CN103320080A - 聚异氰酸酯胶生产工艺 - Google Patents
聚异氰酸酯胶生产工艺 Download PDFInfo
- Publication number
- CN103320080A CN103320080A CN2013102233001A CN201310223300A CN103320080A CN 103320080 A CN103320080 A CN 103320080A CN 2013102233001 A CN2013102233001 A CN 2013102233001A CN 201310223300 A CN201310223300 A CN 201310223300A CN 103320080 A CN103320080 A CN 103320080A
- Authority
- CN
- China
- Prior art keywords
- weight
- reactor
- suction
- parts
- weight part
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种聚异氰酸酯胶生产工艺,包括如下步骤:1)在第一反应釜中,先抽入31-42重量份二苯基甲烷二异氰酸酯、21-32重量份甲苯二异氰酸酯,再抽入62-81重量份氯苯,冷凝器通冷却水、加热、搅拌、回流,在135℃保温7h,完成混配;2)在第二反应釜中抽入42-53重量份氯苯,再加入12-31重量份叔丁酚醛树脂,打开回流冷凝器,加热,搅拌,保持50℃,直至全部溶解;3)将第二反应釜中溶液抽入第一反应釜中,搅拌均匀,冷却,制得成品。本发明提供的聚异氰酸酯胶生产工艺,其工艺简单,制备的聚异氰酸酯胶粘接强度高。
Description
技术领域
本发明涉及聚异氰酸酯胶生产工艺。
背景技术
JQ-1聚异氰酸酯胶又叫JQ-1列克钠胶,危规编号为33645,是一种较为理想的可单独使用或与氯丁胶配合使用的粘合剂,外观为浅棕色液体,主要用于橡胶与金属的粘结、与氯丁橡胶配伍作为固化剂使用。
发明内容
本发明的目的在于提供一种聚异氰酸酯胶生产工艺,其工艺简单,制备的聚异氰酸酯胶粘接强度高。
为实现上述目的,本发明的技术方案是设计一种聚异氰酸酯胶生产工艺,包括如下步骤:
1)在第一反应釜中,先抽入31-42重量份二苯基甲烷二异氰酸酯、21-32重量份甲苯二异氰酸酯,再抽入62-81重量份氯苯,冷凝器通冷却水、加热、搅拌、回流,在135℃保温7h,完成混配;
2)在第二反应釜中抽入42-53重量份氯苯,再加入12-31重量份叔丁酚醛树脂,打开回流冷凝器,加热,搅拌,保持50℃,直至全部溶解;
3)将第二反应釜中溶液抽入第一反应釜中,搅拌均匀,冷却,制得成品。
本发明的优点和有益效果在于:提供一种聚异氰酸酯胶生产工艺,其工艺简单,制备的聚异氰酸酯胶粘接强度高。
具体实施方式
下面结合实施例,对本发明的具体实施方式作进一步描述。以下实施例仅用于更加清楚地说明本发明的技术方案,而不能以此来限制本发明的保护范围。
本发明具体实施的技术方案是:
实施例1
一种聚异氰酸酯胶生产工艺,包括如下步骤:
1)在第一反应釜中,先抽入38重量份二苯基甲烷二异氰酸酯、27重量份甲苯二异氰酸酯,再抽入71重量份氯苯,冷凝器通冷却水、加热、搅拌、回流,在135℃保温7h,完成混配;
2)在第二反应釜中抽入48重量份氯苯,再加入21重量份叔丁酚醛树脂,打开回流冷凝器,加热,搅拌,保持50℃,直至全部溶解;
3)将第二反应釜中溶液抽入第一反应釜中,搅拌均匀,冷却,制得成品。
实施例2
一种聚异氰酸酯胶生产工艺,包括如下步骤:
1)在第一反应釜中,先抽入31重量份二苯基甲烷二异氰酸酯、21重量份甲苯二异氰酸酯,再抽入62重量份氯苯,冷凝器通冷却水、加热、搅拌、回流,在135℃保温7h,完成混配;
2)在第二反应釜中抽入42重量份氯苯,再加入12重量份叔丁酚醛树脂,打开回流冷凝器,加热,搅拌,保持50℃,直至全部溶解;
3)将第二反应釜中溶液抽入第一反应釜中,搅拌均匀,冷却,制得成品。
实施例3
一种聚异氰酸酯胶生产工艺,包括如下步骤:
1)在第一反应釜中,先抽入42重量份二苯基甲烷二异氰酸酯、32重量份甲苯二异氰酸酯,再抽入81重量份氯苯,冷凝器通冷却水、加热、搅拌、回流,在135℃保温7h,完成混配;
2)在第二反应釜中抽入53重量份氯苯,再加入31重量份叔丁酚醛树脂,打开回流冷凝器,加热,搅拌,保持50℃,直至全部溶解;
3)将第二反应釜中溶液抽入第一反应釜中,搅拌均匀,冷却,制得成品。
以上所述仅是本发明的优选实施方式,应当指出,对于本技术领域的普通技术人员来说,在不脱离本发明技术原理的前提下,还可以做出若干改进和润饰,这些改进和润饰也应视为本发明的保护范围。
Claims (1)
1.聚异氰酸酯胶生产工艺,其特征在于,包括如下步骤:
1)在第一反应釜中,先抽入31-42重量份二苯基甲烷二异氰酸酯、21-32重量份甲苯二异氰酸酯,再抽入62-81重量份氯苯,冷凝器通冷却水、加热、搅拌、回流,在135℃保温7h,完成混配;
2)在第二反应釜中抽入42-53重量份氯苯,再加入12-31重量份叔丁酚醛树脂,打开回流冷凝器,加热,搅拌,保持50℃,直至全部溶解;
3)将第二反应釜中溶液抽入第一反应釜中,搅拌均匀,冷却,制得成品。