CN103085452A - 一种用于晶硅太阳能电池银浆印刷实验的网版 - Google Patents
一种用于晶硅太阳能电池银浆印刷实验的网版 Download PDFInfo
- Publication number
- CN103085452A CN103085452A CN2013100430062A CN201310043006A CN103085452A CN 103085452 A CN103085452 A CN 103085452A CN 2013100430062 A CN2013100430062 A CN 2013100430062A CN 201310043006 A CN201310043006 A CN 201310043006A CN 103085452 A CN103085452 A CN 103085452A
- Authority
- CN
- China
- Prior art keywords
- electrode district
- district
- electrode
- grid line
- secondary grid
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种用于晶硅太阳能电池银浆印刷实验的网版,包括网版本体(1),其特征在于所述的网版本体(1)上设有副栅线区(2)和电极区(3),副栅线区(2)由多组宽度不同的副栅线(4)组成且副栅线区(2)位于电极区(3)的一侧。本发明通过将多组试验图形集成到一张网版上,保证了实验条件的一致性和实验结果的精准度,同时降低了网版制作的成本;其中触角电极降低了实验的难度且测试电极保证了电导率测试的精确性,该网版具有结构简单、成本低且方便实用的特点,适宜推广使用。
Description
技术领域
本发明涉及晶硅太阳能电池正面银浆技术领域,具体地说是一种集成多种图形的用于晶硅太阳能电池银浆印刷实验的网版。
背景技术
晶硅太阳能电池正面银浆是应用于晶硅太阳能电池片生产的一种辅料,主要是用来收集电流和引出电极。为保证高效电池片的实现,必须确保浆料的打印效果以及浆料烧结后的导电效果,现有的实验网版都是将一种印刷图形设计在一张网版上,这样就增加了成本;同时,不同的网版由于实验条件会有差异(包括制版时网版与网版之间张力、膜厚等差异,以及印刷时印刷参数设置上的差异),导致实验结果在对比上不精确。另外,由于副栅线太细,导致在电导率的测试上难度较大,难以实现。
发明内容
本发明的目的是针对现有技术存在的问题,提供一种集成多种图形的用于晶硅太阳能电池银浆印刷实验的网版。
本发明的目的是通过以下技术方案解决的:
一种用于晶硅太阳能电池银浆印刷实验的网版,包括网版本体,其特征在于所述的网版本体上设有副栅线区和电极区,副栅线区由多组宽度不同的副栅线组成且副栅线区位于电极区的一侧。
所述的电极区包括触角电极区、不等距电极区和方形回路电极区,触角电极区由宽度不同的副栅线、副栅线两端的触角构成的多组触角电极组成;不等距电极区由多组测试电极组成;方形回路电极区由方形的副栅线构成的多组方形回路电极组成。
所述不等距电极区内的测试电极的宽度大于触角电极区内的副栅线的宽度。
所述的副栅线区位于电极区的左侧或右侧。
所述的触角电极区和不等距电极区位于方形回路电极区的上侧或下侧且触角电极区位于不等距电极区的左侧或右侧。
所述的副栅线区位于电极区的上侧或下侧。
所述的触角电极区和不等距电极区位于方形回路电极区的两侧。
所述的触角电极区和方形回路电极区位于不等距电极区的两侧。
所述的不等距电极区和方形回路电极区位于触角电极区的两侧。
所述的网版本体采用不锈钢轧压网布制成。
本发明相比现有技术有如下优点:
本发明通过将多组试验图形集成到一张网版上,保证了实验条件的一致性和实验结果的精准度,同时降低了网版制作的成本。
本发明的触角电极降低了实验的难度且测试电极保证了电导率测试的精确性,该网版具有结构简单、成本低且方便实用的特点,适宜推广使用。
附图说明
附图1为本发明的结构示意图。
其中:1—网版本体;2—副栅线区;3—电极区;4—副栅线;5—触角电极区;6—不等距电极区;7—方形回路电极区;8—触角;9—触角电极;10—测试电极;11—方形回路电极。
具体实施方式
下面结合附图与实施例对本发明作进一步的说明。
