CN103289483B - 一种含有乙烯-三氟氯乙烯共聚物的防水耐酸碱涂料 - Google Patents

一种含有乙烯-三氟氯乙烯共聚物的防水耐酸碱涂料 Download PDF

Info

Publication number
CN103289483B
CN103289483B CN201310216421.3A CN201310216421A CN103289483B CN 103289483 B CN103289483 B CN 103289483B CN 201310216421 A CN201310216421 A CN 201310216421A CN 103289483 B CN103289483 B CN 103289483B
Authority
CN
China
Prior art keywords
ethylene
chlorotrifluoro
parts
alkali
ethylene copolymer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310216421.3A
Other languages
English (en)
Other versions
CN103289483A (zh
Inventor
林耀朋
张旭
吴军
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Suzhou Xugong New Material Technology Co.,Ltd.
Original Assignee
Suzhou Aitesi Environmental Protection Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Suzhou Aitesi Environmental Protection Material Co Ltd filed Critical Suzhou Aitesi Environmental Protection Material Co Ltd
Priority to CN201310216421.3A priority Critical patent/CN103289483B/zh
Publication of CN103289483A publication Critical patent/CN103289483A/zh
Application granted granted Critical
Publication of CN103289483B publication Critical patent/CN103289483B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种含有乙烯-三氟氯乙烯共聚物的防水耐酸碱涂料,由以下成分按照重量比组成:乙烯-三氟氯乙烯共聚物50~60份,聚偏氟乙烯30~40份,C9石油树脂20~30份,苯胺甲醛树脂10~20份,偏硅酸钙10~20份,石棉5~10份,铝粉5~10份,硫酸钙5~10份,硝基纤维素5~10份,丙酮50~70份。制成的含有乙烯-三氟氯乙烯共聚物的涂料具有良好的防水耐酸碱效果。

