CN103326025A - 用于锂离子电池的石墨烯粉末的制备方法 - Google Patents
用于锂离子电池的石墨烯粉末的制备方法 Download PDFInfo
- Publication number
- CN103326025A CN103326025A CN2013102272792A CN201310227279A CN103326025A CN 103326025 A CN103326025 A CN 103326025A CN 2013102272792 A CN2013102272792 A CN 2013102272792A CN 201310227279 A CN201310227279 A CN 201310227279A CN 103326025 A CN103326025 A CN 103326025A
- Authority
- CN
- China
- Prior art keywords
- graphene powder
- lithium ion
- preparation
- ion battery
- graphene
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Description
Claims (5)