CN103760329A - 沥青热、光、水耦合老化试验箱 - Google Patents

沥青热、光、水耦合老化试验箱 Download PDF

Info

Publication number
CN103760329A
CN103760329A CN201410056038.0A CN201410056038A CN103760329A CN 103760329 A CN103760329 A CN 103760329A CN 201410056038 A CN201410056038 A CN 201410056038A CN 103760329 A CN103760329 A CN 103760329A
Authority
CN
China
Prior art keywords
light
seal box
asphalt
heat
blower fan
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410056038.0A
Other languages
English (en)
Inventor
何兆益
冉龙飞
黄刚
曹青霞
张杰文
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chongqing Jiaotong University
Original Assignee
Chongqing Jiaotong University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chongqing Jiaotong University filed Critical Chongqing Jiaotong University
Priority to CN201410056038.0A priority Critical patent/CN103760329A/zh
Publication of CN103760329A publication Critical patent/CN103760329A/zh
Pending legal-status Critical Current

Abstract

一种沥青热、光、水耦合老化试验箱,所述沥青热、光、水耦合老化试验箱由支架、密封箱、制冷装置、加热装置、加湿装置、干燥装置、紫外线辐照装置、风机、人机对话装置和多个传感器组成;本发明的有益技术效果是:能真实有效的模拟沥青及沥青混合料在热、光、水等自然条件下的老化状况,试验结果的精确度高,试验设备结构简单,操作方便。

Description

沥青热、光、水耦合老化试验箱
技术领域
    本发明涉及一种试验设备,尤其涉及一种沥青热、光、水耦合老化试验箱。
背景技术
    沥青路面在使用过程中由于长期受到高温、紫外光照射、雨水冲洗等作用,会对沥青造成严重的老化,从而导致沥青路面的破坏。沥青路面再生技术在发达国家的应用较为成熟和普及,而我国由于政策、技术等方面的原因,旧沥青路面再生利用的水平还较低,再生沥青混和料主要还用于低等级沥青路面或高速公路沥青路面面层下层和基层,导致大量旧沥青混凝土没有得到充分利用,既浪费了资源,又对环境造成了严重的污染。因此研究沥青再生技术已经到了迫在眉睫的时候,而要研究沥青的再生技术必须先要研究沥青的老化机理。目前,沥青及沥青混合料老化研究主要是通过旋转薄膜烘箱和PAV压力老化试验箱来完成,这些设备主要是研究沥青及沥青混合料的热老化,而现实环境中沥青及沥青混合料还受到紫外光、雨水等多因素的老化,因此需要发明一种能同时模拟热、光、水等自然条件下沥青及沥青混合料老化设备。
发明内容
针对背景技术中的问题,本发明提出了一种沥青热、光、水耦合老化试验箱,其结构为:所述沥青热、光、水耦合老化试验箱由支架、密封箱、制冷装置、加热装置、加湿装置、干燥装置、紫外线辐照装置、风机、人机对话装置和多个传感器组成;密封箱、制冷装置、加热装置、加湿装置、干燥装置、紫外线辐照装置、风机和人机对话装置均设置在支架上;制冷装置和加热装置的热交换部均设置于密封箱的内壁上;加湿装置的出气口与密封箱内部连通;干燥装置的出气口与风机的进气口连通,风机的出气口与密封箱内部连通;紫外线辐照装置的发光部设置于密封箱内;多个传感器设置于密封箱内;制冷装置、加热装置、加湿装置、干燥装置、紫外线辐照装置、风机和多个传感器均与人机对话装置通信连接。
本发明的装置原理是:将沥青样品放置在密封箱内后,可通过制冷装置、加热装置、加湿装置和干燥装置对密封箱内的温度和湿度进行调节,同时,还能通过紫外线辐照装置模拟出太阳辐射,这就使得沥青热、光、水耦合老化试验箱可以同时模拟出真实环境中的温度、湿度和辐照,所需装置均为常用的仪器设备,操作简单、高效。
优选地,所述多个传感器包括温度传感器、湿度传感器和气压传感器。温度传感器、湿度传感器和气压传感器可对密封箱内的环境状态进行监测,并实时动态地通过人机对话装置反馈给操作人员,便于操作人员进行操作。
优选地,所述人机对话装置由显示屏和多个薄膜按钮组成。
本发明的有益技术效果是:能真实有效的模拟沥青及沥青混合料在热、光、水等自然条件下的老化状况,试验结果的精确度高,试验设备结构简单,操作方便。
附图说明
图1、本发明的结构示意图;
图中各个标记所对应的装置名称分别为:密封箱1、制冷装置2、加热装置3、加湿装置4、干燥装置5、紫外线辐照装置6、风机7。
具体实施方式
一种沥青热、光、水耦合老化试验箱,其结构为:所述沥青热、光、水耦合老化试验箱由支架、密封箱1、制冷装置2、加热装置3、加湿装置4、干燥装置5、紫外线辐照装置6、风机7、人机对话装置和多个传感器组成;密封箱1、制冷装置2、加热装置3、加湿装置4、干燥装置5、紫外线辐照装置6、风机7和人机对话装置均设置在支架上;制冷装置2和加热装置3的热交换部均设置于密封箱1的内壁上;加湿装置4的出气口与密封箱1内部连通;干燥装置5的出气口与风机7的进气口连通,风机7的出气口与密封箱1内部连通;紫外线辐照装置6的发光部设置于密封箱1内;多个传感器设置于密封箱1内;制冷装置2、加热装置3、加湿装置4、干燥装置5、紫外线辐照装置6、风机7和多个传感器均与人机对话装置通信连接。
所述多个传感器包括温度传感器、湿度传感器和气压传感器。
所述人机对话装置由显示屏和多个薄膜按钮组成。

Claims (3)

1.一种沥青热、光、水耦合老化试验箱,其特征在于:所述沥青热、光、水耦合老化试验箱由支架、密封箱(1)、制冷装置(2)、加热装置(3)、加湿装置(4)、干燥装置(5)、紫外线辐照装置(6)、风机(7)、人机对话装置和多个传感器组成;密封箱(1)、制冷装置(2)、加热装置(3)、加湿装置(4)、干燥装置(5)、紫外线辐照装置(6)、风机(7)和人机对话装置均设置在支架上;制冷装置(2)和加热装置(3)的热交换部均设置于密封箱(1)的内壁上;加湿装置(4)的出气口与密封箱(1)内部连通;干燥装置(5)的出气口与风机(7)的进气口连通,风机(7)的出气口与密封箱(1)内部连通;紫外线辐照装置(6)的发光部设置于密封箱(1)内;多个传感器设置于密封箱(1)内;制冷装置(2)、加热装置(3)、加湿装置(4)、干燥装置(5)、紫外线辐照装置(6)、风机(7)和多个传感器均与人机对话装置通信连接。
2.根据权利要求1所述的沥青热、光、水耦合老化试验箱,其特征在于:所述多个传感器包括温度传感器、湿度传感器和气压传感器。
3.根据权利要求1所述的沥青热、光、水耦合老化试验箱,其特征在于:所述人机对话装置由显示屏和多个薄膜按钮组成。
CN201410056038.0A 2014-02-19 2014-02-19 沥青热、光、水耦合老化试验箱 Pending CN103760329A (zh)