CN103341458A - High-power concentrating photovoltaic conversion receiver circuit board cleaning technology - Google Patents
High-power concentrating photovoltaic conversion receiver circuit board cleaning technology Download PDFInfo
- Publication number
- CN103341458A CN103341458A CN201310235516XA CN201310235516A CN103341458A CN 103341458 A CN103341458 A CN 103341458A CN 201310235516X A CN201310235516X A CN 201310235516XA CN 201310235516 A CN201310235516 A CN 201310235516A CN 103341458 A CN103341458 A CN 103341458A
- Authority
- CN
- China
- Prior art keywords
- cleaning
- electronic conversion
- circuit plate
- acceptor circuit
- high power
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to a high-power concentrating photovoltaic conversion receiver circuit board cleaning technology and belongs to the technical field of solar photovoltaic power generating. The high-power concentrating photovoltaic conversion receiver circuit board cleaning technology includes the following steps that an aluminum disc of an unbonded photovoltaic conversion receiver circuit board is conveyed to a high-temperature spraying and cleaning machine and fixed in the high-temperature spraying and cleaning machine. Technological parameters of the cleaning machine are set and a power supply is started to perform cleaning. After cleaning is finished, a product is put into a drying box. Technological parameters of a drying machine are set and a power supply is started to dry. According to the high-power concentrating photovoltaic conversion receiver circuit board cleaning technology, the surface of the high-power concentrating photovoltaic conversion receiver circuit board is uniform in cleanliness. Surface smudginess and an oxidation layer are effectively treated. When a cell piece is bonded with a circuit board, better bonding performance is obtained, the reject ratio of products is reduced to the utmost and therefore, extra cost caused by repairing the products is controlled to the utmost.
Description
Technical field
The present invention relates to a kind of manufacturing cleaning process flow, relate in particular to a kind of high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate cleaning, belong to the solar photovoltaic technology field.
Background technology
High power concentrator photovoltaic opto-electronic conversion receiver, it is one of assembly most crucial in the high power concentrator volt opto-electronic conversion module, because the core of high power concentrator photovoltaic cell sheet is high efficiency GaInP/GaInAs/Ge three knot condensation photovoltaic battery chips, when with high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate bonding after, form high power concentrator photovoltaic opto-electronic conversion receiver, but before bonding, the quality that how to guarantee high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate is very important, directly influences the q﹠r of high power concentrator photovoltaic opto-electronic conversion receiver.
The technological process of most of makers' cleaning high power concentrator photovoltaic opto-electronic conversion acceptor circuit plates at present; namely when high power concentrator photovoltaic cell sheet and circuit board bonding; high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate takes out from vacuum bag; manufactory all be with alcohol or erasing rubber directly to high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate surface dirty and oxide layer handle; though above method is very effective; but invisible central high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate surface coating meeting is destroyed and the circuit board surface cleannes are inconsistent; when cleaning with erasing rubber; also can operating environment of pollution; product is caused secondary pollution and can't clean row high power concentrator battery sheet surface; to high power concentrator battery sheet and circuit board bonding the time; cause bonding failure through regular meeting; bonding line comes off and phenomenons such as false bonding; cause reprocessing difficulty; cause high power concentrator battery sheet and circuit board to scrap; comparatively speaking; the rate that manufactures a finished product of enterprise is low; the cost height, and reliability of products and life-span will can not get ensureing.
Nowadays, the high power concentrator photovoltaic industry is grown up fast in the whole world, only based on previous reasons, the cleaning that how to solve high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate is that we must face and will conscientiously study, and solves the high efficiency of product and the cost of enterprise with this.
Summary of the invention
The objective of the invention is to be to provide a kind of high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate cleaning, this technology technical problem to be solved is to overcome the deficiencies in the prior art.
In order to realize above-mentioned technical purpose, the technical scheme that the present invention takes is: a kind of high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate cleaning, it is characterized in that, comprise and to be equipped with not that the aluminium dish of the opto-electronic conversion acceptor circuit plate of bonding is transported to high temperature spray Cleaning for High Capacity board, and be fixed in the high temperature spray Cleaning for High Capacity machine; Set the cleaning machine technological parameter, and start the power supply cleaning; Product after cleaning is finished is put into drying baker; Set the dryer technological parameter, and start four steps of power supply oven dry.