如图1所示:一种用于晶硅太阳能电池银浆印刷实验的网版,包括采用不锈钢轧压网布制成的网版本体1,在网版本体1上设有副栅线区2和电极区3,副栅线区2由多组宽度不同的副栅线4组成且副栅线区2位于电极区3的一侧,电极区3包括触角电极区5、不等距电极区6和方形回路电极区7,当副栅线区2位于电极区3的左侧或右侧时,触角电极区5和不等距电极区6位于方形回路电极区7的上侧或下侧且触角电极区5位于不等距电极区7的左侧或右侧;当副栅线区2位于电极区3的上侧或下侧时,触角电极区5和不等距电极区6位于方形回路电极区7的两侧或者触角电极区5和方形回路电极区7位于不等距电极区6的两侧或者不等距电极区6和方形回路电极区7位于触角电极区5的两侧。触角电极区5由宽度不同的副栅线4、副栅线4两端的触角8构成的多组触角电极9组成,不等距电极区6由多组测试电极10组成,方形回路电极区7由方形的副栅线4构成的多组方形回路电极11组成;不等距电极区6内的测试电极10的宽度大于触角电极区5内的副栅线4的宽度。
图1为本发明的一个实施例,其中在网版本体1上设有副栅线区2和电极区3,副栅线区2由多组宽度不同的副栅线4组成且副栅线区2位于电极区3的左侧,电极区3包括触角电极区5、不等距电极区6和方形回路电极区7,其中触角电极区5和不等距电极区6位于方形回路电极区7的上侧且触角电极区5位于不等距电极区7的左侧;触角电极区5由宽度不同的副栅线、副栅线两端的触角8构成的多组触角电极9组成,不等距电极区6由多组测试电极10组成,方形回路电极区7由方形的副栅线4构成的多组方形回路电极11组成;上述不等距电极区6内的测试电极10的宽度大于触角电极区5内的副栅线4的宽度。该网版在晶硅太阳能电池正面银浆研发过程中,用于检验浆料的打印效果以及导电效果。其中副栅线区2内的副栅线4用于检验浆料的打印效果,确认是否有虚印、断栅、粗点、断线,并通过显微镜测试打印后栅线的高宽比;触角电极区5内的触角电极9和不等距电极区6内的测试电极10用于测试浆料打印烧结后的电导率,以确认烧结后浆料的导电效果;方形回路电极区7内的方形回路电极11用于确认浆料在直角拐角处的打印效果。
本发明通过将多组试验图形集成到一张网版上,保证了实验条件的一致性和实验结果的精准度,同时降低了网版制作的成本;其中触角电极9降低了实验的难度且测试电极10保证了电导率测试的精确性,该网版具有结构简单、成本低且方便实用的特点,适宜推广使用。
以上实施例仅为说明本发明的技术思想,不能以此限定本发明的保护范围,凡是按照本发明提出的技术思想,在技术方案基础上所做的任何改动,均落入本发明保护范围之内;本发明未涉及的技术均可通过现有技术加以实现。
Claims (10)
1.一种用于晶硅太阳能电池银浆印刷实验的网版,包括网版本体(1),其特征在于所述的网版本体(1)上设有副栅线区(2)和电极区(3),副栅线区(2)由多组宽度不同的副栅线(4)组成且副栅线区(2)位于电极区(3)的一侧。
2.根据权利要求1所述的用于晶硅太阳能电池银浆印刷实验的网版,其特征在于所述的电极区(3)包括触角电极区(5)、不等距电极区(6)和方形回路电极区(7),触角电极区(5)由宽度不同的副栅线(4)、副栅线(4)两端的触角(8)构成的多组触角电极(9)组成;不等距电极区(6)由多组测试电极(10)组成;方形回路电极区(7)由方形的副栅线(4)构成的多组方形回路电极(11)组成。
3.根据权利要求2所述的用于晶硅太阳能电池银浆印刷实验的网版,其特征在于所述不等距电极区(6)内的测试电极(10)的宽度大于触角电极区(5)内的副栅线(4)的宽度。
4.根据权利要求2所述的用于晶硅太阳能电池银浆印刷实验的网版,其特征在于所述的副栅线区(2)位于电极区(3)的左侧或右侧。
5.根据权利要求4所述的用于晶硅太阳能电池银浆印刷实验的网版,其特征在于所述的触角电极区(5)和不等距电极区(6)位于方形回路电极区(7)的上侧或下侧且触角电极区(5)位于不等距电极区(7)的左侧或右侧。
6.根据权利要求2所述的用于晶硅太阳能电池银浆印刷实验的网版,其特征在于所述的副栅线区(2)位于电极区(3)的上侧或下侧。
7.根据权利要求6所述的用于晶硅太阳能电池银浆印刷实验的网版,其特征在于所述的触角电极区(5)和不等距电极区(6)位于方形回路电极区(7)的两侧。
8.根据权利要求6所述的用于晶硅太阳能电池银浆印刷实验的网版,其特征在于所述的触角电极区(5)和方形回路电极区(7)位于不等距电极区(6)的两侧。
9.根据权利要求6所述的用于晶硅太阳能电池银浆印刷实验的网版,其特征在于所述的不等距电极区(6)和方形回路电极区(7)位于触角电极区(5)的两侧。
10.根据权利要求1所述的用于晶硅太阳能电池银浆印刷实验的网版,其特征在于所述的网版本体(1)采用不锈钢轧压网布制成。