CN103073249B - 一种彩色砂浆 - Google Patents

一种彩色砂浆 Download PDF

Info

Publication number
CN103073249B
CN103073249B CN201310052040.6A CN201310052040A CN103073249B CN 103073249 B CN103073249 B CN 103073249B CN 201310052040 A CN201310052040 A CN 201310052040A CN 103073249 B CN103073249 B CN 103073249B
Authority
CN
China
Prior art keywords
parts
water
mortar
organic polymer
frostproofer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310052040.6A
Other languages
English (en)
Other versions
CN103073249A (zh
Inventor
王兴文
孙忠
刘天汉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu blue circle new material Limited by Share Ltd
Original Assignee
JIANGSU LANQUAN NEW MATERIAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU LANQUAN NEW MATERIAL CO Ltd filed Critical JIANGSU LANQUAN NEW MATERIAL CO Ltd
Priority to CN201310052040.6A priority Critical patent/CN103073249B/zh
Publication of CN103073249A publication Critical patent/CN103073249A/zh
Application granted granted Critical
Publication of CN103073249B publication Critical patent/CN103073249B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种彩色砂浆,包括以下按重量配比的组分:水泥6-13份,粉煤灰1-2份,黄砂32-50份,砂浆稠化粉1-2份,无机颜料0.3-2.5份,防冻剂0.1-0.6份;防冻剂包括以下按重量配比的组分:减水剂5-10份,有机高分子材料50-65份,三萜皂苷0.05-0.1份。本发明制备的彩色砂浆能够应用于-20~-30℃的极低负温条件下的外墙面施工。

Description

一种彩色砂浆
技术领域
    本发明涉及一种彩色砂浆,具体涉及一种适用于较低负温区间的彩色砂浆。
背景技术
干粉砂浆是指干燥筛分处理的骨料、无机胶凝材料和添加剂等按一定比例进行物理混合而成的一种颗粒状或粉状,以袋装或散装的形式运至工地,加水拌和后即可直接使用的物料。干粉砂浆在建筑业中以薄层发挥粘结、衬垫和防护等作用,应用极为广泛。采用彩色砂浆进行外墙装饰时,由于与墙体结合力不高,且在冬季,容易出现冻裂脱落。尤其是在我国的“三北”地区,冬季持续时间长,工程建设期缩短,当气温低于0℃时,负温下砂浆拌合水的冻结不但会使其中水泥的水化停滞,同时水结冰产生的体积膨胀会导致水泥水化产物结构形成损伤。
发明内容
本发明的目的是为了解决现有技术中存在的缺陷,提供一种掺量少,且最低应用负温低的彩色砂浆。
为了达到上述目的,本发明提供了一种彩色砂浆,包括以下按重量配比的组分:水泥6-13份,粉煤灰1-2份,黄砂32-50份,砂浆稠化粉1-2份,无机颜料0.3-2.5份,防冻剂0.1-0.6份;防冻剂包括以下按重量配比的组分:减水剂5-10份,有机高分子材料 50-65份,三萜皂苷 0.05-0.1份。
其中,减水剂采用聚羧酸高性能减水剂,优选烯丙基聚氧乙烯醚-丙烯酸高分子聚合物。
有机高分子材料采用有机物与分子量大于3000的水溶性高分子材料复合而成,两者的摩尔比为1:250。
无机颜料为氧化铁系列无机颜料。
本发明相比现有技术具有以下优点:采用三萜皂苷作为引气剂,能形成大量微细气泡,改善冻胀应力。利用有机高分子材料作为防冻组分,在较低的含量下就能使溶液达到饱和而使溶液的冰点降低,能大大降低掺量,且无需载体;同时不含钠盐,有助于防止碱骨料反应,提高砂浆的耐久性和使用寿命。利用减水剂聚合物以及有极高分子材料的共同作用,有效避免了砂浆色彩的脱落和褪色。本发明制备的彩色砂浆能够应用于 -20~-30℃的极低负温条件下的外墙面施工。
具体实施方式
    下面结合具体实施例对本发明彩色砂浆进行详细说明。
实施例一
取42.5普通硅酸盐水泥6重量份、Ⅱ级粉煤灰1重量份、天然黄砂(含泥量为0.9%,细度模数为2.3,表观密度为2640kg/m3)32重量份、砂浆稠化粉(常州弘正建材有限公司所售的HZ-P高效保水稠化粉)1重量份、氧化铁红0.3重量份和防冻剂0.1重量份。
防冻剂的制备:取聚羧酸高性能减水剂(烯丙基聚氧乙烯醚-丙烯酸高分子聚合物)5重量份、有机高分子材料50重量份、三萜皂苷0.05重量份混合,搅拌均匀即可。
制备的彩色砂浆施工时,加入20%的水搅拌均匀。在-30℃的负温条件下喷涂或滚涂在外墙面,与墙体具有良好的结合力(>0.65Mpa),不易开裂,憎水性好(240min的吸水量均小于2.0g),与传统的涂料饰面层比较,其防水透气性能更佳。
实施例二
取42.5普通硅酸盐水泥13重量份、Ⅱ级粉煤灰2重量份、天然黄砂(含泥量为0.9%,细度模数为2.3,表观密度为2640kg/m3)50重量份、砂浆稠化粉(常州弘正建材有限公司所售的HZ-P高效保水稠化粉)2重量份、氧化铁蓝2.5重量份和防冻剂0.6重量份。
防冻剂的制备:取聚羧酸高性能减水剂10重量份、有机高分子材料65重量份、三萜皂苷0.1重量份混合,搅拌均匀即可。
制备的彩色砂浆施工时,加入20%的水搅拌均匀。在-30℃的负温条件下喷涂或滚涂在外墙面,与墙体具有良好的结合力(>0.65Mpa),不易开裂,憎水性好(240min的吸水量均小于2.0g),与传统的涂料饰面层比较,其防水透气性能更佳。

Claims (3)

1.一种彩色砂浆,其特征在于,包括以下按重量配比的组分:水泥6份,粉煤灰1份,黄砂32份,砂浆稠化粉1份,无机颜料0.3份,防冻剂0.1份;所述防冻剂包括以下按重量配比的组分:减水剂5份,有机高分子材料 50份,三萜皂苷 0.05份;所述减水剂为聚羧酸高性能减水剂;所述有机高分子材料采用有机物与分子量大于3000的水溶性高分子材料复合而成;所述有机物与水溶性高分子材料的摩尔比为1:250。
2. 一种彩色砂浆,其特征在于,包括以下按重量配比的组分:水泥13份,粉煤灰2份,黄砂50份,砂浆稠化粉2份,无机颜料2.5份,防冻剂0.6份;所述防冻剂包括以下按重量配比的组分:减水剂10份,有机高分子材料 65份,三萜皂苷 0.1份;所述减水剂为聚羧酸高性能减水剂;所述有机高分子材料采用有机物与分子量大于3000的水溶性高分子材料复合而成;所述有机物与水溶性高分子材料的摩尔比为1:250。
3.根据权利要求1或2所述的彩色砂浆,其特征在于:所述无机颜料为氧化铁系列无机颜料。
CN201310052040.6A 2013-02-18 2013-02-18 一种彩色砂浆 Active CN103073249B (zh)