CN103336019A - 一种线路板的导电阳极丝失效分析方法 - Google Patents

一种线路板的导电阳极丝失效分析方法 Download PDF

Info

Publication number
CN103336019A
CN103336019A CN2013102079403A CN201310207940A CN103336019A CN 103336019 A CN103336019 A CN 103336019A CN 2013102079403 A CN2013102079403 A CN 2013102079403A CN 201310207940 A CN201310207940 A CN 201310207940A CN 103336019 A CN103336019 A CN 103336019A
Authority
CN
China
Prior art keywords
wiring board
conductive anode
inefficacy
silk
anode silk
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013102079403A
Other languages
English (en)
Inventor
严泽军
张盘新
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
MICROTEK (CHANGZHOU) PRODUCT SERVICES Co Ltd
Original Assignee
MICROTEK (CHANGZHOU) PRODUCT SERVICES Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by MICROTEK (CHANGZHOU) PRODUCT SERVICES Co Ltd filed Critical MICROTEK (CHANGZHOU) PRODUCT SERVICES Co Ltd
Priority to CN2013102079403A priority Critical patent/CN103336019A/zh
Publication of CN103336019A publication Critical patent/CN103336019A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种线路板的导电阳极丝失效分析方法,使用逐步分割的方式锁定失效区域,直至找到相邻的两个失效过孔,再对两个失效过孔进行研磨,精确定位导电阳极丝的形成位置,最后垂直导电阳极丝进行第二次研磨,使用扫描电镜和能谱仪观察导电阳极丝的截面,分析导电阳极丝形成原因,该发明具有对导电阳极丝形成位置定位快速、准确的优点。

