CN103170448A - 一种木材面混色油漆工艺 - Google Patents

一种木材面混色油漆工艺 Download PDF

Info

Publication number
CN103170448A
CN103170448A CN2013100882229A CN201310088222A CN103170448A CN 103170448 A CN103170448 A CN 103170448A CN 2013100882229 A CN2013100882229 A CN 2013100882229A CN 201310088222 A CN201310088222 A CN 201310088222A CN 103170448 A CN103170448 A CN 103170448A
Authority
CN
China
Prior art keywords
oil
brush
paint
painting
putty
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013100882229A
Other languages
English (en)
Inventor
王程皓
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2013100882229A priority Critical patent/CN103170448A/zh
Publication of CN103170448A publication Critical patent/CN103170448A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种木材面混色油漆工艺,所述方法包括步骤如下:(1)清理木器表面。(2)刷底子油,A、操清油一遍,B、抹腻子,C、磨砂纸。(3)刷第一遍油漆:刷铅油——抹腻子——磨砂纸。(4)刷第二遍油漆:刷铅油——磨砂纸。(5)刷最后一遍油漆:涂刷时要多刷多理,要注意刷油饱满,刷油动作要敏捷,不流不坠、光亮均匀、色泽一致。通过本发明油漆颜色均匀,不存在流坠、发汗、发笑现象,增强附着力,不易脱落,保证油漆工艺质量,提高了木材的装饰效果和使用寿命。

Description

一种木材面混色油漆工艺
技术领域
本发明涉及一种油漆工艺,具体是一种木材面混色油漆工艺。
背景技术
目前传统木材的油漆工艺是通过喷涂、帖纸、转印、覆膜、网印等处理方法,机器设备投入成本高,而油漆颜色不均匀,图案单调,存在流坠、发汗、发笑,附着力不佳,易脱落等不足,质量难以保证,直接影响到木材的装饰效果和使用寿命。
发明内容
本发明所要解决的技术问题是提供一种操作简单,颜色均匀,不存在流坠、发汗、发笑,不易脱落的木材面混色油漆工艺。
本发明是通过以下技术方案来实现的:
本发明的一种木材面混色油漆工艺,所述方法包括步骤如下:
(1)清理木器表面:铲去脂囊将脂迹刮净,流松香的节疤挖掉,较大的脂囊应用木纹相同的材料用胶镶嵌;磨砂纸,先磨线角后磨四口平面,顺木纹打磨,有小活翘皮用小刀撕掉,有重皮的地方用小钉子钉牢固;点漆片,在木节疤和油迹处,用酒精漆片点刷。
(2)刷底子油:
A、操清油一遍:清油用汽油、光油配制,略加一些红土子(避免漏刷不好区分)。
B、抹腻子:腻子的重量配合比为石膏粉∶熟桐油∶松香∶水=16-20∶5-7∶1-3∶6-9。待操作的清油干透后将钉孔、裂缝、节疤以及边棱残缺处,用石膏油腻子刮平整,腻子要横抹竖起,将腻子刮入钉孔或裂纹内。
C、磨砂纸:打砂纸时应顺着木纹打磨。
(3)刷第一遍油漆:刷铅油——抹腻子——磨砂纸。
(4)刷第二遍油漆:刷铅油——磨砂纸。
(5)刷最后一遍油漆:涂刷时要多刷多理,要注意刷油饱满,刷油动作要敏捷,不流不坠、光亮均匀、色泽一致。
进一步地技术方案,所述腻子的重量优选配合比为石膏粉∶熟桐油∶松香∶水=16∶5∶1∶6。
进一步地技术方案,所述涂刷时的要求依照先上后下、先难后易、先左后右、先里后外的顺序和横刷竖顺的操作方法施工。
本发明的有益效果是:通过本发明油漆颜色均匀,不存在流坠、发汗、发笑现象,增强附着力,不易脱落,保证油漆工艺质量,提高了木材的装饰效果和使用寿命。
具体实施方式
本发明的一种木材面混色油漆工艺,所述方法包括步骤如下:
(1)清理木器表面:铲去脂囊将脂迹刮净,流松香的节疤挖掉,较大的脂囊应用木纹相同的材料用胶镶嵌;磨砂纸,先磨线角后磨四口平面,顺木纹打磨,有小活翘皮用小刀撕掉,有重皮的地方用小钉子钉牢固;点漆片,在木节疤和油迹处,用酒精漆片点刷。
(2)刷底子油:
A、操清油一遍:清油用汽油、光油配制,略加一些红土子(避免漏刷不好区分)。
B、抹腻子:腻子的重量配合比为石膏粉∶熟桐油∶松香∶水=16-20∶5-7∶1-3∶6-9。待操作的清油干透后将钉孔、裂缝、节疤以及边棱残缺处,用石膏油腻子刮平整,腻子要横抹竖起,将腻子刮入钉孔或裂纹内。
C、磨砂纸:打砂纸时应顺着木纹打磨。
(3)刷第一遍油漆:刷铅油——抹腻子——磨砂纸。
(4)刷第二遍油漆:刷铅油——磨砂纸。
(5)刷最后一遍油漆:涂刷时要多刷多理,要注意刷油饱满,刷油动作要敏捷,不流不坠、光亮均匀、色泽一致。
其中,所述腻子的重量优选配合比为石膏粉∶熟桐油∶松香∶水=16∶5∶1∶6。
所述涂刷时的要求依照先上后下、先难后易、先左后右、先里后外的顺序和横刷竖顺的操作方法施工。
本发明的有益效果是:通过本发明油漆颜色均匀,不存在流坠、发汗、发笑现象,增强附着力,不易脱落,保证油漆工艺质量,提高了木材的装饰效果和使用寿命。
以上所述,仅为本发明的具体实施方式,但本发明的保护范围并不局限于此,任何不经过创造性劳动想到的变化或替换,都应涵盖在本发明的保护范围之内。因此,本发明的保护范围应该以权利要求书所限定的保护范围为准。

