CN103290832A - 一种以石蜡和沙子为原料制备憎水沙的方法 - Google Patents
一种以石蜡和沙子为原料制备憎水沙的方法 Download PDFInfo
- Publication number
- CN103290832A CN103290832A CN2013102740400A CN201310274040A CN103290832A CN 103290832 A CN103290832 A CN 103290832A CN 2013102740400 A CN2013102740400 A CN 2013102740400A CN 201310274040 A CN201310274040 A CN 201310274040A CN 103290832 A CN103290832 A CN 103290832A
- Authority
- CN
- China
- Prior art keywords
- sand
- hydrophobic
- paraffin
- wax
- preparation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明公开了一种以细沙和石蜡为原料制备憎水沙的方法。主要工艺过程是将石蜡加热下形成液体石蜡,加入细沙搅拌使石蜡均匀分布在沙的表面即得憎水沙。本方法制备的憎水沙性能很好。本方法制备的憎水沙可用于城市绿化的节水,干旱地区土壤的水分保持及沙漠防治等方面,并有望发挥很大的作用。
Description
技术领域
本发明涉及可用于城市园林、治沙及供其他节水领域应用的一种憎水沙的制备方法,特别指以石蜡和细沙为原料来制备憎水沙的方法。
背景技术
本发明主要针对目前水资源短缺、灌溉用水严重浪费;荒漠化日益严重等方面的问题。利用石蜡及成本很低的细沙为原料制备一种表面由石蜡覆盖的细沙,由于该沙的表面为石蜡,因此不会保留水分,而且不亲水,可以使雨水或者灌溉水顺利渗入地下;同时由于细沙表面不亲水,可以有效降低水分通过土壤以毛细现象吸水,然后再蒸发造成土壤失水。
由于本发明是利用石蜡和沙子为主要原料,制备的憎水沙成本较低廉,目前还未见该方面的相关报道,而其独特的性能使其在荒漠化防治和城市绿化及景观美化(如果制备时在沙的表面附着不同颜色)方面将有广阔的应用前景。
发明内容
本发明要解决的技术问题是提供一种憎水沙的制备方法,这种制备方法以细沙、石蜡为原料,经合理配比,通过一定的工艺过程而制得憎水沙。
本发明要解决的技术问题是由如下方案解决的:一种石蜡和沙子为原料制备憎水沙的方法,其特征是:将石蜡加热到70℃-95℃,在加热保温70℃-95℃下加入细沙,在加热下搅拌,使石蜡均匀附着于细沙表面,自然冷却后即得憎水沙,其中石蜡与细沙的质量比为1:8-13。
上述一种石蜡和沙子为原料制备憎水沙的方法中的细沙是指:海沙、河沙及其他来源的沙子
本发明的优点是:1、用本方法制备的憎水沙成本较低。2、其表面由很薄的石蜡覆盖,因而不亲水。3、将其应用于城市绿化或者荒漠化防治可以节约灌溉用水、减少蒸发以抑制荒漠化的进程,以达到节水和治理荒漠化的目的。
附图说明
图1是以石蜡和沙子为原料制备憎水沙的工艺流程图。
具体实施方式
实施例1:
将10 g石蜡加热到700C形成液体石蜡,加入80g细沙,维持加热使温度在700C左右情况下搅拌均匀,出料、自然冷却,包装即得产品。
实施例2:
将10 g石蜡加热到750C形成液体石蜡,加入90g细沙,维持加热使温度在750C左右情况下搅拌均匀,出料、自然冷却,包装即得产品。
实施例3:
将10 g石蜡加热到800C形成液体石蜡,加入100g细沙,维持加热使温度在800C左右情况下搅拌均匀,出料、自然冷却,包装即得产品。
实施例4:
将10 g石蜡加热到850C形成液体石蜡,加入110 g 细沙,维持加热使温度在850C左右情况下搅拌均匀,出料、自然冷却,包装即得产品。
实施例5:
将10 g石蜡加热到900C形成液体石蜡,加入120g细沙,维持加热使温度在900C左右情况下搅拌均匀,出料、自然冷却,包装即得产品。
实施例6:
将10 g石蜡加热到950C形成液体石蜡,加入130g细沙,维持加热使温度在950C左右情况下搅拌均匀,出料、自然冷却,包装即得产品。
Claims (2)
1.一种石蜡和沙子为原料制备憎水沙的方法,其特征是:将石蜡加热到70℃-95℃,在加热保温70℃-95℃下加入细沙,在加热下搅拌,使石蜡均匀附着于细沙表面,自然冷却后即得憎水沙,其中石蜡与细沙的质量比为1:8-13。
2.权利要求1中的细沙是指:海沙、河沙及其他来源的沙子。