of steam well;
D) arrangement, inspection, packaging get product.
Wherein, the whole boiling hot concrete steps of described step c) are as follows: by the spot of the first finished product PUT pneumatic spraying decontamination rifle alignment surface of the clothes made, spray distance is 40mm, nozzle bore is 0.6mm, rated pressure is 0.4Mpa, emitted dose is 80ml/min, mist amplitude is Φ 10 mm, adopt adhesive tape the end of a thread on surface and dust to be sticked out, then start whole scalding, the pressure of flatiron is 30Mpa, time is 1h, quantity of steam is 5kw/h, whole boiling hot be all-cotton fabric then temperature at 185 DEG C, whole boiling hot be dacron then temperature between 150 DEG C; If be the comprehensive of all-cotton fabric and dacron, then temperature is at 170 DEG C; After riding apparel plates.
Wherein, the age of the children of step a) is 5 ~ 10 years old, height comprises 80 ~ 90cm, 90 ~ 100cm, 100 ~ 110cm, 110 ~ 120cm, 120 ~ 130cm, 130cm ~ 140cm, and different weight comprises 15 ~ 20kg, 20 ~ 25kg, 25 ~ 30kg, 30 ~ 35kg, 35 ~ 40kg, 40 ~ 45kg, 45 ~ 50kg, 50 ~ 55kg.
The size of children special-purpose riding apparel that wherein prepared by said method has XXXS, XXS, XS, S, M, L 6 kinds of models.
Wherein, the material behavior that the knee portions of leg regions of described riding apparel adopts is: Unit Weight is 100g/m
2, thickness is 0.8mm, and heat insulation temperature is 0.7Clo, and rigidity is within 3, and elastic modelling quantity forward is through being 0.7, and elastic modelling quantity returns through being 0.7, and elastic modelling quantity forward latitude is 0.7, and elastic modelling quantity returns latitude latitude 0.6, retardation through being 0.2, retardation latitude latitude 0.2.
Embodiment 2
A preparation method for children special-purpose bicycle riding apparel, concrete steps are as follows:
A) cutting: 40 degree celsius temperature and 50% humidity under cotton cloth carried out cutting respectively according to the requirement of the height of children, body weight, style obtain garment piece;
B) make: various types of garment pieces step a) obtained are made respectively and obtained clothes just finished product, and described method of sewing comprises one or more in overseam, flat-seam class, eyelet class and chain seam class; Wide three lines of the tape edge obtained after making are 0.35cm, and four lines are 0.5cm, and five lines are 0.7cm;
C) wholely to scald: riding apparel just finished product whole boiling hot time, strictly will control the temperature of flatiron, the weight that the temperature of flatiron is good should be determined according to the formation of grey cloth kind and fibrous raw material, control temperature, pressure, time and quantity of steam well;
D) arrangement, inspection, packaging get product.
Wherein, the whole boiling hot concrete steps of described step c) are as follows: by the spot of the first finished product PUT pneumatic spraying decontamination rifle alignment surface of the clothes made, spray distance is 80 mm, nozzle bore is 0.8mm, rated pressure is 0.6 Mpa, emitted dose is 110ml/min, mist amplitude is Φ 40 mm, adopt adhesive tape the end of a thread on surface and dust to be sticked out, then start whole scalding, the pressure of flatiron is 50Mpa, time is 5h, quantity of steam is 5kw/h, whole boiling hot be all-cotton fabric then temperature at 195 DEG C, whole boiling hot be dacron then temperature between 165 DEG C; If be the comprehensive of all-cotton fabric and dacron, then temperature is at 180 DEG C; After riding apparel plates.
Wherein, the age of the children of step a) is 5 ~ 10 years old, height comprises 80 ~ 90cm, 90 ~ 100cm, 100 ~ 110cm, 110 ~ 120cm, 120 ~ 130cm, 130cm ~ 140cm, and different weight comprises 15 ~ 20kg, 20 ~ 25kg, 25 ~ 30kg, 30 ~ 35kg, 35 ~ 40kg, 40 ~ 45kg, 45 ~ 50kg, 50 ~ 55kg.
The size of children special-purpose riding apparel that wherein prepared by said method has XXXS, XXS, XS, S, M, L 6 kinds of models.
Wherein, the material behavior that the knee portions of leg regions of described riding apparel adopts is: Unit Weight is 1 00g/m
2, thickness is 0.8mm, and heat insulation temperature is 0.7Clo, and rigidity is within 3, and elastic modelling quantity forward is through being 0.7, and elastic modelling quantity returns through being 0.7, and elastic modelling quantity forward latitude is 0.7, and elastic modelling quantity returns latitude latitude 0.6, retardation through being 0.2, retardation latitude latitude 0.2.
Embodiment 3
A preparation method for children special-purpose bicycle riding apparel, concrete steps are as follows:
A) cutting: 30 degree celsius temperature and 45% humidity under cotton cloth carried out cutting respectively according to the requirement of the height of children, body weight, style obtain garment piece;
B) make: various types of garment pieces step a) obtained are made respectively and obtained clothes just finished product, and described method of sewing comprises one or more in overseam, flat-seam class, eyelet class and chain seam class; Wide three lines of the tape edge obtained after making are 0.35cm, and four lines are 0.5cm, and five lines are 0.7cm;
C) wholely to scald: riding apparel just finished product whole boiling hot time, strictly will control the temperature of flatiron, the weight that the temperature of flatiron is good should be determined according to the formation of grey cloth kind and fibrous raw material, control temperature, pressure, time and quantity of steam well;
D) arrangement, inspection, packaging get product.
Wherein, the whole boiling hot concrete steps of described step c) are as follows: by the spot of the first finished product PUT pneumatic spraying decontamination rifle alignment surface of the clothes made, spray distance is 60mm, nozzle bore is 0.7mm, rated pressure is 0.5Mpa, emitted dose is 95ml/min, mist amplitude is Φ 25 mm, adopt adhesive tape the end of a thread on surface and dust to be sticked out, then start whole scalding, the pressure of flatiron is 40Mpa, time is 3h, quantity of steam is 5kw/h, whole boiling hot be all-cotton fabric then temperature at 190 DEG C, whole boiling hot be dacron then temperature between 160 DEG C; If be the comprehensive of all-cotton fabric and dacron, then temperature is at 175 DEG C; After riding apparel plates.
Wherein, the age of the children of step a) is 5 ~ 10 years old, height comprises 80 ~ 90cm, 90 ~ 100cm, 100 ~ 110cm, 110 ~ 120cm, 120 ~ 130cm, 130cm ~ 140cm, and different weight comprises 15 ~ 20kg, 20 ~ 25kg, 25 ~ 30kg, 30 ~ 35kg, 35 ~ 40kg, 40 ~ 45kg, 45 ~ 50kg, 50 ~ 55kg.
The size of children special-purpose riding apparel that wherein prepared by said method has XXXS, XXS, XS, S, M, L 6 kinds of models.
Wherein, the material behavior that the knee portions of leg regions of described riding apparel adopts is: Unit Weight is 100g/m
2, thickness is 0.8mm, and heat insulation temperature is 0.7Clo, and rigidity is within 3, and elastic modelling quantity forward is through being 0.7, and elastic modelling quantity returns through being 0.7, and elastic modelling quantity forward latitude is 0.7, and elastic modelling quantity returns latitude latitude 0.6, retardation through being 0.2, retardation latitude latitude 0.2.
The above is only the preferred embodiment of the present invention; be noted that for those skilled in the art; under the premise without departing from the principles of the invention, can also make some improvements and modifications, these improvements and modifications also should be considered as protection scope of the present invention.