Description

一种含有乙烯-三氟氯乙烯共聚物的防水耐酸碱涂料
技术领域
本发明涉及一种防水耐酸碱涂料,特别是涉及一种含有乙烯-三氟氯乙烯共聚物的防水耐酸碱涂料。
背景技术
随着各行各业的快速发展,在这个过程中,涂料行业也得到了快速进步。同时人们对涂料的需求是越来越广泛,同时对涂料的质量要求也是越来越高。在涉及到防水并耐酸碱涂料的专业领域,如一些家居、装饰等领域,以及一些其他的特殊领域,对防水耐酸碱型涂料的要求也是随之增高,目前市场上同时具有防水和耐酸碱效果的涂料种类较少,因此开发一种同时具有良好的防水性和耐酸碱性的涂料有很大的市场需求。
发明内容
要解决的技术问题:常规涂料耐水耐酸碱效果较差的问题。
技术方案:本发明为一种含有乙烯-三氟氯乙烯共聚物的防水耐酸碱涂料,由以下成分按照重量比组成:乙烯-三氟氯乙烯共聚物50~60份,聚偏氟乙烯30~40份,C9石油树脂20~30份,苯胺甲醛树脂10~20份,偏硅酸钙10~20份,石棉5~10份,铝粉5~10份,硫酸钙5~10份,硝基纤维素5~10份,丙酮50~70份。通过将各种成分投入反应釜中不断进行搅拌,待搅拌均匀后即可获得具有良好防水耐酸碱效果的涂料。
有益效果:制备好含有乙烯-三氟氯乙烯共聚物的防水耐酸碱涂料后,对其防水性和耐酸碱性进行了实验,将涂料均匀喷涂在马口铁表面后,将试样放入水中进行防水试验,防水试验时长为50~60天,另取均匀喷涂好涂料的马口铁试样进行耐酸碱实验,碱液为2mol/L的氢氧化钠溶液,酸液为2mol/L的磷酸溶液,时间为20~30天。结果表明本发明制成的含有乙烯-三氟氯乙烯共聚物的涂料在50~60天内没有开裂起泡现象,具有良好的防水性,另外在2mol/L的氢氧化钠溶液和2mol/L的磷酸溶液下20~30天内也没有异常的起泡现象,具有良好的耐酸碱效果。
具体实施方式
实施例1
打开反应釜,取乙烯-三氟氯乙烯共聚物50kg,投入反应釜中,搅拌,同时加入聚偏氟乙烯30kg,不停搅拌,再加入C9石油树脂20kg,加入苯胺甲醛树脂10kg,再加入偏硅酸钙10kg,再依次加入石棉5kg,铝粉5kg,硫酸钙5kg,硝基纤维素5kg,最后加入丙酮50kg,待彻底搅拌均匀后可得含有乙烯-三氟氯乙烯共聚物的涂料。将涂料均匀喷涂在马口铁表面后,将试样放入水中进行防水试验,防水试验时长为50天,另取均匀喷涂好涂料的马口铁试样进行耐酸碱实验,碱液为2mol/L的氢氧化钠溶液,酸液为2mol/L的磷酸溶液,时间为20天。结果表明本发明制成的含有乙烯-三氟氯乙烯共聚物的涂料在50天内没有开裂起泡现象,具有良好的防水性,另外在2mol/L的氢氧化钠溶液和2mol/L的磷酸溶液中20天内也没有起泡或其他异常现象,具有良好的耐酸碱效果。
 实施例2
打开反应釜,取乙烯-三氟氯乙烯共聚物60kg,投入反应釜中,搅拌,同时加入聚偏氟乙烯40kg,不停搅拌,再加入C9石油树脂30kg,加入苯胺甲醛树脂20kg,再加入偏硅酸钙20kg,再依次加入石棉10kg,铝粉10kg,硫酸钙10kg,硝基纤维素10kg,最后加入丙酮70kg,待彻底搅拌均匀后可得含有乙烯-三氟氯乙烯共聚物的涂料。将涂料均匀喷涂在马口铁表面后,将试样放入水中进行防水试验,防水试验时长为60天,另取均匀喷涂好涂料的马口铁试样进行耐酸碱实验,碱液为2mol/L的氢氧化钠溶液,酸液为2mol/L的磷酸溶液,时间为30天。结果表明本发明制成的含有乙烯-三氟氯乙烯共聚物的涂料在60天内没有开裂起泡现象,具有良好的防水性,另外在2mol/L的氢氧化钠溶液和2mol/L的磷酸溶液中30天内也没有起泡或其他异常现象,具有良好的耐酸碱效果。
实施例3
打开反应釜,取乙烯-三氟氯乙烯共聚物55kg,投入反应釜中,搅拌,同时加入聚偏氟乙烯35kg,不停搅拌,再加入C9石油树脂25kg,加入苯胺甲醛树脂15kg,再加入偏硅酸钙15kg,再依次加入石棉7kg,铝粉8kg,硫酸钙8kg,硝基纤维素7kg,最后加入丙酮60kg,待彻底搅拌均匀后可得含有乙烯-三氟氯乙烯共聚物的涂料。将涂料均匀喷涂在马口铁表面后,将试样放入水中进行防水试验,防水试验时长为55天,另取均匀喷涂好涂料的马口铁试样进行耐酸碱实验,碱液为2mol/L的氢氧化钠溶液,酸液为2mol/L的磷酸溶液,时间为25天。结果表明本发明制成的含有乙烯-三氟氯乙烯共聚物的涂料在55天内没有开裂起泡现象,具有良好的防水性,另外在2mol/L的氢氧化钠溶液和2mol/L的磷酸溶液中25天内也没有起泡或其他异常现象,具有良好的耐酸碱效果。

Claims (1)

1.一种含有乙烯-三氟氯乙烯共聚物的防水耐酸碱涂料,其特征在于,所述的涂料的制备方法为:打开反应釜,取乙烯-三氟氯乙烯共聚物60Kg,投入反应釜中,搅拌,同时加入聚偏氟乙烯40Kg,不停搅拌,再加入C9石油树脂30Kg,加入苯胺甲醛树脂20Kg,再加入偏硅酸钙20Kg,再依次加入石棉10Kg,铝粉10Kg,硫酸钙10Kg,硝基纤维素10Kg,最后加入丙酮70Kg,待彻底搅拌均匀后可得含有乙烯-三氟氯乙烯共聚物的涂料。
CN201310216421.3A 2013-06-04 2013-06-04 一种含有乙烯-三氟氯乙烯共聚物的防水耐酸碱涂料 Active CN103289483B (zh)