Eider down washing finishing agent and preparation method thereof
Technical field
The invention belongs to washing and nursing article, specifically a kind of eider down washing finishing agent and preparation method thereof.
Background technology
Eider down is widely used in making down jackets, but comes from animal due to eider down, usually with more bacterium, has fishy smell.With general articles for washing, foul can be washed away, but there is no sterilizing function, and easily damage eider down, cause and harden, no longer have original elasticity and loftiness, thermal property reduces, therefore, be badly in need of research have eider down have washing concurrently, nursing that nursing, taste removal, sterilizing function are taken into account and washing agent.
Summary of the invention
The object of this invention is to provide a kind of eider down washing finishing agent and preparation method thereof.
Technical scheme of the present invention is as follows:
A kind of eider down washing finishing agent, is characterized in that being made up of the raw material of following weight portion: Tea Saponin 1-1.2, natrium citricum 1-1.2, neopelex 2-2.4, ethyl acetate 2-3, ethylene glycol 3-4, tert-butyl hydroperoxide 1.2-1.5, morpholine 3-3.5, dibenzyl xenol polyoxyethylene polyoxypropylene ether 1-1.2, polyoxyethylene oleic acid ester 1-1.2, silane coupler KH-572 2-3, age resistor TPPD 1-2, sodium bicarbonate 2-3, softener 3-4, water 200.
Described softener is made up of the raw material components of following weight portion: Tea Polyphenols 0.2-0.3, sodium peroxydisulfate 0.3-0.4, glycerin monostearate 2.3-2.5, morpholine 1-1.2, trihydroxy ethylamine oleate soap 0.8-0.9, amido silicon oil 3.4-3.8, polyoxyethylene ether 1.2-1.5, titanate coupling agent TMC-TTS 1.2-1.5, citric acid 2.0-2.4, di-n-octyl-4-isothiazoline-3-ketone 0.3-0.5, water 15-18; Sodium peroxydisulfate is added suitable quantity of water to dissolve by preparation method, drops in the mixture of other residual components, stirs 40-50 minute, be then warming up to 70-80 DEG C, stirring reaction 1-2 hour and get final product.
The preparation method of described eider down washing finishing agent, Tea Saponin, natrium citricum, ethyl acetate, ethylene glycol, morpholine, dibenzyl xenol polyoxyethylene polyoxypropylene ether is it is characterized in that to be added to the water, be heated to 60-70 DEG C, stirring reaction 30-40 minute, then adds tert-butyl hydroperoxide, stirring reaction 50-60 minute, then, add other residual components, be warming up to 90-100 DEG C, continue to stir 60-80 minute, to obtain final product.
The present invention effectively can remove the dirt on eider down, and bactericidal action is strong, and have good conditioning, nursing role to eider down, eider down recovers original elasticity and bulk shape, keeps original thermal property.
Detailed description of the invention
A kind of eider down washing finishing agent, is characterized in that being made up of the raw material of following weight portion (kilogram): Tea Saponin 1-1.2, natrium citricum 1-1.2, neopelex 2-2.4, ethyl acetate 2-3, ethylene glycol 3-4, tert-butyl hydroperoxide 1.2-1.5, morpholine 3-3.5, dibenzyl xenol polyoxyethylene polyoxypropylene ether 1-1.2, polyoxyethylene oleic acid ester 1-1.2, silane coupler KH-572 2-3, age resistor TPPD 1-2, sodium bicarbonate 2-3, softener 3-4, water 200.
The preparation method of eider down washing finishing agent, Tea Saponin, natrium citricum, ethyl acetate, ethylene glycol, morpholine, dibenzyl xenol polyoxyethylene polyoxypropylene ether are added to the water, be heated to 60-70 DEG C, stirring reaction 30-40 minute, then adds tert-butyl hydroperoxide, stirring reaction 50-60 minute, then, add other residual components, be warming up to 90-100 DEG C, continue to stir 60-80 minute, to obtain final product.
Described softener is made up of the raw material components of following weight portion (kilogram): Tea Polyphenols 0.2, sodium peroxydisulfate 0.3, glycerin monostearate 2.3, morpholine 1, trihydroxy ethylamine oleate soap 0.9, amido silicon oil 3.4, polyoxyethylene ether 1.2, titanate coupling agent TMC-TTS 1.2, citric acid 2.0, di-n-octyl-4-isothiazoline-3-ketone 0.3, water 15; Sodium peroxydisulfate is added suitable quantity of water to dissolve by preparation method, drops in the mixture of other residual components, stirs 40-50 minute, be then warming up to 70-80 DEG C, stirring reaction 1-2 hour and get final product.