Description

一种线路板的导电阳极丝失效分析方法
技术领域
本发明涉及线路板的绝缘性能测试技术领域,特别涉及一种线路板的导电阳极丝失效分析方法。 
背景技术
导电阳极丝(CAF)是可以导致电气短路或开路的电化学腐蚀过程的副产物。通常表现为从电路的阳极发散出来,沿着玻纤与环氧之间的界面朝着阴极方向迁移,形成导电性细丝物。导电阳极丝多形成于线路板相邻的过孔与过孔之间。 
随着对电子设备的印制线路板可靠性要求越来越高,传统的绝缘性能测试已不能确保线路板在应用环境下的可靠性。目前行业中,常用IPC标准规定的测试图形和试验条件来对线路板的导电阳极丝(CAF)失效现象进行分析测试。但是传统绝缘测试只能确定线路板的某个单元出现了导电阳极丝失效现象,而每个单元含有数百个按序排列的过孔,上述分析方法不能确定具体是哪对过孔失效导致了整个单元失效,更无法确定导电阳极丝的精确位置。 
发明内容
为解决上述技术问题,本发明提供了一种线路板的导电阳极丝失效分析方法,以达到快速、准确定位线路板中导电阳极丝形成位置的目的。 
为达到上述目的,本发明的技术方案如下:一种线路板的导电阳极丝失效分析方法,包括如下步骤: 
a、将线路板切割为两块,分别测量两块线路板的阻值; 
b、取阻值较小的那块线路板,并重复上述a步骤,直至线路板上只有两个相邻的过孔,这两个相邻的过孔即是一对失效过孔; 
c、对线路板进行第一次研磨,并用光学显微镜观察,直至导电阳极丝出现在线路板的研磨剖面上,确定了导电阳极丝的精确位置; 
d、垂直于导电阳极丝方向对线路板进行第二次研磨,并用扫描电镜和 能谱仪观察导电阳极丝的截面,用以分析导电阳极丝形成原因。 
优选的,当失效过孔圆心的连线平行于线路板任一侧边时,第一次研磨从线路板平行于失效过孔圆心连线的侧边开始,并沿垂直于失效过孔圆心连线的方向进行;当失效过孔圆心的连线与线路板任一侧边均不平行时,第一次研磨从线路板幅面开始,并沿着垂直于幅面的方向进行。 
通过上述技术方案,本发明提供的一种线路板的导电阳极丝失效分析方法使用逐步分割的方式锁定失效区域,直至找到相邻的两个失效过孔,再对两个失效过孔进行研磨,精确定位导电阳极丝的形成位置,最后垂直导电阳极丝进行第二次研磨,使用扫描电镜和能谱仪观察导电阳极丝的截面,分析导电阳极丝形成原因,具有对导电阳极丝形成位置定位快速、准确的优点。 
具体实施方式
下面将对本发明实施例中的技术方案进行清楚、完整地描述。 
本发明提供了一种线路板的导电阳极丝失效分析方法,包括如下步骤: 
a、将线路板切割为面积相同的两块,分别测量这两块线路板的阻值; 
b、取阻值较小的那块线路板,并重复上述a步骤,逐步切割直至线路板上只有两个相邻的过孔,这两个相邻的过孔即是一对失效过孔; 
c、对线路板进行第一次研磨,并用光学显微镜观察,直至导电阳极丝出现在线路板的研磨剖面上,确定了导电阳极丝的精确位置; 
d、垂直于导电阳极丝方向对线路板进行第二次研磨,并用扫描电镜和能谱仪观察导电阳极丝的截面,用以分析导电阳极丝形成原因。 
导电阳极丝多形成于过孔之间,而且具体走向是不确定的,在进行步骤c的时候,为使导电阳极丝尽量完整地呈现在研磨剖面上,研磨方向按下述标准选择:当失效过孔圆心的连线平行于线路板任一侧边时,第一次研磨从线路板平行于失效过孔圆心连线的侧边开始,并沿垂直于失效过孔圆心连线的方向进行;当失效过孔圆心的连线与线路板任一侧边均不平行时,第一次研磨从线路板幅面开始,并沿着垂直于幅面的方向进行。 
本发明提供的一种线路板的导电阳极丝失效分析方法使用逐步分割的方式锁定失效区域,直至找到相邻的两个失效过孔,再对两个失效过孔进行研磨,精确定位导电阳极丝的形成位置,最后垂直导电阳极丝进行第二次研磨,使用扫描电镜和能谱仪观察导电阳极丝的截面,分析导电阳极丝的形成原因,具有对导电阳极丝形成位置定位快速、准确的优点。 
对所公开的一种线路板的导电阳极丝失效分析方法实施例的上述说明,使本领域专业技术人员能够实现或使用本发明。对这些实施例的多种修改对本领域的专业技术人员来说将是显而易见的,本文中所定义的一般原理可以在不脱离本发明的精神或范围的情况下,在其它实施例中实现。因此,本发明将不会被限制于本文所示的这些实施例,而是要符合与本文所公开的原理和新颖特点相一致的最宽的范围。 

Claims (2)

1.一种线路板的导电阳极丝失效分析方法,其特征在于,包括如下步骤:
a、将线路板切割为两块,分别测量两块线路板的阻值;
b、取阻值较小的那块线路板,并重复上述a步骤,直至线路板上只有两个相邻的过孔,这两个相邻的过孔即是一对失效过孔;
c、对线路板进行第一次研磨,并用光学显微镜观察,直至导电阳极丝出现在线路板的研磨剖面上,确定了导电阳极丝的精确位置;
d、垂直于导电阳极丝方向对线路板进行第二次研磨,并用扫描电镜和能谱仪观察导电阳极丝的截面,用以分析导电阳极丝形成原因。
2.一种基于权利要求1所述的线路板导电阳极丝失效分析方法,其特征在于,当失效过孔圆心的连线平行于线路板任一侧边时,第一次研磨从线路板平行于失效过孔圆心连线的侧边开始,并沿垂直于失效过孔圆心连线的方向进行;当失效过孔圆心的连线与线路板任一侧边均不平行时,第一次研磨从线路板幅面开始,并沿着垂直于幅面的方向进行。
CN2013102079403A 2013-05-28 2013-05-28 一种线路板的导电阳极丝失效分析方法 Pending CN103336019A (zh)