CN103660279A - Plastic welding method - Google Patents

Plastic welding method Download PDF

Info

Publication number
CN103660279A
CN103660279A CN201310614356.XA CN201310614356A CN103660279A CN 103660279 A CN103660279 A CN 103660279A CN 201310614356 A CN201310614356 A CN 201310614356A CN 103660279 A CN103660279 A CN 103660279A
Authority
CN
China
Prior art keywords
plastic
welding
welding method
plastics
welded
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310614356.XA
Other languages
Chinese (zh)
Inventor
苏伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Suzhou Keber Precision Machinery Co Ltd
Original Assignee
Suzhou Keber Precision Machinery Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Suzhou Keber Precision Machinery Co Ltd filed Critical Suzhou Keber Precision Machinery Co Ltd
Priority to CN201310614356.XA priority Critical patent/CN103660279A/en
Publication of CN103660279A publication Critical patent/CN103660279A/en
Pending legal-status Critical Current

Abstract

The invention discloses a plastic welding method comprising the steps as follows: (1), firstly fixing a piece of plastic to be welded with a fixture; (2), heating a welding head; (3), then placing another piece of plastic nearby the plastic to be welded, contacting the plastic through the welding head to enable the two pieces of plastic to be connected with each other after melting; and (4), finally blowing and cooling the part where the two pieces of plastic are welded until the part is solidified. According to the plastic welding method, after hot melting is performed on the plastic through the welding head, the welding part is blown and cooled to be solidified immediately, so that the welding part of the plastic is high in welding strength, the welding efficiency is also high, and the normal requirement of production is met.

Description

A kind of Plastic Welding method
Technical field
The present invention relates to a kind of welding method, relate in particular to a kind of welding method for plastics.
Background technology
The welding method of plastic products has a variety of, generally can be divided into thermal weld, friction welding and electromagnetism welding.Wherein thermal weld is a kind of generally Plastic Welding of application.But this welding method exists some shortcomings in operation, plastic products are when adopting thermal weld, all generally directly to adopt soldering tip to weld plastic products, the easy like this wire drawing phenomenon that occurs, cause welding unsuccessful, poor welding quality, welding efficiency is low, has affected normal production.
Summary of the invention
Technical problem for above-mentioned existence, the object of the invention is: proposed a kind of Plastic Welding method that welding quality and welding efficiency are high.
Technical solution of the present invention is achieved in that a kind of Plastic Welding method, comprises the following steps:
One, first plastics of required welding are fixed up with fixture;
Two, soldering tip is heated;
Three, then another piece plastics are placed near the plastics of required welding, then utilize soldering tip to contact it, make to link together after two plastic moltings;
Four, finally wind is carried out in the position of its welding cooling until it is solidified.
Due to the utilization of technique scheme, the present invention compared with prior art has following advantages:
Plastic Welding method of the present invention, utilizes soldering tip to carry out after hot melt fusing at plastics, more at once cooling the making of wind is carried out in the position of welding and solidify, and makes like this position weld strength of Plastic Welding high, and welding efficiency is also high, has met the normal demand of producing.
The specific embodiment
A kind of Plastic Welding method of the present invention, a kind of Plastic Welding method, comprises the following steps: one, first plastics of required welding are fixed up with fixture; Two, soldering tip is heated; Three, then another piece plastics are placed near the plastics of required welding, then utilize soldering tip to contact it, make to link together after two plastic moltings; Four, finally wind is carried out in the position of its welding cooling until it is solidified.
Plastic Welding method of the present invention, utilizes soldering tip to carry out after hot melt fusing at plastics, more at once cooling the making of wind is carried out in the position of welding and solidify, and makes like this position weld strength of Plastic Welding high, and welding efficiency is also high, has met the normal demand of producing.
Above-described embodiment is only explanation technical conceive of the present invention and feature; its object is to allow person skilled in the art can understand content of the present invention and be implemented; can not limit the scope of the invention with this; all equivalences that Spirit Essence is done according to the present invention change or modify, and all should be encompassed in protection scope of the present invention.

Claims (1)

1. a Plastic Welding method, is characterized in that comprising the following steps:
First plastics of required welding are fixed with fixture;
Soldering tip is heated;
Then another plastics are placed on the plastics of required welding, then utilize soldering tip to contact it, make to link together after two plastic moltings;
Finally wind is carried out in the position of its welding cooling until it is solidified.
CN201310614356.XA 2013-11-28 2013-11-28 Plastic welding method Pending CN103660279A (en)