CN103503920A - 一种改性活性炭消毒剂及其制备方法 - Google Patents
一种改性活性炭消毒剂及其制备方法 Download PDFInfo
- Publication number
- CN103503920A CN103503920A CN201310387296.2A CN201310387296A CN103503920A CN 103503920 A CN103503920 A CN 103503920A CN 201310387296 A CN201310387296 A CN 201310387296A CN 103503920 A CN103503920 A CN 103503920A
- Authority
- CN
- China
- Prior art keywords
- active carbon
- water
- disinfectant
- parts
- hour
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种改性活性炭消毒剂,其特征在于由下列重量份的原料制成:活性炭100-120、硝酸银1-2、聚乙烯醇7-9、生石灰12-14、过硫酸氢钾0.5-1、沸石粉20-23、改性凹凸棒土8-10、水适量。本发明使用了硝酸银,过硫酸氢钾,能够氧化消毒,净化空气、水;本发明还使用了聚乙烯醇,改善了活性炭易崩解的缺点,从而可以用来净化水,不会造成水的二次污染;本发明原料易得,工艺简单,成本低,适合工业化生产,无有害物质生成,具有良好的应用前景。
Description
技术领域
本发明涉及一种非金属矿的改性方法,尤其涉及一种改性活性炭消毒剂及其制备方法。
背景技术
随着科技的发展,现代化工业的逐步建设,各种化学品被开发利用,给人们生活带来了便利,同时由于化学品产生了对环境和人体有害的物质,也成了人们不得不面对的问题。
目前空气中的污染物主要是工业燃料燃烧产生的气体、汽车尾气、生产中产生的有毒有害气体。水污染主要是工业生产排放的污水里含有大量有毒物质,还有人们生活中的污水产生很多有害物质。人们生活中也有很多时候需要脱除毒素,比如空调过滤网上有很多细菌、毒素,新装修的间有甲醛等有害物质,都需要脱除毒素。目前都脱除毒素经常用到吸附剂,主要有硅胶、活性氧化铝、活性炭、分子筛等,另外还有针对某种组分选择性吸附而研制的吸附材料。但是这些吸附剂大多吸附能力有限,需要针对不同的要求研究不同的吸附剂,发挥最好的作用。同时,寻找新的原料,以增强吸附效果,节约成本。
发明内容
本发明的目的在于提供一种改性活性炭消毒剂及其制备方法。
本发明的技术方案如下:
一种改性活性炭消毒剂,其特征在于由下列重量份的原料制成:活性炭100-120、硝酸银1-2、聚乙烯醇7-9、生石灰12-14、过硫酸氢钾0.5-1、沸石粉20-23、改性凹凸棒土8-10、水适量;所述改性凹凸棒土由以下重量份的原料制成:凹凸棒土120-130、碳酸钠3-4、铝矾土5-6、硼化钒1-2、玉石粉3-4、硫酸亚铁1-2、硫酸钛14-18、活性炭12-14、麦饭石2-3、氧化镧1-2、氧化铬3-4、吗啉1-2、水适量;将凹凸棒土、铝矾土、玉石粉、活性炭送入煅烧炉中,在850-870℃下煅烧4-5小时,取出,再放入适量水中研磨,调节研磨液PH值为4-5,研磨1-2小时,得到100-150目浆料,再调节研磨液PH值为中性,加入其它剩余成分,继续研磨,得到200-300目浆料,喷雾干燥,即得。
所述改性活性炭消毒剂的制备方法,其特征在于包括以下步骤:将沸石粉送入煅烧炉中在840-880℃下煅烧3-4小时,取出,与活性炭、硝酸银、聚乙烯醇、生石灰混合,加入到适量水中,搅拌均匀,加入过硫酸氢钾,研磨2-3小时,得到200-300目浆料,调节研磨浆料PH值为中性,喷雾干燥,与改性凹凸棒土混合均匀,送入250-280℃热处理炉中,处理3-4小时,取出即得。
分发明的有益效果
本发明使用了硝酸银,过硫酸氢钾,能够氧化消毒,净化空气、水;本发明还使用了聚乙烯醇,改善了活性炭易崩解的缺点,从而可以用来净化水,不会造成水的二次污染;本发明原料易得,工艺简单,成本低,适合工业化生产,无有害物质生成,具有良好的应用前景。
具体实施方式
一种改性活性炭消毒剂,由下列重量份(公斤)的原料制成:活性炭110、硝酸银1、聚乙烯醇8、生石灰13、过硫酸氢钾0.5、沸石粉21、改性凹凸棒土9、水适量;
所述改性凹凸棒土由以下重量份(公斤)的原料制成:凹凸棒土110、碳酸钠3、铝矾土5、硼化钒1、玉石粉3、硫酸亚铁1、硫酸钛15、活性炭13、麦饭石2、氧化镧1、氧化铬3、吗啉1、水适量;将凹凸棒土、铝矾土、玉石粉、活性炭送入煅烧炉中,在860℃下煅烧4小时,取出,再放入适量水中研磨,调节研磨液PH值为4,研磨1小时,得到100目浆料,再调节研磨液PH值为中性,加入其它剩余成分,继续研磨,得到200目浆料,喷雾干燥,即得。
所述改性活性炭消毒剂的制备方法,包括以下步骤:将沸石粉送入煅烧炉中在860℃下煅烧3小时,取出,与活性炭、硝酸银、聚乙烯醇、生石灰混合,加入到适量水中,搅拌均匀,加入过硫酸氢钾,研磨2小时,得到200目浆料,调节研磨浆料PH值为中性,喷雾干燥,与改性凹凸棒土混合均匀,送入270℃热处理炉中,处理3小时,取出即得。
经测定,其碘值1541mg/g,亚甲基蓝吸附值26.3mL/0.1g。
Claims (2)
1.一种改性活性炭消毒剂,其特征在于由下列重量份的原料制成:活性炭100-120、硝酸银1-2、聚乙烯醇7-9、生石灰12-14、过硫酸氢钾0.5-1、沸石粉20-23、改性凹凸棒土8-10、水适量;所述改性凹凸棒土由以下重量份的原料制成:凹凸棒土120-130、碳酸钠3-4、铝矾土5-6、硼化钒1-2、玉石粉3-4、硫酸亚铁1-2、硫酸钛14-18、活性炭12-14、麦饭石2-3、氧化镧1-2、氧化铬3-4、吗啉1-2、水适量;将凹凸棒土、铝矾土、玉石粉、活性炭送入煅烧炉中,在850-870℃下煅烧4-5小时,取出,再放入适量水中研磨,调节研磨液PH值为4-5,研磨1-2小时,得到100-150目浆料,再调节研磨液PH值为中性,加入其它剩余成分,继续研磨,得到200-300目浆料,喷雾干燥,即得。
2.根据权利要求1所述改性活性炭消毒剂的制备方法,其特征在于包括以下步骤:将沸石粉送入煅烧炉中在840-880℃下煅烧3-4小时,取出,与活性炭、硝酸银、聚乙烯醇、生石灰混合,加入到适量水中,搅拌均匀,加入过硫酸氢钾,研磨2-3小时,得到200-300目浆料,调节研磨浆料PH值为中性,喷雾干燥,与改性凹凸棒土混合均匀,送入250-280℃热处理炉中,处理3-4小时,取出即得。