CN103497611A - Green energy-saving high polymer coating material - Google Patents
Green energy-saving high polymer coating material Download PDFInfo
- Publication number
- CN103497611A CN103497611A CN201310411875.6A CN201310411875A CN103497611A CN 103497611 A CN103497611 A CN 103497611A CN 201310411875 A CN201310411875 A CN 201310411875A CN 103497611 A CN103497611 A CN 103497611A
- Authority
- CN
- China
- Prior art keywords
- parts
- coating material
- green energy
- polymer coating
- high polymer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a green energy-saving high polymer coating material which is composed of the following components in parts by weight: 1-3 parts of glass fiber, 3-4 parts of mica, 24-31 parts of POE (polyolefin elastomer), 11-24 parts of poly-4-methyl-1-pentylene, 5-9 parts of bisphenol A polycarbonate, 100 parts of silicone-acrylic emulsion, 6-10 parts of nano calcium carbonate, 9-12 parts of PS (polystyrene), 11-32 parts of EVA (ethylene-vinyl acetate), 20-21 parts of bonding agent, 10 parts of foaming agent, 1-5 parts of thickener, 1-3 parts of dispersant and 0.5-1 part of antioxidant. The coating material has the advantages of high high-temperature stability, high strength, wear resistance, high toughness, environment friendliness, flame retardancy, self-cleaning property, thermal insulation and cost saving, and is convenient for construction.
Description
Technical field
The present invention relates to a kind of polymeric coating material.
Background technology
Modern society's energy consumption increases day by day, has consumed electric power resource and the coal resources of a large amount of preciousnesses.Along with people recognize the finiteness of resource and the ecocrisis that energy consumption causes gradually, energy-conservationly become environment protection and one of the important content that economizes on resources, thermal insulation technology is widely applied in each field, as various lagging materials, reflective insulation coating etc.Yet, the tradition heat preserving and insulating material is to reduce thermal conductivity and transmissibility factor is main, the fiber-like lagging material will be given full play to the effect of transmission of heat by convection and radiative transfer in environment for use, must use thick and heavy coating, and section bar class lagging material assembling construction is loaded down with trivial details, seam affect more attractive in appearance, work-ing life is shorter.At present, the domestic thermal insulating coating on market exists function singleness, effect is limited and validity period is short problem, is difficult to widespread use, and the import composite coating material is effective, purposes is wide, but price is higher, has increased production cost.Now oneself is through being penetrated into the industry-by-industry department of national economy for polymeric coating material, and it has the superior physicochemical properties such as good visible ray and infrared reflectivity, higher thermal infrared emittance, high-temperature stability.Therefore, a kind of energy-conserving and environment-protective, high strength are developed in design, the low-cost environment-friendly high polymer composite coating material that high temperature resistant, the thermal insulation separation temp effect is good is technical problem urgently to be resolved hurrily.
Summary of the invention
Technical problem to be solved by this invention is: a kind of environmentally friendly high polymer composite coating material is provided, there is superior high-temperature stability, and high strength, wear-resisting, high tenacity, environmental protection, fire-retardant, self-cleaning, insulation, easy construction simultaneously, cost-saving.
For solving the problems of the technologies described above, the technical solution used in the present invention is:
A kind of green energy conservation polymeric coating material, be comprised of the composition of following parts by weight: glass fibre 1-3 part, mica 3-4 part, POE24-31 part, poly--4-methyl-1-pentene 11-24 part, bisphenol A polycarbonate 5-9 part, 100 parts of organosilicon crylic acid latexs, nano-calcium carbonate 6-10 part, PS9-12 part, EVA11-32 part, 20-21 part tackiness agent, 10 parts of whipping agents, 1-5 part thickening material, 1-3 part dispersion agent, oxidation inhibitor 0.5-1 part.
The invention has the beneficial effects as follows: there is superior high-temperature stability, high strength, wear-resisting, high tenacity, environmental protection, fire-retardant, self-cleaning, insulation, easy construction simultaneously, cost-saving.
Embodiment
Embodiment 1
A kind of green energy conservation polymeric coating material, be comprised of the composition of following parts by weight: glass fibre 1-3 part, mica 3-4 part, POE24-31 part, poly--4-methyl-1-pentene 11-24 part, bisphenol A polycarbonate 5-9 part, 100 parts of organosilicon crylic acid latexs, nano-calcium carbonate 6-10 part, PS9-12 part, EVA11-32 part, 20-21 part tackiness agent, 10 parts of whipping agents, 1-5 part thickening material, 1-3 part dispersion agent, oxidation inhibitor 0.5-1 part.
Claims (1)
1. a green energy conservation polymeric coating material, be comprised of the composition of following parts by weight: glass fibre 1-3 part, mica 3-4 part, POE24-31 part, poly--4-methyl-1-pentene 11-24 part, bisphenol A polycarbonate 5-9 part, 100 parts of organosilicon crylic acid latexs, nano-calcium carbonate 6-10 part, PS9-12 part, EVA11-32 part, 20-21 part tackiness agent, 10 parts of whipping agents, 1-5 part thickening material, 1-3 part dispersion agent, oxidation inhibitor 0.5-1 part.