CN103862912B - 用于保护书籍的保护膜的制备方法 - Google Patents

用于保护书籍的保护膜的制备方法 Download PDF

Info

Publication number
CN103862912B
CN103862912B CN201410101632.7A CN201410101632A CN103862912B CN 103862912 B CN103862912 B CN 103862912B CN 201410101632 A CN201410101632 A CN 201410101632A CN 103862912 B CN103862912 B CN 103862912B
Authority
CN
China
Prior art keywords
plastic sheeting
coating
books
coating solution
diaphragm
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201410101632.7A
Other languages
English (en)
Other versions
CN103862912A (zh
Inventor
罗铮
肖蓉
周群英
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiaxing Vocational and Technical College
Original Assignee
Jiaxing Vocational and Technical College
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiaxing Vocational and Technical College filed Critical Jiaxing Vocational and Technical College
Priority to CN201410101632.7A priority Critical patent/CN103862912B/zh
Publication of CN103862912A publication Critical patent/CN103862912A/zh
Application granted granted Critical
Publication of CN103862912B publication Critical patent/CN103862912B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了用于保护书籍的保护膜的制备方法,它包括以下步骤:(1)、制取包衣液:选取80%浓度的乙醇95g,搅拌状态下一次性慢慢撒入5-15g薄膜包衣粉,继续搅拌45min用100目筛筛选两次,直至液体均匀既得包衣液;(2)、包衣:调试包衣锅使喷枪可喷出雾状液滴,设定输液速度至30-50r/min,将面积约为300cm2的塑料薄膜若干片置于包衣锅内,包衣锅内放置三块挡板、给予热风使塑料薄膜温度达到40-60℃,开启包衣锅喷入包衣液直至达到塑料薄膜表面色泽均匀一致,停喷包衣液,取出塑料薄膜,60℃干燥。本发明的有益效果是在用于包裹书籍的塑料薄膜外包上一层包衣,提高塑料薄膜的抗热性能、耐湿耐水性能,对书籍提供更高级别的安全保护。