Claims (3)

1.一种木材面混色油漆工艺,其特征在于,所述方法包括步骤如下:
(1)清理木器表面:铲去脂囊将脂迹刮净,流松香的节疤挖掉,较大的脂囊应用木纹相同的材料用胶镶嵌;磨砂纸,先磨线角后磨四口平面,顺木纹打磨,有小活翘皮用小刀撕掉,有重皮的地方用小钉子钉牢固;点漆片,在木节疤和油迹处,用酒精漆片点刷。
(2)刷底子油:
A、操清油一遍:清油用汽油、光油配制,略加一些红土子(避免漏刷不好区分)。
B、抹腻子:腻子的重量配合比为石膏粉∶熟桐油∶松香∶水=16-20∶5-7∶1-3∶6-9。待操作的清油干透后将钉孔、裂缝、节疤以及边棱残缺处,用石膏油腻子刮平整,腻子要横抹竖起,将腻子刮入钉孔或裂纹内。
C、磨砂纸:打砂纸时应顺着木纹打磨。
(3)刷第一遍油漆:刷铅油——抹腻子——磨砂纸。
(4)刷第二遍油漆:刷铅油——磨砂纸。
(5)刷最后一遍油漆:涂刷时要多刷多理,要注意刷油饱满,刷油动作要敏捷,不流不坠、光亮均匀、色泽一致。
2.根据权利要求1所述木材面混色油漆工艺,其特征在于:所述腻子的重量优选配合比为石膏粉∶熟桐油∶松香∶水=16∶5∶1∶6。
3.根据权利要求1所述木材面混色油漆工艺,其特征在于:所述涂刷时的要求依照先上后下、先难后易、先左后右、先里后外的顺序和横刷竖顺的操作方法施工。
CN2013100882229A 2013-03-07 2013-03-07 一种木材面混色油漆工艺 Pending CN103170448A (zh)