Described manufacturing process personnel are placed into high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate in the special-purpose aluminium dish with manual mode orientation according to the rules, the aluminium dish that product is housed are placed on the rack for cleaning of high temperature spray Cleaning for High Capacity machine and fix.
Described high temperature spray Cleaning for High Capacity machine can be automatic, semi-automatic or manual form, and temperature and time is all adjustable.
Described manufacturing process personnel arrange corresponding high temperature spray Cleaning for High Capacity machine parameter according to high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate model.
Described drying baker can be other form such as automatic, semi-automatic or manual.
Described manufacturing process personnel arrange corresponding dryer parameter according to high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate model.
Advantage of the present invention and good effect are: 1. this technology can allow high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate surface obtain conforming cleannes, effectively handles with oxide layer the surface is dirty; 2. this technology can access better bonding performance when battery sheet and circuit board bonding; 3. this technology can the maximum fraction defective that reduces product, produces extra cost thereby control product to greatest extent because reprocessing.
Description of drawings
Fig. 1 is a kind of high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate cleaning process flow figure.
Wherein: 1,2,3,4 is the cleaning process flow step.
Specific embodiments
To further instruction of the present invention, the composition processing step in the annex map might not meet ratio, but describes out flow process of the present invention in the mode of emphasizing below in conjunction with accompanying drawing.
Referring to Fig. 1, be the flow chart of steps of manufacturing process of the present invention.At first in step 1, manufacturing process personnel are placed into high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate in the special-purpose aluminium dish with manual mode orientation according to the rules, the aluminium dish that product is housed are placed on the rack for cleaning of high temperature spray Cleaning for High Capacity machine and fix; In step 2, manufacturing process personnel set the cleaning machine technological parameter according to high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate model, and the startup power supply cleans high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate; In step 3, the product after manufacturing process personnel finish cleaning is put into drying baker; In step 4, manufacturing process personnel set the dryer technological parameter according to high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate model, and the startup power supply is dried high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate.
Among the present invention; above-described specific embodiment; purpose of the present invention, technical scheme and effect are had been described in detail; institute should understand is; the above is specific embodiments of the invention only, and is not intended to limit the scope of the invention, and is within the spirit and principles in the present invention all; any modification, replacement and the improvement etc. made all should be included in protection scope of the present invention.
Claims (6)
1. a high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate cleaning is characterized in that, comprises that the aluminium dish of the opto-electronic conversion acceptor circuit plate of bonding is transported to high temperature spray Cleaning for High Capacity board with being equipped with not, and is fixed in the high temperature spray Cleaning for High Capacity machine; Set the cleaning machine technological parameter, and start the power supply cleaning; Product after cleaning is finished is put into drying baker; Set the dryer technological parameter, and start four steps of power supply oven dry.
2. a kind of high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate cleaning according to claim 1, it is characterized in that described manufacturing process personnel are placed into high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate in the special-purpose aluminium dish with manual mode orientation according to the rules, the aluminium dish that product is housed is placed on the rack for cleaning of high temperature spray Cleaning for High Capacity machine and fixes.
3. according to claim 1 and 2 described a kind of high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate cleanings, it is characterized in that described high temperature spray Cleaning for High Capacity machine can be automatic, semi-automatic or manual form, and temperature and time is all adjustable.
4. a kind of high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate cleaning according to claim 1 is characterized in that described manufacturing process personnel arrange corresponding high temperature spray Cleaning for High Capacity machine parameter according to high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate model.
5. a kind of high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate cleaning according to claim 1 is characterized in that described drying baker can be other form such as automatic, semi-automatic or manual.
6. a kind of high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate cleaning according to claim 1 is characterized in that described manufacturing process personnel arrange corresponding dryer parameter according to high power concentrator photovoltaic opto-electronic conversion acceptor circuit plate model.