CN103427085A - Battery panel nickel sheet welding product - Google Patents

Battery panel nickel sheet welding product Download PDF

Info

Publication number
CN103427085A
CN103427085A CN201310321830XA CN201310321830A CN103427085A CN 103427085 A CN103427085 A CN 103427085A CN 201310321830X A CN201310321830X A CN 201310321830XA CN 201310321830 A CN201310321830 A CN 201310321830A CN 103427085 A CN103427085 A CN 103427085A
Authority
CN
China
Prior art keywords
nickel sheet
pad
welding product
cell panel
sheet welding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310321830XA
Other languages
Chinese (zh)
Inventor
李海飞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
KUNSHAN YUANSONG ELECTRONIC SCIENCE AND TECHNOLOGY Co Ltd
Original Assignee
KUNSHAN YUANSONG ELECTRONIC SCIENCE AND TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by KUNSHAN YUANSONG ELECTRONIC SCIENCE AND TECHNOLOGY Co Ltd filed Critical KUNSHAN YUANSONG ELECTRONIC SCIENCE AND TECHNOLOGY Co Ltd
Priority to CN201310321830XA priority Critical patent/CN103427085A/en
Publication of CN103427085A publication Critical patent/CN103427085A/en
Pending legal-status Critical Current

Abstract

The invention discloses a battery panel nickel sheet welding product, which comprises a nickel sheet and a PCB (Printed Circuit Board), wherein a PAD is arranged on the PCB; one surface of the nickel sheet is welded to the PAD; the PAD is formed by a plurality of small PADs; the small PADs are isolated via ink. The welding between the nickel sheet and the PAD is more firm by arranging tin blocks in the PAD and arranging an oblique line knurling on a welding surface of the nickel sheet, as a result, the phenomena of tin balls, less tin and the like, generally existing in the welding process, are reduced, and the quality and stability of the product are greatly improved.

Description

A kind of cell panel nickel sheet welding product
Technical field
The present invention relates to technical field of electronic components, relate in particular to a kind of cell panel nickel sheet welding product.
Background technology
Along with scientific and technical develop rapidly, electronic product is to miniaturization and multifunction development, the short and small frivolous main flow trend that become, so yet the miniaturization of cell panel product and technological requirement also more and more higher current product ubiquity in the process of welding production are produced to unfavorable condition, deficient in stability and the reliabilities such as tin sweat(ing) and few tin.
Summary of the invention
In order to overcome the deficiencies in the prior art, the invention provides a kind of quality more reliable and stable, the cell panel nickel sheet welding product that technological level is higher.
Technical problem to be solved by this invention is achieved through the following technical solutions:
A kind of cell panel nickel sheet welding product, it is characterized in that: comprise nickel sheet, pcb board, described pcb board is provided with PAD, and the nickel sheet simultaneously is welded on PAD.
Preferably, described nickel sheet is rectangle, on the minor face of rectangular both sides, respectively has a breach.
Preferably, described PAD is rectangle, and with nickel sheet size 1:1, PAD is comprised of the little PAD of some rectangles, and between little PAD, spacing is 0.25mm, with printing ink, isolates.
Preferably, described nickel sheet material is pure nickel.
Preferably, the solder side of described nickel sheet arranges the oblique line embossing, and the embossing degree of depth is 0.03-0.05mm.
Preferably, described PAD is long is provided with some rectangle block tins in the little PAD at two ends, and the little PAD in the middle of PAD does not establish block tin, keeps the 0.2mm spacing in same little PAD between each block tin.
The beneficial effect that the present invention reaches is: with conventional batteries plate welding product, compare, weld strength of the present invention is higher, and quality is more stable, has significantly reduced the manpower maintenance cost.
The accompanying drawing explanation
Fig. 1 is the structural representation of the upper block tin arranged of PAD and PAD in the present invention;
Fig. 2 is the structural representation at the nickel sheet back side in the present invention;
Fig. 3 is the structural representation of nickel sheet solder side in the present invention;
Fig. 4 is that nickel sheet of the present invention is welded on the structural representation on PAD.
Embodiment
In order to further describe technical characterstic of the present invention and effect, below in conjunction with the drawings and specific embodiments, the present invention is described further.
Referring to figs. 1 through Fig. 4, a kind cell panel nickel sheet welding product, comprise nickel sheet 2, pcb board, and described pcb board is provided with PAD1, described nickel sheet 2 materials are pure nickel, it is upper that one side is welded on PAD1, and described PAD1 and nickel sheet 2 are rectangle, and size designs according to 1:1, have breach 21 on the minor face of the rectangle both sides of nickel sheet 2, described PAD1 is comprised of the little PAD11 of some rectangles, and the spacing between adjacent little PAD11 is 0.25mm, and isolates with printing ink.In order to make nickel sheet 2 more firm with the welding of PAD1, solder side at nickel sheet 2 is provided with oblique line embossing 22, the embossing degree of depth is 0.03-0.05mm, be provided with some rectangle block tins 12 in described PAD1 length in the little PAD11 at two ends, little PAD11 in the middle of PAD1 does not establish block tin 12, keep the 0.2mm spacing between interior each the adjacent block tin 12 of same little PAD11, the embossing face of weld of nickel sheet 2 is welded on PAD1 by block tin.
Above-described embodiment does not limit the present invention in any form, all take to be equal to replace or technical scheme that the form of equivalent transformation obtains, within all dropping on protection scope of the present invention.

Claims (6)

1. a cell panel nickel sheet welding product, is characterized in that, comprise nickel sheet, pcb board, described pcb board is provided with PAD, and the nickel sheet simultaneously is welded on PAD.
2. a kind of cell panel nickel sheet welding product according to claim 1, is characterized in that, described nickel sheet is rectangle, on the minor face of rectangular both sides, respectively has a breach.
3. a kind of cell panel nickel sheet welding product according to claim 1, is characterized in that, described PAD is rectangle, and with nickel sheet size 1:1, PAD is comprised of the little PAD of some rectangles, and between little PAD, spacing is 0.25mm, with printing ink, isolates.
4. a kind of cell panel nickel sheet welding product according to claim 1, is characterized in that, described nickel sheet material is pure nickel.
5. a kind of cell panel nickel sheet welding product according to claim 1, is characterized in that, the solder side of described nickel sheet arranges the oblique line embossing, and the embossing degree of depth is 0.03-0.05mm.
6. a kind of cell panel nickel sheet welding product according to claim 1, it is characterized in that, described PAD is long is provided with some rectangle block tins in the little PAD at two ends, and the little PAD in the middle of PAD does not establish block tin, between interior each the adjacent block tin of same little PAD, keeps the 0.2mm spacing.
CN201310321830XA 2013-07-29 2013-07-29 Battery panel nickel sheet welding product Pending CN103427085A (en)