CN103321120A - 保湿润路面 - Google Patents

保湿润路面 Download PDF

Info

Publication number
CN103321120A
CN103321120A CN2012100868782A CN201210086878A CN103321120A CN 103321120 A CN103321120 A CN 103321120A CN 2012100868782 A CN2012100868782 A CN 2012100868782A CN 201210086878 A CN201210086878 A CN 201210086878A CN 103321120 A CN103321120 A CN 103321120A
Authority
CN
China
Prior art keywords
pavement
water
people
moisture
road surface
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012100868782A
Other languages
English (en)
Inventor
刘祖学
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2012100868782A priority Critical patent/CN103321120A/zh
Publication of CN103321120A publication Critical patent/CN103321120A/zh
Pending legal-status Critical Current

Abstract

时至目前,为防止机动车行驶时路面扬起灰尘影响人们的健康和环境卫生,均采用向路面洒水的方法。但这种方法有较多缺陷,为了克服这些缺陷,这里发明了一种新的技术方案,就是在人们居住和活动较多区域内的机动车路的修建和改建中,铺路面时向水泥沙浆中加入适量吸水保水材料,这种路面的特征是,一旦受水淋湿后,即便天气干热时仍能较长时间(3天左右)湿润,在一般的晴天时可保持5天左右的路面湿润,其一劳多逸,节能环保。为人们的生活和出行提供清新舒适的环境条件。

Description

保湿润路面
技术领域
在发明公开了一种机动车路面,具体涉及到路面保持较长时间湿润。 
背景技术
由于机动车行驶速度较快,体积较大,其在较干的路面行驶时,极易扬起灰尘,直接影响人们的身体健康和环境卫生。为了克服这种现象,目前人们采取的是定时向路面洒水的方法。这种方法对控制路面扬尘起到了一定作用,但是具有如下缺陷:1、大量浪费水资源和能源;2、洒水时对行人有影响;3、天干热时,路面干的很快,每天要多次洒水,很麻烦费事。 
发明内容
为了克服以上缺陷,尽量达到一劳多逸,这里采取技术方案是,在人们居住和活动多的区域的机动车道路修建或改建时,向铺设路面的材料中加入适量的吸水保水材料,由于这种材料具有很强的吸水和保水作用,所以经过这种材料后修建的路面,在接受水分后可较长时间保持路面的湿润,防止了路面扬尘的现象。 
附图说明
图1保湿润路面结构示意图 
附图标记说明 
1、坚实路基  2、钢筋混凝土层  3、含有吸水保水材料的水泥沙浆层 
具体实施方式
铺设这种路面的方法与通常的方法完全相同,首先处理好坚实的路基1,再铺设钢筋和混凝土层2,最后铺上含有吸水保水材料的水泥沙浆层3,向水泥砂浆里加吸水保水材料的方法是:将800-1000目的吸水保水材料取水泥体积的0.7%份充分泡胀且除去多余水分,混合入正常比例已拌匀的水泥沙浆中并再次充分拌匀,最后按7cm左右厚度将路面铺平、收浆、待其凝固定形后即可投入使用。这种路面的特征为:当充分接受一次水分后,在一般的情况下可至少保持5天路面湿润,在天气干燥时,其需洒水的次数是普通路面需洒水次数的八分之一到十分之一,达到了一劳多逸的效果,为人们的出行和生活提供了清新舒适的良好环境条件。 

Claims (1)

1.一种机动车路面可较长时间保持湿润,其技术方案是:在修建或改建机动车路时,在铺路面的这道工序,先向水泥沙浆里加入适量吸水保水材料,这种路面凝固定形后其特征为:受水淋湿后可较长时间保持路面湿润,可有效地避免机动车行驶扬起灰尘,为人们的出行和生活提供清新舒适的环境条件。
CN2012100868782A 2012-03-17 2012-03-17 保湿润路面 Pending CN103321120A (zh)