CN103613816A - 一种耐腐蚀橡胶 - Google Patents
一种耐腐蚀橡胶 Download PDFInfo
- Publication number
- CN103613816A CN103613816A CN201310607567.0A CN201310607567A CN103613816A CN 103613816 A CN103613816 A CN 103613816A CN 201310607567 A CN201310607567 A CN 201310607567A CN 103613816 A CN103613816 A CN 103613816A
- Authority
- CN
- China
- Prior art keywords
- rubber
- dipropylene glycol
- carboxylic acid
- magnesium stearate
- ethyl propionate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种耐腐蚀橡胶,包括橡胶原液24-37%、胶原水解物0.5-2.4%、硬脂酸镁12-18%、3-乙氧基丙酸乙酯16-21%、吡咯烷酮羧酸一三乙醇胺盐1.8-2.3%、丙酮酸丙酯13-15%、二乙二醇单乙醚1-5%和二丙二醇丁醚等二丙二醇单烷基醚1-3%。所述的百分数均为质量百分数。本橡胶耐腐蚀性能强,耐强酸强碱,不易发生取代反应,有利于工业生产和人们生活。
Description
技术领域
本发明属于材料领域,特别涉及一种耐腐蚀橡胶。
背景技术
橡胶应用在生活生产的各个领域当中,有些时候橡胶的工作环境比较艰苦,如果遇到强酸强碱会收到腐蚀而影响其性能,并影响大家的正常工作,目前的橡胶多采用化工原料制成,耐腐蚀性通常有限,不利于生产生活。
发明内容
本发明的一是提供耐腐蚀橡胶,本种橡胶耐腐蚀性能强,有利于工业生产和人们生活。
采用的技术方案是:
一种耐腐蚀橡胶,包括橡胶原液24-37%、胶原水解物0.5-2.4%、硬脂酸镁12-18%、3- 乙氧基丙酸乙酯16-21%、吡咯烷酮羧酸一三乙醇胺盐1.8-2.3%、丙酮酸丙酯13-15%、二乙二醇单乙醚1-5%和二丙二醇丁醚等二丙二醇单烷基醚1-3%。
所述的百分数均为质量百分数。
其优点在于:
本橡胶耐腐蚀性能强,,耐强酸强碱,不易发生取代反应,有利于工业生产和人们生活。
具体实施方式
实施例1
一种耐腐蚀橡胶,包括橡胶原液24%、胶原水解物0.5%、硬脂酸镁12%、3-乙氧基丙酸乙酯16%、吡咯烷酮羧酸一三乙醇胺盐1.8%、丙酮酸丙酯13%、二乙二醇单乙醚1%和二丙二醇丁醚等二丙二醇单烷基醚1%。
所述的百分数均为质量百分数。
实施例2
一种耐腐蚀橡胶,包括橡胶原液37%、胶原水解物2.4%、硬脂酸镁18%、3-乙氧基丙酸乙酯21%、吡咯烷酮羧酸一三乙醇胺盐2.3%、丙酮酸丙酯15%、二乙二醇单乙醚5%和二丙二醇丁醚等二丙二醇单烷基醚3%。
所述的百分数均为质量百分数。
实施例3
一种耐腐蚀橡胶,包括橡胶原液27%、胶原水解物0.7%、硬脂酸镁15%、3- 乙氧基丙酸乙酯19%、吡咯烷酮羧酸一三乙醇胺盐2%、丙酮酸丙酯14%、二乙二醇单乙醚2%和二丙二醇丁醚等二丙二醇单烷基醚2%。
所述的百分数均为质量百分数。
Claims (4)
1.一种耐腐蚀橡胶,其特征在于:包括橡胶原液24-37%、胶原水解物0.5-2.4%、硬脂酸镁12-18%、3- 乙氧基丙酸乙酯16-21%、吡咯烷酮羧酸一三乙醇胺盐1.8-2.3%、丙酮酸丙酯13-15%、二乙二醇单乙醚1-5%和二丙二醇丁醚等二丙二醇单烷基醚1-3%;所述的百分数均为质量百分数。
2.根据权利要求1所述的一种耐腐蚀橡胶,其特征在于:橡胶原液24%、胶原水解物0.5%、硬脂酸镁12%、3-乙氧基丙酸乙酯16%、吡咯烷酮羧酸一三乙醇胺盐1.8%、丙酮酸丙酯13%、二乙二醇单乙醚1%和二丙二醇丁醚等二丙二醇单烷基醚1%。
3.根据权利要求1所述的一种耐腐蚀橡胶,其特征在于:橡胶原液37%、胶原水解物2.4%、硬脂酸镁18%、3-乙氧基丙酸乙酯21%、吡咯烷酮羧酸一三乙醇胺盐2.3%、丙酮酸丙酯15%、二乙二醇单乙醚5%和二丙二醇丁醚等二丙二醇单烷基醚3%。
4.根据权利要求1所述的一种耐腐蚀橡胶,其特征在于:橡胶原液27%、胶原水解物0.7%、硬脂酸镁15%、3- 乙氧基丙酸乙酯19%、吡咯烷酮羧酸一三乙醇胺盐2%、丙酮酸丙酯14%、二乙二醇单乙醚2%和二丙二醇丁醚等二丙二醇单烷基醚2%。