Description

用于保护书籍的保护膜的制备方法
技术领域
本发明涉及图书外包装,尤其涉及用于保护书籍的保护膜的制备方法。
背景技术
书籍是人类进步的阶梯,使精神的食粮,图书馆就是保存这些精神食粮的地方,由于书籍长时间存放在不见光的封闭环境内容易生虫、腐蚀,且易生潮、起火,如果没有妥善的保护措施图书就会损毁,一些珍贵书籍可能就此失传。现如今的图书馆内一般都是采用大型的集成系统改进其内部环境,使其通风,且需要定期对图书进行维护保养,维护麻烦,成本高昂。
发明内容
本发明要解决的技术问题是现有的图书馆没有专门的书籍保护装置,书籍直接暴漏在空气中容易损坏,为此提供一种用于保护书籍的保护膜的制备方法。
本发明的技术方案是:用于保护书籍的保护膜的制备方法,它包括以下步骤:(1)、制取包衣液:选取80%浓度的乙醇95g,搅拌状态下一次性慢慢撒入5-15g薄膜包衣粉,继续搅拌45min用100目筛筛选两次,直至液体均匀既得包衣液;(2)、包衣:调试包衣锅使喷枪可喷出雾状液滴,设定输液速度至30-50r/min,将面积约为300cm2的塑料薄膜若干片置于包衣锅内,包衣锅内放置三块挡板、给予热风使塑料薄膜温度达到40-60℃,开启包衣锅喷入包衣液直至达到塑料薄膜表面色泽均匀一致,停喷包衣液,取出塑料薄膜,60℃干燥既得保护膜。
上述方案的改进是所述塑料薄膜在置于包衣锅之前浸入液体石蜡中3-5min。
上述方案的进一步改进是所述塑料薄膜浸入液体石蜡的同时对其加热,加热温度为30-40℃。
本发明的有益效果是在用于包裹书籍的塑料薄膜外包上一层包衣,提高塑料薄膜的抗热性能、耐湿耐水性能,对书籍提供更高级别的安全保护,且操作简单,成本低廉,易于推广。
具体实施方式
实施例1:(1)、制取包衣液:选取80%浓度的乙醇95g,搅拌状态下一次性慢慢撒入5g薄膜包衣粉,继续搅拌45min用100目筛筛选两次,直至液体均匀既得包衣液;(2)、包衣:调试包衣锅使喷枪可喷出雾状液滴,设定输液速度至30r/min,将面积约为300cm2的塑料薄膜若干片置于包衣锅内,包衣锅内放置三块挡板、给予热风使塑料薄膜温度达到40℃,开启包衣锅喷入包衣液直至达到塑料薄膜表面色泽均匀一致,停喷包衣液,取出塑料薄膜,60℃干燥既得保护膜。
薄膜包衣粉的色泽可自由选择,如彩色、红色、紫色、白色等等,制作出来的保护膜一方面色彩艳丽,美观大方,另一方面可用于给书籍分类,通过不同的颜色给不同类型的书籍分类,一目了然。
塑料薄膜的优点是轻盈透明,质地柔软,所以可以用来包裹书籍,但它不耐热不耐湿,且有一定毒性,经过包衣处理后提高了耐热耐湿性能,且包衣五毒无害,对环境友好。
塑料薄膜表面可能有不光洁,起皱、起泡等缺陷,如果直接放入包衣锅内喷涂包衣液会影响成品保护膜的观感度和保护度,为此最好将塑料薄膜在置于包衣锅之前浸入液体石蜡中3-5min,可以清洁塑料薄膜的表面,使其光滑平整,为了增强塑料薄膜表面修复效果,可以在塑料薄膜浸入液体石蜡的同时对其加热,加热温度为30-40℃。
本发明制得的保护膜放置于250w的红外灯下15处受热4h,观察保护膜表面无明显变化,说明其抗热性能好。
将保护膜置于恒温培养箱中经过一定时间,以增重为指标,观察保护膜的耐湿性,发现重量无明显变化,说明其耐湿性良好;将保护膜放入蒸馏水中浸渍5min后,取出干燥,比较浸渍前后保护膜的失重,也无明显变化,说明保护膜的耐水性良好。
实施例2:(1)、制取包衣液:选取80%浓度的乙醇95g,搅拌状态下一次性慢慢撒入15g薄膜包衣粉,继续搅拌45min用100目筛筛选两次,直至液体均匀既得包衣液;(2)、包衣:调试包衣锅使喷枪可喷出雾状液滴,设定输液速度至50r/min,将面积约为300cm2的塑料薄膜若干片置于包衣锅内,包衣锅内放置三块挡板、给予热风使塑料薄膜温度达到60℃,开启包衣锅喷入包衣液直至达到塑料薄膜表面色泽均匀一致,停喷包衣液,取出塑料薄膜,60℃干燥既得保护膜。
优选实施例3:(1)、制取包衣液:选取80%浓度的乙醇95g,搅拌状态下一次性慢慢撒入10g薄膜包衣粉,继续搅拌45min用100目筛筛选两次,直至液体均匀既得包衣液;(2)、包衣:调试包衣锅使喷枪可喷出雾状液滴,设定输液速度至40r/min,将面积约为300cm2的塑料薄膜若干片浸入液体石蜡中3min后取出置于包衣锅内,期间对塑料薄膜加热,加热温度为30℃,包衣锅内放置三块挡板、给予热风使塑料薄膜温度达到50℃,开启包衣锅喷入包衣液直至达到塑料薄膜表面色泽均匀一致,停喷包衣液,取出塑料薄膜,60℃干燥既得保护膜。
优选实施例4:(1)、制取包衣液:选取80%浓度的乙醇95g,搅拌状态下一次性慢慢撒入10g薄膜包衣粉,继续搅拌45min用100目筛筛选两次,直至液体均匀既得包衣液;(2)、包衣:调试包衣锅使喷枪可喷出雾状液滴,设定输液速度至40r/min,将面积约为300cm2的塑料薄膜若干片浸入液体石蜡中5min后取出置于包衣锅内,期间对塑料薄膜加热,加热温度为40℃,包衣锅内放置三块挡板、给予热风使塑料薄膜温度达到50℃,开启包衣锅喷入包衣液直至达到塑料薄膜表面色泽均匀一致,停喷包衣液,取出塑料薄膜,60℃干燥既得保护膜。
使用时将保护膜裁剪至和需要包裹的书籍大小一致即可进行包裹。
上面结合实施例对本发明进行了示例性描述,显然本发明具体实现并不受上述方式的限制,只要采用了本发明的方法构思和技术方案进行的各种非实质性的改进,或未经改进将本发明的构思和技术方案直接应用于其它场合的,均在本发明的保护范围之内。

Claims (3)

1.用于保护书籍的保护膜的制备方法,其特征是它包括以下步骤:(1)、制取包衣液:选取80%浓度的乙醇95g,搅拌状态下一次性慢慢撒入5-15g薄膜包衣粉,继续搅拌45min用100目筛筛选两次,直至液体均匀既得包衣液;(2)、包衣:调试包衣锅使喷枪可喷出雾状液滴,设定输液速度至30-50r/min,将面积约为300cm2的塑料薄膜若干片置于包衣锅内,包衣锅内放置三块挡板、给予热风使塑料薄膜温度达到50-60℃,开启包衣锅喷入包衣液直至达到塑料薄膜表面色泽均匀一致,停喷包衣液,取出塑料薄膜,60℃干燥既得保护膜。
2.如权利要求1所述的用于保护书籍的保护膜的制备方法,其特征是所述塑料薄膜在置于包衣锅之前浸入液体石蜡中3-5min。
3.如权利要求2所述的用于保护书籍的保护膜的制备方法,其特征是所述塑料薄膜浸入液体石蜡的同时对其加热,加热温度为30-40℃。
CN201410101632.7A 2014-03-19 2014-03-19 用于保护书籍的保护膜的制备方法 Expired - Fee Related CN103862912B (zh)