CN103938433A - Making method for loofah sponge with negative oxygen ions - Google Patents

Making method for loofah sponge with negative oxygen ions Download PDF

Info

Publication number
CN103938433A
CN103938433A CN201310020837.8A CN201310020837A CN103938433A CN 103938433 A CN103938433 A CN 103938433A CN 201310020837 A CN201310020837 A CN 201310020837A CN 103938433 A CN103938433 A CN 103938433A
Authority
CN
China
Prior art keywords
negative oxygen
oxygen ion
tourmaline
luffa
loofah sponge
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310020837.8A
Other languages
Chinese (zh)
Inventor
邬汝源
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201310020837.8A priority Critical patent/CN103938433A/en
Publication of CN103938433A publication Critical patent/CN103938433A/en
Pending legal-status Critical Current

Abstract

The invention discloses a making method for a loofah sponge with negative oxygen ions. The making method comprises the first step of selecting basic materials, the second step of preparing nanometer tourmaline negative oxygen ion slurry, the third step of injecting or fusing the prepared nanometer tourmaline negative oxygen ion slurry on the basic materials, and the fourth step of drying the basic materials with the sprayed nanometer tourmaline negative oxygen ion slurry, and then the loofah sponge finished product with the negative oxygen ions is obtained. The basic materials selected in the first step is the loofah sponge, the nanometer tourmaline negative oxygen ion slurry prepared in the second step is tourmaline solved in water, and the weight ratio between the tourmaline and the water is 4: 6. According to the third step, the nanometer tourmaline negative oxygen ion slurry is evenly sprayed or fused inside or on the surface of the basic materials. The making method for the loofah sponge with the negative oxygen ions has the advantages of being practical, low in production cost and convenient to use, and the made loofah sponge with the negative oxygen ions can effectively improve the air environment of people such as the air quality in a car and the air quality in a living room.

Description

A kind of manufacture method with negative oxygen ion luffa
Technical field
The present invention relates to a kind of manufacture method with negative oxygen ion product, particularly a kind of manufacture method with negative oxygen ion luffa.
Background technology
Negative oxygen ion colorless and odorless, its function is but very surprising, is consequently become by medical circle " air vitamin ".First, it can enter in human body by blood and refreshing level system, and people's organism physiology activity is exerted an influence.In the time that negative oxygen ion enters brain, can, by adjusting corticocerebral function, play and improve sleep quality, the effect of reducing blood pressure.When negative oxygen ion enters after human respiratory tract, can make bronchial smooth muscle lax, improve cardiorespiratory system function, increase work efficiency.Negative oxygen ion can reduce human-body fatigue in blood, improves human body reaction, improves body immunity.Secondly, negative oxygen ion can also play catharsis to airborne oil smoke, second-hand-cigarette, thus the RDs such as prevention pneumonia, tracheitis, and alleviate the negative effect that smoking causes.
Negative oxygen ion is the indispensable material of human body, 13,000,000,000 negative oxygen ions of human body needs every day, but the negative oxygen ion that urbanite can only obtain 2,000,000,000 left and right every day particularly general indoor obtainable just still less, main because present air pollution is more and more serious, airborne negative oxygen ion reason less and less causes.
At present, also there is no well to manufacture the method for anion material, and anion product, in addition, luffa is also called a day trailing plants muscle, there is fascicular feature, be convenient to the volatilization of negative oxygen ion or shed, general luffa, has substantially all disposed as rubbish, caused the very large wasting of resources, luffa is not reasonably utilized.
Summary of the invention
Technical problem to be solved by this invention is for the deficiencies in the prior art, and a kind of manufacture method with negative oxygen ion luffa is provided.
To achieve these goals, the measure that the present invention takes:
With a manufacture method for negative oxygen ion luffa, the first step: choose sill; Second step: preparation of nano tourmaline negative oxygen ion slurries; The 3rd step: the nano-tourmaline anion slurries spray that above-mentioned second step is prepared or fuse on sill; The 4th step: the sill that spray is good is dried, can obtain with negative oxygen ion luffa finished product;
The sill that the described first step is chosen is luffa;
The nano-tourmaline negative oxygen ion slurries of described second step preparation are for to be dissolved in tourmaline in water, and the weight ratio of tourmaline and water is 4: 6;
The 3rd described step is by the uniform spray of nano-tourmaline negative oxygen ion slurries or fuses sill inside or surperficial;
The 4th described step is dried as air-dry at 15~50 DEG C of temperature.
Beneficial effect of the present invention: practicality, production cost is low, easy to use, and produced negative oxygen ion luffa can effectively improve people's ambient air environment, as: the air quality in compartment, the air quality in parlor.
Detailed description of the invention
With a manufacture method for negative oxygen ion luffa, the first step: choose sill; Second step: preparation of nano tourmaline negative oxygen ion slurries; The 3rd step: the nano-tourmaline anion slurries spray that above-mentioned second step is prepared or fuse on sill; The 4th step: the sill that spray is good is dried, can obtain with negative oxygen ion luffa finished product, and negative oxygen ion luffa finished product when in use, can improve the quality of surrounding air; The sill that the described first step is chosen is luffa, effectively reduces production cost, and luffa is reasonably used, and the vascular bundle feature of luffa is convenient to being dispersed in air of negative oxygen ion, easy to use; The nano-tourmaline negative oxygen ion slurries of described second step preparation are for to be dissolved in tourmaline in water, and the weight ratio of tourmaline and water is 4: 6, makes the nano-tourmaline content in solution high, and the product of producing is long service time; The 3rd described step is for by the uniform spray of nano-tourmaline negative oxygen ion slurries or to fuse sill inner or surperficial, and production cost is low, is convenient to nanometer acetylene to improve air, evaporate in air; The 4th described step is dried as air-dry at 15~50 DEG C of temperature, can ensure sill, and the negative oxygen ion content in luffa is high, thereby realizes object of the present invention.
Those ordinary skill in the art's simple change and replacement are all within protection scope of the present invention.

Claims (5)

1. with a manufacture method for negative oxygen ion luffa, it is characterized in that:
The first step: choose sill;
Second step: preparation of nano tourmaline negative oxygen ion slurries;
The 3rd step: the nano-tourmaline anion slurries spray that above-mentioned second step is prepared or fuse on sill;
The 4th step: the sill that spray is good is dried, can obtain with negative oxygen ion luffa finished product.
2. a kind of manufacture method with negative oxygen ion luffa according to claim 1, is characterized in that: the sill that the described first step is chosen is luffa.
3. a kind of manufacture method with negative oxygen ion luffa according to claim 1, is characterized in that: the nano-tourmaline negative oxygen ion slurries of described second step preparation are for to be dissolved in tourmaline in water, and the weight ratio of tourmaline and water is 4: 6.
4. a kind of manufacture method with negative oxygen ion luffa according to claim 1, is characterized in that: the 3rd described step is by the uniform spray of nano-tourmaline negative oxygen ion slurries or fuses sill inside or surperficial.
5. a kind of manufacture method with negative oxygen ion luffa according to claim 1, is characterized in that: the 4th described step is dried as air-dry at 15~50 DEG C of temperature.
CN201310020837.8A 2013-01-21 2013-01-21 Making method for loofah sponge with negative oxygen ions Pending CN103938433A (en)